Claims
- 1. A process for making an inorganic powder comprising:
- preparing an aqueous solution comprising oxalic acid,
- adding a hydrolyzable metal compound to the aqueous solution of oxalic acid at a molar ratio of oxalic acid to metal compound of from about 0.9:1 to about 1.1:1, optionally, adding deionized water,
- adding ammonia or ammonium hydroxide solution,
- adjusting the pH of the solution to about 8-10 thereby forming a slurry containing a solid comprising an amino metal oxalate having the structure ##STR2## recovering said oxalate via filtration, and reacting said oxalate with water at a temperature of about 200.degree. C. to 250.degree. C. under pressure to yield an inorganic metal oxide powder.
- 2. The process of claim 1 wherein the amino metal oxalate contains a metal selected from the group consisting of zinc, tin, antimony mixed with tin, iron, zirconium, aluminum, chromium, yttrium and europium.
- 3. The process of claim 1 wherein said powder comprises:
- at least one oxide of metals selected from the group of titanium, zirconium, silicon, aluminum, yttrium, europium, tin, antimony, iron, zinc, wherein said powder has an average crystallite size of about 1 to 100 nm.
- 4. The process of claim 1 wherein said process is performed in a non-oxidizing atmosphere.
- 5. The process of claim 1 wherein said process is performed in the presence of at least one dopant metal selected from the group consisting of tin, titanium, aluminum, antimony, zirconium, zinc, cerium, germanium, manganese, vanadium, ruthenium, iridium, osmium, tungsten, molybdenum, niobium, cobalt, lead, silicon, indium, tantalum, yttrium, europium, iron, copper and nickel; wherein said metals and said dopant metals are chemically distinct.
Parent Case Info
This a continuation of application Ser. No. 08/548,987 filed Oct. 27, 1995, now abandoned.
US Referenced Citations (21)
Foreign Referenced Citations (1)
Number |
Date |
Country |
2100224 |
Jul 1993 |
CAX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
548987 |
Oct 1995 |
|