The present invention relates to induction heat-seal liners for sealing the mouth of a container and a method of manufacture. In one embodiment, a heat-seal liner allows an aroma of a product in the container to permeate the seal, and/or allows visual detection of the product, while maintaining the barrier properties of the seal and preventing leakage of the substance from the container. In another embodiment, a dual heat-seal liner having a dispensing aperture is provided that heat seal bonds to both the cap and container to form a non-removable closure assembly that protects the metal-foil layer from degradation by the product being dispensed.
Seals have been used on containers for many years, to prevent leakage or contamination of the substance within the container and to increase the shelf life of the product. For example, seals are used on containers for cosmetics, foods, drinks, medicines and other items in the form of creams, gels, powders, or liquids. Seals used for this purpose are typically placed over the opening of the container or, in some instances, within the cap on the container.
However, consumers often want to smell items having a fragrance or aroma, such as lotions, creams, body washes, shampoos, deodorants, perfumes, laundry detergents, air fresheners, coffee and spices, before purchasing the items. As a result, many products are sold today without seals because there is no commercially viable seal on the market that allows consumers to smell the scent of the product within the container. Specifically, prior art seals are essentially hermetic seals intended to prevent leakage of the product from the container and to limit air flow into and out of the container to preserve the product and maximize the product's shelf life. In so doing, they trap the scent or aroma of the product within the container.
As a result, scented products are often sold in containers without seals, so that consumers can remove the cap and smell the scent prior to purchase. The fact that many scented products are still sold in containers without seals today is evidence that the prior art seals do not allow adequate scent permeation and prevent leakage in a cost effective manner.
The absence of a seal increases the possibility of spillage during transportation and the chances that a product may be tampered with or tainted prior to sale to the consumer. It is not uncommon for consumers to go beyond simply removing the cap and smelling the item, by actually applying some of the product onto their body to sample the product and its fragrance. In so doing, the consumer may stick their fingers into the substance or on the opening where the substance comes out. Oftentimes, after sampling the product, the consumer closes the cap and returns the container to the shelf in the store.
This sampling of the product causes several problems. From the consumer's perspective, by placing their fingers into the substance and/or coming in contact with the opening where the substance comes out, the sampler may be contaminating the substance and spreading germs/bacteria. Additionally, each time a consumer samples the product and then returns it to the shelf, the volume of the substance within the container decreases. As a result, the consumer that eventually purchases the product is unknowingly purchasing less than a full container of a product that may have been contaminated and/or contain germs/bacteria.
From the retailer's perspective, consumers that sample products and then return them to the shelf sometimes do not place the cap on tightly, which may result in spillage if the container is tilted or falls on its side. Additionally, the shelf life of the substance within the container may be reduced or altered by the absence of a seal on the container or having been opened and exposed to the surrounding environmental conditions by a sampling consumer prior to sale. Also, the absence of a seal on a container may result in the substance contacting and/or accumulating within the cap on the container, which may cause spillage when the cap is removed and a less appealing presentation to the consumer. These situations may result in the retailer being unable to sell the product or generating product returns or charge-backs, which may have an adverse effect on the retailer's, product manufacturer's or distributor's reputation and financial performance. Additionally, the retailer, manufacturer and/or distributor may incur liability if a consumer is harmed by the contaminated product.
In one embodiment of the invention, an induction heat-seal liner is provided that allows a scent or aroma from a product to be detected through the seal, and/or allows a visual inspection of the product to be made through the seal, while the seal remains secured to the container. In another embodiment, a dual heat-seal liner having a dispensing aperture is provided that heat seal bonds to both the cap and container to form a non-removable closure assembly that protects the metal-foil layer from degradation by the product being dispensed.
In one embodiment of the invention, an induction heat-seal liner is provided comprising:
a top closure-facing layer, a bottom heat-seal bonding layer, and an intermediate metal-foil layer disposed in a thickness direction between the top and bottom layers,
the top, bottom and intermediate layers being bonded to form an integral induction heat-seal liner,
the metal-foil layer having a central opening surrounded by a metal-foil portion configured to lie above a container rim surrounding an open mouth of a container body, and the bottom layer having a heat-seal bonding area configured to lie above the container rim that is activated by heating of the metal-foil portion to induction heat-seal the bonding area to the container rim.
In one embodiment,
the liner has a central portion, aligned in the thickness direction with the central opening of the metal-foil layer, comprising one or more materials or spaces that provide visibility into and/or aroma penetration from the open mouth of the container, allowing visible detection of and/or aroma detection of a product in the container body.
In one embodiment,
one or both of the top and bottom layers fills or partially fills the central opening of the metal-foil layer.
In one embodiment,
the integral liner comprises an adhesive, extrusion or thermally laminated body.
In one embodiment,
the liner is an adhesive laminated body and includes adhesive between one or more of the top, intermediate and bottom layers, and the adhesive fills or partially fills the central opening of the metal-foil layer.
In one embodiment,
the central liner portion is clear or translucent to permit visible detection of the product in the container body.
In one embodiment, a method of forming the liner comprises:
a) providing the metal-foil layer having the central opening; and subsequently
b) laminating the metal-foil layer between the top and bottom layers to form the integral liner.
In one embodiment,
the laminating step comprises adhesive laminating the metal-foil layer between the top and bottom layers.
In one embodiment,
during the laminating step adhesive layers fills or partially fills the central opening of the metal-foil layer.
In one embodiment,
the providing step includes providing a support layer having a central opening, and
the laminating step includes disposing the metal-foil layer and the support layer with their central openings aligned between the top and bottom layers to form the integral liner.
In one embodiment,
the providing step includes providing a sheet comprising the metal-foil layer and a sheet comprising the support layer, and forming the central openings through both sheets simultaneously.
In one embodiment, the method of forming the liner comprises:
a) providing top, intermediate and bottom sheets for forming the top, intermediate and bottom layers respectively;
b) laminating the sheets together to form a laminated composite sheet with the intermediate sheet laminated between the top and bottom sheets; and
c) forming individual liners from the laminated composite sheet by cutting through the composite sheet in a thickness direction.
In one embodiment, the central opening in the metal foil layer is formed prior to the laminating step.
In one embodiment, during the laminating step the central opening is wholly or partially filled in.
In one embodiment, the method is a sequential in-line method including steps of:
prior to the laminating step, forming the central openings for a plurality of liners in the intermediate sheet;
the laminating step comprises feeding the sheets through one or more roller pairs for laminating the sheets together to from the laminated composite sheet;
the forming step comprises cutting through the laminated composite sheet in the thickness direction to form the plurality of liners.
In one embodiment, the steps of forming the central openings and cutting to form the individual liners each comprise hole punching.
In one embodiment, the central opening and individual liner are formed simultaneously.
According to another embodiment of the invention, a dual induction heat-seal liner is provided comprising:
a top closure-facing heat-seal bonding layer, a bottom heat-seal bonding layer, and an intermediate metal-foil layer disposed in a thickness direction between the top and bottom layers,
the top, bottom and intermediate layers being bonded to form an integral dual induction heat-seal liner,
the metal-foil layer having a central opening surrounded by a metal-foil portion configured to lie above a container rim surrounding an open mouth of a container body, and the bottom layer having a heat-seal bonding area configured to lie above the container rim that is activated by heating of the metal-foil portion to induction heat-seal the bottom layer bonding area to the container rim,
the liner having a central through-hole aligned in the thickness direction and extending through the central opening of the metal-foil layer and though the top and bottom layers,
the top closure-facing layer having a heat-seal bonding area to induction heat-seal the top layer bonding area to an inner surface of a closure, thus heat-seal bonding the liner to both the container rim and the closure inner surface, while allowing a product to be dispensed through the open mouth of the container, the central through-hole of the liner, and out of a dispensing aperture of the closure.
In one embodiment,
one or both of the top and bottom layers partially fills the central opening of the metal-foil layer to form a perimeter of the central-though hole that prevents contact between the product and the metal-foil layer.
In one embodiment,
the integral liner comprises an adhesive, extrusion or thermally laminated body.
In one embodiment,
the liner has a circular or a multi-sided perimeter.
In one embodiment,
the liner is an adhesive laminated body and includes adhesive between one or more of the top, intermediate and bottom layers, and the adhesive partially fills the central opening of the metal-foil layer to form a perimeter of the central though-hole that prevents contact between the product and the metal-foil layer.
In one embodiment, a method of forming the liner is provided comprising:
a) providing the metal-foil layer having the central opening; and subsequently
b) laminating the metal-foil layer between the top and bottom layers to form the integral liner.
In one embodiment,
the laminating step comprises adhesive laminating the metal-foil layer between the top and bottom layers.
In one embodiment,
during the laminating step adhesive partially fills the central opening of the metal-foil layer to form a perimeter of the central though-hole that prevents contact between the product and the metal-foil layer.
In one embodiment,
the providing step includes providing a support layer having a central opening, and
the laminating step includes disposing the metal-foil layer and the support layer with their central openings aligned between the top and bottom layers to form the integral liner.
In one embodiment,
the providing step includes providing a sheet comprising the metal-foil layer and a sheet comprising the support layer, and forming the central openings through both sheets simultaneously.
In one embodiment, a method of forming the dual induction heat-seal liner is provided comprising:
a) providing top, intermediate and bottom sheets for forming the top, intermediate and bottom layers respectively;
b) laminating the sheets together to form a laminated composite sheet with the intermediate sheet laminated between the top and bottom sheets; and
c) forming individual liners from the laminated composite sheet by cutting through the composite sheet in a thickness direction.
In one embodiment, the central opening in the metal foil-layer is formed prior to the laminating step.
In one embodiment, during the laminating step the central opening is partially filled to form a perimeter of the central though-hole that prevents contact between the product and the metal-foil layer.
In one embodiment, the method is a sequential in-line method including steps of:
prior to the laminating step, forming the central openings for a plurality of liners in the intermediate sheet;
the laminating step comprises feeding the sheets through one or more roller pairs for laminating the sheets together to from the laminated composite sheet;
the forming step comprises cutting through the laminated composite sheet in the thickness direction to form the plurality of liners.
In one embodiment, the steps of forming the central openings and cutting to form the individual liners each comprise hole punching.
In one embodiment, the central through-holes and individual liners are formed simultaneously.
In one embodiment, the method includes subsequent to forming the central openings, forming the through-holes, followed by forming the liners.
The above and further advantages and features of various embodiments of the invention will be understood by referring to the following description in conjunction with the accompanying drawings in which:
a top closure-facing layer 20, a bottom heat-seal bonding layer 30, and an intermediate metal-foil layer 40 disposed in a thickness direction (TD) between the top and bottom layers,
the top, bottom and intermediate layers being bonded to form an integral induction heat-seal liner 10,
the metal-foil layer 40 having a central opening 42 surrounded by a continuous metal-foil portion 44 configured to lie above a container rim 82 surrounding an open mouth 84 of a container body 86, and the bottom layer 30 having a heat-seal bonding area 32 configured to lie above the container rim 82 that is activated by heating of the continuous portion 44 to heat-seal bond the bottom layer 30 to the container rim 82.
As shown in
In various embodiments, the top, intermediate and bottom component layers 20, 40, 30 may each comprise a single layer, or multiple layers; they may include adhesive layers for adhesively laminating the layers together to form the integral liner 10, as described hereinafter (adhesive layers A shown in
As shown in
The cap 60 is sized to cover the open mouth 84 of the container 80; the cap includes a cylindrical top wall 61 having a peripheral sidewall 64 extending downwardly from the outer periphery of the top wall 61. The inner surface 64IS of the cap sidewall, and the outer surface 840S of the container mouth, include complimentary threads 64THR and 84THR that are disposed in a radial space RS between 64IS and 84OS. In use, the liner 10 is disposed in the cap 60 adjacent the inner top wall 62, and the cap is then twisted down onto the container rim 82 by threadably engaging 64THR and 84THR to secure the liner between the cap inner wall 62 and the container rim 82. The sealed container 80 can be readily opened (e.g. by the consumer) by untwisting the cap (in the opposite direction) to unthread 64THR and 84THR, allowing the consumer to remove the cap and then remove the heat-seal liner 10 by peeling the liner from the rim (this later step may be aided by providing a pull tab (e.g., 314 as shown in
The liner of the present embodiment provides a number of advantageous features that will now be described. One feature of the liner is to provide the metal-foil layer 40 with a central opening 42 (a through hole in the thickness direction TD); this positions the peripheral metal-foil area 44 (surrounding the central opening 42) where it is most useful for induction heating, i.e., over the container rim, and reduces the amount of metal foil material required. The central opening 42 in the foil also enables the liner to be see-through, wherein the user can view (visually detect) the contents (product P) in the sealed container, without removing the heat-seal liner 10 from the container rim 82 (as shown in
As shown in
Providing the support layer 122 with a central opening 123 enables benefits both in the final (laminated) liner assembly 110, such as preventing wrinkling or tearing of the metal-foil layer 140. It also provides benefits during manufacture, e.g., in the process of
In one embodiment, a polymer film (forming support layer 122) can be applied to one surface of a metal-foil sheet (forming metal-foil layer 140) by an adhesive lamination process, e.g., use of a solvent adhesive to bond the layers. The central openings 123, 142 in both the support layer 122 and the metal-foil layer 140 can be the same size as the rim inner diameter RID, or can be less than RID (e.g., the size can be adjusted depending on the desired visibility through the liner, and/or aroma penetration through the liner, based on the various material properties and dimensions of the liner layers).
Also advantageous in this embodiment, the metal-foil layer 240 can have an initial central opening 242 that is larger (e.g., of greater diameter) than the common central opening 212 (liner ID), and the material(s) of the top and/or bottom layers 220, 230 (or adhesive A forming part of those layers) is then allowed to flow into or otherwise fill the space defined by the initial central opening 242 (in the metal-foil layer 240), so as to fully or partially fill that space with adhesive 242A. The fully or partially filled space provides an area that surrounds the periphery of the central opening 212 in the metal-foil layer 240, in order to prevent the product P that is being dispensed through the common central opening 212, from reaching the metal-foil peripheral portion 244 of layer 240. This prevention (of product to metal-foil contact) will reduce the damaging effects of such contact which may include one or more of corrosion of the metal-foil layer, delamination of the liner layers, and/or a defective heat-seal bond with the container rim or the inner top wall of the cap.
The liners described herein may be manufactured from various materials and by various methods to achieve the aforementioned advantages.
As used herein the top, bottom and/or intermediate layers may be single layer or multi-layer embodiments, wherein one or more layers is provided as a coating layer, and/or one or more layers are continuous or less than continuous across the liner area (in a direction transverse to the thickness direction).
In various embodiments, the top, bottom and/or intermediate layers may include one or more polymer materials, such as polyolefins (e.g., polypropylene (PP) or polyethylene (PE) based polymers), polyesters (e.g., polyethylene terephthalate (PET) based polymers), polyamides (e.g., nylon based polymers), including copolymers, and blends thereof. Furthermore, one or more paper layers may be present.
In various embodiments, the metal-foil layer may be formed of one or more of metals, such as aluminum (Al), tin, copper or steel.
The liner may be formed by any one of various lamination methods, including adhesive lamination, extrusion lamination or thermal lamination (without adhesives). For adhesive lamination, the adhesive layers may comprise one or more of the top, bottom or intermediate layers, adjacent to the intermediate metal-foil layer, and/or between other layers of a multi-layer structure. The adhesive (glue) can be applied to the top or bottom layers, e.g., a PET heat seal layer, or to a polypropylene layer. It may be less preferred (e.g., more difficult) to apply adhesive to the metal-foil layer because of the central opening.
The induction heat-seal bonding material may be included in the top and/or bottom layers as a surface layer, e.g., as a solvent coating to a base film (e.g., DuPont Teijin Mylar CL Polyester Film), as an extrusion coating to a base film (e.g., as a hot melt adhesive), or as a distinct layer. The induction heat-seal bonding materials may comprise one or more polymer materials that bond in a temperature range of from 60 to 210 degrees Celsius. Representative materials include polyolefin, polyester and nylon materials. Typically the heat-seal material is a continuous layer across the entire liner area (transverse to the thickness direction TD); however it can be a partial layer that is applied only to the liner periphery where needed to bond to the container rim (i.e., a continuous peripheral area around the periphery of the liner).
The material used for the cap and container will depend upon the particular application. In one embodiment, the cap is made of polypropylene (PP), and the container is made from polyethylene terephthalate (PET), polypropylene (PP) or polyethylene (PE). The container may be made from an injection molded preform, the body portion of which is blow molded to form the container body. The rim may have an OD in a range of 28-89 mm, and a wall thickness in a range of 0.045 to 0.110 inch. For the non-removable closure embodiment, the dual heat-seal bonded cap, liner and container assembly can preferably withstand a torque or at least 50 inch-pounds, and more preferably 70 inch-pounds, without loss of the dual heat-seal bonds or distortion of the cap or container.
In one adhesive lamination method embodiment, the three component layers (top, intermediate, bottom) of the liner can be laminated in one step, by first applying adhesive to the top and bottom layers and sending all three layers (with the hole-punched metal-foil intermediate layer in the middle) through a nip of a pair of rotating rollers as shown in
In one heat lamination method embodiment, a support film of PET/EAA can be used (e.g., Dow Primacor Ethylene Acrylic Acid) that adheres well to Al foil to form the intermediate layer. All three layers (top and bottom, with the intermediate layer in between) are then sent through a nip of a pair of rotating rollers as shown in
The shape of the container rim, and complementary liner shape, is not required to be disc (circular) or annular (ring-shaped). Other rim shapes can be utilized, including any multi-sided shape with straight or curved sides, having sharp or rounded junctions between the sides. Another embodiment shown in
There are multiple applications where visual detection, and/or aroma detection, would be of great value to the consumer, and where the container must also provide protection against leakage, spoilage or contamination of the product and thus requiring use of a heat-seal liner. Products that would benefit from visual and/or aroma detection, without removal of the heat-seal liner, include products such as foods, beverages, cosmetics, confectionery, household products, air care and other items in the form of creams, gels, powders, liquids or solids, so as to permit the scent or aroma of the product to be released though the seal (or visual observation of the product) without providing direct access to the product.
These and other alternative embodiments are intended to fall within the scope of the pending claims.
Number | Name | Date | Kind |
---|---|---|---|
3951293 | Schultz | Apr 1976 | A |
4685580 | Towns | Aug 1987 | A |
4789074 | Han | Dec 1988 | A |
4863051 | Eibner et al. | Sep 1989 | A |
5176271 | Painchaud et al. | Jan 1993 | A |
5577625 | Baird | Nov 1996 | A |
5579936 | Costa et al. | Dec 1996 | A |
5688544 | Bolton | Nov 1997 | A |
5730306 | Costa et al. | Mar 1998 | A |
5988448 | Foth | Nov 1999 | A |
6065642 | Brown | May 2000 | A |
6378715 | Finkelstein et al. | Apr 2002 | B1 |
6602309 | Vizulis | Aug 2003 | B2 |
6983857 | Miller | Jan 2006 | B2 |
7163113 | Manganiello et al. | Jan 2007 | B2 |
7342501 | Abbott | Mar 2008 | B2 |
7461754 | Walsh | Dec 2008 | B2 |
7648764 | Yousif | Jan 2010 | B2 |
7900789 | Johnston et al. | Mar 2011 | B2 |
7909204 | Antal, Sr. | Mar 2011 | B2 |
7959028 | Leon | Jun 2011 | B2 |
8080118 | Yousif | Dec 2011 | B2 |
8220649 | Walsh | Jul 2012 | B2 |
8225954 | Triquet | Jul 2012 | B1 |
9708110 | Walsh | Jul 2017 | B2 |
9834331 | Bruna | Dec 2017 | B2 |
10589917 | Mir | Mar 2020 | B1 |
20010023870 | Mihalov et al. | Sep 2001 | A1 |
20040262418 | Smith et al. | Dec 2004 | A1 |
20050252918 | McKnight et al. | Nov 2005 | A1 |
20060228620 | Martinson et al. | Oct 2006 | A1 |
20080260917 | Sankey et al. | Oct 2008 | A1 |
20090230078 | Walsh | Sep 2009 | A1 |
20090250464 | Jongsma et al. | Oct 2009 | A1 |
20110089177 | Thorstensen-Woll | Apr 2011 | A1 |
20120111758 | Lo | May 2012 | A1 |
20130341325 | Bruna | Dec 2013 | A1 |
20140061196 | Thorstensen-Woll | Mar 2014 | A1 |
20140076898 | Wiening | Mar 2014 | A1 |
Number | Date | Country |
---|---|---|
2465790 | Jun 2012 | EP |
2017058886 | Apr 2017 | WO |
Entry |
---|
International Search Report in International Application No. PCT/US2016/012324 dated Mar. 11, 2016. |
Written Opinion in International Application No. PCT/US2016/012324 dated Mar. 11, 2016. |
International Search Report and Written Opinion in related International Application Na PCT/US2020/019780 dated Jul. 2, 2020. |
Number | Date | Country | |
---|---|---|---|
20200277113 A1 | Sep 2020 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 16290030 | Mar 2019 | US |
Child | 16290066 | US |