Hybrid sealing technique

Information

  • Patent Grant
  • 6817918
  • Patent Number
    6,817,918
  • Date Filed
    Friday, June 8, 2001
    23 years ago
  • Date Issued
    Tuesday, November 16, 2004
    20 years ago
Abstract
The present invention is a hybrid sealing technique. According to one or more embodiments of the present invention, an unsealed lamp body is heated and a partial pinch seal is performed on a first side of the lamp body at an outer junction area. Then, a shrink seal is applied which completes the sealing process at the first side of the lamp body by sealing an inner junction area on the same side of the lamp body. The present invention retains the benefits of the shrink seal, but alleviates the difficulty associated with holding the electrode assemblies in place when performing a traditional shrink seal. In addition, the machine which holds the electrode assemblies in place is greatly simplified.
Description




Portions of the disclosure of this patent document contain material that is subject to copyright protection. The copyright owner has no objection to the facsimile reproduction by anyone of the patent document or the patent disclosure as it appears in the Patent and Trademark Office file or records, but otherwise reserves all copyright rights whatsoever.




BACKGROUND OF THE INVENTION




1. Field of the Invention




The present invention relates to the manufacture of lamps, and in particular to a hybrid sealing technique that enhances productivity when manufacturing the lamps.




2. Background Art




When manufacturing lamps, two electrodes are typically sealed within a lamp body to form a sealed enclosure where light is produced. Two methods are typically used to seal the enclosure. A first method is a pinch seal. A second method is a shrink seal. Shrink seals are superior to pinch seals, but it is difficult to position the electrodes and to secure them in place when performing a shrink seal.




Typical Lamp Configuration




A typical lamp configuration is shown in

FIG. 1

where lamp body


5


contains a first electrode


15


and a second electrode


20


which are located opposite one another and which are respectively connected to a molybdenum foil part


25


and a molybdenum foil part


30


. The connections between first electrode


15


and second electrode


20


and foil parts


25


and


30


are maintained by inner junction


80


and inner junction


85


within hermetically sealed portions


45


and


50


respectively. In addition, molybdenum wires


55


and


60


are connected to foil parts


25


and


30


by outer junctions


90


and


95


.




Pinch Seal




To form a pinch seal, the lamp body


5


, which may be comprised of quartz glass or other suitable material, is heated. When heated, the lamp body


5


becomes malleable. Pressure is applied in the area of foil parts


25


and


30


to pinch the malleable glass to the foil parts which creates a vacuum tight seal where junctions


35


and


90


are sealed at the same time. Pinch seals are disadvantageous because it is essential to not only seal the lamp but to also clean all impurities from the inside of the lamp before sealing it. Pinch seals offer no mechanism to effectively clean the sealed inside portion of the lamp. In addition, the pinch seal causes a large amount of pressure to the lamp body and electrode assemblies and the seal is often non-uniform which can lead to premature lamp failures and limits the pressure the lamps can be operated with.




Shrink Seal




To form a shrink seal, the unsealed lamp body is placed in a vacuum as shown in FIG.


2


. To perform a shrink seal, the glass lamp body


200


is heated and a vacuum pumps pressure in opposing directions


210


and


220


which cause the lamp body to shrink and seal around foil parts


230


and


240


. Shrink seals are beneficial because the vacuum pressure that pulls air from the inside of the lamp body also pulls impurities from the lamp body as well. Moreover, this type of seal is advantageous since a better glass uniformity around junctions


35


and


40


can be achieved. This leads to better reliability and better maintenance. When performing a shrink seal, it is crucial to position the electrode and to secure the electrode assembly in place.




To position and hold the electrode assembly in place while performing a shrink seal is an expensive and difficult process because a machine must be used to hold the electrode assemblies at the molybdenum wire portions


55


and


60


and to adjust the position of the molybdenum wires


55


and


60


so that the entire electrode assembly is positioned exactly in the right position when the shrink seal is achieved. In addition, the positioning of the electrode assembly must occur in vacuum conditions which makes the process even more difficult.




SUMMARY OF THE INVENTION




The present invention is a hybrid sealing technique. According to one or more embodiments of the present invention, an unsealed lamp body is heated and a partial pinch seal is performed on one side of the lamp body at an outer junction area. Then, a shrink seal is applied to that portion of the lamp body to completely seal the electrode within the lamp body by sealing an inner junction area.




In one embodiment, Nitrogen is flushed through the unsealed lamp body from the bottom of the lamp and over the electrodes to avoid oxidation and clean the lamp. In other embodiments, an inert gas like Argon, Neon, or other suitable gas is used. Then, the glass is heated and a partial pinch seal is performed at the bottom portion of the lamp only around an outer junction area. After that, a vacuum at the top of the lamp body pulls air out. Thereafter the glass is allowed to cool for a short time, 5 seconds for instance. Then, a burner is turned on and moved up the length of the area to be sealed (near the partially pinch sealed area) and in conjunction with the vacuum this causes the glass to soften and a shrink seal is achieved around an inner junction area.




The present invention retains the benefits of the shrink seal, but alleviates the difficulty associated with holding the electrode assemblies in place when performing a traditional shrink seal in vacuum conditions. In addition, the machine which holds the electrode assemblies in place is greatly simplified since the partial pinch seal holds the electrode in place while the shrink seal is occurring.











BRIEF DESCRIPTION OF THE DRAWINGS




These and other features, aspects and advantages of the present invention will become better understood with regard to the following description, appended claims and accompanying drawings where:





FIG. 1

is a diagram of a typical lamp configuration.





FIG. 2

is a diagram of a typical shrink seal.





FIG. 3

is a flowchart showing a hybrid sealing technique according to an embodiment of the present invention.





FIG. 4

is a diagram of a hybrid sealing technique according to an embodiment of the present invention.





FIG. 5

is a flowchart showing a hybrid sealing technique according to another embodiment of the present invention.











DETAILED DESCRIPTION OF THE INVENTION




The invention relates to a hybrid sealing technique. In the following description, numerous specific details are set forth to provide a more thorough description of embodiments of the invention. It will be apparent, however, to one skilled in the art, that the invention may be practiced without these specific details. In other instances, well known features have not been described in detail so as not to obscure the invention.




According to one or more embodiments of the present invention, an unsealed lamp body is heated and a partial pinch seal is performed on one side of the lamp body in a junction area between a foil part and a molybdenum wire (outer junction area). Then, a shrink seal is applied to the same side of the lamp body to complete the seal at an inner junction area where the electrode joins the foil part. An embodiment of the present invention is described in FIG.


3


. At step


300


an unsealed lamp body is heated. Then, a partial pinch seal is applied at step


310


to an outer junction area on a first side of the unsealed lamp body. Next, a vacuum is applied in one direction at a second side of the lamp body at step


320


. Thereafter, the vacuum causes a shrink seal to the first side at an inner junction which completes the hybrid sealing process for that side of the lamp body.





FIG. 4

is a diagram of the process of performing the hybrid sealing technique. Lamp body


400


is heated which causes the body to soften. Then, a first unsealed portion


410


is partially pinch sealed at junction


470


. Then, a vacuum


420


is applied to a second portion


430


of the lamp body


400


which remains unsealed. Vacuum


420


pulls air from lamp body


400


in the direction indicated by arrow


440


. Thereafter, the vacuum pressure in conjunction with the lamp body which has been softened by heating causes a shrink seal to occur at a second junction area


480


.




In one embodiment, Nitrogen is used to clean the lamp body before a hybrid sealing technique is applied. This embodiment of the present invention is shown in the flowchart of FIG.


5


. At step


500


Nitrogen is flushed through the unsealed lamp body from the bottom of the lamp and over the electrodes to avoid oxidation and clean the lamp. In other embodiments, an inert gas like Argon, Neon, or other suitable gas is used. Then, at step


510


the lamp body is heated and a partial pinch seal is performed at the bottom portion of the lamp body at step


520


. After that, a vacuum at the top of the lamp body pulls air out at step


530


. Thereafter, at step


540


, the glass is allowed to cool for a short time, 5 seconds for instance. Then, a burner is turned on and moved up the length of the bottom portion at step


550


. The application of the burner in conjunction with the vacuum causes the glass to soften and a shrink seal is achieved on the bottom portion of the lamp body at step


560


.




The present invention retains the benefits of the shrink seal, but alleviates the difficulty associated with holding the electrode assemblies in place under vacuum conditions when performing a traditional shrink seal. In addition, the machine which holds the electrode assemblies in place is greatly simplified. Thus, a hybrid sealing technique is described in conjunction with one or more specific embodiments. The invention is defined by the claims and their full scope of equivalents.



Claims
  • 1. A method for sealing a lamp comprising:applying a first heating step to said lamp; performing a partial pinch seal on a first portion of said lamp at an outer junction area; applying a vacuum to a second portion of said lamp; applying a cooling step to said lamp; and applying a second heating step to said lamp wherein said second heating step in conjunction with said vacuum causes a shrink seal to occur at said first portion of said lamp at an inner junction area.
  • 2. The method of claim 1 wherein said outer junction area extends over a molybdenum wire and a foil part.
  • 3. The method of claim 1 wherein said inner junction area extends over an electrode and a foil part.
  • 4. The method of claim 1 further comprising: flushing said lamp with Nitrogen, Argon, or Neon.
  • 5. The method of claim 1 wherein said lamp is made of a quartz glass.
US Referenced Citations (4)
Number Name Date Kind
2716584 Retzer Aug 1955 A
3685880 Sobieski Aug 1972 A
5984749 Nishibori et al. Nov 1999 A
6354900 Ohshima et al. Mar 2002 B1