The present invention relates to an installation for preparing wood fibers for use in the composition of a cultivation substrate, which installation comprises a defibration sheath having an inlet for wood chips and an outlet for the fibers obtained from said chips, the sheath containing two parallel screws suitable for being driven in rotation in such a manner as to mesh with each other via their respective threads, said threads having, in succession, in the direction going from upstream to downstream, at least an upstream series of segments and a downstream series of segments, each of which comprises a drive upstream zone having forward threads, and a braking downstream zone having reverse threads, the threads in the braking zones having notches, the notches in the threads of the braking downstream zone of the downstream series being smaller than the notches in the threads of the braking zone of the upstream series.
It is known to be advantageous to use wood fibers in the composition of a cultivation substrate.
Thus an installation of the above-mentioned type is known from European Patent EP 0 324 689. That document recommends using an installation having two parallel screws turning in the same direction and meshing with each other. Those two screws are provided with threads that are successively forward and reverse threads so as to determine a succession of drive zones and of compression zones, the reverse threads being provided with windows through which the material passes, it being possible for those windows to be smaller for the braking zone of the downstream series than for the braking zone of the upstream series. An adhesive binder for clumping the fibers is fed in during the defibration. The time taken for the material to pass through that installation is very short, and of the order of a few seconds. In order to guarantee that the temperature necessary for sterilizing the fibers is obtained, the machine is provided with heater jackets upstream from the zone at which the adhesive binder is fed in. In addition, insofar as the adhesive binder is a thermosetting binder, the machine is also provided with cooling jackets in the region in which said binder is fed in, so as to prevent it from setting. Thus, that machine is relatively complex and has relatively high energy consumption.
In addition, French Patent FR 2 248 780 filed in 1974, discloses cultivation media made from wood fibers, without addressing in any detail the method of obtaining such fibers.
European Patent EP 0 472 684 discloses a method and an installation for manufacturing a peat-substitute cultivation substrate, and recommends breaking up a fibrous organic material such as wood chips, mixing additional substances with it, and reducing the mixture to fibers and grinding it in a grinder having two contra-rotating parallel screws, with temperature control requiring heating or cooling. The resulting material is not homogeneous and must be sieved so as to recirculate any lumps that are too large into the inlet of the grinder. That document recommends heating the fibers to temperatures lying in the range 60° C. to 120° C. with a view to sterilizing and drying them.
An object of the invention is to improve the above-mentioned state of the art by proposing an installation that makes treatment conditions (treatment time and treatment temperature) possible that facilitate sterilizing the fibers or decontaminating them of micro-organisms, thereby making them fit for use as a cultivation substrate, while also preserving their intrinsic qualities, in particular as regards their capacity to retain moisture.
This object is achieved by the fact that the number of notches per thread in each braking zone lies in the range 2 to 6 and by the fact that the section-to-output ratio RSO of the sum of the sections of the notches of a thread of the braking downstream zone of the downstream series to the fiber output rate lies in the range 60 square millimeters per cubic meter per hour (mm2/m3h−1) to 80 mm2/m3h−1, and preferably in the range 70 mm2/m3h−1 to 75 mm2/m3h−1.
The fiber output rate is determined, in compliance with French Standard NF EN 12580, by measuring the volume of fibers collected at the outlet of the sheath, expressed in cubic meters (m3), in one hour.
After many tests, the Applicant has observed that the combination of these parameters makes it possible naturally to obtain a temperature of the order of in the range 120° C. to 150° C., without supplying external heat and without providing cooling, with a treatment time and a pressure that are sufficient for decontaminating the fibers effectively while they are being produced from the wood chips, and without burning them. Thus, the treatment time may be in the range 15 seconds (s) to 80 s, and the pressure upstream from the braking downstream zone of the upstream series, is of the order of 90 bars or more. The pressure taken into account is the sum of the static and dynamic pressures in the sheath. In addition, the above-mentioned ratio RSO of the sum of the sections of the notches of a thread to the fiber output rate makes it possible to obtain fibers that are aerated. Thus, for maritime pine, a porosity of greater than 85%, and in particular lying in the range 85% to 97% is obtained at the outlet of the installation. The porosity is the ratio of the volume of voids between the fibers to the total volume (apparent volume). Porosity is measured using Standard EN 13041.
The Applicant has observed that a temperature higher than 150° C. tends to bake the wood in a manner tantamount to beginning thermotransformation or to thermostabilization, adversely affecting its qualities as a cultivation substrate, in particular by reducing its capacity to retain water. As explained below, this pressure of approximately at least 90 bars can he obtained, with the above-mentioned ratio RSO of the sum of the sections of the notches of a thread to the fiber output rate, by taking account of the lengths of the parallel screws and of their drive and braking zones, their speed of rotation, and the loading of the sheath with wood chips. The maximum pressure is reached upstream from the first braking zone, i.e. immediately upstream from the braking downstream zone of the upstream series, at the interface between the drive upstream zone of said series and said braking downstream zone. In the portion of the sheath that is situated downstream from this place, the pressure falls to close to atmospheric pressure. After the very high compression, this reduction in pressure makes it possible to inject additives.
In addition, the transit time of approximately in the range 15 s to 80 s makes it possible to subject the fibers to a temperature of in the range 120° C. to 150° C. for a lapse of time that is long enough to decontaminate the fibers of harmful micro-organisms.
Advantageously, the number of notches per thread in each braking zone lies in the range 3 to 5.
These notches are preferably uniformly angularly distributed, with such a number of notches, the size of the notches that makes it possible to obtain the above-mentioned ratio RSO of the sum of the sections of the notches of a thread to the fiber output rate is optimized.
In an advantageous embodiment, the threads also have an intermediate series comprising a drive upstream zone having forward threads and a braking downstream zone having reverse threads between the upstream series and the downstream series, and the number of notches per thread in each braking zone is 5.
Adding an intermediate series with its braking zone makes it possible to improve the distribution of work between the various zones for obtaining, thereby enhancing the homogeneity of the fibers obtained at the outlet, as regards particle size, decontamination, water retention capacity, and pH. This is due, in particular, to the fact that this distribution of the work over a plurality of zones facilitates maintaining the desired high temperature over the length of the screws.
Advantageously, the screws are suitable for turning at a speed lying in the range 250 revolutions per minute (rpm) to 400 rpm, and preferably in the range 300 rpm to 380 rpm.
In other words, the motor, which, if necessary, is equipped with a gearbox at its outlet, is configured to cause the screws to turn within the indicated range. For example, the motor may be a variable-speed DC electric motor delivering power of the order of 1000 kilowatts (kW) and having a maximum output speed of 1200 rpm.
This speed of rotation for the screws is quite high in order to ensure that the chips are defibrated effectively. The length of the screws and the loading of the sheath with wood chips can then be determined to achieve the desired transit time for which the fibers stay in the sheath. For example, screws are chosen that are of length lying in the range 1600 millimeters (mm) to 3000 mm.
The presence of the above-mentioned intermediate series is particularly advantageous if the length of the screws exceeds 2000 mm or 2300 mm.
The invention can be well understood and its advantages appear more clearly from the following detailed description of an embodiment described by way of non-limiting example.
The description refers to the accompanying drawings, in which:
The installation shown in the figures comprises a sheath 10 in which two screws 12, 14 are disposed that mesh with each other. The distance e between the axes of the two screws is less than the outside diameter of their threads. The shafts 12A and 14A of the screws 12 and 14 are driven in rotation by a motor H and are supported in rotation by bearings, such as the bearings 15.
As can he seen more clearly in
The chips or shavings 16 that are to be defibrated, i.e. reduced to fibers, are loaded into the sheath via a feed 20 situated at the upstream end 10A of the sheath and, for example, being in the form of a hopper situated on the top face of the sheath, into which the chips are brought by any suitable means, e.g. by a screw conveyor (not shown).
At its downstream end 10B, the sheath has an outlet 22. For example, the outlet is constituted by a chute situated on the bottom face of the sheath and allowing the fibers 24 to fall by gravity onto the belt conveyor 26. The conveyor may be equipped with a tunnel (not shown), ventilated with a gas, such as air (preferably filtered air), so as to cool the fibers progressively as they are being conveyed.
The opening in the wall of the sheath that is formed at the feed 20 is advantageously symmetrical about the vertical midplane between the axes 12A and 12B of the screws so as to guarantee good distribution of the chips onto the two screws as soon as said chips enter the sheath. Similarly, the opening formed at the outlet 22 of the sheath is advantageously symmetrical about the same vertical midplane.
Due to the rotation of the screws, the chips are driven in the direction S going from upstream to downstream. While they are being driven, they are ground by the threads of the two screws, thereby reducing them to fibers.
One or more extraction filters 28 are disposed in the bottom wall of the sheath, which filters serve to extract the liquor coming from the defibration or the water for washing the chips, thereby making it possible to regulate the final humidity of the product. For example, said filters are placed at the upstream ends of the braking zones that are described below.
The two screws 12 and 14 turn in the same direction R and at the same speed of rotation. Over each segment of the facing screws, the threads of the two screws are of the same direction.
For each screw, the threads have an upstream series SM of segments and a downstream series of segments SA. In this example, the threads also have an intermediate series SI situated between the upstream series SM and the downstream series SA. Thus, the series SM, SI, and SA are disposed in succession along the sheath from upstream to downstream.
Each of the series itself comprises a drive upstream zone, respectively SME, SIE, and SAE for the upstream, intermediate, and downstream segments, and a braking downstream zone, respectively SMF, SIF, and SAF for the upstream, intermediate and downstream series. These drive zones and braking zones are respectively referred to as “upstream” and as “downstream” because, for each series, the drive zone is upstream from the braking zone in the direction S in which the chips advance during defibration.
It can be seen that, in the drive zones SME, SIE, and SAE, the threads 12B and 14B of the screws 12 and 14 are forward threads. This means that, by turning the screw in the direction R, these threads cause the material that is situated between them to advance downstream naturally. Conversely, in the braking zones SMF, SIF, and SAF, the threads 12B and 14B are reverse threads, i.e. turning the screw in the direction R tends to cause the material situated between them to move back upstream.
As a result, for each series, the material being defibrated tends to clump together at the interface between the drive zone and the braking zone. In order to enable the material to be conveyed, nevertheless, downstream through each braking zone, the threads of the braking zones have interruptions or notches 12C, 14C. Thus, these notches form constriction zones through which the material is forced to pass, under the effect of the thrust exerted, upstream, by the material driven downstream by the drive upstream zone.
The notches can be seen more clearly in
The axes of the screws are referenced 12A and 14A, which are the axes of rotation of their carrier shafts, respectively 12P and 14P. Since the screw segments can advantageously be disassembled, their threads are carried by sleeves, respectively 12M and 14M, which are mounted on the carrier shafts and are constrained in rotation therewith by any suitable means, e.g. by axial fluting (not shown).
For each thread, the notches are defined radially between the radially outer periphery of the thread and its radially inner periphery defined by the outside surface of the sleeve, respectively 12M and 14M. For example, the outside diameter of each screw, defined by the radially outer periphery of its thread, is 240 mm, the radial height h of a notch is 44 mm and the width of a notch is 16 mm. For a thread, i.e. by following a thread of the screw through an angle of 360°, a sum of the sections of the notches of the thread is obtained that is as follows: 5×44×16=3520 square millimeters (mm2).
Advantageously, in a braking zone of the screw 12 or 14, the notches 12C or 14C of two consecutive threads of the same screw are angularly offset to a small extent. In order to illustrate this characteristic, in
The installation is fed continuously and the feed flow-rate is adjusted to satisfy the above-mentioned pressure and temperature parameters.
Thus, the installation advantageously includes at least one temperature sensor CT situated upstream from the downstream braking zone SMF of the upstream series (in the region of the section plane III-III). A correspondence table giving correspondences between temperature and pressure may be established. Thus, a rise in temperature revealed by the temperature sensor CT can indicate too high a risk of an increase in pressure. The installation can then be regulated by reducing the wood chip feed flow-rate. It is also possible to make provision for the pressure to be measured directly by means of a pressure sensor CP situated in the same region as the temperature sensor CT. The measurements made by these sensors (at least the measurement made by the temperature sensor CT) may be input into a microprocessor that delivers a command to the wood chip feed system, e.g. an endless screw, as indicated above. If no direct pressure measurement is available, the microprocessor may, in a memory, have a temperature/pressure correspondence table. If the pressure is measured directly, the microprocessor can control the wood chip feed system on the basis of the two items of data (temperature and pressure) that are delivered to it. For a determined species of wood and for a known humidity, it is possible to establish a relationship between the pressure & temperature parameters and the electrical power consumed by the motor that drives the screws in rotation (or the electrical current, when the voltage is constant, as it often is). This relationship can be determined empirically by testing. With this relationship being known, it is possible to obtain the desired pressure and temperature parameters by adjusting the wood chip feed in such a manner as to consume a target amount of power.
Examples are given below of installations having two parallel screws mounted to turn in the same direction and at the same speed and that are suitable for implementing the method of the invention.
Example 1—machine in which the screws have three series of segments.
Length of screws (inside length of the sheath) 2620 mm
Diameter of the screws: 240 mm
Pitch of the forward threads: 110 mm
Pitch of the reverse threads: 60 mm
Speed of rotation of the screws: 330 rpm
Pitch of the forward threads: 110 mm
Pitch of the reverse threads: 60 mm
Speed of rotation of the screws: 330 rpm
The Applicant has observed that the transit time/pressure/temperature parameters are optimized if the chip feed of the machine is managed in such a manner as to obtain a fiber output rate such that, knowing the total section of the notches of each thread in the downstream series SA, the ratio RSO remains within the range 60 mm2/m3h−1 to 80 mm2/m3h−1, and preferably within the range 70 mm2/m3h−1 to 75 mm2/m3h−1.
In the above examples, the notches 12C, 14C in the threads of the braking downstream zone SAF of the downstream series SA are smaller than the notches in the threads of the braking downstream zone SMF of the upstream series SM. In addition, when an intermediate series is present, the size of the notches of the threads of the braking downstream zone of said intermediate series is preferably intermediate between the size of the notches of the braking zone of the upstream series and the size of the notches of the braking zone of the downstream series.
This makes it possible to avoid excessive braking in the regions of the upstream series. The further the treated material advances downstream, the more its state approaches the state of wood fibers. In other words, its particle size decreases going from upstream to downstream, so that this reduction in the size of the notches going from upstream to downstream is consistent with this reduction in particle size and makes it possible to obtain the desired pressure gradients at the braking zones. However, since the treated material occupies the entire inside volume of the sheath, the pressure is highest in the region of the braking downstream zone of the upstream series. By choosing notches that are not too small for this braking zone, it is possible to avoid a pressure gradient that is too steep in said braking zone.
Naturally, the adjustments of the installation and of the method may be fine tuned as a function of the species of wood or of the mix of species of wood of the chips that are defibrated. The examples indicated above are given by way of illustrative but non-limiting indication.
With maritime pine, and using the machine of example 1 above, the particle-size distribution of the fibers obtained at the outlet of the installation is as indicated in
An installation is described above that has two parallel screws turning in the same direction and at the same speed in the sheath. It is possible to use a different number of parallel screws, e.g. four such screws.
Number | Date | Country | Kind |
---|---|---|---|