1. Field of the Invention
The present invention relates to a hollow container and an apparatus for manufacturing the same.
2. Description of the Invention
In manufacturing a hollow container to be used as a vehicle fuel tank or the like, there is a case where a container body is produced by blow molding, and then a sub-component to penetrate a wall of the container body is joined to the container body by welding. In such a case, an opening is formed in the wall of the blow-molded container body, and then the sub-component is joined to the blow-molded container body by welding in such a manner that the sub-component plugs and seals the opening (see Japanese Unexamined Patent Application Publication Nos: 2009-534215, 2008-507651, and 2007-092678).
Conventionally, container bodies of hollow containers have been produced by molding a parison including a resin layer. There has been a demand for suppressing the permeation of vaporized fuel through the resin layer from a section of the resin layer created by the formation of the opening to the outside.
The present invention has been made under the above circumstances, and it is an object of the present invention to provide a hollow container that enables the suppression of permeation of the content of the hollow container to the outside and also provide an apparatus for manufacturing the same.
In one aspect, the present invention provides a hollow container comprising:
a container body that is hollow and that has an opening formed in a wall of the container body; and
a sub-component that is inserted in the opening and that is in contact with an outer surface of the wall at a contact portion of the container body to seal the container body, wherein
the container body has a structure of multiple layers including an intermediate barrier layer, and
the wall of the container body is thinner at a circumferential edge portion around the opening as a thinner portion than at the contact portion where the sub-component is in contact with the outer surface of the wall.
This arrangement, in which the circumferential edge portion around the opening is the thinner portion, makes it possible to suppress permeation of the content of the hollow container, for example, vaporized fuel, through the outer layer next to the barrier layer.
The thinner portion may be formed by compression.
This arrangement makes it easy to form the thinner portion.
In another aspect, the present invention provides an apparatus for manufacturing a hollow container:
a container body that is hollow and that has an opening formed in a wall of the container body; and
a sub-component that is inserted in the opening and that is in contact with an outer surface of the wall at a contact portion of the container body to seal the container body, the apparatus manufacturing the container body by blow molding,
wherein
the apparatus comprises a compressor adapted to compress a portion of a parison that encompasses a region where the opening is to be made in order to form a thinner portion, the thinner portion being thinner than the contact portion where the sub-component is in contact with the outer surface of the wall, the parison having a structure of multiple layers including an intermediate barrier layer.
This arrangement makes it possible to manufacture a hollow container that enables the suppression of permeation of the content of the hollow container to the outside.
Moreover, the thinner portion may be cut to form the opening, which facilitates the manufacture of the hollow container, resulting in an improved productivity thereof.
Further, it is ensured that the contact portion has a sufficient thickness. This configuration suppresses the contact portion from being deformed by the welding and eliminates the need to use an apparatus or the like for backing-up the contact portion from inside the hollow container to ensure the reliability in assembling the sub-component into the container body and sealing the container body with the sub-component.
The compressor may be a presser to press the parison against a mold.
The compressor may blow a gas onto the parison in order to form the thinner portion.
According to the present invention, it is possible to provide a hollow container that enables the suppression of permeation of the content of the hollow container to the outside and also provide an apparatus for manufacturing the same.
Hereinafter, with reference to the accompanying drawings, description will be made of embodiments of the present invention wherein container bodies of hollow containers are produced by blow molding. Like components are denoted by like reference numerals, and detailed description thereof will be omitted.
Now, description will be made of a hollow container, and an apparatus for and a method of manufacturing the hollow container, according to a first embodiment of the present invention, with reference to
As shown in
The container body 2A is a hollow resin component produced by blow molding. The container body 2A is formed of a container-body upper part 2UA and a container-body lower part 2L that are joined together.
The container-body upper part 2UA and the container-body lower part 2L each have a structure of multiple layers including an intermediate barrier layer 2x. According to the present embodiment, these parts each have a structure of three layers consisting of an intermediate barrier layer 2x and resin layers (for example, high-density polyethylene layers) 2y, 2y each provided on one side of the barrier layer 2x. The structure of multiple layers is not limited to such a structure of three layers but may be a structure of four or more layers including an adhesive layer or the like.
The container-body upper part 2UA has an opening 2a which is a circular through hole formed in a wall thereof. A circumferential edge portion around the opening 2a is an annular shaped thinner portion 2b. The thinner portion 2b is formed by compression so as to be thinner than the remainder of the container-body upper part 2UA. An outer circumferential portion around the thinner portion 2b is a contact portion 2c where the sub-component 3A is in contact with an outer surface of the wall and where an annular projection 2d extends from an inner surface thereof. Thickness dl of the thinner portion 2b, thickness d2 of the contact portion 2c, and thickness d3 of a section, of the contact portion 2c, at which the projection 2d extends satisfy the relationship:
d1<d2<d3
At the thinner portion 2b, a reduction is made in a cross sectional area of the outer resin layer 2y, which is a cross sectional area from which the content of the hollow container 1A permeates through the outer resin layer 2y to the outside. As a result, the leakage of the content of the hollow container 1A is favorably suppressed.
The sub-component 3A is a component penetrating through and sealing the opening 2a. The sub-component 3A includes an inner larger-diametric portion 3a, an outer smaller diametric portion 3b, a flange portion 3c, and an annular wall portion 3d. The flange portion 3c extends from between the larger diametric portion 3a and the smaller diametric portion 3b. The annular wall portion 3d extends from the outer circumferential edge of the flange portion 3c toward the inside of the hollow container 1A. The larger diametric portion 3a has an outer diameter smaller than the inner diameter of the opening 2a. The flange portion 3c has an outer diameter larger than the inner diameter of the opening 2a. This configuration allows the larger diametric portion 3a to be inserted into the opening 2a by being brought from outside the container body 2A. When the larger diametric portion 3a is inserted in the opening 2a, a top end surface of the annular wall portion 3d is in contact with the outer surface at the contact portion 2c. The sub-component 3A is adapted to seal the opening 2a with the larger diametric portion 3a inserted in the container body 2 while the smaller diametric portion 3b, the flange portion 3c and the annular wall portion 3d are exposed to the outside of the container body 2A. In this state, the top end surface of the annular wall portion 3d is joined by welding to the outer surface of the contact portion 2c to allow the sub-component to seal the opening 2a.
The built-in components 4, 4 are components fastened inside the container body 2A. One built-in component 4 is embedded in the inner surface of the container-body upper part 2UA to a predetermined depth whereas the other built-in component 4 is embedded in the inner surface of the container-body lower part 2L to a predetermined depth.
Now, description will be made of a hollow-container manufacturing apparatus for producing the container body 2A of the hollow container 1A with reference to
As shown in
The parisons P, P are in the form of rectangular sheets. In a case where the hollow container 1A, which is a blow-molded article, is an on-board fuel tank, the parisons P, P each have a structure of multiple layers including the inner thermoplastic resin layer 2y and the outer thermoplastic resin layer 2y which respectively form the inner and outer surfaces of the tank and the barrier layer 2x which is sandwiched between the inner and outer thermoplastic resin layers 2y, 2y. The barrier layer 2x is made of, for example, material with a high impermeability to the fuel. The inner and outer thermoplastic resin layers 2y, 2y contain high-density polyethylene (HDPE) excellent in heat fusion and molding properties.
When the mold members 11,12 are closed against the center frame 13A sandwiched therebetween, the peripheral portions of the parisons P, P are sandwiched between each of the mating surfaces of the center frame 13A and its corresponding one of the mating surfaces of the mold members 11,12. The sandwiched peripheral portions serve as pinch-off portions. The manufacturing apparatus has a function to fasten a built-in component 4 to an internal surface of a parison P. The center frame 13A is provided with a cylinder 15 which serves as an actuator to fasten a built-in component 4 to the parison P. According to the present embodiment, the center frame 13A is provided with cylinders 15, 15 to fasten the built-in components 4, 4 to the parisons P, P provided on both sides of the center frame 13A, as shown in
As shown in
The mold member 11 has, on the other hand, a molding surface with an annular, circular, or C-shaped (here, annular) projection 11a formed at a location opposed to the projection 14a of the jig 14A. When the mold members 11,12 are closed against the center frame 13A sandwiched therebetween, a portion of the parison P is pressed between the projections 11a, 14a and thereby compressed to form the circular or annular shaped (here, annular shaped) thinner portion 2b.
Now, description will be made of the method of manufacturing the hollow container 1A using the hollow-container manufacturing apparatus 10A, with reference to
As shown in
By this being done, one parison P is pressed between the projections 11a, 14a to form the annular thinner portion 2b in the one parison P. The thinner portion 2b is a portion compressed compared to the remainder of the one parison P. The thinner portion 2b encompasses a region where the opening 2a is to be made. Namely, The thinner portion 2b extends across a length from an inner circumferential area around the region where the opening 2a is to be made outward in the radial direction of the region where the opening 2a is to be made. During the formation of the thinner portion 2b, the resin spreads outward from the thinner portion 2b being formed, forming the annular projection 2d onto the inner surface at the contact portion 2c of the one parison P. The projection 2d improves the rigidity of the contact portion 2c. This ensures the rigidity of the contact portion 2c, even with a reduction in the thickness of the contact portion 2c for a cost saving purpose, thereby suppressing the contact portion 2c from being deformed by welding or the like, and also allowing for the manufacture of the hollow container with conventional facilities. The thinner portion 2b may have a circular shape or C-shape rather than an annular shape.
In the meanwhile, simultaneously with the transfer step, the step of fastening the built-in components 4, 4 is performed. The cylinders 15, 15 are actuated to move the built-in components 4, 4 toward the mold members 11,12 so that the base end portions of the built-in components 4, 4 are pressed to be embedded into the parisons P, P to predetermined depths. The built-in components 4, 4 are fastened and then made free of clamps of the clamping mechanisms 16,16, and as shown in
Subsequently, the thinner portion 2b of the container body 2A is cut with a cutter or the like to form the opening 2a, into which the sub-component 3A is then inserted, followed by welding (hot-plate welding) the annular wall portion 3d of the sub-component 3A to the contact portion 2c. The sub-component 3A is thereby secured to the container body 2A, to obtain the hollow container 1A.
According to the hollow container 1A of the first embodiment of the present invention, the circumferential edge portion around the opening 2a is the thinner portion 2b of the thickness dl. This configuration suppresses the content of the hollow container 1A, for example, vaporized fuel, from permeating the outer resin layer 2y next to the barrier layer 2x.
In other words, according to the hollow container 1A, the thickness of the outer resin layer 2y next to the barrier layer 2x is reduced at the thinner portion 2, namely, the cross sectional area of the outer resin layer 2y next to the barrier layer 2x is reduced at the thinner portion 2. This enables the suppression of permeation of the content of the hollow container 1A, for example, vaporized fuel, through the outer resin layer 2y next to the barrier layer 2x.
More particularly, according to the hollow container 1A, the outer resin layer 2y is compressed to cause the barrier layer 2x to come closer to the boundary with the gaseous layer (atmosphere). This enables reduction of the absolute amount of the vaporized fuel that permeates into the outer resin layer 2y to the outside.
Further, according to the hollow container 1A, the thinner portion 2b is formed by compression and thus is easy to form.
Moreover, according to the hollow container 1A, the opening 2a is formed by cutting the annular thinner portion 2b, which facilitates the manufacture of the hollow container 1A, resulting in an improved productivity thereof.
In addition, according to the hollow container 1A, it is ensured that the contact portion 2c has a sufficient thickness. This configuration suppresses the contact portion being deformed by the welding and ensures reliability in welding without using any apparatus or the like for backing-up the contact portion 2c from inside the hollow container 1A.
Further, according to the hollow-container manufacturing apparatus 10A of the first embodiment of the present invention, it is possible to manufacture the hollow container 1A that enables suppression of the permeation of the content of the hollow container 1A through the resin layer.
Moreover, according to the hollow-container manufacturing apparatus 10A, the opening 2a may be formed by cutting the annular thinner portion 2b. This facilitates manufacture of the hollow container 1A, resulting in improved productivity thereof.
In addition, according to the hollow-container manufacturing apparatus 10A, the sufficient thickness d2 of the contact portion 2c is ensured, thereby suppressing the contact portion 2c from being deformed by the welding, and ensuring the reliability in assembly by the welding and in sealing without using any apparatus or the like for backing-up the contact portion 2c from inside the hollow container 1A.
Now, description will be made of an apparatus for manufacturing the hollow container according to a second embodiment of the present invention, focusing on differences thereof from the hollow-container manufacturing apparatus 10A according to the first embodiment. As shown in
The center frame 13B is formed with a flow passage 13a. The jig 14B is formed with a blow passage 14b and a flow passage 14c. The blow passage 14b is annular or circular (here, annular) in cross section. The flow passage 14c is in communication with the blow passage 14b and the flow passage 13a of the center frame. The blow portion 17 supplies, to the flow passage 13a, a gas with a pressure higher than the blow pressure at blow molding (a gas with high flow speed). The supplied high-pressure gas is blown onto an area of an inner surface of the parison P through the flow passage 13a and the blow passage 14b. The portion of the parison P with that area is compressed by the blowing of the gas to form the annular thinner portion in the parison P.
The hollow-container manufacturing apparatus 10B of the second embodiment of the present invention has the same effects as does the hollow-container manufacturing apparatus 10A of the first embodiment.
Now, description will be made of a hollow container according to the third embodiment of the present invention, focusing on differences thereof from the hollow container 1A according to the first embodiment. As shown in
The container body 2C includes a container-body upper part 2UC in place of the container-body upper part 2UA. The container-body upper part 2UC has an annular projection 2e formed on an outer surface thereof. The annular projection 2e is larger in diameter than the O-ring 5 and serves as a stopper to prevent the O-ring 5 slipping out.
The sub-component 3C is a pump or the like and has no annular wall portion 3d. The O-ring 5 is placed between the outer surface of the contact portion 2c of the container body 2C and the inner surface of the flange portion 3c of the sub-component 3C. The cam-lock 6 has one end portion stuck and fixed in the outer resin layer 2y of the container body 2C. The cam-lock 6 has the other end portion engaging the retainer 7 provided at the outer surface of the flange portion 3c of the sub-component 3C. With this arrangement, the sub-component 3C is fixed to the container body 2C.
The hollow container 1C of the third embodiment of the present invention has the same effects as does the hollow container 1A even when another technique than welding is applied to secure the sub-component 3C to the container body 2C.
Description has been made of the embodiments of the present invention. The present invention, however, is not limited to those embodiments, and is modifiable properly in various forms within the scope of the present invention. For example, instead of using the two parisons P, P in the form of sheets to form each of the container bodies 2A and 2C, a cylindrical parison may be used. Further, the thinner portion 2b may be formed by machining the outer resin layer 2y or the like technique. Moreover, the hollow-container manufacturing apparatus may include a compressor that is movable inside a mold and presses a cylindrical parison P against the mold.
Number | Date | Country | Kind |
---|---|---|---|
2012-164053 | Jul 2012 | JP | national |