In-mold labeled article and method

Information

  • Patent Grant
  • 10083634
  • Patent Number
    10,083,634
  • Date Filed
    Monday, November 15, 2010
    14 years ago
  • Date Issued
    Tuesday, September 25, 2018
    6 years ago
Abstract
A labeled article, a method of making the labeled article, and a label for use in such method, contemplate the manufacture of an article having an article body made of a moldable material, and a label, integral with the article body and having an outer label surface coplanar with the outer article body surface. The label is inserted into the mold and molded into place as the article body is molded. The label has an outer film ply defining the outer label surface, a printable sheet ply inward from said outer film ply, and an adhesive layer between the outer film ply and the printable sheet ply. The outer film ply has a length and a width greater than the length and width of the printable sheet ply. The outer film ply extends beyond the printable sheet ply adjacent all edges of the printable sheet ply and shields the printable sheet ply from exposure to the environment surrounding the labeled article.
Description
CROSS-REFERENCE TO RELATED APPLICATIONS

Not applicable.


STATEMENT REGARDING FEDERALLY SPONSORED RESEARCH OR DEVELOPMENT

Not applicable.


BACKGROUND

This relates to a labeled article which has a label applied during a molding process, and to a method of making such an article. The labeled article is highly resistant to harsh environmental conditions to which it may be subjected in use. More particularly, the labeled article resists deterioration from mechanical wear, chemicals, moisture, and abrasion.


Product manufacturers place a high value on the ability to deliver molded articles with high quality graphic surfaces. This has traditionally required a trade-off between the quality of the images, the permanence of the images, and the print media utilized. High quality graphic surfaces have been achieved by lithographically printing adhesive labels, and then applying the labels to the articles. Articles made in this way have suffered from poor label adhesion and degraded label appearance. The loss of adhesion that usually results from aging is exacerbated by environmental factors, such as moisture and large changes in temperature. This loss of adhesion is particularly acute in outdoor and automotive applications. Clearly, it is desirable that labels remain on labeled products and that the graphics on the labels remain esthetically pleasing. Further, it may also be important that the labels on the products remain attached to the products and convey needed information, such as for example product warning messages.


In-mold techniques have been developed to address these problems with articles that are manufactured in a molding process. In an in-mold labeling process, graphics, including text, are typically printed on polymer films that are compatible with the polymer material that is to be used in the molding process. It has been common to use screen-printing techniques to print on clear polymer film materials that are compatible with the polymer material from which the part is molded. The clear film allows the underlying molded polymer to show through. Many in-mold techniques have also used complex, multi-layered films to achieve a satisfactory product. The printed film label is normally placed into the mold so that the molten polymer material flows over the ink, which is trapped between the film and the polymer material. Temperatures and pressures characteristic of this technique necessitate screen printing inks that can withstand this process. The graphic detail quality achievable by these techniques is limited by the environment in which said inks must remain stable and not wash out or flow with the molten polymer. Further, screen printing by separately depositing each of a series of colors increases the cost of the product.


An improved in-mold and in-line decorating method is disclosed in U.S. Pub. App. 2007/0079928, published Apr. 12, 2007. This application teaches using a single sheet layer that allows the placement of the highest possible quality graphics into the surface of products made from a variety of moldable thermoplastic, thermoset, and vulcanizable materials using a variety of molding processes. A label-sized sheet of micro-porous material is printed using a four color process, and the printed sheet is inserted into a mold. The article is then molded, producing a finished, labeled part. While this process represents an advance over the prior art, the surface of the micro-porous sheet is exposed to the environment to which the article is subjected.


It is desired that a labeled article and method of making the article be provided in which the labeled article resists deterioration from exposure to a harsh environment.


SUMMARY

This need is met by a labeled article, a method of making the labeled article, and a label for use in such method, in which a label is molded into the article at the time that the article is molded. The labeled article includes an article body made of a moldable material, having an outer article body surface, and a label, integral with the article body, having an outer label surface that is generally coplanar with the outer article body surface. The label comprises an outer film ply defining the outer label surface, a printable sheet ply inward from the outer film ply, and an adhesive layer between the outer film ply and the printable sheet ply. The outer film ply has a length and width greater than the length and width of the printable sheet ply such that the outer film ply extends beyond the printable sheet ply adjacent all edges of the printable sheet ply and shields the printable sheet ply from exposure to the environment.


The adhesive layer may be a UV curable adhesive. Alternatively, the adhesive layer may be an IR curable adhesive. The printable sheet may be made of a sheet of micro-porous material. The printable sheet may be made of a dimensionally stable, single layer, micro-porous polyethylene film. The label is permanently fused to the article body during the manufacture of the article. The printable sheet ply is printed on the surface thereof facing the outer film ply, such that the printing is visible through the adhesive and the outer film ply.


The printable sheet ply may carry ink jet printing, laser printing, flexographic printing, gravure printing, letterpress printing, intaglio printing, thermal printing, or screen printing.


The method of making the labeled article may comprise the steps of positioning a label in a mold, supplying curable material to the mold, curing the curable material, and ejecting the article from the mold to produce a labeled article. The label comprises an outer film ply defining the outer label surface, a printable sheet ply inward from the outer film ply, and an adhesive layer between the outer film ply and the printable sheet ply. The outer film ply has a length and width greater than the length and width of the printable sheet ply such that the outer film ply extends beyond the printable sheet ply adjacent all edges of the printable sheet ply. The label is positioned with the outer label surface in contact with the mold surface. The outer film ply of the label is generally coplanar with the outer surface of the article, and the outer film ply shields the printable sheet ply from exposure to the environment surrounding the labeled article.


The adhesive layer between the outer film ply and the printable sheet ply may comprise a UV curable adhesive. Alternatively, the adhesive layer between the outer film ply and the printable sheet ply may comprise an IR curable adhesive. The printable sheet may be made of a sheet of micro-porous material. The printable sheet may be made of a sheet of a dimensionally stable, single layer, micro-porous polyethylene film. The step of curing the curable material may include the step of permanently fusing the label to the article body. The printable sheet ply may be printed on the surface thereof facing the outer film ply, such that the printing is visible through the adhesive and the outer film ply. The step of supplying curable material to the mold may includes the step of supplying curable material to a blow mold. The step of supplying curable material to the mold may include the step of supplying curable material to an injection mold. The step of supplying curable material to the mold may include the step of supplying curable material to a compression mold.


A label for in-mold application to a molded article, comprises an outer film ply defining an outer label surface, a printable sheet ply inward from the outer film ply made of a sheet of micro-porous material, and an adhesive layer between the outer film ply and the printable sheet ply. The adhesive is formed of an adhesive which is not reactivated or softened from heating produced during curing of moldable material in a mold. The outer film ply has a length and width greater than the length and width of the printable sheet ply such that the outer film ply extends beyond the printable sheet ply adjacent all edges of the printable sheet ply. The outer film ply shields the printable sheet ply from exposure to the environment surrounding the labeled article. The sheet of micro-porous material may be made of a dimensionally stable, single layer, micro-porous polyethylene film. The adhesive layer may be a UV curable adhesive or an IR curable adhesive. The printable sheet ply may be printed on the surface thereof facing the outer film ply, such that the printing is visible through the adhesive and the outer film ply.





BRIEF DESCRIPTION OF THE DRAWINGS


FIG. 1 is a perspective view of an exemplary labeled article, illustrated as an automobile battery; and



FIG. 2 is a partial, sectional view, taken generally along line 2-2 in FIG. 1, showing an in-mold label applied to the labeled article of FIG. 1.





DETAILED DESCRIPTION

Reference is made to FIG. 1, which shows a labeled article, namely an automobile battery having a first label 12 on a side surface 14 of the battery casing 16, and a second label 18 on the top surface 20 of the battery casing 16. The labels 12 and 18 may carry graphics, brand indicia, and information explaining use restrictions, warnings, and warranty provisions, as well as other information. In the past, it has been common to secure labels of this type to battery casings using adhesives, such as for example pressure sensitive adhesives. The environment to which automobile batteries are exposed during use is quite severe. Most printing inks and substrates are discolored or damaged by occasional and frequent exposure to the elements. It is common for printing inks and adhesive layers to deteriorate in such settings. Testing has demonstrated that chemical resistance at elevated temperatures is difficult to achieve.


Some label manufacturers have used film-rated inks and over-laminates on plastic films to make a durable top surface on batteries. However the acid, or other chemicals, and moisture can seep under the peripheral edges of these constructions, resulting in de-lamination of the label and discoloration of the ink on the label. Since these are pressure sensitive adhesive constructions, there is always an exposed edge where this can occur. The labeled article construction and method, described below, are based on in-mold label technology. By having an overlapping clear top film, as explained below, the edges of the label are sealed and the acid, chemicals, and moisture cannot penetrate the edge of the label. Because of the construction of the label, laminating adhesive and printing ink on the label are not attacked by corrosive material found in the environment of a typical automobile engine compartment.


Reference is made again to FIG. 1, as well, as FIG. 2, in which it will be seen that the article body comprises the casing 16, which is made of a moldable material, and which has an outer article body surface, such as surface 14. The label 12 is integral with the article body 16 and, as shown in FIG. 2, has an outer label surface 22 that is coplanar with the outer article body surface 14. The label 12 has an outer film ply 24 defining the outer label surface 22, a printable sheet ply 26 inward from the outer film ply 24, and an adhesive layer 28 between the outer film ply 24 and the printable sheet ply 26. The outer film ply 24 has a length and width that are greater than the length and width of the printable sheet ply 26 such that the outer film ply 24 extends beyond the printable sheet ply 26 adjacent all edges of the printable sheet ply 24 and shields the printable sheet ply 24 from exposure to the environment surrounding the labeled article 10.


The adhesive layer 28 may be a UV curable adhesive. Alternatively, the adhesive layer may be an IR curable adhesive. With either adhesive, it will be appreciated that it is important that the adhesive chosen not soften significantly when exposed to heat after it is cured, since, as explained below, the label 12 is applied to the article 10 in an in-mold process. The label 12 is permanently fused to the article body during the in-mold manufacture of the article. The printable sheet 26 may be made of a sheet of micro-porous material, such as a dimensionally stable, single layer, micro-porous polyethylene film.


The printable sheet ply 26 is printed on the surface 30 facing the outer film ply 24. Since the outer film ply 24 is transparent, the printing on the sheet ply 26 is visible through ply 24. The adhesive 28 is also transparent, at least with the thickness of the adhesive layer 28, such that the printed information on the labeled article labels can be readily seen by an observer. The ink on the surface 30 may be applied by any of a number of techniques. For example, the ink may be applied by ink jet printing, laser printing, flexographic printing, gravure printing, letterpress printing, intaglio printing, or screen printing. It is only required that the ink be stable when subjected to the temperatures found in the molding process.


The labeled article, such as the battery casing 16, is made through a process including the steps of positioning a label 12 in a mold, supplying curable material to the mold, curing the curable material, and ejecting the article from the mold to produce a labeled article in which the outer film ply 24 of the label 12 is generally coplanar with the outer surface 14 of the article 10, and in which the outer film ply 24 shields the printable sheet ply 26 from exposure to the environment surrounding the labeled article 10. The label comprises an outer film ply 24 defining the outer label surface 22, a printable sheet ply 26 inward from the outer film ply 24, and an adhesive layer 28 between the outer film ply 24 and the printable sheet ply 26. The outer film ply 24 has a length and width greater than the length and width of the printable sheet ply 26 such that the outer film ply 24 extends beyond the printable sheet ply adjacent all edges of the printable sheet ply 26. It will be appreciated that the label 12 is positioned in the mold with the outer label surface 22 in contact with the inner surface of the mold. The adhesive 28 will have been cured prior to the in-mold operation so that it remains dimensionally stable during molding. This curing will have been accomplished by subjecting the adhesive to UV radiation or IR radiation, depending on the type of adhesive selected. The printable sheet 26 will have been previously printed, and is made of a sheet of micro-porous material, such as a dimensionally stable, single layer, micro-porous polyethylene film. Such film permits the curing of the material making up the article to permanently fuse the label to the article body. The printable sheet ply carries printed indicia and graphics on the surface 30 thereof facing the outer film ply 24, such that the printing is visible through the adhesive 28 and the outer film ply 24.


The specific molding operation utilized to produce the labeled article having an in-mold label may be any of a number of known molding process for forming articles from a thermoplastic moldable material. For example, the article may be made through processes that include blow molding, injection molding, or compression molding.


It will be appreciated that the use of a clear overlapping film laminated to a dimensionally smaller printable ply that is molded onto the body of the article, thereby forming sealed edges, achieves highly desirable results. The extended film keeps corrosive materials, such as acid, chemicals and moisture, away from the printed ply and the adhesive. This arrangement provides an exceptional resistance to chemical attack. It will be appreciated that this arrangement will find wide application with all types of articles that are produced through a molding process and which are subjected to challenging conditions in use.

Claims
  • 1. A labeled article, comprising: an article body made of a moldable material, having an outer article body surface, anda label, integral with said article body, having an outer label surface coplanar with said outer article body surface, said label comprising: an outer, transparent, film ply defining said outer label surface,a printable sheet ply inward from said outer film ply, said printable sheet ply having a surface facing the outer film ply and being printed thereon, anda transparent adhesive layer between said outer film ply and said printable sheet ply, said outer film ply having a length and width greater than the length and width of said printable sheet ply such that said outer film ply extends beyond said printable sheet ply adjacent all edges of said printable sheet ply and shields said printable sheet ply from exposure to the environment surrounding said labeled article, the surface of said printable sheet ply opposite said surface facing the outer film ply being substantially free of adhesive and permanently fused to said article body.
  • 2. The labeled article of claim 1, in which said adhesive layer is a UV curable adhesive.
  • 3. The labeled article of claim 1, in which said adhesive layer is an IR curable adhesive.
  • 4. The labeled article of claim 1, in which said printable sheet is made of a sheet of micro-porous material.
  • 5. The labeled article of claim 1, in which said printable sheet is made of a dimensionally stable, single layer, micro-porous polyethylene film.
  • 6. The labeled article of claim 1, in which said label is permanently fused to said article body during the manufacture of said article.
  • 7. The labeled article of claim 1, in which said printable sheet ply carries ink jet printing.
  • 8. The labeled article of claim 1, in which said printable sheet ply carries laser printing.
  • 9. The labeled article of claim 1, in which said printable sheet ply carries flexographic printing.
  • 10. The labeled article of claim 1, in which said printable sheet ply carries gravure printing.
  • 11. The labeled article of claim 1, in which said printable sheet ply carries letterpress printing.
  • 12. The labeled article of claim 1, in which said printable sheet ply carries intaglio printing.
  • 13. The labeled article of claim 1, in which said printable sheet ply carries thermal printing.
  • 14. The labeled article of claim 1, in which said printable sheet ply carries screen printing.
  • 15. A label for in-mold application to a molded article, comprising: a transparent, outer film ply defining an outer label surface,a printable sheet ply inward from said outer film ply made of a sheet of micro-porous material, said printable sheet ply having a surface facing the outer film ply and being printed thereon, anda transparent adhesive layer between said outer film ply and said printable sheet ply formed of an adhesive which is not reactivated from heating produced during curing of moldable material in a mold,said outer film ply having a length and width greater than the length and width of said printable sheet ply such that said outer film ply extends beyond said printable sheet ply adjacent all edges of said printable sheet ply and shields said printable sheet ply from exposure to the environment surrounding said labeled article, the surface of said printable sheet ply opposite said surface facing the outer film ply being substantially free of adhesive.
  • 16. The label for in-mold application to a molded article according to claim 15 in which said sheet of micro-porous material comprises a sheet made of a dimensionally stable, single layer, micro-porous polyethylene film.
  • 17. The label for in-mold application to a molded article according to claim 15 in which said adhesive layer is a UV curable adhesive.
  • 18. The label for in-mold application to a molded article according to claim 15 in which said adhesive layer is an IR curable adhesive.
US Referenced Citations (102)
Number Name Date Kind
4321404 Williams et al. Mar 1982 A
4330578 Nishihira et al. May 1982 A
4369157 Conner Jan 1983 A
4418033 Hatakeyama Nov 1983 A
4427615 Eskesen Jan 1984 A
4544184 Freund et al. Oct 1985 A
4574366 Potember et al. Mar 1986 A
4621837 Mack Nov 1986 A
4650533 Parker et al. Mar 1987 A
4808366 Kaminski et al. Feb 1989 A
4861644 Young et al. Aug 1989 A
4892779 Leatherman et al. Jan 1990 A
4904324 Heider Feb 1990 A
4983348 Barresi et al. Jan 1991 A
5172936 Sullivan et al. Dec 1992 A
5227222 Ogawa et al. Jul 1993 A
5324567 Bratchley et al. Jun 1994 A
5338396 Abdala et al. Aug 1994 A
5401457 Valyi Mar 1995 A
5435963 Rackovan et al. Jul 1995 A
5492370 Chatwin et al. Feb 1996 A
5512227 Grazioli Apr 1996 A
5514427 Ellison et al. May 1996 A
5522623 Soules et al. Jun 1996 A
5536539 Ellison et al. Jul 1996 A
5591384 Abrams et al. Jan 1997 A
5626339 Schickert et al. May 1997 A
5629029 Souder et al. May 1997 A
5637329 Abrams et al. Jun 1997 A
5658672 Lenke et al. Aug 1997 A
5676981 Miyazawa et al. Oct 1997 A
5686504 Ang Nov 1997 A
5698283 Yamasaki et al. Dec 1997 A
5705255 Grazioli Jan 1998 A
5707472 Smith Jan 1998 A
5711839 Dronzek, Jr. Jan 1998 A
5795527 Nakamura et al. Aug 1998 A
5800757 Abrams et al. Sep 1998 A
5897741 Mills et al. Apr 1999 A
5914170 Rabe et al. Jun 1999 A
5935692 Smith Aug 1999 A
5937554 Haugk et al. Aug 1999 A
5951055 Mowry, Jr. Sep 1999 A
6001292 Atake Dec 1999 A
6004682 Rackovan et al. Dec 1999 A
6007759 Ten Tije et al. Dec 1999 A
6025068 Pekala Feb 2000 A
6028518 Rankin et al. Feb 2000 A
6089611 Blank Jul 2000 A
6106110 Gundjian et al. Aug 2000 A
6107920 Eberhardt et al. Aug 2000 A
6114023 Schwarz et al. Sep 2000 A
6117264 Brewster Sep 2000 A
6165576 Freedman et al. Dec 2000 A
6234536 Pittman et al. May 2001 B1
6236753 Inamoto May 2001 B1
6280544 Fox et al. Aug 2001 B1
6319682 Hochman Nov 2001 B1
6357799 Shibata et al. Mar 2002 B1
6417904 Yamaoka et al. Jul 2002 B1
6494943 Yu et al. Dec 2002 B1
6544634 Abrams et al. Apr 2003 B1
6569280 Mehta et al. May 2003 B1
6661339 Muirhead Dec 2003 B2
6692799 Waller, Jr. Feb 2004 B2
6837959 Daems et al. Jan 2005 B2
6898458 Zeng et al. May 2005 B2
6943678 Muirhead Sep 2005 B2
6990723 Hoogland Jan 2006 B1
7119129 Krohn Oct 2006 B2
7166249 Abrams et al. Jan 2007 B2
7259856 Kachanov et al. Aug 2007 B2
7369048 Freund May 2008 B2
7377859 Reardon May 2008 B2
7806158 Freund Oct 2010 B2
7927688 Abrams et al. Apr 2011 B2
20020103439 Zeng et al. Aug 2002 A1
20020195195 Grabau et al. Dec 2002 A1
20030136503 Green et al. Jul 2003 A1
20030173717 Abrams et al. Sep 2003 A1
20030222100 Husband et al. Dec 2003 A1
20040074973 Schneck et al. Apr 2004 A1
20040083918 Jack May 2004 A1
20040094949 Savagian et al. May 2004 A1
20040168618 Muirhead Sep 2004 A1
20040209063 Gallagher et al. Oct 2004 A1
20040224786 Reardon Nov 2004 A1
20040238098 Bleckmann et al. Dec 2004 A1
20040238623 Asp Dec 2004 A1
20050100751 Nishizawa et al. May 2005 A1
20050184505 Barlow Aug 2005 A1
20050237184 Muirhead Oct 2005 A1
20050241548 Muirhead Nov 2005 A1
20060086013 Stegman et al. Apr 2006 A1
20060176180 Freund Aug 2006 A1
20070079928 Abrams et al. Apr 2007 A1
20070154677 Abrams et al. Jul 2007 A1
20070243367 Nagatake et al. Oct 2007 A1
20070254126 Lilienthal Nov 2007 A1
20080145611 Mess et al. Jun 2008 A1
20080173405 Freund Jul 2008 A1
20080176011 Abrams et al. Jul 2008 A1
Foreign Referenced Citations (11)
Number Date Country
10220502 Nov 2003 DE
1 824 673 Aug 2007 EP
1 910 981 Apr 2008 EP
2 327 906 Feb 1999 GB
10128789 May 1998 JP
2007006502 Sep 2007 MX
9532088 Nov 1995 WO
9815414 Apr 1998 WO
03069552 Aug 2003 WO
2006060043 Jun 2006 WO
2007064361 Jun 2007 WO
Non-Patent Literature Citations (8)
Entry
International Search Report and Written Opinion dated Jun. 30, 2006 pertaining to International application No. PCT/US05/27387.
International Search Report and Written Opinion dated Oct. 9, 2007 pertaining to International application No. PCT/US06/24709.
Supplementary European Search Report dated Jul. 15, 2009 pertaining to EP application No. 05778217.9.
IBM Technical Disclosure Bulletin; Mar. 1, 1996; pp. 129-130; vol. 39, Issue #3; 0018-8689-39-3-129.
Office Action pertaining to U.S. Appl. No. 12/056,682 dated Jun. 10, 2009.
Office Action pertaining to U.S. Appl. No. 12/056,682 dated Dec. 29, 2009.
Interview Summary pertaining to U.S. Appl. No. 12/056,682 dated Jul. 29, 2010.
Supplementary European Search Report dated Oct. 18, 2010 in reference to co-pending European Patent Application No. 06847448.5.
Related Publications (1)
Number Date Country
20120119482 A1 May 2012 US