The present invention relates to timing systems, visual indicators and devices and methods for making the same. More specifically, the invention relates to systems, devices and methods of indicating and/or recording; the passage of a duration of time.
There are a number of different timing systems and devices, generally referred to as time-temperature indicators (TTIs), which can be used to monitor the exposure of objects to a range of temperatures over a specified period of time. Time-temperature indicators can have a number of different applications for indicating when an event or activity needs to take place. For example, time-temperature indicators have applications for indicating when the perishable materials have expired and need to be thrown out. Time-temperature indicators also have applications for general inventory management, for monitoring projects, activities and a host of other time and/or temperature dependent events. Therefore, there is a continued need to develop reliable timing systems and devices which can be used for a variety of different applications.
Color changing labels exist which utilize an electro-chemical reaction to deplete a thin metallic film which upon depletion allows for a visual discernment of whatever resides beneath. Such labels are manufactured in a variety of configurations but may suffer from manufacturing, depletion, and depletion problems. Additionally, such device may be unduly susceptible to unwanted external variables.
The present invention is directed to electrochemical indicators for indicating a variable such as time and/or a temperature excursion. In some embodiments, the electrochemical indicators comprise an anode layer and a cathode layer which contact an electrolyte to activate each indicator. In some embodiments, the electrochemical indicator comprises an electrically isolated RFID chip and/or an RFID antenna which are placed in electrical communication in response to the external variable. The completed RFID tag may then be read by a RFID reader. A completed RFID tag may also be incorporated within the electrochemical indicators comprising an anode layer and a cathode layer and where the RFID tag is unshielded and becomes readable as the indicator expires.
In one aspect, an electrochemical timing device comprises a lens for viewing a expiration of the timing device, a base, a cathode layer coupled to the lens and the base; an anode layer comprising a plurality of coated non-metalized sections and coupled to the lens and the base, and an electrolyte, wherein the timing device is activated when the electrolyte comes into contact with the anode layer and the cathode layer, and wherein the electrolyte is prevented from migrating past an edge of depletion by the coated non-metalized sections of the anode layer after the timing device is activated. The anode layer is uniformly depleted from the leading edge across the anode layer. In some embodiments, the electrolyte comprises an unactive solid state that becomes active when the electrolyte liquefies. In these embodiments, the electrolyte liquefies at a predefined temperature activating the device. In some embodiments, one or more of a color, text, and a graphic is uncovered as the timing expires. An RFID antenna may be unshielded to radio frequency as the timing device expires and can be read for temperature excursion information of the timing device. In some embodiments, the device comprises one or more temperature dependent regulators for increasing an accuracy of the device. In some embodiments, the anode layer comprises one or more wedge-shaped plates with an electrolyte ingress point at a smaller end of each plate.
In another aspect, an electrochemical timing system comprises a lens, a base, a plurality of electrically segregated anode cells deposited between the lens and the base and a common cathode layer which covers an entire surface area of the plurality of anode cells. Cell segregation may be accomplished by etching a sheet of anode material to separate the anode material into the plurality anode cells. In some embodiments, the timing system is activated by introducing a quantity of electrolyte into the system. In some embodiments, the plurality of anode cells are sealed in a manner to allow ingress by an electrolyte at a discrete point. In further embodiments, each of the plurality of anode cells comprises a temperature dependent resistor (TDR). The plurality of anode cells may be coated with a UV activated liquid. In some embodiments, the plurality of anode cells are sequentially activated.
In a further aspect, an electrochemical timing system comprises an anode layer, a cathode layer, a quantity of electrolyte, wherein when the electrolyte contacts the anode layer and the cathode layer the timing system is activated and the anode layer begins to deplete in a direction away from an edge of depletion, and an RFID tag underlying the anode layer. In some embodiments, the RFID antenna is unshielded and becomes readable as anode layer is depleted. In some embodiments, the timing system is configured to indicate a temperature excursion. The electrolyte is able to comprise an unactive solid state electrolyte that liquefies at a predefined temperature to become active and activate the device. In some embodiments, an RFID antenna of the RFID tag is electrically decoupled from an RFID antenna. In some of these embodiments, a temperature activated switch of the RFID tag changes state when the timing system reaches a defined temperature causing the RFID tag to become active or non-active. In some embodiments, the temperature activated switch comprises a low melting point substance. In some of these embodiments, the low melting point substance does not conduct between contacts when solid and conducts between contacts when in a liquid state. Alternatively, in some embodiments, the low melting point substance conducts between contacts when solid and does not conduct between contacts when in a liquid state.
Reference will now be made in detail to implementations of indicators for external variables consisting of singular and multiple depletion cells. Each indicator may be configured to indicate a passage of time. Additionally, each indicator may be configured with an applicator to be used as a label and/or attached to an additional object. In the interest of clarity, not all of the routine features of the implementations described herein are shown and described. It will, of course, be appreciated that in the development of any such actual implementation, numerous implementation-specific decisions must be made in order to achieve the developer's specific goals, such as compliance with application and business related constraints, and that these specific goals will vary from one implementation to another and from one developer to another. Moreover, it will be appreciated that such a development effort might be complex and time-consuming, but would nevertheless be a routine undertaking of engineering for those of ordinary skill in the art having the benefit of this disclosure.
Referring now to
In some embodiments, the electrochemical depletion of the thin film anode 103 occurs because the anode 103 is at least partially immersed within the electrolyte 107. The timing system 100 depletes from a bottom of the body 101 up toward a lens 109 with depletion occurring across the entire footprint of the thin film anode 103 at one time. Problems may arise however, in that during the final stages of anode 103 depletion, needed electron paths may brake. From the oxidation process of the anode layer 103 these electron paths become broken and electrical paths needed for the electrons to flow to the cathode 105 are severed. Consequently, islands of un-depleted anode material 103 are left. The result is a visual obscurement limiting the effectiveness of the timing device 100. Particularly, the un-depleted anode layer 103 may block the visual change and may also be used as a shield against RF radiation from contacting an underlying RFID antenna. In such cases, un-depleted anode islands also hinder RF radiation exposure by the RFID antenna.
In some instances a depletion of a thin film anode layer occurs from one cell and progresses to adjacent cells within a timing system comprising multiple cells. In such cases, the cells may have been defined and/or physically segregated by cathode material. Within a multiple cell configuration, many slivers of cathode material are then needed to be assembled within the timing system. The manufacturing of such comb-like cathode material presents a challenge.
The timing system 300 consists of a common cathode layer 305 without separation, running the length of, or covering the entire surface area of the anode cells 309. The anode cell 309 definition or segregation is accomplished by the laser etching 315 of the anode layer 301 to create the anode cells 309 which are electrically separated into cells and/or segments. Etching replaces segregating the cells 309 by assembling the comb-like slivers of cathode material in order to separate the anode cells 309.
As described above, the anode cells 309 are defined by electrically segregating the anode material 303 which has been thin film deposited onto an internal side of an overlying lens material 317. The cells 309 are laser etched into specific shapes by etching the anode material 303 to electrically separate the cells 309 into the desired shapes. Additionally, the cells 309 are sealed in such a manner to allow an ingress by an electrolyte only where desired. In some embodiments, the cell 309 shape and the area of ingress 313 are strategically placed such that a more rapid depletion of the anode cells 309 or specific pattern of depletion will occur. In such a case, each cell (being defined as only having one temperature dependent resistor (TDR) in series with the cathode) sometimes referred to as an eCell, may have multiple ingress points 313. Each eCell may have a separate TDR with an independent resistant value. This allows for a more rapid or slower depletion of adjacent cells 309, by increasing or decreasing the value of resistance within the TDR. In this way a more rapid or slower visual change can be accomplished.
Referring now to
In the step 430, the thin-film anode layer is coated with a UV liquid that hardens under exposure to ultraviolet radiation. Specifically, the etched thin-film anode layer is coated on the metal side with the UV liquid. Then, in the step 440, the coating is exposed to UV radiation. Once an even and thin coating of the UV liquid is achieved, a pattern is prescribed by exposing only portions of the coating to UV radiation. Methods of limiting UV exposure to specific patterns of the thin-film layer may include rotating a drum whose surface consists of a mask which would allow for the transference of UV radiation except for the prescribed areas. The anode cell layer, coated with the UV activated liquid would be in contact with the drum's external side and rotated with the drum such that when the UV radiation source emanates from the center of the drum, radiation transfers through the mask to the external layer hardening the UV liquid. Unhardened liquid is then washed from the layer leaving a UV coating in the prescribed pattern. Other manufacturing processes may include using LDPE however, with a UV laser running at reduced power levels so that it renders the UV liquid cured. These methods can achieve micron level accuracy at very high speeds and allow for miniaturization of an electro-chemical time temperature indicator (eTTI).
A common cathode may reside adjacent to the electrochemical cells or run the length and width of all the cells. Since edge depletion is preferred, the bottom portion of the cells are coated with an insulating material where insulation from the electrolyte is desired and leaving openings where desired. Such openings then provide ingress for the electrolyte to deplete the anode horizontally from an edge.
For example, as shown within
When the hardened UV coating contacts an area of the anode cell layer 503 which has had the Al etched off, a seal is created, limiting access/ingress to by the electrolyte once the device 500 is in operation. When the hardened UV coating 519 comes in contact with the Al coating, as opposed to areas where the Al has been etched off, an electrolyte “ingress” point 513 is created.
Within a multi-cell configuration, the shape of each cell is important. As shown in
With edge depletion a certain amount of time is required for anode material to deplete from a point “A”, on a horizontal plane, to a point “B” on the same plane. The time it takes for depletion to travel this distance is usually referred to as the “timing mechanism” of the cell. With edge depletion, the internal resistance (RID) of the cell is partially dependent upon the distance from the leading edge (depletion edge) of the anode to the cathode. As depletion occurs this resistance becomes greater, as does the internal resistance. The current produced by the cell then decreases as depletion proceeds. Since, in some embodiments, the depletion rate relative to temperature is controlled by a temperature dependant material placed in series within the external electron return path which regulates current flow. Any internal fluctuation in current, not dependent upon temperature changes, e.g. fluctuation in current due to increasing resistance caused by the increase in distance between the anode and cathode, will render the timing mechanism inaccurate.
In some embodiments, the RID is mitigated by increasing the exposure of anode material to the electrolyte, by progressively increasing the size of the anode layer the further the depletion migrates away from the cathode. Since the maximum current capacity of the Galvanic cell will be achieved when the anode and cathode (plates) have approximately the same surface area, any reduction in plate size of one over the other will render a reduction in current flow. In this embodiment depletion begins with the size of one over the other will render a reduction in current flow. In this embodiment depletion begins with the plates being different sizes with the cathode being much larger than the anode and as RID increases, tending to increase current flow. In this way the current within each cell does not change due to RID and is therefore only changed by external temperature dependent material.
As shown within
In some multi-cell embodiments, the anode layer in each cell is configured with one or more wedge-shaped plates with ingress points located toward the smaller end of each plate.
Accuracy tolerance and repeatability in performance of timing systems/labels of this type is important. One of the factors which contributes to such accuracy is resistance imposed by the TDR placed within the electron return path between a cathode layer and an anode layer. Highly accurate means exist for mixing compounds to make up the TDR. Measuring and placing such compounds within timing devices may prove more challenging though with the existing methods of application such as ink jet and other types of printing. Since resistances associated with the TDR are comprised of parallel resistance values of a column of TDR material, diameter and shape of a printed TDR would need to be held to a tighter tolerance than what might be available through ink jet printing. One embodiment includes a means to mitigate unacceptable tolerances in application of TDR material. Within the center layer which lays between a top lens layer and a bottom base layer, a series of holes are placed. This example is illustrated in
As shown within
In the past electro-chemical color changing labels have been activated by introducing an electrolyte into a compartment containing the cathode and the anode. Once the electrolyte comes into contact with the electrodes, a galvanic action is initiated. Labels may need to be held in inventory or on the shelf for some period of time prior to activation. Problems regarding excessive costs may arise from having to manufacture holding reservoirs, which prevent the electrolytes from coming in contact with the electrodes until activation. Such reservoirs need to contain the electrolyte for the period of time on the shelf and be able to manipulated in such a way as to release the electrolyte upon activation. Typically, the method of activation for such reservoirs is mechanical rupture. In some embodiments, UV radiation is used to degrade the material used for the containment of the reservoir ending in rupture.
During manufacturing the timing device is flooded with an ion-free solution. This ion-free solution will not interact chemically or electro-chemically with the electrodes. As a result, a shelf life of the label may remain indefinite. As described above, the salt crystals are placed onto the base layer which is positioned within the flooded compartment and coated with the weak and brittle material. In some embodiments, the salt crystals are placed within a wafer coated with a weak and brittle material and which resides within the flooded compartment. Activation occurs by bending the wafer or coated salt until its weak and coated encapsulate has ruptured which allows the ion-free solution to come into contact with and dissolve the exposed salt. The ion-free solution becomes ion rich and the cell becomes activated.
Some applications of time temperature indicators require providing more information than simple time and temperature. They may, for example, require recording of extraordinary temperature readings known as excursions which may occur within the timing period. Temperature points of interested excursions are defined and designed into the devices in advance. One important temperature point is termed “freeze/thaw” and occurs at zero degrees centigrade. In the past electro-chemical time temperature indicators (eTTI) labels utilized the expansion properties of freezing water to activate a cell. A droplet of water is encapsulated and upon freezing, expands and ruptures its capsule. This in turn causes the rupture of an electrolyte capsule or dissolves a salt resulting in the activation of the excursion cell. Other temperature points are of interest for recording excursions as well.
Products, perishable or pharmaceuticals may have critical “not-to-exceed” temperatures which must be monitored. In such cases, materials with specific melting points are used to activate an excursion cell. Polyethelye Glycol (PEG) for instance, may exist with different molecular lengths. Progressively longer chain lengths yield properties with progressively higher viscosities even to the melting point of a solid. PEG has been used as an electrolyte itself. When the solid form is used, it must be melted before it becomes an electrolyte suitable for the eTTI to become activated. Since it melts at a specific temperature it is used as the means for activating an excursion cell. Materials including PEG are utilized which have varying melting points to activate excursion cells at different temperature points in this way.
In other embodiments, excursion cell activation may occur electronically by reversing a direction of the electrical current. In this embodiment, an electronic circuit known as a Wheatstone Bridge (
In another embodiment, three of the resistors are matched and only one resistor comprises TDR material and in such case the polarity changes when the TDR value becomes greater or less than the opposing resistor. An unlimited number of temperature excursion points can be defined in this way, activating an unlimited number of excursion cells at temperatures above or below the excursion point. During manufacturing, the application of TDRs within the eTTIs is simple and straightforward as compared to fabricating and inserting capsules of water and simpler than inventorying and inserting PEG of varying molecular chains. In addition, this electronic method lends itself to miniaturization more readily than the others.
Anode depletion as a result of each excursion can also be suspended with any of the methods, as described above. Since the anode is conductive it can also be used as an electrical trace or path for galvanic activities related to an excursion. Eliminating any portion of such a trace will suspend galvanic activities associated with the excursion. Such a trace can be eliminated by a depletion of the main anode material.
Within devices having multiple cells it may be desirable to initiate activation of cells sequentially where the completion of one cell initiates activation of an adjacent cell, such as described in relation to
In another embodiment, multiple eCells are allowed to come into contact with a common electrolyte where each subsequent cell is subjected to an electrical charge of reversed polarity which is equal and opposite from that which the eCell is producing itself. In such a case, the eCell is held in suspense preventing depletion of the anode layer. Once an electrical connection equal and opposite to the charge is broken anode depletion can occur and the eCell becomes active. In such an embodiment, the equal and opposite charge is created by eCells housed within the same device. In some embodiments, the polarity is reversed using a Wheatstone Bridge, such as described above.
As described above, with edge depletion a certain amount of time is required for anode material to deplete from a point “A”, on a horizontal plane, to a point “B” on the same plane. The time it takes for depletion to travel this distance is usually used as the “timing mechanism” of the cell. Of course, this time is also dependent upon the resistance values involved with the circuit both internally and externally. Internal resistances, involving an electrolyte can be engineered at the time of manufacture. External resistance properties with regards to the series resistor, typically, TDR can be engineered as well. In some embodiments, a timing mechanism can be engineered to span months or longer. Within the same device some cells may be required to change suddenly over the course of hours. This poses a challenge in that sudden depletion may be desired within a cell utilizing slow depletion as its timing mechanism and while using the same electrolyte, anode material and common cathode. This scenario may occur when a single cell is utilized having a longer timing mechanism but with a sudden visual change at the end of the timing period.
One method of accomplishing a more rapid depletion rate is to include multiple electrolyte ingress points into the same cell within the area designed to change suddenly, thus initiating depletion at multiple points.
In another embodiment, internal resistance is reduced in the area desired to change suddenly. This may be accomplished by exposing anode material to cathode material, which is closer in proximity to the anode.
In a further embodiment, the electrolyte is allowed to enter a previously dry compartment of the cell, thus allowing the anode and cathode to be in electrical contact. Yet still electrolyte may be allowed to enter a wet, however ion free, compartment allowing the anode and cathode to become in electrical contact.
Another embodiment includes two eCells electrically opposed to each other with opposite polarities and when such opposition is reversed, depletion becomes electrically supported with the desired depletion becoming accelerated. The galvanic action of one cell accelerates the depletion of another cell. Such a method may use a Wheatstone Bridge, such as described above, whereby the polarity of the cell is reversed due to an intentionally caused “imbalance” of resistances within the bridge.
Radio Frequency Identification Devices (RFID) typically transmit binary sets of numbers upon activation. This set of numbers is usually programmed into the chip in advance. Some devices contain their own power supply and some acquire power externally from absorption of radio frequency radiation by an exposed antenna. Antennas of these devices are typically tuned to resonate only to a narrow range of carrier frequencies that are centered on the designated RFID systems frequency. Data contained within the device intended to be transmitted is usually limited to that which was programmed initially, and does not change Such devices are typically unable to sense changes in external variables like temperature, radiation, humidity, etc.
Most metals will shield radio frequency (RF) radiation. In some embodiments, anode material is composed of metal, not limited to metallic aluminum. Aluminum film is used in RF shielding of sensitive electronics in many industries and fields. Since an intact anode within an eLabel or eCell consists of RF shielding material, RF sensitive materials or components can be shielded from RF radiation. Shielding can remain intact until the anode becomes depleted to the point that RF radiation is no longer shielded.
In one embodiment, RFID antennas are placed behind an undepleted anode such that the Al, or other metal anode shields the antenna from RF radiation. As the anode depletes, RF shielding diminishes and it allows RF radiation to come into contact with the antenna, or portion of the antenna which is no longer shielded, thus activating and reading a passive RFID antenna and/or reading an active RFID antenna. One or more antennas may be placed in this shielded position such that when the anode depletion exposes the antennas they become active. In such a case, the RFID antenna may be electrically isolated from the anode layer and from any galvanic action. In this way, a third dimension may be added to the RFID because one or multiple RFIDs become active as a function of some external variable such as temperature, radiation, or humidity, etc. For example, a human inspecting a series of products may use an RFID reader to determine that product XX has exceeded a maximum temperature limit of YY, or that product ZZ is 50% into its degradation cycle.
In another embodiment, a depleting anode may be used to expose increasing portions of an RFID antenna such that it becomes tuned to resonate to a different range of carrier frequencies such that the change in carrier frequency becomes representative of the external variable being sensed by the eLabel device.
In yet another embodiment, a depleting anode will deplete an electrical trace such that the anode material becomes orphaned or electrically decoupled. When such orphaned anode material overlays the cathode material a capacitor with a specific value may remain. Since capacitors are often used in tuning electrical circuits, including some RFID antennas the capacitor created by a depleting anode can be used as components in circuits that generate data representative of external variables such as temperature, humidity, or radiation, etc.
In some embodiments, a depleting anode may expose a two-dimensional or three-dimensional bar code, which can then be read by an electronic bar-code reader.
The depleting anode may reveal a change in color as well as an RFID antenna. Any color layer may consist of a non-shielding material. In this way the device may reveal a color change upon anode depletion as well as a radio frequency response from an RFID antenna as time and or other variable progress. In such case, for example, a human inspecting a series of products may wish to electronically read the RFID tags which visually indicate a change in an external variable. This method may save incalculable time and cost with such data acquisition.
In further embodiments, a top shielding material is chemically dissolved revealing an RFID or its antenna. For example, as shown in
In yet another embodiment, an RFID tag is deposited directly onto a thin-film metallic coating of dissimilar material than the antenna itself and of a material which is anodic relative to the material making up the antenna. In such a case the materials are in electrical contact with one another. Once the two dissimilar materials come in contact with a common electrolyte, galvanic action initiates with the anodic material “anode” depleting away from the cathodic “cathode” “antenna” material. Since both the anode and the cathode material are conductive and in electrical contact with each other and receptive to RF radiation, the antenna is not electrically presented independently and therefore will not allow for prescribed absorption of RF radiation, or prescribed transmission of data from the RFID. Once electrical contact is severed between the anode “thin-film” coating and the cathode “RFID antenna” prescribed RF radiation absorption takes place as well as prescribed transmission of data. Depletion of the anode occurs rapidly immediately adjacent to the cathode severing electrical contact. Numerous methods and processes exist for deposition of possible cathode material onto thin-film coated anode material which are not limited to evaporative techniques, sputter, silk screen, direct printing and photo lithography.
When such an embodiment is combined with a timing mechanism such as shown in
In another embodiment, temperature excursions alone, without the element of time, can be detected and logged.
In some embodiments, remaining anode material is electrically connected with independent cathode material resulting in continued depletion of the anode material, even after the cathode RFID antenna has been electrically decoupled from the anode material. In some embodiments, an RFID temperature excursion indicator uses the cathode as a ground plane for the RFID antenna.
In further embodiment, such as shown in
In a further embodiment, such as shown in
In some embodiments, the low melting point substance 1721 is used as the temperature activated switch to couple and decouple the RFID antenna. For example, one embodiment uses a substance which is normally non-conductive, electrically open, which has a salt added to it. When in the solid state the salt is crystallized and the substance is non-conductive. When the substance melts, the solid dissolves and the liquid substance becomes ionized and therefore conducts and is able to pass current. Other methods may include using acids, bases or ionic liquids as the substance. In some embodiments, a low melting point metallic substance is used such that the switch is normally closed but becomes electrically open once the metallic substance melts. A temperature activated switch can be used to couple and/or decouple an antenna or multiple antennas from a RFID tag or RFID tags and may also modify a pattern of the antenna to modify its response frequency. In such case, exposure to numerous temperature events can be recorded.
In further embodiments, contact closure of a switch is accomplished by incorporating the expansion properties vs. the temperature properties of a material, such that when the temperature increases, the material expands. As the material expands, it physically closes a normally open switch in series with the RFID antenna. Once the switch is closed, the RFID becomes active. In some embodiments, the switch is momentary and is held closed for as long as the critical temperature remains. In alternative embodiments, the switch becomes latched and will not decouple after, no matter the temperature excursion. In further embodiments, as the expanding material expands, it contacts multiple electrical contact points with each contact point leading to a different antenna and/or an expansion of the same antenna. In this way the same RFID may transmit multiple different frequencies and at different temperature points.
In some embodiments, the expanding material comprises a non-conductive material with a conductive trace and attached contact point. Alternatively, in some embodiments, the expanding material comprises a conducting metal.
In some embodiments, as shown within
In some embodiments, one or multiple temperature points are detected by the same RFID by using multiple tuned to different center frequencies. In some embodiments, such as shown within
In some embodiments, the expanding qualities of a freezing liquid are used to close a switch completing a circuit in series with an RFID antenna. In this way a freeze alter indicator may be incorporated with an RFID tag. As shown within
Upon freezing, the water solidifies and expands and as it does it pushes the plunger 2037 out of the tube 2035. As the plunger 2037 is pushed from the tube 2035, the end of the plunger 2037 pushes on the open switch which is connected in series with the RFID antenna 2010. Once the expanding water/ice expands far enough, the switch is closed completing the circuit and the RFID becomes active. The RFID remains active until the water melts and the plunger 2037 is retracted into the tube 2035. When configured with a latch, the switch will stayed in the closed position. Alternatively, when configured without a latch, the switch will return to the open configuration. In this manner, the RFID may alarm momentarily of a freezing situation or latch permanently indicating that the RFID tag has experienced a freezing condition.
In some embodiments, as depicted in
In operation, the timing devices and/or the temperature indicators as described above have many advantages. As described above sensing materials of varying types are able to be incorporated within the timing device to indicate a total elapsed time including a time of exposure to a temperature and an environmental attribute. Additionally, the indicators may consist of singular and multiple depletion cells. Additionally, each indicator may be configured with an applicator to be used as a label and/or attached to an additional object. Further, each indicator may be implemented with one or multiple RFID tags tuned to different center frequencies. The RFID tags are activatable to indicate an exposure of the device to an attribute and for a defined period of time. The above devices have applications for marking when any number of different events need to take place and/or for timing the duration of any number of different events. For example, the timing device has applications for indicating when perishable materials have expired and need to be thrown out, indicating the age of inventory and managing when the inventory needs to be rotated, tracking a deadline and a host of other time and/or temperature dependent events. As such, the indicating devices and systems as described herein have many advantages.
The present invention has been described in terms of specific embodiments incorporating details to facilitate the understanding of the principles of construction and operation of the invention. As such, references, herein, to specific embodiments and details thereof are not intended to limit the scope of the claims appended hereto. It will be apparent to those skilled in the art that modifications can be made in the embodiments chosen for illustration without departing from the spirit and scope of the invention.
This patent application claims priority under 35 U.S.C. 119(e) of the the U.S. provisional patent application, Application No. 62/047,595, filed on Sep. 8, 2014, and entitled “eLabel electro-chemical-time/temperature indicator (eTTI), Generic indicator (GI) for external variables consisting of a singular or multiple eCells”, the U.S. provisional patent application, Application No. 62/049,308, filed on Sep. 11, 2014, and entitled “eLabel electro-chemical-time/temperature indicator (eTTI), Generic indicator (GI) for external variables consisting of a singular or multiple eCells”, and the U.S. provisional patent application, Application No. 62/050,586, filed on Sep. 15, 2014, and entitled “eLabel electro-chemical-time/temperature indicator (eTTI), Generic indicator (GI) for external variables consisting of a singular or multiple eCells”, which are all hereby incorporated in its entirety by reference.
Number | Name | Date | Kind |
---|---|---|---|
2651755 | Triplett | Sep 1953 | A |
3119754 | Blumenfeld et al. | Jan 1964 | A |
3138686 | Mitoff | Jun 1964 | A |
3210662 | Steinmetz et al. | Oct 1965 | A |
3336212 | Nicholas | Aug 1967 | A |
3512049 | Hoberman | May 1970 | A |
3543582 | Sessler | Dec 1970 | A |
3564347 | Peck | Feb 1971 | A |
3613002 | Trenkler et al. | Oct 1971 | A |
3638120 | Jost | Jan 1972 | A |
3768015 | Moser | Oct 1973 | A |
3849657 | Hamblem | Nov 1974 | A |
3942467 | Witonsky | Mar 1976 | A |
3967579 | Seiter | Jul 1976 | A |
3974495 | Jones | Aug 1976 | A |
3977900 | Luehrs | Aug 1976 | A |
3999946 | Patel et al. | Dec 1976 | A |
4044707 | Bryne | Aug 1977 | A |
4084511 | Svrjcek | Apr 1978 | A |
4100490 | Peck | Jul 1978 | A |
4153345 | Duchene et al. | May 1979 | A |
4212153 | Kydonieus et al. | Jul 1980 | A |
4277974 | Karr et al. | Jul 1981 | A |
4308486 | Gange | Dec 1981 | A |
4314874 | Abe et al. | Feb 1982 | A |
4327117 | Lenack et al. | Apr 1982 | A |
4392236 | Sandstorm et al. | Jul 1983 | A |
4408557 | Bradley | Oct 1983 | A |
4431313 | Hemperly | Feb 1984 | A |
4488780 | Nicholson | Dec 1984 | A |
4505595 | Rose et al. | Mar 1985 | A |
4527522 | Cerny | Jul 1985 | A |
4629330 | Nichols | Dec 1986 | A |
4646066 | Baughman | Feb 1987 | A |
4797864 | Stano et al. | Jan 1989 | A |
4804275 | Kang et al. | Feb 1989 | A |
4844622 | Weiss | Jul 1989 | A |
4860269 | Hennings et al. | Aug 1989 | A |
4929090 | Grahm | May 1990 | A |
5034233 | McCoy, Jr. | Jul 1991 | A |
5045283 | Patel | Sep 1991 | A |
5053339 | Patel | Oct 1991 | A |
5085802 | Jalinski | Feb 1992 | A |
5182212 | Jalinski | Jan 1993 | A |
5254473 | Patel | Oct 1993 | A |
5317987 | Muller | Jun 1994 | A |
5339024 | Kuo et al. | Aug 1994 | A |
5368905 | Ohno | Nov 1994 | A |
5396177 | Kuo | Mar 1995 | A |
5418086 | Bailey | May 1995 | A |
5420000 | Patel et al. | May 1995 | A |
5446705 | Haas | Aug 1995 | A |
5544925 | Ikeda | Aug 1996 | A |
5555223 | Barainsky | Sep 1996 | A |
5602804 | Haas | Feb 1997 | A |
5633835 | Haas et al. | May 1997 | A |
5667303 | Arens et al. | Sep 1997 | A |
5672465 | Patel et al. | Sep 1997 | A |
5673028 | Levy | Sep 1997 | A |
5699326 | Haas et al. | Dec 1997 | A |
5709472 | Prusik et al. | Jan 1998 | A |
5719828 | Haas et al. | Feb 1998 | A |
5756356 | Yangai et al. | May 1998 | A |
5785354 | Haas | Jul 1998 | A |
5797344 | Rothschild et al. | Aug 1998 | A |
5802015 | Rothschild et al. | Sep 1998 | A |
5822280 | Haas | Oct 1998 | A |
5830683 | Hendricks et al. | Nov 1998 | A |
5912759 | Good et al. | Jun 1999 | A |
5930023 | Mitchell, Jr. et al. | Jun 1999 | A |
5930206 | Haas et al. | Jul 1999 | A |
5947369 | Frommer et al. | Sep 1999 | A |
5959295 | Braun | Sep 1999 | A |
5989852 | Hendricks et al. | Nov 1999 | A |
5997927 | Gics | Dec 1999 | A |
6042264 | Prusik et al. | Mar 2000 | A |
6103351 | Ram et al. | Aug 2000 | A |
6113857 | Manico et al. | Sep 2000 | A |
6198701 | De Jonghe et al. | Mar 2001 | B1 |
6243192 | Mitchell, Jr. et al. | Jun 2001 | B1 |
6244208 | Qiu et al. | Jun 2001 | B1 |
6269764 | Adamy et al. | Aug 2001 | B1 |
6285492 | Good et al. | Sep 2001 | B1 |
6295252 | Holt et al. | Sep 2001 | B1 |
6331076 | Coll | Dec 2001 | B1 |
6373786 | Kagan et al. | Apr 2002 | B1 |
6426503 | Wuest | Jul 2002 | B1 |
6435128 | Qiu et al. | Aug 2002 | B2 |
6452873 | Holt et al. | Sep 2002 | B1 |
6544925 | Prusik et al. | Apr 2003 | B1 |
6750458 | Rourk | Jun 2004 | B1 |
6801477 | Braunberger | Oct 2004 | B2 |
6826119 | Fortune | Nov 2004 | B2 |
6968804 | Barbieri | Nov 2005 | B1 |
6974249 | Fair | Dec 2005 | B1 |
7079452 | Harrison | Jul 2006 | B2 |
7215976 | Brideglall | May 2007 | B2 |
7254095 | Braunberger | Aug 2007 | B1 |
7294379 | Ko et al. | Nov 2007 | B2 |
7362663 | Kagan | Apr 2008 | B2 |
7372780 | Braunberger | May 2008 | B1 |
7463558 | Braunberger | Dec 2008 | B2 |
7476874 | Patel | Jan 2009 | B2 |
7489596 | Kuczynski | Feb 2009 | B2 |
7589331 | Havens | Sep 2009 | B2 |
8018347 | Tehrani et al. | Sep 2011 | B2 |
8077553 | Braunberger | Dec 2011 | B2 |
8503269 | Braunberger | Aug 2013 | B2 |
8717854 | Braunberger | May 2014 | B2 |
8727209 | Shih | May 2014 | B1 |
8800472 | Park | Aug 2014 | B2 |
9188962 | Braunberger | Nov 2015 | B2 |
20030053377 | Spevacek | Mar 2003 | A1 |
20030104353 | Brielmeier et al. | Jun 2003 | A1 |
20030104848 | Brideglall | Jun 2003 | A1 |
20030112711 | Braunberger | Jun 2003 | A1 |
20030151985 | Braunberger | Aug 2003 | A1 |
20030152483 | Munagavalasa et al. | Aug 2003 | A1 |
20040092023 | Wright | May 2004 | A1 |
20040232052 | Call et al. | Nov 2004 | A1 |
20050248455 | Pope et al. | Nov 2005 | A1 |
20050276165 | Chien | Dec 2005 | A1 |
20060145091 | Patel | Jul 2006 | A1 |
20060145863 | Martin et al. | Jul 2006 | A1 |
20060227669 | Pennaz | Oct 2006 | A1 |
20060260534 | Petrakis | Nov 2006 | A1 |
20070064541 | Kagan | Mar 2007 | A1 |
20070089433 | McDonell et al. | Apr 2007 | A1 |
20070268785 | Braunberger | Nov 2007 | A1 |
20080023362 | Genosar | Jan 2008 | A1 |
20080043804 | Goldsimth et al. | Feb 2008 | A1 |
20080210152 | Robinson et al. | Sep 2008 | A1 |
20090010304 | Skinner et al. | Jan 2009 | A1 |
20090016176 | Braunberger | Jan 2009 | A1 |
20090266291 | Braunberger | Oct 2009 | A1 |
20090303041 | Tehrani et al. | Dec 2009 | A1 |
20100149929 | Braunberger | Jun 2010 | A1 |
20100219351 | Roberts et al. | Sep 2010 | A1 |
20100251955 | Knoll | Oct 2010 | A1 |
20100275835 | Su et al. | Nov 2010 | A1 |
20110017123 | Maschietti et al. | Jan 2011 | A1 |
20110037541 | Johnson et al. | Feb 2011 | A1 |
20110084128 | Haarer et al. | Apr 2011 | A1 |
20110096388 | Agrawal | Apr 2011 | A1 |
20110286314 | Braunberger | Nov 2011 | A1 |
20120256727 | Moore, Jr. | Oct 2012 | A1 |
20130107676 | Braunberger | May 2013 | A1 |
20160012310 | Kozicki | Jan 2016 | A1 |
Number | Date | Country |
---|---|---|
200182006 | Nov 2001 | WO |
2003052524 | Jun 2003 | WO |
2004077172 | Sep 2004 | WO |
2009038806 | Mar 2009 | WO |
20100099340 | Sep 2010 | WO |
2011098830 | Aug 2011 | WO |
Entry |
---|
International Search Report and Written Opinion from the International Application No. PCT/US18/17861. |
Number | Date | Country | |
---|---|---|---|
20160070237 A1 | Mar 2016 | US |
Number | Date | Country | |
---|---|---|---|
62050586 | Sep 2014 | US | |
62049308 | Sep 2014 | US | |
62047595 | Sep 2014 | US |