Claims
- 1. A process of fabricating a hermetically sealed tube for encasing optical fibers comprising:
- (a) rolling at least two annealed wires into sections, said sections capable of fitting together to form a cylindrical tube having an inner diameter sufficient to accept at least one or a plurality of buffered optical fibers;
- (b) forming a tube around said buffered optical fibers from the sections of step (a); and
- (c) joining hermetically said sections into a tube.
- 2. A process according to claim 1 wherein the joining is performed by laser welding.
- 3. A process according to claim 2 wherein the annealed wires are selected from stainless steel or high tensile nonferrous alloys.
- 4. A process according to claim 1 wherein said sections undergo precipitation hardening prior to welding to increase the yield strength of the finished sections.
- 5. The process according to claim 4 further comprising injecting an elastomer into a section and onto said buffered optical fibers prior to forming said tube.
- 6. The process according to claim 5 wherein the joining of said sections forms a tube which exhibits a yield stress greater than about 100,000 psi.
- 7. The process according to claim 6 further comprising forming a high temperature resistant plastic coating around said hermetically sealed tube.
- 8. The process according to claim 7 wherein the joining of said sections forms a tube which exhibits a yield stress greater than about 150,000 psi.
- 9. The process according to claim 8 wherein said sections have a yield strain greater than about 0.85.
- 10. The process according to claim 9 further comprising heating said sections to between about 300.degree. F. to about 500.degree. F. during the joining thereof by laser welding.
- 11. The process according to claim 1 further comprising injecting an elastomer into a section and onto said buffered optical fibers prior to forming said tube.
- 12. The process according to claim 11 wherein the joining of said sections forms a tube which exhibits a yield stress greater than about 100,000 psi.
- 13. The process according to claim 12 further comprising forming a high temperature resistant plastic coating around said hermetically sealed tube.
- 14. The process according to claim 13 wherein the joining of said sections forms a tube which exhibits a yield stress greater than about 150,000 psi.
- 15. The process according to claim 14 wherein said sections have a yield strain greater than about 0.85.
Parent Case Info
This is a division of application Ser. No. 408,971, filed Aug. 17, 1982, now U.S. Pat. No. 4,504,112.
US Referenced Citations (4)
Foreign Referenced Citations (3)
Number |
Date |
Country |
2920428 |
Nov 1980 |
DEX |
1073958 |
Jun 1967 |
GBX |
2029048 |
Mar 1980 |
GBX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
408971 |
Aug 1982 |
|