This application claims the benefit of priority from Chinese Patent Application No. 202210717648.5, filed on Jun. 23, 2022. The content of the aforementioned application, including any intervening amendments thereto, is incorporated herein by reference in its entirety.
The present application relates to high-temperature superconducting (HTS) pinning magnetic levitation (maglev), and more particularly to a high-temperature superconducting (HTS) maglev Dewar capable of increasing damping and levitation force and a width calculating method thereof.
High-temperature superconductors (HTS) have a higher critical temperature (higher than 77 K) than other ordinary superconducting materials, and can reach a superconducting state at a boiling point of liquid nitrogen. The HTS pinning maglev system provides levitation force to trains based on the flux-pining effect of the HTS. Unfortunately, the damping of the bulk superconductor material in the HTS pinning maglev system is too small to effectively suppress the system vibration. Therefore, it is urgently needed to improve damping and levitation force of the HTS pinning maglev system.
In order to overcome the problems in the prior art, the present disclosure provides a Dewar capable of increasing damping and levitation force of high-temperature superconducting maglev and a width calculation method thereof.
Technical solutions of the disclosure are described as follows.
In a first aspect, the present disclosure provides a high-temperature superconducting (HTS) maglev Dewar capable of increasing damping and levitation force, comprising:
an outer container; and
an inner container;
wherein the inner container is provided in the outer container, and is fixedly connected to the outer container through a connecting column; the inner container has a cavity configured to accommodate liquid nitrogen; a bottom of the inner container is provided with a bulk superconductor; the inner container is communicated with outside through a liquid nitrogen feeding pipe; and the outer container is made of an electrically conductive material.
In a second aspect, the present disclosure provides a method for calculating a width of the above-mentioned HTS maglev Dewar, comprising:
acquiring parameter information of a permanent magnet rail;
performing static magnetic field distribution calculation according to the parameter information by using a finite element analysis software to obtain a simulation result;
acquiring, according to the simulation result, a magnetic field distribution state of the permanent magnet rail on a cross section; and
calculating a width of the HTS maglev Dewar according to the magnetic field distribution state and a preset magnetic field gradient range.
Compared to the prior art, this application has the following beneficial effects.
Regarding the HTS maglev Dewar provided herein, the outer container, which is closest to the permanent magnet rail, and has a large magnetic field gradient and the largest area directly opposite to the permanent magnet rail, plays a role in increasing the system damping. Therefore, compared to the prior art where the stainless steel material is employed to improve the damping, this application can improve the system damping without any structural changes.
Other features and advantages of the present disclosure will be described below, or are understood based on the embodiments of the present disclosure. The objects and other advantages of the present disclosure may be realized and obtained by means of the structure specially indicated in the description, claims and drawings.
The drawings needed in the description of embodiments of the disclosure will be briefly described below to explain the technical solutions of the present disclosure more clearly. Obviously, presented in the accompany drawings are merely some embodiments of the present disclosure, and other drawings can be obtained by those skilled in the art based on the drawings provided herein without paying creative effort.
In the drawings, 1, cover; 2, corrugated pipe; 3, liquid nitrogen feeding pipe; 4, mounting base; 5, connecting column; 6, outer container; 7, inner container; 9, baffle; 10, positioning column; 11, bulk superconductor; 12, permanent magnet rail; 13, enclosed frame; 31, first pipe portion; 32, second pipe portion; and 33, third pipe portion.
The disclosure will be described completely and clearly below with reference to the accompanying drawings and embodiments to make the object, technical solutions, and beneficial effects of the present disclosure clearer. Obviously, provided below are merely some embodiments of the disclosure, which are not intended to limit the disclosure. The components described and illustrated in the drawings can be arranged and designed in various configurations. Therefore, the embodiments provided in the accompanying drawings are merely illustrative, and are not intended to limit the scope of the present disclosure. Based on the embodiments of the present disclosure, all other embodiments obtained by those skilled in the art without paying any creative effort shall fall within the scope of the present disclosure.
It should be noted that similar reference numerals or letters indicate similar elements in the following drawings. Therefore, once a certain element has been defined in one drawing, it does not need to further define and explain such element in subsequent drawings. As used herein, the terms “first”, “second”, etc. are only used to distinguish the elements referred to, and cannot be understood as indicating or implying relative importance.
The superconductor employed in a HTS pinning maglev system is a bulk non-ideal type II superconductor, which has a third state, namely mixed state, in addition to the superconducting and normal states. In the mixed state, the superconductor can pin the flux lines passing therethrough to block changes of the external magnetic field, In this case, both repulsive and attractive forces can be generated, achieving the stable levitation of the HTS pinning maglev system.
Due to a flux-pining effect of HTS, a bulk superconductor 11 and a permanent magnet rail 12 generate a non-source self-stabilization pining force, such that the HTS pinning maglev system provides a levitation force in the vertical direction and a guiding force in the lateral direction to a maglev train. The HTS has a strong nonlinear electromagnetic constitutive relation, which determines that a force on the HTS above the permanent magnet rail 12 has a strong nonlinearity, leading to a hysteretic nonlinear magnet-rail relationship in maglev applications. The magnet-rail relationship is dependent on material properties. When the HTS pinning maglev system vibrates, due to the alternating current (AC) loss and flux motion inside the superconductor, the hysteresis in the magnet-rail relationship plays a damping role in the vibration of the bulk superconductor 11, where an equivalent damping is small. From the view of vibration system, the HTS pinning maglev system, the HTS pinning maglev system is a light-damping system. When the HTS pinning maglev system applies in trains, damping of the trains may fail to suppress the violent vibration of the HTS pinning maglev system when a speed and vibration increase, or even the vibration instability may occur, affecting the safety of the HTS pinning maglev system.
Referring to
As shown in
Regarding the HTS maglev Dewar provided herein, the outer container, which is closest to the permanent magnet rail 12, has a large magnetic field gradient and has the largest area directly opposite to the permanent magnet rail 12, is employed as equipment for increasing damping, such that the damping of the HTS pinning maglev system can be improved without any change comparing to the prior art using stainless steel material. In addition, the outer container 6 made of 7050-T7451 aluminum alloy will affect an interaction between the bulk superconductor 11 and the permanent magnet rail 12. Also, since no additional equipment has been introduced, no need for additional calculation of a weight of dampers when designing the bulk superconductor 11 and the permanent magnet rail 12. The material with high conductivity is suitable for the HTS pinning maglev system since it has low speed, small displacement and high frequency during vibration. The material with high conductivity has a low saturation speed and a large equivalent damping at low speed, thus can provide great resistance to suppress vibration at low speed. It breaks through a limitation of small self-damping of superconductor and increases the damping of the HTS pinning maglev system, improving a dynamic performance of the HTS pinning maglev system. During the motion at the vertical direction, the outer container 6 made of aluminum alloy can induce an eddy current and generate an ohmic loss to consume an energy of vibration. A variation of a damping force on the outer container 3 with time is shown in
In order to further utilize the magnetic field of the permanent magnet rail 12 to generate a damping force, a width of the outer container 6 is greater than a width of the permanent magnet rail 12.
In an embodiment, in order to reduce a heat exchange between the liquid nitrogen in the inner container 7 and outside, the outer container 6 includes a damper. The damper has a cavity structure. The damper is provided with a first opening. A cover 1 fitting the first opening is arranged at the first opening. The outer container 6 is connected to the cover 1 through a bolt. The inner container 7 is arranged in a cavity enclosed by the damper and the cover 1. A gap is provided between the inner container and an inner wall of the outer container 6. The gap is vacuumized through a vacuum pump to form a vacuum insulation layer. By constructing the gap, a vacuum protective layer is constructed between the inner container 7 and the outer container 6 to reduce the heat exchange between the liquid nitrogen and outside.
In an embodiment, the cover 1 is made of stainless steel while prior art uses high strength polymer materials. By means of the excellent welding performance of the stainless steel, the assembly of the cover 1 with a corrugated pipe 2 and a mounting base can be simplified. This application uses welding instead of bonding, which improves connection reliability and air impermeability, and reduces the failure frequency.
In order to further reduce the heat exchange between the liquid nitrogen and outside, a top of the inner container 7 is fixedly connected to the cover 1 through a connecting column 5. Specifically, the connecting column 5 is made of G10 fiber reinforced plastic (FRP). By means of the connecting column 5, the cover 1 and the connecting column 5 has an indirect contact. The G10 FRP, as a high thermal resistance material, can effectively increase the heat resistance between the inner container 7 and the cover 1, and reduce the heat conduction, which further improves the thermal insulation, reduces the consumption rate of liquid nitrogen and prolongs the working time of the HTS maglev Dewar, leading to a better economic efficiency.
Referring to
Referring to
Referring to
In an embodiment, in order to increase structural stiffness, a positioning column 10 is provided between a side wall of the inner container 7 and a side wall of the outer container 6 to increase structural stiffness and positioning stiffness, which prevents the inner container 7 from being greatly deformed under stress, and ensures the reliability of structural connection. The positioning column 10 is made of polymer material such as G10 FRP, which has large thermal resistance and will not affect the thermal insulation of the HTS maglev Dewar.
Referring to
Provided is a method for calculating a width of the HTS maglev Dewar of Embodiment 1, including the following steps.
(S10) Parameter information of the permanent magnet rail 12 is acquired.
Specifically, the parameter information includes a width, length, height and magnetization intensity of a permanent magnet, and a width of the permanent magnet rail 12.
(S20) Static field distribution calculation is performed on the parameter information by using a finite element analysis software to obtain a simulation result.
Specifically, the finite element analysis is ANASYS Maxwell finite element software. The simulation result is shown in
(S30) A magnetic field distribution state of the permanent magnet rail on a cross section of the permanent magnet rail is acquired according to the simulation result.
(S40) A width of the outer container (i.e., the damper) of the HTS maglev Dewar is calculated according to the magnetic field distribution state and a preset magnetic field gradient range.
Step (S40) includes the following steps.
(S41) A magnetic flux density distribution on a horizontal plane under the magnetic field distribution state is extracted. The horizontal plane is a top surface of the permanent magnet rail 12.
(S42) An intersection between a centerline of the cross section of the permanent magnet rail 12 and the top surface of the permanent magnet rail 12 is taken as a zero point. Two first positions with a magnetic flux density equal to a first threshold are extracted under the magnetic flux density distribution.
The object of the step (S42) is to extract a critical position with the first threshold as a boundary according to the magnetic flux density distribution of the permanent magnet rail 12 in the horizontal direction. The first threshold is 0.1. A transverse magnetic flux density of a region greater than the first threshold may provide an eddy-current damping during vertical vibration of Embodiment 1.
(S43) Two second positions are extracted under the magnetic field distribution with the two first positions as a boundary, in which a magnetic flux density gradient of the two second positions is larger than a second threshold. A distance between the two second positions is taken as the width of the outer container (i.e., the damper).
The object of the step (S43) is to optimize the width of the HTS maglev Dewar of Embodiment 1, that is, within a width range defined by the first threshold, a region with a gradient difference of more than 0.002 T/mm is taken as the width of the HTS maglev Dewar of Embodiment 1, that is, the second threshold is 0.002.
Described above are merely preferred embodiments of this disclosure, which are not intended to limit the scope of the present disclosure. Any changes, modifications and replacements made by those killed in the art without departing from the spirit of this disclosure should fall within the scope of the present disclosure defined by the appended claims.
Although some embodiments of the present disclosure have been illustrated above, various replacement and variations to these embodiments can be made by those skilled in the art without departing from the principle and spirit of the present disclosure. The scope of the present disclosure is defined solely by the appended claims or equivalents thereof.
Number | Date | Country | Kind |
---|---|---|---|
202210717648.5 | Jun 2022 | CN | national |
Number | Name | Date | Kind |
---|---|---|---|
5334965 | Dolgin | Aug 1994 | A |
5442928 | Laskaris et al. | Aug 1995 | A |
6411187 | Rotem | Jun 2002 | B1 |
20020024338 | Saho | Feb 2002 | A1 |
20080278270 | Hull | Nov 2008 | A1 |
Number | Date | Country |
---|---|---|
103322117 | Sep 2013 | CN |
106653281 | May 2017 | CN |
107120522 | Sep 2017 | CN |
107941280 | Apr 2018 | CN |
207352144 | May 2018 | CN |
109003774 | Dec 2018 | CN |
109141575 | Jan 2019 | CN |
210227592 | Apr 2020 | CN |
112196927 | Jan 2021 | CN |
112259319 | Jan 2021 | CN |
113035486 | Jun 2021 | CN |
113053613 | Jun 2021 | CN |
113096908 | Jul 2021 | CN |
215069486 | Dec 2021 | CN |