Claims
- 1. A method for producing low-density, high-porosity, high surface area alumina from an aqueous alumina slurry produced by the water hydrolysis of aluminum alkoxides and containing up to about 32 weight percent Al.sub.2 O.sub.3, said method comprising:
- a. mixing said aqueous alumina slurry with an organic solvent selected from the group consisting of ethanol, propanol, isopropanol, butanol, isobutanol and tertiary butanol to form a solvent-aqueous alumina mixture containing said solvent in an amount equal to from about 25 to about 250 percent of the amount of solvent required to azeotropically remove the water from said aqueous alumina slurry upon drying said mixture,
- b. drying said solvent-aqueous alumina mixture; and,
- c. recovering alumina having a pore volume (0-10000 A) from about 1.0 to about 2.75 cc/g, a loose bulk density from about 7.5 to about 25 lb/ft.sup.3 and a surface area from about 260 to about 400 m.sup.2 /g.
- 2. The method of claim 1 wherein said aqueous alumina slurry contains from about 5 to about 25 weight percent Al.sub.2 O.sub.3 and is contacted with said organic solvent in an amount at least sufficient to form an azeotropic mixture with the water present.
- 3. The method of claim 2 wherein said aqueous alumina slurry contains from about 10 to about 20 weight percent Al.sub.2 O.sub.3.
- 4. The method of claim 1 wherein said alumina has a loose bulk density from about 9 to about 15 lb/ft.sup.3, a pore volume from about 1.5 to about 2.75 cc/g and a surface area from about 300 to about 400 m.sup.2 /g.
- 5. In a method for producing alpha alumina monohydrate by the water hydrolysis of aluminum alkoxides containing from about 1 to about 30 carbon atoms, said method consisting of
- a. reacting said aluminum alkoxides with an aqueous solution to produce an aqueous alumina slurry and an organic portion;
- b. separating said organic portion and said aqueous alumina slurry; and
- c. drying said aqueous alumina slurry, the improvement comprising; mixing an organic solvent selected from the group consisting of ethanol, propanol, isopropanol, butanol, isobutanol, and tertiary butanol with said aqueous alumina slurry to form a solvent-aqueous alumina mixture containing said solvent in an amount equal to from about 25 to about 250 percent of the amount of said solvent required to azeotropically remove the water from said aqueous alumina slurry prior to drying.
- 6. The improvement of claim 5 wherein said solvent is present in an amount equal to from about 25 to about 250 percent of the amount of solvent required to remove the water present in said aqueous alumina slurry.
BACKGROUND OF THE INVENTION
This application is a continuation-in-part of my earlier filed application entitled "High-Porosity, High-Surface Area, Low-Bulk Density Alumina," Ser. No. 246,028, filed Apr. 20, 1972, and Ser. No. 191,085 of the same title, filed Oct. 20, 1971, both now abandoned.
US Referenced Citations (5)
Foreign Referenced Citations (1)
Number |
Date |
Country |
1,903,066 |
Sep 1970 |
DT |
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
246028 |
Apr 1972 |
|