Claims
- 1. A method of making a graphite material, the method comprising the steps of:
- a) grinding flexible graphite into a powder having a particle size in the range of 25 to 80 mesh;
- b) expanding said graphite powder 8-10 times;
- c) mixing the expanded graphite powder, in an amount ranging between approximately 45%-60% graphite powder by weight, with a thermoplastic material in an amount ranging between approximately 40%-55% by weight; and
- d) injecting into a mold the graphite powder mixed with the thermoplastic material.
- 2. The of claim 1 further including the step of removing said graphite material from said mold when said plastic material is at a temperature of approximately 250.degree. F.
- 3. The method of claim 1 wherein said plastic material formed has a density of approximately 1.7 grams/centimeter cube.
- 4. The method of claim 1 wherein said thermoplastic material includes polyphenylene sulfide.
- 5. The method of claim 1 wherein said graphite of step a is recycled graphite foil.
- 6. The method of claim 1 wherein the injection step is performed for approximately 1 minute.
- 7. A method of making a graphite material, the method comprising the steps of:
- a) grinding flexible graphite into a powder having a particle size in the range of 25 to 80 mesh;
- b) expanding said graphite powder 8-10 times;
- c) mixing the expanded graphite powder, in an amount ranging between approximately 45%-60% graphite powder by weight, with a thermoplastic material in an amount ranging between approximately 40%-55% by weight;
- d) providing a compound by mixing the expanded graphite powder and the thermoplastic material with 20% by weight nickel coated carbon fibers; and
- e) injecting into a mold the compound.
- 8. The method of claim 7 wherein an electrical resistance of said graphite material is in range of 0.01 to 0.0008 ohm inches.
- 9. The method of claim 7 further including the step of removing said plastic material from said mold when said plastic material is at a temperature of approximately 250.degree. F.
- 10. The method of claim 7 wherein said plastic material formed has a density of approximately 1.7 grams/centimeter cube.
- 11. The method of claim 7 wherein said thermoplastic material includes polyphenylene sulfide.
- 12. The method of claim 7 wherein said graphite of step a is recycled graphite foil.
- 13. The method of claim 7 wherein the injection step is performed for approximately 1 minute.
Parent Case Info
This is a continuation-in-part of U.S. patent application Ser. No. 08/591,363 filed Jan. 25, 1996, now U.S. Pat. No. 5,582,781, which is a continuation of U.S. patent application Ser. No. 08/262,743 filed Jun. 20, 1994, now abandoned.
US Referenced Citations (3)
Continuations (1)
|
Number |
Date |
Country |
Parent |
262743 |
Jun 1994 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
591363 |
Jan 1996 |
|