The present invention relates to an end fitting for a flexible tubular pipe the resistance of which to being torn out of the pipe is enhanced.
Flexible tubular pipes, and particularly those for transporting hydrocarbons in a marine environment, comprise, from inside to outside, on the one hand an internal structure consisting of several concentric layers designed to provide in particular the seal and the resistance to radial forces, and on the other hand at least one sheet of tensile armor layers wound with a long pitch making it possible to absorb the tensile forces which are applied to the pipe itself. In the present application, “wound with a long pitch” means any helical winding at a helix angle of less than 60°. Typically, the helix angle of the tensile armor layer sheets is between 25° and 55°.
Such flexible pipes are described in standard documents API 17J and API RP 17B published by the American Petroleum Institute.
Underwater flexible tubular pipes installed at a great depth, in practice at more than 1000 meters, must withstand very considerable stresses. This is particularly the case for riser pipes connecting the sea bed to a production unit situated on the surface, for example to a floating structure. Specifically, because of the great length of the riser, the stress applied to the upper portion by the weight of the pipe may reach several hundreds of tons. That is why the sheets of tensile armor layers of such pipes are usually made of steel with high mechanical characteristics. This makes it possible to increase the tensile resistance of the pipe while limiting its weight.
The steel wires used to manufacture such sheets of tensile armor layers are usually obtained by cold drawing and/or by cold rolling. Specifically, plastic deformation carried out at low temperature during these operations makes it possible not only to precisely form the wire to the desired geometry, but also to greatly increase its tensile yield strength and its ultimate tensile strength. These methods make it possible to manufacture at an advantageous cost carbon steel wires that have an ultimate tensile strength of more than 1400 MPa. These wires however have the disadvantage of not being very ductile and sensitive to temperature which causes difficulties that will be explained below.
Such wires are used for the manufacture of tensile armor layer sheets for the flexible tubular pipes that have to be installed at great depth.
An end fitting is connected to each end of each flexible tubular pipe. Naturally, the tensile forces that are applied to the pipe are also transferred to the end fitting. In the aforementioned case of the upper end fitting of a flexible riser, the tension transmitted to the fitting may reach a very high level. The device for connecting the tensile armor layer sheets to the end fitting must therefore have great resistance to being torn out. In addition, because of the swell, the floating structure to which the flexible riser is connected may oscillate vertically, which has the effect of varying the tension transmitted by the upper end fitting and therefore of generating a fatigue phenomenon. Such a dynamic loading may lead, in certain extreme circumstances, to the pipe being torn out of the end fitting.
To alleviate this, the tensile armor layers must be solidly anchored into the end fitting. For this, the end fitting usually comprises a sleeve which has a portion for connection to the pipe and at the opposite end, a portion for attachment to the floating structure, the connection portion having a portion for housing the free ends of armor layer. Those skilled in the art call this sleeve the end vault. The connection portion and the pipe to which it is connected are fitted into a ring which covers the housing portion and thereby the ends of the armor layers, forming a sealed annular chamber. Those skilled in the art call this ring the end cap. This sealed annular chamber is then covered with a curable polymer which traps the free ends of the armor layers. This solution is simple to apply, but has the disadvantage of requiring a sealed annular chamber of large dimensions, which increases the size and the cost of the end fitting. Specifically, in this solution, the anchoring mechanism relies only on the one hand on the adhesion between the wires and the cured polymer, and on the other hand on the capstan effect associated with the fact that the wires do not extend in a straight line inside the cured polymer.
Therefore, in order to reduce the size of the end fitting while improving its resistance to being torn out, solutions have been thought up that comprise additional immobilization means. These additional means consist in locally deforming the ends of the armor layer wires and in trapping these deformed zones in the cured polymer of the sealed annular chamber.
Thus, document U.S. Pat. No. 6,412,825 discloses a solution in which these local deformations spiral or twist. Document U.S. Pat. No. 6,161,880 discloses another solution in which these local deformations have the shape of a wave. Also known is a third solution, disclosed notably in
These known solutions however have the disadvantage of being difficult to apply in the case of armor layer wires having high mechanical characteristics. Specifically, such wires have the disadvantage of being not very ductile, so much so that it is difficult to manufacture, at ambient temperature, the local deformations in the twist, wave or hook shape. In addition, the wire may crack at these zones that are greatly deformed when cold, which may have the effect of reducing the tear-out resistance of the end fitting, in particular in the case of fatigue stresses. To prevent this cracking problem, it is possible to locally heat the wires before deforming them. However, this solution has the disadvantage of considerably reducing the mechanical characteristics of the wires and therefore of affecting the tear-out strength of the end fitting. Consequently, irrespective of the solution adopted to create the local deformations, namely cold deformation or hot deformation, there is a considerable decline in the case of wires having high mechanical characteristics, which requires the use of an annular chamber of large dimensions, and therefore significantly increases the size and cost of the end fittings designed for deep sea applications.
Document EP 1 206 659 discloses another solution designed mainly for flexible pipes having tensile armor layers made of composite materials, but also being able to be applied to steel armor layers. For this, axial immobilization holes are made in a portion forming a collar secured to the connection portion and the armor layers threaded into these immobilization holes are fitted with widener elements to locally widen the cross section of the armor layers and thereby prevent them from moving in translation through the collar. The widener elements are inserted like a wedge into an axial slot made in the armor layer.
However, such an installation requires not only a substantial transformation of the end fittings currently used in order to be able to pierce immobilization holes, but also it requires axially splitting the tensile armor layers with precision. These arrangements and these methods of application are both costly in material and time. In addition, this installation requires great precision of installation in order to ensure that the various wires are immobilized with the same stress and that the axial clearances of the various immobilization means are identical for all of the wires. If they are not, the stress is not distributed evenly to all the wires, which generates the risk that certain overloaded wires end up breaking, which then increases the loading of the other wires and may end up causing a cascade breakage and a tearing-out of the end fitting.
A problem which then arises and which the present invention aims to solve is to provide an end fitting for a flexible tubular pipe which is not only capable of being produced at an advantageous cost but also which can better resist being torn out than most of those of the flexible pipes currently forming part of the prior art.
For the purpose of solving this problem, the present invention, according to a first object, proposes an end fitting for a flexible tubular pipe, said flexible tubular pipe comprising at least one sheet of tensile armor layers wound with a long pitch, said end fitting comprising a ring and a sleeve, said sleeve having a portion for connection to said pipe and at the opposite end an attachment portion, said connection portion having a portion for housing the armor layers and said connection portion being capable of being engaged in said ring in order to form an annular chamber about said housing portion, said armor layers of said sheet of tensile armor layers having a free end of armor layer suitable for extending into said annular chamber when said sleeve is mounted onto said pipe, said annular chamber being capable of receiving a pouring of a material suitable for solidifying inside said annular chamber, the free ends of armor layers having respectively anchoring means suitable for being trapped in said solidified material in order to prevent said free ends from moving in translation in said annular chamber; according to the invention, said anchoring means comprise respectively a widener element attached to said free ends of armor layer.
Therefore, one feature of the invention lies in the use of widener elements, attached to the free ends, which make it possible to locally widen the free ends of armor layer. In this way, the anchoring means sunk into the solidified material of the annular chamber are totally prevented from moving in translation since the passageways delimited in the material by the free ends have an insufficient cross section to allow the widener elements to pass through. Consequently, the tensile forces that are applied to the armor layers are notably absorbed by the solidified material and by the sleeve by means of the widener elements. The latter, with the extra thickness of the free ends, are prevented from moving in translation at the entrance of the aforementioned passageways.
In addition, said widener elements are advantageously welded to said free ends of armor layer, so that the tensile forces that are applied to the armor layers and that are transmitted to their free ends are not only absorbed by the forces of adhesion and the capstan effect that are exerted between the cured material and the free ends but also by the widener elements, via their welds. Because specifically, the armor layer which defines a passageway inside the cured material can obviously not slide therein since the local widening prevents the free end of armor layer from engaging in this passageway. Furthermore, however great the tensile forces, they could cause neither the deformation nor the shrinking of the local widening.
Advantageously, said widener elements are made of steel and they are therefore easier to weld, for example by electric arc welding or with any other means as will be explained below.
In addition, according to one particularly advantageous embodiment of the invention, said widener elements and said free ends of armor layer have respectively at least one surface portion of widener element and one surface portion of free end of armor layer which together form a cavity that is open to the outside delimited by a concave surface, for example of the recessed groove type. Said open cavity is filled with a molten solder to weld and secure said surface portions together. Therefore, the solder is confined in this open cavity and it then forms a more cohesive and stronger mass of weld. Preferably, said widener element surface portion and free end of armor layer surface portion extend respectively longitudinally in order to form a longitudinal cavity that is open to the outside and therefore the open cavity is furnished with a bead of weld ensuring better adhesion between the two surface portions. Consequently, the binding force between the free end of armor layer and the widener element is increased.
According to a first variant embodiment of the invention, said widener elements extend longitudinally and they have a cross section that is substantially rectangular and identical to the cross section of said free ends of armor layer. Therefore they can not only be made at an advantageous cost by previously sampling armor layer portions, but also, having the same characteristics, they are capable of being welded together with a bead of weld adhering in an identical manner to both.
Preferably, said widener elements and said free ends of armor layer have respectively lateral edges that are beveled so as to form laterally V-shaped longitudinal cavities, when said widener elements are respectively applied longitudinally to said free ends of armor layer. Therefore, not only does the longitudinal cavity thus formed allow an ideal confinement for the solder in order to form the bead of weld, but also the tensile forces are transmitted longitudinally on the bead of weld. This allows a greater strength of the weld itself. Therefore, it has been discovered that this embodiment of the invention makes it possible to achieve great mechanical strength and to do so despite the decline in the mechanical characteristics of the steel at the weld and its heat-affected zone. Therefore, by limiting the cross section of the longitudinal cavities to a value of less than 20% of the section of the wire, advantageously 15%, and by choosing a length of weld bead of the order of 20 to 30 mm, it is possible to produce an immobilization device having an ultimate tensile strength of more than 90% of the ultimate tensile strength of the armor layer wire. The load not absorbed by this immobilization device may easily be absorbed by the adhesion effect and the capstan effect without it being necessary to significantly increase the size of the annular chamber and the cost of the end fitting.
Advantageously, said lateral edges are beveled so that said widener element surface portion and free end of armor layer surface portion are respectively inclined with respect to one another at an angle of between 70° and 110°, preferably of the order of 90°.
According to a second variant embodiment of the invention, said free ends of armor layer have a circular cross section, while said widener elements extend respectively at least partially around said free ends of armor layer. For example, the widener element is formed of a ring that is heat-shrunk onto the free end of armor layer.
According to a second aspect, the present invention proposes a method for connecting an end fitting and a flexible tubular pipe, said flexible tubular pipe comprising at least one sheet of tensile armor layers wound with a long pitch, said armor layers of said sheet of tensile armor layers having a free end of armor layer, said end fitting comprising a ring and a sleeve, said sleeve having a portion for connection to said pipe and at the opposite end an attachment portion, said connection portion having a portion for housing the armor layers, said connection method being of the type in which said sleeve is mounted at the end of said flexible tubular pipe; anchoring means are formed at the free ends of armor layers; said free ends of armor layer are extended level with said housing portion; said ring is engaged about said connection portion in order to form an annular chamber about said housing portion; a material suitable for solidifying inside said annular chamber is poured in order to trap said anchoring means and prevent said free ends from moving in translation in said annular chamber; according to the invention, a widener element is attached to said free ends of armor layer in order to form said anchoring means.
Other features and advantages of the invention will emerge on reading the description given below of particular embodiments of the invention, given as an indication but not being limiting, with reference to the appended drawings in which:
Reference will be made to
Reference will now again be made to
As illustrated in
Advantageously, these two beads of weld 34, 36 are produced by an electric welding method, of the arc welding type, and preferably in a controlled atmosphere, for example according to the MIG (Metal Inert Gas) or MAG (Metal Active Gas) method.
The connection between the two respective surface portions 24, 32 and 26, 30 is all the stronger because the materials of free end of armor layer 12 and of widener element 14 have the same characteristics. It is the case in this instance and therefore the mechanical strength of the welds is improved.
Therefore, it has been discovered that despite the prejudices of those skilled in the art, this embodiment of the invention makes it possible to produce end fittings having a good mechanical resistance to being torn out. The prejudices were associated with the fact that steels with high mechanical characteristics usually comprising the armor layers are very sensitive to temperature and see their characteristics fall sharply, in practice by more than 50%, when they are subjected to a temperature of more than 1000° C. That is why those skilled in the art usually avoid subjecting these wires to such temperatures and avoid using high-temperature welding methods requiring the melting of the steel.
It seems that the good performance of this embodiment of the invention is mainly associated with the longitudinal orientation of the two beads of weld 34, 36. Specifically, the main mechanical force that these beads of weld must withstand is a shearing in the direction D of the armor layer, a shearing which tends to separate the widener element 14 from the free end of armor layer 12 when the end fitting sustains a stress tending to tear it out. However, orientating the beads of weld parallel with this shearing force makes it possible, with the dimensions being equal, to increase their resistance to this force. This favorable effect partially compensates for the reduction in the mechanical characteristics of the steel in the vicinity of the welds.
Advantageously, the length L of the widener element 14 is greater than or equal to 20 mm. In addition, if the armor layer 10 has a width 11 of more than 20 mm, the length L is preferably greater than or equal to the width 11. Specifically, increasing the length L makes it possible, with the stress being equal, to reduce the shearing stresses in the beads of weld 34, 36 and therefore to increase the resistance of the end fitting from being torn out. On the other hand, the excessive increase in the length L generates the disadvantage of increasing the length of the end fitting. The lengths indicated above offer the best compromise.
In addition, preferably, the chamfers 24, 26, 30, 32 have a slope relative to the mid plane defined by the contact surface 16 of the order of 45°, which makes it possible to facilitate the welding operation while improving the resistance to shearing of the welds.
In addition, advantageously, the height h and the width a of the chamfers 24, 26, 30, 32 are between 45% and 75% of the thickness el of the armor layer, and preferably between 55% and 70%. Thus, it has been observed that the resistance against the end fitting being torn out is further improved.
Reference will now be made to
In this way, there is therein again an armor layer 10′ having a free end of armor layer 12′ which is surmounted by a widener element 14′. The latter has a rectangular cross section identical to that of the free end of armor layer 12′, and it is adjusted backward of an end edge 40 of the free end of armor layer 12′. In addition, the widener element 14′ has a front cross section 42 and a rear cross section 44 at the back of the drawing, and the free end of armor layer 12′ has a bearing surface 28′. The front cross section 42 and rear cross section 44 and the bearing surface 28′ then form respectively surface portions also defining two opposite and transverse open cavities, into which extend two opposite beads of weld 34′, 36′. These beads of weld are made identically to those described above in
Reference will now be made to
In this way, the free end of armor layer 48 which defines a free outer surface, resting against the semi-cylindrical surface, defines two double surface portions respectively with the two opposite edges 52, 54, then forming two longitudinal open cavities, into which open cavities extend respectively two opposite longitudinal beads of weld 56, 58.
Finally, according to a fourth embodiment illustrated in
According to an advantageous feature, the free end of armor layer 48′ may be mounted by heat-shrinking in the crown 60.
Reference will now be made to
Furthermore, with respect to the flexible tubular pipe 68, the tensile armor layers 76 comprise armor layers 92 the free ends 94 of which are capable of extending into the annular chamber 90 and are fitted with widener elements 96. The widener elements 96 and the free ends of armor layer 94 are respectively linked together according to any one of the aforementioned embodiments with reference to
Therefore, according to another aspect, the present invention relates to a method for connecting the end fitting 66 to the end of the flexible tubular pipe 68. According to said method, first of all the sleeve 80 is mounted at the end of the pipe 68 extending the free ends of armor layer 94 level with the housing portion 86. Then, or previously, the widener elements 96 are fitted to the free ends of armor layer 94 in order to locally widen the cross section thereof. Then the ring 88 is engaged around the connection portion 82 forming the annular chamber 90 about the housing portion 86. The free ends of armor layer then extend into the annular chamber 90. And finally, an epoxy resin is poured which then solidifies in said annular chamber 90 in order to trap the free ends of armor layer 94 therein. Of course, thanks to the adhesive and mechanical characteristics of the epoxy resin after curing, the free ends of armor layer 94 are held in a fixed position in the end fitting 66. Specifically, the epoxy resin forms an indeformable solid in the annular chamber 90.
In this way, the stress forces F which are exerted on the tensile armor layers of the tensile armor layers 76 and which are transferred to the free ends of armor layer 94 are not only absorbed by the capstan effect procured by the curvatures of the free ends of armor layer 94 in the annular chamber 90, but also and above all thanks to the widener elements 96 welded to the surface of the free ends of armor layer 94 which are opposite a resistance R oriented toward the attachment portion 84 and opposed to the stress force F.
Number | Date | Country | Kind |
---|---|---|---|
0608557 | Sep 2006 | FR | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/FR2007/001480 | 9/13/2007 | WO | 00 | 5/6/2009 |