Claims
- 1. A method for providing a thermoformable composite film with reduced line draw comprising:
- (a) extruding a first polymeric film;
- (b) orienting the first film to substantially the same extent in both the longitudinal and transverse directions;
- (c) extruding a second polymeric film comprising an oxygen barrier layer sufficient to protect packaged food products; and
- (d) bonding the second film to the first film over most of a major surface after effecting biaxial orientation of said first film.
- 2. A method according to claim 1 wherein the first film is oriented up to a maximum of about 3.5:1 in both the longitudinal and transverse directions.
- 3. A method according to claim 1 wherein the second layer is bonded to the first layer by corona bonding.
- 4. A method according to claim 1 wherein the first film, prior to the bonding step, is irradiated.
- 5. A method according to claim 4 wherein the first film is irradiated to from about 4 to about 9 megarads of irradiation.
Parent Case Info
This is a divisional application of application Ser. No. 842,530, filed March 21, 1986.
US Referenced Citations (9)
Foreign Referenced Citations (6)
Number |
Date |
Country |
132565 |
Feb 1985 |
EPX |
147078 |
Jul 1985 |
EPX |
1381883 |
Nov 1964 |
FRX |
5059 |
Feb 1971 |
JPX |
124648 |
Jul 1983 |
JPX |
1416625 |
Dec 1975 |
GBX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
842530 |
Mar 1986 |
|