1. Technical Field
The present disclosure generally relates to a housing with a multicolor appearance and a method for making the same.
2. Description of Related Art
Electronic devices having a decorative housing are attractive. In-Mold Labeling (IML) is a typical method for producing decorative housings. Specifically, a preformed plastic film with a decorative layer of ink can be in-mold labeled with a plastic substrate within a mold. However, the decorative layer made of ink usually presents an appearance of only one simple color and it can be difficult to present a multicolor appearance.
Therefore, there is room for improvement within the art.
Many aspects of the housing and method for making the housing can be better understood with reference to the following drawings. The components in the drawings are not necessarily to scale, the emphasis instead being placed upon clearly illustrating the principles of the present housing and method for making the same.
The substrate 11 may be molded by a plastic e.g., polymethyl methacrylate (PMMA), polyethylene (PE), acrylonitrile-butadiene-styrene (ABS), or polycarbonate (PC). Alternatively, the substrate 11 may be made of a metal. The substrate 11 has a working surface 110.
The base paint layer 12 is formed on the working surface 110. The base paint layer 12 may be made of an ultraviolet curable paint and can strengthen the bonding of the vacuum coated layer 13 and the substrate 11.
The vacuum coated layer 13 is formed on the base paint layer 12 and may have a metallic appearance. When the housing 10 is used for an electronic device with telecommunication function, the vacuum coated layer 13 can be nonconductive to have no effect on the transmission of radio frequency signals (RF).
The first colored paint layer 14 is formed on the vacuum coated layer 13. The first colored paint layer 14 has a first color and a degree of transparency. The first colored paint layer 14 covers the whole vacuum coated layer 13. The first colored paint layer 14 may be made of an ultraviolet curable paint.
The second colored paint layer 15 is formed on a portion of the first colored paint 14. The second colored paint layer 15 has a second color different from the first color. The second colored paint layer 15 also has a degree of transparency. The second colored paint layer 15 has a first section 152 and a second section 154. The first section 152 has a thick distribution density of a second colored paint. The first section 152 covers a part of the first colored paint layer 14. The second section 154 has a thin distribution density of the second colored paint. The density of the second colored paint of the second section 154 decreases gradually away from one end 1540 of the second section 154. The end 1540 is close to the first section 152. The second colored paint layer 15 may be made of an ultraviolet curable paint.
The top paint layer 16 is coated on the second colored paint layer 15 and the portions of the first colored paint layer 14 exposed from the second colored paint layer 15. The top paint layer 16 is transparent and may be made of a paint having a soft tactility.
It should be understood, the first colored paint layer 14 may cover a section of the vacuum coated layer 13. Accordingly, the second colored paint layer 15 may be formed on remainder of the vacuum coated layer 13 (not covered with the first colored paint layer 14) and partially overlap the first colored paint layer 14.
It should be understood, the base paint layer 12 and the vacuum coated layer 13 can be omitted, accordingly, the first colored paint layer 14 being directly formed on the working surface 110 of the substrate 11.
In a step S1, the plastic substrate 11 is provided. The substrate 11 has the working surface 110.
In a step S2, the base paint layer 12 is formed (e.g., painted or brushed) on the working surface 110.
In a step S3, the vacuum coated layer 13 is formed on the base paint layer 12 for example, by using a vacuum evaporating method or a vacuum sputtering method.
In a step S4, the first colored paint layer 14 is formed (e.g., painted) on the whole vacuum coated layer 13.
In a step S5, a second colored paint layer 15 is painted on a section of the first colored paint 14.
In a step S6, the second colored paint layer 15 and the portions of the first colored paint layer 14 that are not covered with the second colored paint layer 15 are coated with a top paint layer 16.
It should be understood, however, that even though numerous characteristics and advantages of the present embodiments have been set forth in the foregoing description, together with details of the structures and functions of the embodiments, the disclosure is illustrative only, and changes may be made in detail, especially in matters of shape, size, and arrangement of parts within the principles of the invention to the full extent indicated by the broad general meaning of the terms in which the appended claims are expressed.
| Number | Date | Country | Kind |
|---|---|---|---|
| 200910304494.1 | Jul 2009 | CN | national |