The present invention is directed to an article of manufacture and method for producing photovoltaic energy. More particularly, the invention is related to an article of manufacture based on a nanoporous substrate of high surface area and further having a thin, well controlled conducting and also semi-conducting oxide layers deposited by atomic layer deposition enabling creation of a highly efficient solar cell and photon conversion medium. Further, the coated nanoporous component is arranged in a photovoltaic device structure so as to drastically reduce the photoelectron diffusion path and diffusion time to a transparent conducting oxide electrode which greatly improves collection efficiency.
Since the mid 1980's it has been clear that dyes (and later other sensitizers such as quantum dots) attached to semiconductor surfaces such as TiO2 efficiently inject charge into the semiconductor conduction band when photoexcited. Since that development, it has been widely recognized that with such heterojunctions, appropriately arranged with a conducting electrode and counter electrode, might enable construction of efficient solar cells. These architectures were termed sensitized solar cells (SSC hereinafter).
The electronic band structure of such an SSC cell is depicted in
While the solar cell described in
Researchers have subsequently attempted to increase the heterojunction absorbance by simply increasing the loading of the sensitizer molecule. This approach was however quickly abandoned when it was realized that although the absorbance increased in such cells, the efficiency per photon dropped precipitously. Ultimately it was demonstrated that only the first monolayer of dye would efficiently inject electrons into the TiO2, all other layers simply lost excitation by generating heat.
The first successful cells based on these heterojunction ideas came from Michael Gratzel's laboratory in Switzerland. Here the absorbance was increased by using a compressed nanoparticle array of TiO2 particles coated with a sensitizer dye as depicted in
When this architecture was first announced, Gratzel produced cells of ˜10% efficiency and created a sensation. The subsequent flurry of studies has in many ways justified the excitement. Degradation studies for instance have demonstrated that Gratzel photocells have a mean operating life measured in decades. Cost studies have demonstrated that Gratzel photocells are significantly cheaper, made of more abundant material, and are easier to produce than Si based photovoltaics. Thus, if the efficiency of such cells could be raised to about 15%, it is likely that they would totally replace Si cells. This promise has lead to the establishment of a number of companies focused on producing panels of Gratzel photocells and generating many significant public demonstrations (see for instance website http://www.dyesol.com).
Unfortunately, Gratzel photocell efficiencies have increased only marginally (10%->11.2%) in the past decade despite theoretically possible efficiencies approaching 30%. However, the reason for this lack of progress is now clear. Injected photoelectrons have a long and slow path to travel in the TiO2 nanoparticle array in order to find the TCO electrode. During this traverse, which may require seconds, there are many opportunities for losses which in fact do occur at the electrolyte TiO2 interface (see
The article of manufacture of a heterojunction photovoltaic cell is constructed to overcome the above-described prior art deficiencies by first creating a photoabsorption area which enables a large number (such as 103 or more) opportunities for photoabsorption by a dye monolayer. Further, the heterojunction is arranged such that the photoelectron carrier path length for collection is shortened by a factor of about 103 and the diffusion time reduced by about 106. The thin film conductor and semiconductor architecture forming the foundation for the cell employs a nanoporous substrate, such as anodic aluminum oxide (hereinafter “AAO”) or aerogels. Atomic layer deposition (hereinafter “ALD”) can then be used to form highly uniform, thin layers of conducting and semiconducting oxides on the large surface area of the AAO substrate (or otherwise high surface area substrate). In a preferred form of the invention the architecture comprises an array of hollow wires with the wire cross section made up of an array of concentric hollow cylinders. A base TCO electrode comprised of F:SnO2 (tin oxide doped with fluorine) was formed by spray pyrolysis which closes the porous AAO network on a bottom surface. The preferred method of preparation includes using ALD to deposit a nanolaminant of a film of about 10 nanometers of Sb:SnO2 (tin oxide doped with antimony), a transparent conducting oxide disposed under about 10 nm of TiO2 along the entire AAO pore structure and an exposed layer of F:SnO2. These nanowires are then coated with a photoabsorbent dye disposed inside the wire. This architecture further includes a redox shuttle, such as a solution of 3I−/I3− and a platinum anode. Further improvements in performance can be gained by using ALD to apply additional layers such as insulating Al2O3 layers to prevent the recombination of electrons in the TiO2 with holes in the electrolyte as will be described below.
These features and other aspects of the invention will be described in more detail hereinafter with reference to the figures described below.
A thin film semiconducting oxide architecture 10 of a heterojunction photovoltaic cell constructed in accordance with the invention is illustrated in
Disks of the AAO substrate 20 have been prepared with a thickness of 60 μm with hexagonal arrays of vertically aligned, 100 nm (+−3 nm) pores and with a cell density exceeding 1×1010 cm−2. Thus, initially at least the AAO substrate 20 has a surface area in excess of about 1500 times that of a flat film, equivalent to the roughness factor achieved in the best nanoparticle based SSCs. The AAO substrate 20 is transparent over a wide wavelength range, adding no adsorptive losses to the solar cell of the architecture 10. In our first experiments, the AAO substrate 20 was coated on its bottom surface with a thick TCO electrode 30, such as for example, F:SnO2. This was done by spray pyrolosis, closing the pore network at this end and forming the TCO electrode 30. Then, the ALD method was used to uniformly and completely deposit a nanolaminate film, such as for example, a 6 nm film of Sb:SnO2 (also a TCO) 40 under a 10 nm TiO2 film 50 along the entire AAO pore structure and the exposed F:SnO2 of the TCO electrode 30. Additional examples of TCO electrode 30 include but are not limited to aluminum-doped zinc oxide, indium doped with tin, zinc, or combinations of tin and zinc, and antimony-doped tin oxide. These resulting nanowires 60 were then coated with a sensitizer dye 70, such as a N719 dye, on the inside of the wire 60 by conventional impregnation. The resulting complete architecture 10 is illustrated in detail in
In addition to the preferred embodiment described hereinbefore, there are many parameters that can be varied in the architecture 10 proposed herein. Those include, without limitation, the length, thickness, morphology, and composition of each component layer, interfaces between layers can be extraordinarily abrupt or graded, and the final surface produced has a dense array of attachment moieties providing for interesting opportunities in dye quantum dot coupling to the framework.
ALD can coat many nanocrystalline frameworks in addition to coating of aerogels described hereinbefore. Because the filaments which make up the preferred aerogel substrate 20 expand with each new atomic layer, the surface area of the material increases; and this allows the synthesis method to intrinsically determine the best surface area to use. Further coating of aerogel substrate 20 makes initially delicate substrates able to withstand capillary forces. Because of their extremely large surface area, the aerogel substrate 20 represent a highly preferred substrate for the SSC type of solar cells for manufacture. In all other respects the same arguments for AAO apply here. One extension of this concept would be to place the aerogel substrate 20 inside a more robust macro-porous material, such as microchannel plates.
The capability of inserting thin and ultra-thin TiO2 and TCO layers enables new approaches to the design and study of SSCs generally. In the existing SSCs, photogenerated electrons travel in an ambipolar diffusion process through the nanoporous TiO2 layer requiring times of millisecond up to seconds. During this time period the photoelectron is susceptible to loss via various recombination mechanisms imposing very stringent requirements on the cell design. In particular, the 3I−/I3− redox shuttle 80 is indispensable due to its slow electron re-capture rate. However, the 3I−/I3− redox shuttle 80 has a roughly 0.6 V potential mismatch with respect to the most commonly used sensitizer dyes, incurring the single largest loss mechanism in present cells (see
This new synthesis method also allows the redox shuttle 80 itself to be removed (see
The new synthesis method also enables the synthesis of structures with ultrathin semiconducting oxide layers. This can be extremely important since such layers would allow hot electrons to transport through them into the TCO layer 30 without the loss of their original energy. The capture of hot electrons holds the promise of increasing the efficiency of solar cells beyond the Queisser-Shockley limit. Under ideal conditions, hot electron capture resembles an infinite stack of single threshold junctions that is matched to the solar spectrum, thus approaching an efficiency of 65%. Hot electrons arise when upon absorption of a photon the energy of the sensitizer is higher than its relaxed excited state (see
In regard to the improved method of manufacture, this synthesis method allows in the hot electron context careful control of barrier widths (in the single monolayer range) and careful control of barrier heights. This control extends beyond controlling the materials to include the ability to deposit intimately mixed compound oxides. Such oxides have intermediate band heights. A further variation on this idea is to use ALD's ability to use chemistry to deposit polycrystalline materials at very low temperatures, thus being able to adjust band edges by crystal type (for example, anatase vs rutile TiO2).
In yet another embodiment of the invention, one can address the problem of the long time exposure of electrons to loss as transport occurs in the TiO2 framework. While the ALD method is conventionally thought to coat everywhere, for greasy molecules such as the dyes used on the surface of SSCs, we have determined that ALD can coat around the sensitizer dye molecules. If for instance we coat with alumina, then the sensitizer dye 70 is still exposed to the redox shuttle 80 and attached to the TiO2 surface 50. In principle then its operation as a sensitizer dye is unaffected. However, the rest of the TiO2 surface will be insulated from the electrolyte, dramatically decreasing the loss of electrons. We have demonstrated this technique as shown in
The foregoing description of embodiments of the present invention have been presented for purposes of illustration and description. It is not intended to be exhaustive or to limit the present invention to the precise form disclosed, and modifications and variations are possible in light of the above teachings or may be acquired from practice of the present invention. The embodiments were chosen and described in order to explain the principles of the present invention and its practical application to enable one skilled in the art to utilize the present invention in various embodiments, and with various modifications, as are suited to the particular use contemplated.
The United States Government has rights in this invention pursuant to Contract No. W-31-109-ENG-38 between the United States Government and The University of Chicago and/or pursuant to Contract No. DE-AC02-06CH11357 between the United States Government and UChicago Argonne, LLC representing Argonne National Laboratory.
Number | Name | Date | Kind |
---|---|---|---|
6649824 | Den et al. | Nov 2003 | B1 |
20050009224 | Yang et al. | Jan 2005 | A1 |
20050098205 | Roscheisen et al. | May 2005 | A1 |
20080072961 | Liang et al. | Mar 2008 | A1 |
Number | Date | Country | |
---|---|---|---|
20090000660 A1 | Jan 2009 | US |