Claims
- 1. A method of incorporating a mineral containing particulate into a Portland cement manufacturing process having a burning step, the method comprising:agglomerating the mineral containing particulate and an agglomerating material to produce an additive; and introducing the additive into the Portland cement manufacturing process before the burning step.
- 2. The method of claim 1, wherein at least one of the mineral containing particulate and the agglomerating material is a waste product.
- 3. The method of claim 1, wherein both the mineral containing particulate and the agglomerating material are waste products.
- 4. The method of claim 1, wherein the additive has a b.t.u./lb rating of less than 5000.
- 5. The method of claim 1, wherein the additive has a b.t.u./lb rating of less than 8000.
- 6. The method of claim 1, wherein the mineral containing particulate comprises at least one of lime kiln dust, cement kiln dust, mineral extraction tailings, cracking catalyst fines, iron ore fines, fly ash, baghouse fines, and powder coating dust.
- 7. The method of claim 1, wherein the agglomerating material comprises at least one of a water soluble paint, a water soluble ink, a paint sludge, a paint wash water, and an adhesive.
- 8. The method of claim 1, wherein the step of agglomerating further comprises mixing the mineral containing particulate and the agglomerating material.
- 9. The method of claim 1, wherein a ratio of a weight of the agglomerating material to a weight of the mineral containing particulate is between 1:0.5 and 1:5.
- 10. The method of claim 1, wherein the step of introducing the additive comprises adding the additive to a raw feed of a Portland cement making process.
- 11. The method of claim 1, further comprising the step of drying the additive before the step of introducing.
- 12. The method of claim 1, wherein the burning step comprises at least one of calcining, roasting, and autoclaving.
- 13. The method of claim 1, wherein the burning step further comprises forming lumps of cement clinker comprised at least in part of minerals from the mineral containing particulate and a portion of the agglomerating material.
- 14. The method of claim 1, wherein the additive is introduced into a kiln.
- 15. A method of incorporating a mineral containing particulate into a Portland cement manufacturing process having a burning step, the method comprising:agglomerating the mineral containing particulate and an agglomerating material to produce an additive, wherein the agglomerating material comprises at least one of a water soluble paint, a water soluble ink, a paint sludge, a paint wash water, and an adhesive; and introducing the additive into the Portland cement manufacturing process before the burning step.
- 16. A method of incorporating a mineral containing particulate into a Portland cement manufacturing process having a burning step, the method comprising:agglomerating the mineral containing particulate and an agglomerating material to produce an additive, wherein the mineral containing particulate comprises at least one of lime kiln dust, cement kiln dust, mineral extraction tailings, cracking catalyst fines, iron ore fines, fly ash, baghouse fines, and powder coating dust, and the agglomerating material comprises at least one of a water soluble paint, a water soluble ink, a paint sludge, a paint wash water, and an adhesive; and introducing the additive into the Portland cement manufacturing process before the burning step.
Parent Case Info
This application claims the benefit of U.S. provisional application No. 60/272,168 filed on Feb. 27, 2001 incorporated herein by reference in its entirety.
US Referenced Citations (7)
Provisional Applications (1)
|
Number |
Date |
Country |
|
60/272168 |
Feb 2001 |
US |