The disclosure relates to a micro-biosensor, and more particularly to an implantable micro-biosensor adapted to be implanted under skin of a body to continuously monitor a physiological parameter of an analyte in a biological fluid of the body. The disclosure also relates to a method for manufacturing the implantable micro-biosensor.
The rapid increase in the population of diabetic patients emphasizes the need to monitor and control the variation of glucose concentration in a body of a subject. As a result, many studies are moving towards the development of implantable continuous glucose monitoring systems, so as to address the inconvenience associated with repeated procedures of blood collection and tests. The basic configuration of the continuous glucose monitoring system includes a biosensor and a transmitter. The biosensor measures a physiological signal in response to a glucose concentration in the body, and the measurement thereof is mostly based on an electrochemical process. Specifically, glucose is subjected to a catalysis reaction with glucose oxidase (GOx) to produce gluconolactone and a reduced glucose oxidase, followed by an electron transfer reaction between the reduced glucose oxidase and oxygen in a biological fluid of the body to produce hydrogen peroxide (H2O2) as a byproduct. The glucose concentration is then derived from an oxidation reaction of the byproduct H2O2. The reaction mechanism of the electrochemical process is shown below.
Glucose+GOx(FAD)→GOx(FADH2)+Gluconolactone
GOx(FADH2)+O2→GOx(FAD)+H2O2
In the above reaction mechanism, FAD (i.e., flavin adenine dinucleotide) is an active center of GOx.
However, if interfering substances, such as ascorbic acid (a major component of vitamin C), acetaminophen (a common analgesic ingredient), uric acid, protein, glucose analogs, or the like, are present in the blood or the tissue fluid and the oxidation potentials thereof are proximate to the oxidation potential of H2O2, the measurement of glucose concentration will be adversely affected. Therefore, it is difficult to ensure that the physiological parameters of a subject are truly reflected by the measurement values and to maintain a long-term stability of the measured signal when the continuous glucose monitoring system is in operation.
At present, the aforesaid shortcomings are solved, for example, by providing a polymer membrane to filter out the interfering substances. However, it remains difficult to filter out the interfering substances completely. Alternatively, a plurality of working electrodes optionally coated with an enzyme or different types of enzymes are respectively applied with potentials to read a plurality of signals from the working electrodes. The signals are then processed to accurately obtain the physiological parameter of the analyte. However, such conventional processes, which involves the use of the working electrodes, are very complicated.
In addition, stable sensing potentials can be obtained by using a silver/silver chloride as a material of the reference electrode or the counter/reference electrode. Silver chloride of the reference electrode or the counter electrode should be maintained at a minimal amount without being completely consumed, so as to permit the biosensor to be stably maintained in a test environment for measuring the physiological signal and for achieving a stable ratio relationship between the physiological signal and the physiological parameter of the analyte to be detected.
However, silver chloride would be dissolved, resulting in the loss of chloride ions, which will cause a shift of the reference potential. When the silver/silver chloride is used for the counter electrode so as to be actually involved in a redox reaction, silver chloride would be even more consumed by reduction of silver chloride to silver. Accordingly, the service life of the biosensor is often limited by the amount of silver chloride on the reference electrode or the counter electrode. The problem is addressed by many prior arts. For example, in the two-electrode system, the counter electrode has a consumption amount of about 1.73 mC/day (microcoulomb/day) under an average sensing current of 20 nA (nanoampere). That is, if the biosensor is intended to be buried under the skin of the body for continuously monitoring glucose for 16 days, a minimum consumption capacity of 27.68 mC is required. Therefore, existing technology attempts to increase the length of the counter electrode to be greater than 10 mm. However, in order to avoid being implanted deeply into subcutaneous tissue, the biosensor needs to be implanted at an oblique angle, which results in problems such as a larger wound, a higher infection risk, and the like. In addition, the pain caused by the implantation is more pronounced.
Along with the development of a miniaturized version of the continuous glucose monitoring system, development of a biosensor that can improve the measurement accuracy, extend the service life, simplify the manufacturing process, and reduce the manufacturing cost, is an urgent goal to be achieved.
Therefore, a first object of the disclosure is to provide an implantable micro-biosensor which has an accurate measurement and an extended service life, and which can monitor a physiological parameter of an analyte continuously.
A second object of the disclosure is to provide a method for manufacturing the implantable micro-biosensor.
According to a first aspect of the disclosure, there is provided an implantable micro-biosensor adapted to be implanted under skin of a body to continuously monitor a physiological parameter of an analyte in a biological fluid of the body. The implantable micro-biosensor includes a substrate, a first electrode, a second electrode, a third electrode, and a chemical reagent layer.
The substrate includes an implanting end portion which is elongated in a longitudinal direction and which is to be implanted under the skin along an implanting direction perpendicular to the skin.
The first electrode is disposed on one surface of the substrate and used as a counter electrode, and includes a front portion and a rear portion both disposed at the implanting end portion. The front portion extends along the longitudinal direction, and the rear portion extends along the longitudinal direction and away from the front portion. A sensing section of the first electrode at least includes the front portion.
The second electrode is disposed on the one surface of the substrate and spaced apart from the first electrode, and includes a sensing section disposed at the implanting end portion and having an area less than that of the sensing section of the first electrode.
The third electrode is disposed on the substrate and used as a working electrode, and includes a sensing section disposed at the implanting end portion.
The chemical reagent layer at least covers the sensing section of the third electrode so as to permit the third electrode to selectively cooperate with the first electrode or the first and second electrodes to measure a physiological signal in response to the physiological parameter of the analyte.
According to a second aspect of the disclosure, there is provided a method for manufacturing the implantable micro-biosensor, which includes the steps of:
A) providing the substrate which includes the implanting end portion;
B) forming on the one surface of the substrate the first electrode which is disposed on the one surface of the substrate and used as a counter electrode, and which includes a front portion and a rear portion both disposed at the implanting end portion, wherein the front portion extends along the longitudinal direction, and the rear portion extends along the longitudinal direction and away from the front portion, a sensing section of the first electrode at least including the front portion;
C) forming on the one surface of the substrate the second electrode which is spaced apart from the first electrode, and which includes the sensing section disposed at the implanting end portion and having the area less than that of the sensing section of the first electrode;
D) forming on the substrate the third electrode which includes the sensing section disposed at the implanting end portion; and
E) applying the chemical reagent layer to at least covering the sensing section of the third electrode.
In the implantable micro-biosensor according to the disclosure, the first working electrode, the at least one second working electrode, and the at least one counter electrode are included, and a relative position of the first sensing section and the second sensing section is assigned, such that the implantable micro-biosensor according to the disclosure not only can execute the measurement of the analyte and reduce the influence of the interfering substances, but also can regenerate silver halide by applying a potential difference to the counter electrode. Measurement of the analyte, reduction of the influence of the interfering substances, and regeneration of silver halide may be adjustably performed according to practical needs. Therefore, the implantable micro-biosensor according to the disclosure has an accurate measurement and an extended service life, and can monitor a physiological parameter of an analyte continuously.
Other features and advantages of the disclosure will become apparent in the following detailed description of the embodiments with reference to the accompanying drawings, of which:
Before the disclosure is described in greater detail, it should be noted that where considered appropriate, reference numerals or terminal portions of reference numerals have been repeated among the figures to indicate corresponding or analogous elements, which may optionally have similar characteristics.
The term “analyte” as used herein refers to any substance to be detected that exists in an organism, for example, glucose, lactose, and uric acid, but are not limited thereto. In the embodiments illustrated below, the analyte is glucose. In certain embodiments, the implantable micro-biosensor is an implantable glucose micro-biosensor, which is used for detecting a concentration of glucose in an interstitial fluid of a body. The term “a biological fluid” as used herein may be, for example, the interstitial fluid, but is not limited thereto. The term “a physiological parameter” as used herein may be, for example, a concentration, but is not limited thereto.
The term “at least one” as used herein will be understood to include one as well as any quantity more than one.
An implantable micro-biosensor according to the disclosure is adapted to be implanted under skin of a body to continuously monitor a physiological parameter of an analyte in a biological fluid of the body. The implantable micro-biosensor includes a substrate, a first electrode, a second electrode, a third electrode, and a chemical reagent layer.
The substrate includes an implanting end portion which is elongated in a longitudinal direction and which is to be implanted under the skin along an implanting direction perpendicular to the skin.
The first electrode is disposed on one surface of the substrate and used as a counter electrode, and includes a front portion and a rear portion both disposed at the implanting end portion. The front portion extends along the longitudinal direction, and the rear portion extends along the longitudinal direction and away from the front portion. A sensing section of the first electrode at least includes the front portion.
The second electrode is disposed on the one surface of the substrate and spaced apart from the first electrode, and includes a sensing section disposed at the implanting end portion and having an area less than that of the sensing section of the first electrode.
The third electrode is disposed on the substrate and used as a working electrode, and includes a sensing section disposed at the implanting end portion.
The chemical reagent layer at least covers the sensing section of the third electrode so as to permit the third electrode to selectively cooperate with the first electrode or the first and second electrodes to measure a physiological signal in response to the physiological parameter of the analyte.
In certain embodiments, the front and rear portions of the first electrode are disposed respectively proximate to two adjacent sides of the second electrode.
In certain embodiments, a total of a width of the sensing section of the second electrode and a width of the rear portion of the first electrode is less than a width of the front portion of the first electrode.
In certain embodiments, the third electrode is disposed on the other surface of the substrate opposite to the one surface of the substrate on which the first electrode is disposed.
In certain embodiments, the chemical reagent layer covers the sensing section of the third electrode and the sensing section of the first electrode.
In certain embodiments, the chemical reagent layer further covers the sensing section of the second electrode.
In certain embodiments, the second electrode is used as a reference electrode or another working electrode.
In certain embodiments, the second electrode is used as the another working electrode, and a surface material of the sensing section of the first electrode includes a silver/silver halide.
In certain embodiments, the surface material of the sensing section of the first electrode further includes a conductive material covering the silver/silver halide.
A method for manufacturing the implantable micro-biosensor according to the disclosure includes the steps of:
A) providing the substrate which includes the implanting end portion;
B) forming on the one surface of the substrate the first electrode which is disposed on the one surface of the substrate and used as a counter electrode, and which includes a front portion and a rear portion both disposed at the implanting end portion, wherein the front portion extends along the longitudinal direction, and the rear portion extends along the longitudinal direction and away from the front portion, a sensing section of the first electrode at least including the front portion;
C) forming on the one surface of the substrate the second electrode which is spaced apart from the first electrode, and which includes the sensing section disposed at the implanting end portion and having the area less than that of the sensing section of the first electrode;
D) forming on the substrate the third electrode which includes the sensing section disposed at the implanting end portion; and
E) applying the chemical reagent layer to at least covering the sensing section of the third electrode.
In certain embodiments, in step C), the second electrode is used as a reference electrode or another working electrode.
In certain embodiments, the second electrode is used as the reference electrode, and the steps B) and C) are implemented simultaneously by the sub-steps of:
a1) forming a backing material layer on the one surface of the substrate;
a2) applying a precursor material on a portion of the backing material layer;
a3) subjecting the backing material layer and the precursor material to patterning so as to divide the one surface into two areas which are separated from each other and which are free of electrical connection, one of the two areas being used for forming the first electrode, and the other one of the two areas being used for forming the second electrode, at least a portion of the precursor material being disposed on the backing material layer at the other one of the two areas; and
a4) converting the precursor material disposed at the other one of the two areas to a reference electrode material so as to form the sensing section of the second electrode.
In certain embodiments, in step a3), a portion of the precursor material is disposed at the one of the two areas, and a remaining portion of the precursor material is disposed at the other one of the two areas.
In certain embodiments, the second electrode is used as the reference electrode, and the steps B) and C) are implemented simultaneously by the sub-steps of:
b1) forming a backing material layer on the one surface of the substrate;
b2) subjecting the backing material layer to patterning so as to divide the backing material layer into two areas which are separated from each other and which are free of electrical connection, one of the two areas being used for forming the first electrode, and the other one of the two areas being used for forming the second electrode; and
b3) applying a reference electrode material on the other one of the two areas so as to form the sensing section of the second electrode.
In certain embodiments, the second electrode is used as the another working electrode, and the steps B) and C) are implemented simultaneously by the sub-steps of:
c1) forming a backing material layer on the one surface of the substrate;
c2) subjecting the backing material layer to patterning so as to divide the backing material layer into two areas which are separated from each other, one of the two areas being used for forming the first electrode;
c3) applying a precursor material on at least a portion of the backing material layer at the one of the two areas; and
c4) converting the precursor material to a reference electrode material so as to form the sensing section of the first electrode.
In certain embodiments, in sub-step a1), the backing material layer is formed as a single-layered configuration or a multi-layered configuration, each of which is made from carbon, silver, or a combination thereof.
Electrode Configuration and Manufacturing Process of Implantable Micro-biosensor:
Referring to
Referring to
The substrate 1 has a first surface 11 and a second surface 12 opposite to the first surface 11. The substrate 1 may be made of any material which is useful for making an electrode substrate and which has flexibility and insulation properties. Example of the material for making the substrate 1 may be polyester, polyimide, and the like, and combinations thereof, but are not limited thereto.
The first working electrode 2 is disposed on the first surface 11 of the substrate 1, and includes a first sensing section 20 located at the first sensing region (C) and covered by the chemical reagent layer 6, a first connecting section 21 located at the first signal connecting region (B), and a first output section 22 located at the first signal output region (A). A surface material of the first sensing section 20 at least includes a first conductive material 1C. The first sensing section 20 is driven by a first potential difference to permit the first conductive material 1C to react with hydrogen peroxide, which is a product of a reaction of the chemical reagent layer 6 with glucose, to produce a current signal. A physiological signal in response to a glucose concentration is obtained when a ratio relationship between the value of the current signal and the concentration of hydrogen peroxide is achieved.
Examples of the first conductive material 1C include carbon, platinum, aluminum, gallium, gold, indium, iridium, iron, lead, magnesium, nickel, molybdenum, osmium, palladium, rhodium, silver, tin, titanium, zinc, silicon, zirconium, combinations thereof, and derivatives thereof (for example, alloys, oxides, metal compounds, or the like). In certain embodiments, the first conductive material 1C is a noble metal, a derivative thereof, or a combination thereof.
The second working electrode 3 is disposed on the first surface 11 of the substrate 1, and includes a second sensing section 30, a second connecting section 31, and a second output section 32. The second sensing section 30 is disposed proximate to the first sensing section 20 and is located at the first sensing region (C). The second connecting section 31 is located at the first signal connecting region (B). The second output section 32 is located at the first signal output region (A). A surface material of the second sensing section 30 at least includes a second conductive material 2C. The second sensing section 30 is driven by a second potential difference to permit the second conductive material 2C to consume at least a portion of an interfering substance in the body which approaches the second sensing section 30. Examples of the second conductive material 2C may be the same as those described above for the first conductive material 1C.
Referring to
Furthermore, when the second working electrode 3 is driven by the second potential difference, the second conductive material 2C may react with hydrogen peroxide to produce another current signal, such that some of the hydrogen peroxide which should be sensed by the first working electrode 2 so as to accurately measure the concentration of the analyte is consumed by the second working electrode 3, causing a negative affect on the accurate measurement of the concentration of the analyte. Therefore, when the first conductive material 1C of the first working electrode 2 is driven by the first potential difference to have a first sensitivity in response to hydrogen peroxide and the second conductive material 2C of the second working electrode 3 is driven by the second potential difference to have a second sensitivity, the first sensitivity of the first conductive material 1C should be greater than the second sensitivity of the second conductive material 2C. Therefore, the first conductive material 1C is different from the second conductive material 2C. In certain embodiments, the first conductive material 1C may be a noble metal, such as gold, platinum, palladium, iridium, or combinations thereof. Desirably, the second conductive material 2C does not has any sensitivity to hydrogen peroxide and may be, but not limited to, carbon, nickel, copper and so on.
In Embodiment 1, the first conductive material 1C is platinum, the first potential difference ranges from 0.2 V (volt) to 0.8 V, for example, 0.4 V to 0.7 V. The second conductive material 2C is carbon. The second potential difference ranges from 0.2 V to 0.8 V, for example, 0.4 V to 0.7 V. The first potential difference may be the same as the second potential difference.
Referring to
Return to
In Embodiment 1, the material for the counter electrode 4 includes a silver/silver halide (R) so as to permit the counter electrode 4 to function as a reference electrode as well. That is, the counter electrode 4 can be cooperated with the first working electrode 2 to from a loop so as to allow the electrochemical reaction occurring at the first working electrode 2 and to provide a stable relative potential as a reference potential. A non-limiting example of the silver halide is silver chloride, and silver iodide is also available. In view to reduce the production cost and enhance the biological compatibility of the implantable micro-biosensor of the disclosure, the silver/silver halide (R) may be included only on the surface of the counter electrode 4. The silver/silver halide (R) may be blended with a carbon material (for example, a carbon paste) in a suitable ratio as long as the counter electrode 4 can execute the intended function.
The amount of the silver halide in the third sensing section 40 of the counter electrode 4 should be in a safe range, so as to avoid complete consumption of the silver halide and to permit the implantable micro-biosensor of the disclosure to be stably maintained in a test environment for measuring the physiological signal. Therefore, referring to
In addition, in order to miniaturize the implantable micro-biosensor of the disclosure and to maintain the amount of the silver halide in a safe range, a third potential difference may be applied between the counter electrode 4 and the first working electrode 2 or between the counter electrode 4 and the second working electrode 3 to permit the counter electrode 4 to have a potential higher than that of the first or second working electrode 2, 3, so as to regenerate the silver halide and to maintain the silver halide at the third sensing section 40 of the counter electrode 4 to be in a safe range. Specifically, a weight ratio of silver to silver halide may be, but is not limited to, 95 wt %: 5 wt %, 70 wt %: 30 wt %, 60 wt %: 40 wt %, 50 wt %: 50 wt, 40 wt %: 60 wt %, 30 wt %: 70 wt %, or 5 wt %: 95 wt % based on 100 wt % of a total weight of silver and silver halide. In other words, a weight ratio of the silver halide to the silver/silver halide (R) is greater than 0 and less than 1. In particular, the abovementioned weight ratio ranges between 0.01 and 0.99, more particularly, between 0.1 and 0.9, between 0.2 and 0.8, between 0.3 and 0.7, or between 0.4 and 0.6.
As described above, the chemical reagent layer 6 covers at least a portion of the first conductive material 1C of the first sensing section 20. Referring specifically to
Except for exposure of the sensing regions (including the first and second sensing regions (C, F)) for signal-sensing and the signal output regions (including the first and second signal output regions (A, D)) for signal-outputting, it is necessary to insulate the first, second, and third signal connecting sections 21, 31, 41 in the signal connecting regions (including the first and second signal connecting regions (B, E)). Therefore, the first insulation layer 71 is located at the first signal connecting region (B), and covers the first connecting section 21 of the first working electrode 2 and the second connecting section 31 of the second working electrode 3. The second insulation layer 72 is located at the second signal connecting region (E), and covers the third connecting section 41 of the counter electrode 4 on the second surface 12 of the substrate 1. The second insulation layer 72 has a length which may be the same as or different from that of the first insulation layer 71. The insulation layer unit 7 may be made of any insulation material, for example, parylene, polyimide, PDMS, LCP or SU-8 of MicroChem, and so on, but is not limited thereto. Each of the first and second insulation layers 71, 72 may have a single-layered or multi-layered configuration. The chemical reagent layer 6 may also cover a portion of the first insulation layer 71 and/or the second insulation layer 72 in addition to the first, second, and third sensing sections 20, 30, 40.
The chemical reagent layer 6, the first insulation layer 71, and the second insulation layer 72 may be covered with a polymer confinement layer (not shown), so as to confine undesirable substances from entering into the implantable micro-biosensor which may affect the measurement of the analyte.
Referring specifically to
Referring to
Referring specifically to
(A) providing the substrate 1 having the first surface 11;
(B) forming the first work electrode 2 on the first surface 11 of the substrate 1, the first work electrode 2 at least including the first sensing section 20 which includes the first conductive material 1C;
(C) forming the at least one second work electrode 3 on the first surface 11 of the substrate 1, the second work electrode 3 at least including the second sensing section 30, which is disposed proximate to at least one side of the first sensing section 20 and which includes the second conductive material 2C different from the first conductive material 1C;
(D) forming the counter electrode 4 on the substrate 1 so as to cooperate with the first work electrode 2 to measure the physiological parameter of the analyte; and
(E) forming the chemical reagent layer 6 which at least covers the first conductive material 1C of the first sensing section 20 so as to react with the analyte to generate a product.
Specifically, the first surface 11 of the substrate 1 includes the first signal output region (A), the first signal connecting region (B), and the first sensing region (C). Steps B) and C) are implemented by the sub-steps of:
(a) applying the second conductive material 2C on the first surface 11 of the substrate 1;
(b) subjecting the second conductive material 2C to patterning according to predetermined sizes, positions, lengths, areas, and the like of the first and second working electrodes 2, 3, to divide the second conductive material 2C into a first area and at least one second area that are separated from each other; and
(c) applying the first conductive material 1C at the first sensing region (C) to cover at least a portion of the second conductive material 2C at the first area to form the first sensing section 20 of the first working electrode 2 and to permit the second conductive material 2C at the at least one second area to be configured as the second working electrode 3, which includes the second signal output section 32 located at the first signal output region (A), the second signal connecting section 31 located at the first signal connecting region (B), and the second sensing section 30 located at the first sensing region (C). Therefore, both of the first and second sensing sections 20, 30 in Embodiment 1 manufactured by the abovementioned process are located at the first sensing region (C).
Specifically, referring to
In a variation of Embodiment 1, the first conductive material 1C can only cover a portion of the second conductive material 2C of the first sensing region (C) as shown in
In another variation of Embodiment 1, the first conductive material 1C may not only cover the second conductive material 2C at the first sensing region (C), but also extend to cover a portion of the second conductive material 2C at the first signal connecting region (B) by modification of sub-steps (b) and (c).
In further another variation of Embodiment 1, the second conductive material 2C at the first area may have a length less than that of the second conductive material 2C at the second area by modification of sub-step (b). For example, the second conductive material 2C at the first area may be located only at the first signal output region (A) and the first signal connecting region (B). Thereafter, the first conductive material 1C not only is formed at the first sensing region (C), but also cover the second conductive material 2C at the first signal connecting region (B) by sub-step (c), so as to permit the first sensing section 20 to be connected to the first signal output section 22.
Referring to
The positions and the areas of the first signal output region (A), the first signal connecting region (B), and the first sensing region (C) may be defined by an insulation layer. Therefore, in certain embodiments, sub-step (b) may be followed by a sub-step (b′) of forming the first insulation layer 71 on the first surface 11 of the substrate 1 so as to define the first signal connecting region (B), at which the first insulation layer 71 is located, the first sensing region (C), which is not covered by the first insulation layer 71 and which is to be implanted under the skin of the body, and the first signal output region (A), which is not covered by the first insulation layer 71 and which is to be connected to the transmitter. At the first signal connecting region (B), each of the first connecting section 21 of the first working electrode 2 and the second connecting section 31 of the second working electrode 3 has a layered configuration which at least includes a layer of the second conducive material 2C.
In certain embodiment, sub-step (b) is performed to allow the second sensing section 30 to be spaced apart from the at least one side of the first sensing section 20 by a distance of up to 0.2 mm.
In certain embodiments, sub-step (a) is implemented by a screen printing process. Sub-step (b) is implemented by an etching process, and preferably a laser engraving process. Sub-step (d) is implemented with a conductive material by a sputtering process, but preferably a plating process.
Step (E) is implemented by immersing the substrate 1 formed with the first working electrode 2, the second working electrodes 3 and the counter electrode 4 into a solution containing the chemical reagent, so as to permit the first conductive material 1C of the first sensing section 20, the second conductive material 2C of the second sensing section 30 and the third sensing section 40 of the counter electrode 4 to be covered simultaneously with the chemical agent.
In certain embodiments, before step (E), step (D′) is implemented by forming a third electrode (not shown) on the substrate 1. The third electrode is spaced apart from the counter electrode 4 and the first working electrode 2, and may be a reference electrode or a third working electrode.
In certain embodiments, step (E) may be followed by step (D″) of forming the second insulation layer 72 on the second surface 12 of the substrate 1, so as to define the second sensing region (F) on the second surface 12 of the substrate 1.
It should be understood that the process for manufacturing Embodiment 1 of the implantable micro-biosensor according to the disclosure is not limited to the aforesaid steps, sub-steps, and order, and that the order of the aforesaid steps and sub-steps may be adjusted according to practical requirements.
In the process for manufacturing Embodiment 1 of the implantable micro-biosensor according to the disclosure, two sensing sections having different materials on the surfaces thereof may be formed on a same sensing region, such that the sensing sections can be covered simultaneously with a same chemical agent layer so as to simplify the conventional process. In addition, the geometries and sizes of the first and second working electrodes 2, 3, and the clearance between the first and second working electrodes 2, 3, and the like, can be controlled precisely by the patterning process. Furthermore, the processing performed on the second surface 12 of the substrate 1 may be modified according to practical requirements.
Referring to
In order to effectively reduce the interference of the interfering substance on the measurement of the physiological signal so as to be in an acceptable error range, in Embodiment 2, the second sensing section 30 is disposed along and spaced apart from at least three sides of the first sensing section 20 by a distance. In other words, the at least three sides of the first sensing section 20 are surrounded by and spaced apart from the second sensing section 30 by the distance. In certain embodiments, the distance is up to 0.2 mm. In certain embodiments, the distance ranges from 0.02 mm to 0.05 mm. Specifically, the second sensing section 30 is disposed in a U-shaped geometry along and spaced apart from the at least three sides of the first sensing section 20. Therefore, referring to
A process for manufacturing Embodiment 2 is substantially similar to that for manufacturing Embodiment 1 except for the following differences.
In sub-step (b), the second conductive material 2C is patterned to permit the second conductive material 2C at the second area to be formed as a U-shaped geometry and to surround the second conductive material 2C at the first area. Therefore, the geometry of the second sensing section 30 and the extension of the second sensing section 30 to surround the first sensing section 20 may be modified by patterning the second conductive material 2C.
In addition, in other variations of Embodiment 2, the first and second sensing sections 20, 30 may be positioned as shown in
Referring to
Specifically, the first connecting section 21 and the first output section 22 are disposed on the second surface 12 of the substrate 1. The first sensing section 20 includes a first portion disposed on the first surface 11 of the substrate 1, a second portion disposed on the second surface 12 of the substrate 1 and extending toward the first connecting section 21, and a middle portion extending through the substrate 1 to interconnect the first and second portions.
Referring to
In Embodiment 3, the implantable micro-biosensor further includes a reference electrode 9 disposed on the second surface 12 of the substrate 1 and spaced from the counter electrode 4. A surface material of the reference electrode 9 at least includes the silver/silver halide (R). The reference electrode 9 has an area less than that of the counter electrode 4, so as to provide a sufficient capacity and to adjust the amount of the silver/silver halide (R).
Specifically, the counter electrode 4 is disposed on the second surface 12 of the substrate 1, and the third sensing section 40 of the counter electrode 4 includes a front portion 40a extending longitudinally along the second sensing region (F) and a rear portion 40b extending longitudinally toward a direction away from the second sensing region (F). In Embodiment 3, the third sensing section 40 of the counter electrode 4 is composed of the front and rear portions 40a, 40b. The reference electrode 9 is spaced apart from the counter electrode 4, and includes the fourth sensing section 90 located at the second sensing region (F). The fourth sensing section 90 has an area less than that of the third sensing section 40. Specifically, the front and rear portions 40a, 40b of the third sensing section 40 are disposed proximate to two adjacent sides of the fourth sensing section 90 of the reference electrode 9 to permit the counter electrode 4 to be configured as an L-shaped geometry. A total of the widths of the fourth sensing section 90 and the rear portion 40b of the counter electrode 4 is less than that of the front portion 40a of the counter electrode 4. In addition, the first and second insulation layers 71, 72 may have same lengths. Referring specifically to
Referring to
In another variation of Embodiment 3, at least a portion of the silver/silver halide (R) on the fourth sensing section 90 of the reference electrode 9 may be covered by the third conductive material 3C, so as to decrease the exposure area of the silver halide, thereby reducing the possibility of the silver halide being lost due to dissociation. Therefore, the side edge and/or the surface of the reference electrode 9 which is not covered by the third conductive material 3C may cooperate with the first working electrode 2 and the counter electrode 4 to conduct the measurement. In certain embodiments, the third conductive material 3C is carbon.
A process for manufacturing Embodiment 3 of the implantable micro-biosensor according to the disclosure is substantially similar to the process for manufacturing Embodiment 2 except for the following differences.
In step (D), the counter electrode 4 is formed on the second surface 12 of the substrate 1, and includes the third sensing section 40 located at the second sensing region (F). The third sensing section 40 includes the front portion 40a and the rear portion 40b.
In step (D′), the reference electrode 9 is formed on the second surface 12 of the substrate 1, and is spaced apart from the counter electrode 4. The reference electrode 9 includes the fourth sensing section 90 located at the second sensing region (F).
It is noted that, before the micro-biosensor is ready for shipping out of the plant for sale, the counter electrode 4 of Embodiment 1 or 2, or the reference electrode 9 of Embodiment 3 can have no silver halide (that is, the initial amount of the silver halide can be zero) but silver. An initial amount of the silver halide can be generated on the counter electrode 4 or the reference electrode 9 by oxidizing the silver coated on the counter electrode 4 or the reference electrode 9 during a very first replenishment period after the micro-biosensor is implanted subcutaneously into the patient and before a first measurement is proceeded. In such case, the silver is oxidized to silver ion thus to be combined with chloride ion in the body fluid to form the silver halide. The measurement can be performed after a predetermined ratio between silver and silver halide is reached.
Accordingly, referring to
(a1) forming a backing material layer (L) on the second surface 12 of the substrate 1; and
(a2) applying a reference electrode material (for example, silver-silver halide) or a precursor material (P) (for example, silver) of the reference electrode material on a portion of the backing material layer (L);
(a3) subjecting the backing material layer (L) and the reference electrode material or the precursor material (P) to patterning so as to define a third area and a fourth area which are separated from each other and which are not connected electrically to each other, the backing material layer (L) at the third area being configured as the counter electrode 4.
Specifically, the active area of the counter electrode 4 and the reference electrode 9, the cooperated configuration between the above two, the location or size of the silver-silver halide on the surface of the electrode can be easily controlled through sub-step (a2) so as to complete the manufacture of the counter electrode 4 and the reference electrode 9 and control the amount of the silver-silver halide.
Specifically, the backing material layer (L) located at the third area has a different width along a longitudinal direction of the third area. A front portion of the backing material layer (L) having a greater width is used for forming the front portion 40a of the third sensing section 40 of the counter electrode 4, and a rear portion of the backing material layer (L) having a smaller width is used for forming the rear portion 40b of the third sensing section 40 of the counter electrode 4. A portion or whole of the reference electrode material or the precursor material (P) is located at the fourth area. If the reference electrode material is applied in sub-step (a2), the fourth sensing section 90 of the reference electrode 9 is formed directly thereby. Alternatively, if the precursor material (P) is applied in sub-step (a2), an additional sub-step (a4) is implemented to convert the precursor material (P) at the fourth area to the reference electrode material to form the fourth sensing section 90 of the reference electrode 9. Referring specifically to
In Embodiment 3, a portion of the precursor material (P) is located at the fourth area, and a remaining portion of the precursor material (P) is located at the third area. In another variation of Embodiment 3, in sub-step (a3), whole of the precursor material (P) may be located at the fourth area.
In a second process for manufacturing Embodiment 3 of the implantable micro-biosensor, steps (D) and (D′) are implemented by the sub-steps of:
(b1) forming the backing material layer (L) on the second surface 12 of the substrate 1;
(b2) subjecting the backing material layer (L) to patterning to define a third area and a fourth area which are separated from each other and which are not connected electrically to each other, the backing material layer (L) at the third area being configured as the counter electrode 4; and
(b3) applying the reference electrode material or the precursor material (P) of the reference electrode material to at least a portion of the fourth area, so as to permit the fourth area to be configured as the reference electrode 9.
If the reference electrode material is applied in sub-step (b3), the fourth sensing section 90 of the reference electrode 9 is formed directly thereby.
Alternatively, if the precursor material (P) is applied in sub-step (b3), an additional sub-step (a4) is implemented to convert the precursor material (P) at the fourth area to the reference electrode material to form the fourth sensing section 90 of the reference electrode 9.
In certain embodiments, the backing material layer (L) may be formed as a single-layered configuration or a multi-layered configuration, each of which is made from carbon, silver, or a combination thereof. Specifically, the backing material layer (L) may be formed as a single-layered configuration made of carbon, such that the third sensing section 40 of the counter electrode 4 is configured as a carbon layer. Alternatively, the backing material layer (L) may be formed as a two-layered configuration, which includes a silver layer disposed on the second surface of the substrate 1 and a carbon layer disposed on the silver layer.
Referring to
In Embodiment 4, the counter electrode 4 also functions as a reference electrode, and the reference electrode 9 in Embodiment 2 is replaced with a third working electrode 5. The material and configuration for the third working electrode 5 may be the same as those described above for the first working electrode 2 or the second working electrode 3. Specifically, the configuration of the third working electrode 5 in Embodiment 4 is the same as that of the first working electrode 2 in Embodiment 1, and includes a carbon layer and a platinum layer disposed on the carbon layer. In certain embodiments, the third working electrode 5 may be disposed on the first surface 11 of the substrate 1. In other words, the third working electrode 5 and the counter electrode 4 may be disposed on the same surface or different surfaces of the substrate 1. In addition, the configuration of the third working electrode 5 is not limited to Embodiment 4 and can be arranged as Embodiment 1 shown in
Referring specifically to
In the process for manufacturing Embodiment 4, in step (D′), the third working electrode 5 is formed on the second surface 12 of the substrate 1, and is spaced apart from the counter electrode 4. The third working electrode 5 includes a fourth sensing section 50 located at the second sensing region (F). The fourth sensing section 50 is parallel to the rear portion 40b of the third sensing section 40, and is spaced apart from the front portion 40a of the third sensing section 40 along a longitudinal direction of the counter electrode 4. In other words, the counter electrode is configured as an L-shaped geometry, such that the third sensing section 40 of the counter electrode is spaced part from the fourth sensing section 50 of the third working electrode 5.
In certain embodiments, step (D) is implemented by the sub-steps of:
(c1) forming a backing material layer (L) on the second surface 12 of the substrate 1;
(c2) defining on the second surface 12 of the substrate 1, a third area and a fourth area which are separated from each other, the third area being used for the counter electrode 4, and the backing material layer (L) located at the third area has a different width along a longitudinal direction of the third area. A front portion of the backing material layer (L) having a greater width is used for forming the front portion 40a of the third sensing section 40 of the counter electrode 4, and a rear portion of the backing material layer (L) having a smaller width is used for forming the rear portion 40b of the third sensing section 40 of the counter electrode 4; and
(c3) applying the reference electrode material (for example, silver-silver halide) or the precursor material (P) (for example, silver) of the reference electrode material on at least a portion of the backing material layer (L) at the third area, and specifically, at the front portion 40a of the third sensing section 40.
If the precursor material (P) is applied in sub-step (c3), an additional sub-step (c4) is implemented to convert the precursor material (P) to the reference electrode material, so as to permit the front portion 40a of the counter electrode 4 to be used as the third sensing section 40 and to function as a reference electrode as well.
In certain embodiments, in sub-step (c1), the backing material layer (L) may be formed as a single-layered configuration or a multi-layered configuration, each of which is made from carbon, silver, or a combination thereof.
It should be understood that the counter electrode 4 may be formed as a single-, double-, or triple-layered configuration. The counter electrode 4 formed as a double-layered configuration may include a conductive material layer (for example, a carbon layer, but is not limited thereto) disposed on the substrate 1, and a layer of the silver/silver halide (R) covering the conductive material layer. The conductive material layer is provided to avoid impedance problem due to excessive halogenation of silver in sub-step (c4) or the abovementioned initial halogenation step.
When the conductive material layer is a carbon layer, another conductive material layer (for example, a silver layer) may be disposed between the second surface 12 of the substrate 1 and the conductive material layer to permit the counter electrode 4 to be formed as a triple-layered configuration, so as to reduce the high impedance problem which may occur at the second signal output region (D) when the carbon layer is disposed directly on the second surface 12 of the substrate 1.
In certain embodiments, the counter electrode 4 may be formed as a single-layered configuration. Therefore, the backing material layer (L) in sub-step (c1) may be made from the silver/silver halide, a mixture of the silver/silver halide and a conductive material (for example, carbon), or a mixture of silver and the conductive material (for example, carbon), and sub-step (c3) may be omitted. The counter electrode 4 is thus formed as a single-layered configuration including silver/silver halide or the mixture of the silver/silver halide and the conductive material (for example, carbon). The amount of the silver/silver halide present in the counter electrode 4 is not specifically limited as long as the counter electrode 4 executes the intended operation. Formation of the counter electrode 4 using the mixture of the silver/silver halide and the conductive material may alleviate the insulation problem during halogenation, the adhesion problem during lamination, and the high impedance problem of the second signal output region (D).
Similarly, in Embodiment 4, the first working electrode 2 is used for measuring the physiological signal, and the second working electrode 3 is used to reduce the interference of the interfering substance in the body to the measurement. However, regeneration of silver halide is carried out by cooperation of the third working electrode 5 with the counter electrode 4. Specifically, the third potential difference is applied between the counter electrode 4 and the third working electrode 5 to permit the counter electrode 4 to have a potential higher than that of the third working electrode 5, so as to permit the counter electrode 4 to perform an oxidation reaction to regenerate the silver halide, thereby enhancing the efficiency of the measurement, the consumption of the interference, and the regeneration of silver halide.
Referring to
In Embodiment 5, two of the second working electrodes 3, 3′ are included. Similar to the second working electrode 3 described above, the second working electrode 3′ includes a second sensing section 30′, a second connecting section 31′, and a second output section 32′. The second sensing sections 30, 30′ of the second working electrodes 3, 3′ may have the same or different lengths and/or areas. A distance between one of the two second sensing sections 30, 30′ and the first sensing section 20 may be different from that between the other one of the two second sensing sections 30, 30′ and the first sensing section 20.
A process for manufacturing Embodiment 5 of the implantable micro-biosensor according to the disclosure is substantially similar to the process for manufacturing Embodiment 1 except for the following differences.
In the process for manufacturing Embodiment 5 of the implantable micro-biosensor according to the disclosure, in sub-step (b), two of the second areas are formed to define the two second working electrodes 3, 3′, and the two second sensing sections 30, 30′ of the two second working electrodes 3, 3′ are disposed, respectively, along two opposite sides of the first sensing section 20 of the first working electrode 2.
Embodiment 4 of the implantable micro-biosensor according to the disclosure is used in Application Embodiment 1, and includes the substrate 1, the first working electrode 2, the second working electrode 3, the counter electrode 4, the third working electrode 5, and the chemical reagent layer 6. The first sensing section 20 of the first working electrode 2 includes a carbon layer, and a platinum layer covering the carbon layer. The second sensing section 30 of the second working electrode 3 is formed as a U-shaped geometry and surrounds around the first sensing section 20, and includes a carbon layer. The third sensing section 40 of the counter electrode 4 includes a carbon layer and a silver/silver chloride layer covering the carbon layer. The fourth sensing section 50 of the third working electrode 5 has a configuration which is the same as that of the first sensing section 20 of the first working electrode 2. The chemical reagent layer 6 covers the first, second, third, fourth sensing sections 20, 30, 40, 50.
Referring to
During the first time section (T1), switch S1 is switched to a close-circuit state and the first potential difference (for example, 0.5 V, but is not limited thereto) is applied between the first working electrode 2 and the counter electrode 4 to permit the first working electrode 2 to have a potential V1 higher than a potential V4 of the counter electrode 4, so as to permit the first working electrode 2 to perform the aforesaid oxidation reaction and to perform the electrochemical reaction with the chemical reagent layer 6 and the analyte to obtain the physiological signal (i1). At the same time, the counter electrode 4 carries out a reduction reaction to reduce silver chloride to silver according to an equation below.
2AgCl+2e−→2Ag+2Cl−
In addition, a value of the first time section (T1) can be a constant, such as 2.5 seconds, 5 seconds, 15 seconds, 30 seconds, 1 minute, 2.5 minutes, 5 minutes, 10 minutes or 30 minutes. Preferably, the value of the first time section (T1) is 30 seconds.
During the second time section (T2), switch S2 is switched to a close-circuit state and the second potential difference (for example, 0.5 V, but is not limited thereto) is applied between the second working electrode 3 and the counter electrode 4 to permit the second working electrode 3 to have a potential V2 higher than the potential V4 of the counter electrode 4, so as to permit the second working electrode 3 to perform a reaction on the surface thereof, thereby consuming the interfering substance.
During the third time section (T3), switch S3 is switched to a close-circuit state and the third potential difference is applied between the counter electrode 4 and the third working electrode 5 to permit the potential V4 of the counter electrode 4 to be higher than a potential V3 of the third working electrode 5, so as to permit the counter electrode 4 to perform an oxidation reaction, thereby regenerating the silver chloride by oxidizing silver to silver ions, which is then combine with chloride ions in the biological fluid to form silver chloride.
The steps of obtaining the physiological signal, consuming the interfering substance, and regenerating the silver chloride may be implemented simultaneously or separately by proper arrangement of the potentials V1, V2, V3, V4 of the first, second, and third working electrodes 2, 3, 5 and the counter electrode 4, proper arrangement of the first, second, and third potential differences, and proper switching of switches S, S2, S3. In other words, the first, second, and third time sections (T1, T2, T3) my partially or fully overlap with one another, or are free from overlapping with one another. In addition, each of the first, second, and third time sections (T1, T2, T3) may be a constant or variable time period.
Specifically, referring to
In addition, during a time interval (i.e., a corresponding one of the third time sections (T3)) between two adjacent ones of the first time sections (T1), the counter electrode 4 cooperates with the third working electrode 5 to execute the regeneration of the silver chloride. In other words, the first time sections (T1) and the third time sections (T3) do not overlap with each other.
Referring to
In Application Embodiment 2, the detecting time period (T) includes five of the first time section (T1), six of the second time sections (T2), and two of the third time sections (T3). The first time sections (T1) and the second time sections (T2) do not overlap with each other. That is to say, when the first working electrode 2 performs the measurement of the analyte during the first time sections (T1), the second working electrode 3 can be operated by implementing an open circuit or by grounding. In addition, the silver chloride regeneration action can be performed after several measurement actions or interference eliminating actions. For example, the two third time sections (T3) in Application Embodiment 2 only overlap with two of the second time sections (T2). That is to say, the silver chloride regeneration action is performed after two measurement actions and three interference eliminating actions. In addition, the first interference eliminating action may be carried out prior to the first measurement action so as to effectively avoid the interference of the interfering substance in the body to the measurement.
Referring to
In Application Embodiment 3, the detecting time period (T) includes five of the first time sections (T1), six of the second time sections (T2), and five of the third time sections (T3). The first time sections (T1) and the second time sections (T2) partially overlap with each other. The second time sections (T2) and the third time sections (T3) partially overlap with each other. The first time sections (T1) and the third time sections (T3) do not overlap with each other. Similarly, the first interference eliminating action may be carried out prior to the first measurement action so as to effectively avoid the interference of the interfering substance to the measurement. Regeneration of the silver chloride may be performed during a time interval between two adjacent ones of the first time sections (T1), so as to permit an amount of silver halide present in the third sensing section 40 of the counter electrode 4 to be maintained in a safe range.
The procedures for Application Embodiment 4 are substantially similar to those of Application Embodiment 1 except for the following differences.
In Application Embodiment 4, Embodiment 2 of the implantable micro-biosensor according to the disclosure is used, and includes the substrate 1, the first working electrode 2, the second working electrode 3, the counter electrode 4, and the chemical reagent layer 6. The first sensing section 20 of the first working electrode 2 includes a carbon layer and a platinum layer covering the carbon layer. The second sensing section 30 of the second working electrode surrounds 3 is formed as a U-shaped geometry and surrounds the first sensing section 20, and includes a carbon layer. The third sensing section 40 of the counter electrode 4 includes a carbon layer and a silver/silver chloride layer covering the carbon layer. The chemical reagent layer 6 covers the first, second, and third sensing sections 20, 30, 40. Specifically, the third working electrode 5 is not included in Embodiment 2 of the implantable micro-biosensor.
Referring to
Regeneration of the silver chloride is executed by applying the third potential difference between the counter electrode 4 and the second working electrode 3 to permit the potential V4 of the counter electrode 4 to be higher than the potential V2 of the second working electrode 3, and to permit the counter electrode 4 to function as a working electrode to perform the oxidation reaction so as to regenerate silver chloride. Specifically, switch S2 may be selectively connected to a relatively high potential (i.e., a potential higher than the potential V4 of the counter electrode 4) to allow the second working electrode 3 to execute the consumption of the interference, or a relatively low potential (i.e., a potential lower than the potential V4 of the counter electrode 4) to allow the second working electrode 3 to execute the regeneration of silver chloride.
Alternatively, referring specifically to
Referring specifically to
The operation procedures for Application Embodiment 5 are substantially similar to those of Application Embodiment 4 except for the following differences.
In Application Embodiment 5, regeneration of the silver chloride is executed by applying the third potential difference between the counter electrode 4 and the first working electrode 2 to permit the potential V4 of the counter electrode 4 to be higher than the potential V1 of the first working electrode 2. Specifically, the first working electrode 2 in Application Embodiment 5 may not only cooperate with the counter electrode 4 to consume the interference during the second time sections (T2), but also cooperate with the counter electrode 4 to regenerate the silver halide during the second time sections (T3). That is, the first working electrode 2 has two functions herein.
Referring specifically to
The in vitro elimination of the interference was carried out using the Embodiment 4 of the implantable micro-biosensor according to the operation procedures of Application Embodiment 1. The interference to be consumed was acetaminophen.
Referring to
As shown by curve 3 in
Contrarily, as shown by curve C1 and curve C2 in
The in vivo elimination of the interference was carried out using Embodiment 4 of the implantable micro-biosensor according to the operation procedures of Application Embodiment 1. The interference to be consumed was acetaminophen (i.e., medical interference). The implantable micro-biosensor cooperates with a base and a transmitter to constitute a continuous glucose monitoring system. The implantable micro-biosensor is hold on to the skin of a subject by the carrier and is partially implanted under the skin to measure a physiological signal in response to a glucose concentration. The transmitter is combined with the base and is connected to the implantable micro-biosensor so as to receive and process the physiological signal measured by the implantable micro-biosensor. The subject took two tablets of Panadol: (acetaminophen, 500 mg), and a time period of medical interference ranges from 4 to 6 hours after taking the tablets. The results are shown in
As shown in
As shown in
The aforesaid results demonstrated that when the implantable micro-biosensor of the disclosure is subjected to consumption of the interference, the error value can be reduced significantly, such that the measurement accuracy can be enhanced.
In summary, in the implantable micro-biosensor according to the disclosure, the first working electrode, the at least one second working electrode, and the at least one counter electrode are included, and a relative position of the first sensing section and the second sensing section is assigned, such that the implantable micro-biosensor according to the disclosure not only can execute the measurement of the analyte and reduce the influence of the interfering substances, but also can regenerate the silver halide by applying a potential difference to the counter electrode. Measurement of the analyte, reduction of the influence of the interfering substances, and regeneration of the silver halide can be adjustably performed according to practical needs. Therefore, the implantable micro-biosensor according to the disclosure can perform an accurate measurement of an analyte and has an extended service life, and can monitor a physiological parameter of an analyte continuously.
In the description above, for the purposes of explanation, numerous specific details have been set forth in order to provide a thorough understanding of the embodiments. It will be apparent, however, to one skilled in the art, that one or more other embodiments may be practiced without some of these specific details. It should also be appreciated that reference throughout this specification to “one embodiment,” “an embodiment,” an embodiment with an indication of an ordinal number and so forth means that a particular feature, structure, or characteristic may be included in the practice of the disclosure. It should be further appreciated that in the description, various features are sometimes grouped together in a single embodiment, figure, or description thereof for the purpose of streamlining the disclosure and aiding in the understanding of various inventive aspects, and that one or more features or specific details from one embodiment may be practiced together with one or more features or specific details from another embodiment, where appropriate, in the practice of the disclosure.
While the disclosure has been described in connection with what are considered the exemplary embodiments, it is understood that this disclosure is not limited to the disclosed embodiments but is intended to cover various arrangements included within the spirit and scope of the broadest interpretation so as to encompass all such modifications and equivalent arrangements.
This application claims priority of U.S. Provisional Application No. 62/882,162, filed on Aug. 2, 2019, and U.S. Provisional Application No. 62/988,549, filed on Mar. 12, 2020, both of which are incorporated by reference herein in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
9891185 | Feldman | Feb 2018 | B2 |
20050033132 | Shults et al. | Feb 2005 | A1 |
20130245412 | Rong et al. | Sep 2013 | A1 |
20170238851 | Duhamel et al. | Aug 2017 | A1 |
20180199873 | Wang et al. | Jul 2018 | A1 |
20190076070 | Nogueira | Mar 2019 | A1 |
20190239825 | Kumar | Aug 2019 | A1 |
Number | Date | Country |
---|---|---|
2005045413 | May 2005 | WO |
Entry |
---|
Search Report, which was issued to European counterpart Application No. 20189122.3 by the EPO dated Nov. 24, 2020. |
Number | Date | Country | |
---|---|---|---|
20210030341 A1 | Feb 2021 | US |
Number | Date | Country | |
---|---|---|---|
62988549 | Mar 2020 | US | |
62882162 | Aug 2019 | US |