1. Field of the Invention
The invention relates to a method and apparatus for repairing damaged portions of tires.
2. Description of the Related Art
It is generally known that a tire may become damaged. Damage may result from encountering road hazards and debris, or may be the result of tire mounting or dismounting, or an accident. In some instances, the damage may include abrasions, lacerations, or punctures.
One prior art method of repairing injuries to the body plies of a tire involves removing the damaged material, overlaying the section along an inside surface of the tire with a patch containing wires or cords, and filling the damaged area with rubber. With this technique, the repair reinforcements are offset relative to the tire's original reinforcements by a distance extending between the tire reinforcement and the reinforcement location within the patch. Therefore, the patch reinforcements are located beyond the interior surface of the tire, which may result in a distance at least 5-6 mm or more from the patch reinforcements to the tire reinforcements. When greater distances between the patch reinforcements and the tire reinforcements exist, shear amplitudes operating between the patch reinforcements and the tire reinforcements increase, which may lead to patch separation and failure. This limits the size and durability of the repairs.
Another repair technique involves removing a large trapezoidal section of the tire sidewall to a predetermined size and shape of a replacement patch section, where the patch reinforcements are substantially aligned within the same plane as the tire reinforcements. This technique is difficult and time consuming to practice, as it requires precise preparation of the trapezoidal tire aperture to match the patch dimensions, which is primarily done from the inside of the tire. It is also inflexible, as the tire is prepared to the predetermined patch size and shape.
Particular embodiments of the present invention include methods for repairing portions of tires. Such repair of tire portions is performed after injury to the tire that results from, for example, interaction with a road hazard. Particular embodiments of methods of the present invention, that are methods of repairing tire portions have steps that include removing at least part of the damaged portion of the tire to form an opening through the tire; forming one or more grooves in the tire adjacent to and extending from the opening; placing at least one repair reinforcement within each of the one or more grooves; placing a patch on the tire to cover the opening and each repair reinforcement; and, applying material to fill the remainder of the opening.
Other embodiments for repairing damaged tire portions have steps that include identifying a tire having a plurality of reinforcements extending through the tire, the tire having a damaged portion in at least one of the sidewall, tread, or shoulder; removing at least part of the damaged portion of the tire to form a cavity; forming one or more grooves in the tire adjacent to and extending from the cavity; placing at least one repair reinforcement within each of the one or more grooves; and placing a patch on the tire to cover and the cavity and each repair reinforcement.
Other embodiments for repairing damaged tire portions have steps that include removing at least part of the damaged portion of the tire to form an aperture or opening through the tire or cavity in the tire; forming one or more grooves in an inner surface of the tire adjacent to and extending from the opening or cavity; applying an adhesive to the one or more grooves; placing at least one repair ply within each of the one or more grooves, the repair play comprising rubber having one or more reinforcements embedded therein; placing a patch on the inner surface of the tire to cover the opening and each repair ply; and, applying material to fill the remainder of the opening or cavity.
The foregoing and other objects, features and advantages of the invention will be apparent from the following more detailed descriptions of particular embodiments of the invention, as illustrated in the accompanying drawing wherein like reference numbers represent like parts of the invention.
a is a side view of an outer portion of the tire shown in
b is a side view of an outer portion of a tire having multiple layers of reinforcements, also shown with damaged portion removed.
a is an inverted perspective view of
b is a perspective view of an inner portion of a tire shown with damage occurring in the tread area of the tire, and a cavity formed in the tire after removal of damaged portion.
a is a section view through line A-A illustrated in
b is a section view similar to
a is a perspective view of the portion of the tire shown in
b is a perspective view of the portion of the tire shown in
a illustrates a cross section of a repair ply having a single reinforcement therethrough.
b illustrates a cross section of a repair ply having a multiple reinforcements therethrough.
c illustrates a cross section of a repair ply having multiple reinforcements therethrough that are offset from the center of the reinforcement.
d illustrates a cross section of a repair ply having five reinforcements coated with a thin layer of rubber.
Particular embodiments of the present invention provide methods for repairing damaged tire portions.
Particular embodiments of the present invention include one or more steps for repairing a tire 10 having a damaged sidewall 12, tread 14, or shoulder 16. The steps may include identifying a tire 10 having a plurality of reinforcements 22 extending through the tire 10, the tire 10 having a damaged portion 18 in at least one of the sidewall 12, tread 14, or shoulder 16. The tire reinforcements 22 may comprise one or more layers of metallic cables, including steel cables; textile cords, including nylon cords, aramid cords, or any other textile cords known in the art; or any other reinforcement known in the art, and any combination thereof. If the tire 10 comprises two or more layers of reinforcements 22, the layers may be arranged in either a biased or radial orientation. Furthermore, the layers can be aligned in a stacked relationship, as illustrated in
The steps may further include the step of removing or excising at least part of the damaged section or portion 18 of the tire 10. Generally, the amount of damaged material removed is not more, or not significantly more, than an amount required to repair the damage. In one particular embodiment, the step may include removing or excising at least part of the damaged section or portion 18 of the tire 10 to form an aperture or opening 20 through the tire 10. In another embodiment, the step may include removing or excising at least part of the damaged section or portion 18 of the tire 10 to form a cavity 21 in the tire 10 rather than an opening 20.
In one particular embodiment, enough material is excised from the tire 10 about the damaged portion 18 such that the remaining material on the tire 10 about the opening 20 is undamaged. In other words, the damaged portion is removed at least to a point where the reinforcements 22 are firmly encased in undamaged rubber. In another particular embodiment, at least two millimeters of cord or cable 22 is removed beyond the visibly damaged cord or cable. If, however, as illustrated in
The damaged section 18 may be cut, ground, burned, or otherwise removed from the outer surface of the tire 10, or if desired, may be removed from the inner surface of the tire 10. In one particular embodiment, removal of the damaged portion comprises not only removing the rubber portion of the tire, but also cutting and removing a portion of one or more damaged reinforcements 22 in the tire as well. In the removal process, standard tools and established techniques can be used, such as grinders, burnishers, or rasps.
In a particular embodiment, after removal of any damaged portion 18, the tire 10 comprises an aperture or opening 20 that extends through the tire 10. In the embodiment of
In one embodiment, as illustrated in the
The methods may further include the step of forming one or more grooves or skivings 24 in the tire 10 adjacent to and extending from the aperture 20 or cavity 21. In a particular embodiment, the grooves 24 are formed by removing material from the tire adjacent to the opening 20 or cavity 21. Typically, the grooves 24 are formed along the interior or inner surface of the tire 10, as illustrated in
The grooves 24 may extend in any direction relative to the tire 10 and opening 20. For example, in
The width of the grooves 24 can be adapted to the user's preferences and as necessary for the particular circumstances. For example, in one embodiment, the grooves 24 are sized to accommodate a single repair reinforcement 32 or repair ply 30a having a single reinforcement 32. In other embodiments, the grooves 24 are sized to accommodate multiple reinforcements 32 or one or more repair plies such as 30b and 30d having multiple reinforcements 32. Furthermore, rather than a plurality of grooves 24 and reinforcements 32 or repair plies 30, in one particular embodiment a single groove 24 is formed that accommodates a single repair ply 30e having multiple reinforcements 32 extending therethrough.
With regard to the depth of the grooves 24, no particular depth is required. However, in one embodiment, the depth of the groove is substantially equal to or slightly shallower than the thickness of the repair reinforcement 30 or 32, as described in more detail below. Generally, the bottom of the groove 24 is as close to the reinforcements 22 as is reasonably practicable under the circumstances.
It is contemplated that the grooves 24 may be of any length. In one particular embodiment, each groove 24 extends outward from the opening 20 by a length L of at least fifty millimeters. In another embodiment as illustrated in
The method may further include the step of placing at least one repair reinforcement within each of the one or more grooves 24. The repair reinforcements 32 may comprise any reinforcement discussed and contemplated above, with reference to the tire reinforcements 22. Alternatively, one or more repair reinforcements 32 can be coated with or embedded within a polymer 34 such as rubber to form a repair ply 30. In one particular embodiment, the repair ply comprises a sheet of rubber having a plurality of reinforcements embedded therein.
The repair reinforcements 30 or 32 extend across or span the aperture 20 when placed in a groove 24.
As mentioned above, in one particular embodiment, the depth DG of the groove 24 is substantially equal to or slightly shallower than the thickness of the repair reinforcements 30, 32. For example, in
Particular embodiments of the disclosed methods comprise any of a plurality of different types of repair reinforcements 30 or 32. In one particular embodiment, the repair reinforcement is a repair ply 30 such as repair plies 30a, 30b, 30c, and 30d having one or more reinforcements 32 contained therein. However, it is also contemplated that the repair reinforcement may be one or more reinforcements 32. Additionally, the repair reinforcements 30, 32 are not required to be the same as the reinforcements 22 in the tire, either in number or composition. For example, if portions of five damaged metallic cables are removed to from aperture 20, any number of repair reinforcements 30 or 32 can be used in the repair, and the repair reinforcements 30 or 32 may comprise either cables or cords. Furthermore, the size, such as the circumference, of the repair reinforcements 30 or 32 may be different from tire reinforcements 22.
Repair ply 30a comprises a single reinforcement 32 contained within a polymer such as skim rubber 34. Repair plies 30b, 30c, and 30d comprise a plurality of reinforcements 32 contained within rubber 34, the reinforcements 32 generally being spaced equally across the width of the respective reinforcement 30b, 30c, or 30d.
Additionally, the reinforcements 32 can be spaced substantially equidistant between the top and bottom of the reinforcement, as in reinforcements 30 and 30b. However, as illustrated in
The method may further include the step of placing a patch 28 on the tire to cover each repair reinforcement 30 or 32. Typically, if an aperture 20 is formed during the repair process, the patch 28 is applied to cover the aperture 20 as well each repair reinforcement 30 or 32. Adhesives can be applied to the patch and/or the tire as needed to form a secure attachment.
In one particular embodiment, as illustrated in
Prior to application of the patch 28, an area 26 about the opening 20 may be buffed and/or cleaned with solvent and vacuumed to remove any debris or demolding lubricant on the surface to which the patch 28 adheres.
The method may further include the step of applying material 40 to fill the remainder of the opening 20 or cavity 21. Generally, the material is applied to fill the remainder of the opening 20 on a side of the tire opposite the repair reinforcements 30 or 32 and patch 28. As mentioned previously, the grooves 24, repair reinforcements 30 or 32, and patch 28 are typically located on an inner surface of the tire 10, and therefore the step of applying material 40 will typically be performed from the outer surface of the tire 10.
If a cavity 21 is formed by the removal of the damaged portion rather than the formation of an aperture 20, as mentioned previously, the method may comprise applying material 40 to fill the remainder of the cavity 21. It is contemplated that this step could be performed before placing the patch 28 or 128 over the repair reinforcements 30 or 32 and the remainder of the cavity 21, so that air is not trapped under the patch 28.
In one particular embodiment, the filler material 40 is a rubber material 40, and the rubber material 40 is applied to the level of the surrounding tire area. After the filler material is applied, it is shaped to blend with the exterior features of the tire. In yet another particular embodiment, one or more of the materials used in the disclosed section repair is uncured rubber. In such an embodiment, at least the portion of the tire that comprises uncured rubber is then cured in the standard manner in an envelope in an autoclave, or with a spotter.
The method may further include the step cutting a repair reinforcement from a spool to a length (L) to fit within a groove, prior to positioning the repair reinforcement into the groove. By cutting one or more of the repair reinforcements from a spool, there is no requirement to form the grooves to a particular length. Furthermore, the ability to cut the repair reinforcements 30 to a given length enables the user the ability to repair damaged areas of different sizes without an increased cost or a requirement to stock multiple lengths of repair reinforcements 30.
While this invention has been described with reference to particular embodiments thereof, it shall be understood that such description is by way of illustration and not be way of limitation. Accordingly, the scope and content of the invention are to be defined only by the terms of the appended claims.
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/US08/68498 | 6/27/2008 | WO | 00 | 12/24/2010 |