Claims
- 1. A method of producing a smooth surfaced extended leakage path ceramic tube wall for a high voltage tube device, the steps comprising:
- providing a highly polished preshaped positive for fabricating an ultrasmooth walled plastic mold having alternating convex and concave circular radius of curvatures of from 1/4 to 1/2 millimeter radii along the wall thereof
- setting plastic on said preshaped positive to form an ultrasmooth walled plastic mold for making a smooth surfaced extended leakage path for said ceramic tube wall;
- removing said preshaped positive from said plastic mold;
- filling said plastic mold with a ceramic particle slurry of a vacuum tube envelope quality alumina of 95% to 98% in a granular glass binder;
- compacting said ceramic particle slurry against the ultrasmooth plastic mold with ultrasonic agitation;
- prebaking the combined said ceramic particle slurry and said ultrasmooth walled plastic mold to produce a ring-shaped green ceramic tube wall;
- removing said plastic mold from said ring-shaped green ceramic tube wall;
- making a trough in at least one end of said ring-shaped green ceramic tube wall;
- high temperature firing said green ceramic tube wall to provide a cured ceramic tube wall; and
- metallizing each end and said trough in at least one end of said ring-shaped cured ceramic tube wall for electrical connection to said high voltage tube device.
- 2. A method as set forth in claim 1 wherein said highly polished preshaped positive is made of brass and said step of removing said preshaped positive from said plastic mold is by slipping the mold off the positive.
- 3. A method as set forth in claim 2 wherein said step of compacting with ultrasonic agitation is by mounting said plastic mold with said ceramic particle slurry therein on a platform and moving said platform by ultrasonic agitation.
- 4. A method as set forth in claim 3 wherein said step of prebaking is at 300.degree. C. to 500.degree. C. for a period of 4-5 hours.
- 5. A method as set forth in claim 4 wherein said step of high temperature firing is at 1600.degree. C. to 1800.degree. C. for 15 hours.
- 6. A method as set forth in claim 5 wherein said plastic material in said step of setting plastic on said highly polished preshaped positive for fabricating an ultrasmooth walled plastic mold is made of a vinyl polymer type thermoplastic with a surface smoothness on the order of molecular dimensions of 0.005 to 0.01 micrometers.
- 7. A method as set forth in claim 6 wherein the step of removing said plastic mold from said ring-shaped green ceramic tube wall is by peeling off the plastic mold that has lost its resiliency in said prebaking step.
Government Interests
The invention described herein may be manufactured, used, and licensed by the U.S. Government for governmental purposes without the payment of any royalties thereon.
US Referenced Citations (8)
Foreign Referenced Citations (3)
Number |
Date |
Country |
1201034 |
Sep 1965 |
DEX |
688312 |
Mar 1953 |
GBX |
953705 |
Mar 1964 |
GBX |