Claims
- 1. In a process for oxidizing polymethylaromatics to their corresponding acids which comprises catalytically oxidizing the polymethylaromatic feedstock with air in an aliphatic acid solvent of 2-5 carbon atoms, in an oxidation zone wherein liquid-phase conditions are maintained, and wherein the weight ratio of the aliphatic acid solvent to the polymethylaromatic feedstock is in the range of about 0.5-4.0:1.0 and the catalyst comprises cobalt, manganese, and bromine components, the improvement comprises employing a combination of sources of cobalt, manganese, and bromine components so as to provide about 0.05 to about 0.4 weight percent total of cobalt and manganese combined, based on the polymethylaromatic feedstock and such that the weight ratio of bromine ions to total metals ions is about 0.5-3.0:1.0, and the manganese content is about 10-50 percent, each by weight of the total metals; adding about 20-200 parts per million by weight of iron based on the weight of the polymethylaromatic and in one or two stages; and conducting the reaction at a temperature of about 100.degree. C. to about 275.degree. C.
- 2. The method of claim 1 wherein the aliphatic acid is acetic acid.
- 3. The process of claim 1 wherein the addition of bromine is conducted in two stages and more than half of the bromine is added in the second stage.
- 4. The process of claim 1 wherein about 20 to about 200 parts by weight of iron based on the polyalkylaromatic feedstock are added.
- 5. The method of claim 1 wherein the catalyst additionally comprises a zirconium component at a level of 1-10 weight percent of the total metal content of the catalyst.
- 6. The method of claim 1 wherein the polymethylaromatic is pseudocumene.
Parent Case Info
This is a continuation of application Ser. No. 738,081, filed May 24, 1985.
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
3920735 |
Wampfler et al. |
Nov 1975 |
|
4314073 |
Crooks |
Feb 1982 |
|
Continuations (1)
|
Number |
Date |
Country |
Parent |
738081 |
May 1985 |
|