Joint between articles of materials of different coefficients of thermal expansion

Information

  • Patent Grant
  • 4930676
  • Patent Number
    4,930,676
  • Date Filed
    Friday, May 23, 1986
    38 years ago
  • Date Issued
    Tuesday, June 5, 1990
    34 years ago
Abstract
A method of providing a joint between articles of materials of different coefficients of thermal expansion comprises providing a preform of Indium between the articles, and, at ambient temperature, applying pressure to the articles to compress the Indium therebetween, the pressure being applied in a cyclical manner. A satisfactory joint is provided without employing complex cleaning of the co-operating surfaces of the constituent parts of the joint.
Description

THIS INVENTION relates to joints between articles of materials of different coefficients of thermal expansion, for example, relating to seals between two glass or ceramic articles, or between a glass, or ceramic, article and a metal article.
One of the articles may be of a glass ceramic; and the other article, to be joined thereto, may be of a Nickel-Iron alloy.
It is usually required that the joint provided is mechanically strong; and usually, but not essentially, the joint is required to provide an hermetic seal between the two articles.
It is desirable that such a joint is able to accommodate any differential thermal expansion between the materials of the articles joined together thereby. It is known for such a joint to include the malleable metal Indium. It is an object of the present invention to provide a novel and advantageous method of providing such a joint.
According to the present invention a method of providing a joint between articles of materials of different coefficients of thermal expansion comprises placing Indium, at least substantially free from impurities, between uncoated surfaces of the articles, which article surfaces are required to be joined together, and are at least substantially free from impurities, and applying pressure to the articles, at ambient temperature, and in a cyclical manner, in order to compress the Indium therebetween, and in order to provide the required joint.
The maximum pressure may be applied for approximately 20 seconds.
Conveniently, the applied pressure may vary between the maximum applied pressure, and approximately half this value, in a cyclical manner.
The maximum applied pressure may be approximately 15.5 .times.10.sup.6 Newtons per square meter.
The present invention will now be described by way of example.





EXAMPLE
An article of a glass ceramic, having a low coefficient of linear expansion of 0.03.times.10.sup.-6 per degree Kelvin at 20.degree. C., is cleaned and degreased in any known way. A second article of a Nickel-Iron alloy, having a low coefficient of linear expansion of less than 1.times.10.sup.-6 per degree Kelvin at 20.degree. C., also is cleaned and degreased in any known way.
After keeping the two articles clean, the articles are assembled in a jig, with a preform of Indium, of wire 1 millimeter in diameter, held between the surfaces of the articles to be joined together. The required Indium preform is produced immediately before the articles are to be joined together, so that there is no surface oxide film on the Indium preform.
Under ambient conditions, or in any atmosphere which is required to be enclosed between the two articles. A maximum possible pressure of approximately 15.5.times.10.sup.6 Newtons per square meter is applied to the articles, the time taken to apply such a pressure being approximately 20 seconds. The pressure is then reduced to half the maximum applied pressure, before the maximum pressure is applied again for approximately 20 seconds. This cycle is repeated two or three times. In this manner, the required joint is formed between the two articles. The joint is mechanically strong, on a joint of 1.3 square centimeters, the breaking force being 17,000,000 Newtons, but the malleability of the Indium ensures that the joint is able to accomodate any differential thermal expansion between the materials of the articles. An hermetic seal is provided between the two articles.
The Indium does not alloy with the materials of the articles under the conditions pertaining for a process in accordance with the present invention, although the materials may be capable of alloying under other conditions.
Such a method, in accordance with the present invention, of providing a joint between the two articles, is advantageous because it does not require heat to be applied; and can be formed under ambient conditions, or in any desired atmosphere.
Further, the complexity of the method is less than for at least some known methods of forming such joints, because the cleaning process steps employed are less complex, and the co-operating surfaces of the constituent parts of the assembly from which the joint is formed do not require any special treatments. Whilst the co-operating surfaces of the articles are required to be at least substantially planar, a satisfactory joint can be provided between scratched surfaces with the method in accordance with the present invention. If the seal provided by such a joint inadvertently is broken, it may be repaired by repeating the method in accordance with the present invention upon the joint.
The joint may be between more than two articles; and the articles may be of more than two materials.
Such a joint may be provided in relation to articles of other materials than those described above, the materials of the articles associated with each such joint having different coefficients of thermal expansion, for example, the joint being between two glass, or ceramic, or metal articles, or an article wholly of glass or ceramic material and a metal article. The ceramic may be silica or alumina. The metal may be brass, copper, aluminium, steel, gold or silver.
Various modifications of the method described above are possible.
The maximum pressure required to be applied varies with the materials of the articles to be joined together. For example, for a gold article and a ceramic article the maximum pressure being 8.times.10.sup.6 Newtons per square meter. Otherwise when one article is of metal the maximum pressure is in the range 13 to 18.times.10.sup.6 Newtons per square meter. In addition, for any particular combination of materials of the articles to be joined together, if the maximum applied pressure is less than the maximum pressure required to be applied, whilst a satisfactory, mechanically strong, joint may be provided, such a joint may not provide an hermetic seal between the articles, which may be acceptable.
Claims
  • 1. A method of providing a joint between articles of materials of different coefficients of thermal expansion, comprising placing a preform of indium, produced immediately before providing said joint such that it is at least substantially free from impurities, between uncoated surfaces of the articles, which article surfaces are required to be joined together, the otherwise untreated surfaces being at least substantially free from impurities, and, at ambient temperature, applying the necessary maximum pressure to compress the indium between the surfaces, and then at least twice reducing and reapplying the maximum pressure whereby a mechanically strong joint is obtained.
  • 2. A method as claimed in claim 1 in which the maximum pressure is applied for approximately 20 seconds.
  • 3. A method as claimed in claim 1 in which the maximum applied pressure is approximately 15.5.times.10.sup.6 Newtons per square meter.
  • 4. A method as claimed in claim 1 in which the applied pressure varies between the maximum applied pressure, and approximately half this value.
Priority Claims (1)
Number Date Country Kind
8236600 Dec 1982 GBX
Parent Case Info

This is a continuation of application Ser. No. 564,907, filed Dec. 23, 1983, abandoned.

US Referenced Citations (18)
Number Name Date Kind
2709147 Ziegler May 1955
2984759 Vine May 1961
3235943 Marafioti Feb 1966
3405207 Vahldiek Oct 1968
3590467 Chase Jul 1971
3634934 Fitzgerald Jan 1972
3671618 Huber Jun 1972
3698620 Geyer Oct 1972
3715070 Shibata Feb 1973
3754674 Wesoloski Aug 1973
3777281 Hochuli Dec 1973
3999698 Conklin Dec 1976
4047658 Frueauff Sep 1977
4073848 Kuehn Feb 1978
4159075 Ljung Jun 1979
4273581 Inoue Jun 1981
4382053 Rigby May 1983
4473526 Buhler Sep 1984
Foreign Referenced Citations (14)
Number Date Country
0610640 Jun 1978 SUX
759200 Oct 1956 GBX
780012 Jul 1957 GBX
890455 Jan 1959 GBX
808766 Feb 1959 GBX
826823 Jan 1960 GBX
845112 Aug 1960 GBX
846864 Aug 1960 GBX
849479 Sep 1960 GBX
1143535 Feb 1969 GBX
1389542 Apr 1975 GBX
1426873 Mar 1976 GBX
2041635A Sep 1980 GBX
2095604A Oct 1982 GBX
Continuations (1)
Number Date Country
Parent 564907 Dec 1983