The present invention relates to a laser welding device and a laser welding method.
A second member is placed in abutment against a first member. An abutment site between the members is welded. From the conventional art, it is widely known to carry out such welding in order to unite the two members in an integral manner.
In carrying out welding, in recent years, a laser beam with high energy density has been used.
With such a laser beam, a technique is known in which curved surfaces are welded together (for example, refer to Patent Document 1).
The technique of Patent Document 1 will be described with reference to
As shown in
The laser beam is irradiated perpendicularly to the curved surface, and therefore, high quality welding can be implemented with favorable weld penetration.
The processing head 103 undergoes movement. On the other hand, a laser oscillator 106 does not move. Therefore, the laser oscillator 106 and the processing head 103 are tethered together via a laser transmitting device 110 including first through third joints 107, 108, 109.
The first through third joints 107, 108, 109 are essential elements, and therefore, the laser welding device according to Patent Document 1 is complex in structure and large in size. As a result, installation costs for such welding equipment increase.
In addition, since the structure is complex, the number of constituent elements increases, and maintenance costs that occur accompanying the replacement of such components tend to rise precipitously.
While seeking a reduction in processing costs, a laser welding device has been desired, which is both simple in structure and small in scale, even in the case of a device that enables welding of curved surfaces.
Patent Document 1: Japanese Laid-Open Patent Publication No. 11-000776
The present invention has the object of providing a laser welding device which is both simple in structure and small in scale, even for a device in which curved surfaces are welded.
The invention according to claim 1 is a laser welding device, comprising a workpiece fixing unit that superimposes a plurality of workpieces in such a manner that a curved surface of a first workpiece is placed in contact with a curved surface of a second workpiece, and constrains the workpieces in such a state, the workpiece fixing unit pressing the plurality of workpieces in a state with the curved surfaces thereof in abutment;
a laser irradiation mechanism that irradiates a laser beam on welding sites of the workpieces, a moving mechanism that moves the laser irradiation mechanism linearly, and a control unit that controls the laser irradiation mechanism and the moving mechanism;
wherein the laser irradiation mechanism includes a function of drawing a focal point of the laser beam in the form of a circle; and
the control unit performs a control to draw the focal point in the form of a helix by combining movement of the moving mechanism and circular motion of the focal point by the laser irradiation mechanism, and performs a control so that a central axis of the helix is formed along the curved surface.
The invention according to claim 2 is a laser welding method that is implemented using the laser welding device of claim 1, wherein, when the laser beam passes through an apex of the curved surface, the control unit causes the laser beam to be perpendicular to a tangent line that passes through the apex, and causes the laser beam to incline toward a center of curvature of the curved surface at welding sites that are distanced from the apex of the curved surface.
With the invention according to claim 1, the focal point of the laser beam is drawn in the form of a helix, and a central axis of the helix is formed along the curved surface. The helix overlaps itself at locations distanced from the apex of the curved surfaces in the workpieces. When performed in this manner, a semi-solidified portion is re-melted, and the re-melted portion becomes a semi-solidified portion, and by repeating the re-melting of the semi-solidified portion again and again, the melting depth increases. Thus, even at ends of the curved surface, a sufficient melting depth can be obtained.
According to the present invention, despite the welding sites existing on a curved surface, the laser irradiation mechanism can be moved linearly. Due to such linear motion, the moving mechanism is simplified and is small in scale. Thus, by the present invention, a laser welding device is provided, which is both simple in structure and small in scale, even for a device in which curved surfaces are welded.
With the invention according to claim 2, when the laser beam passes through an apex of the curved surface, the control unit causes the laser beam to be perpendicular to a tangent line that passes through the apex, and causes the laser beam to incline toward a center of curvature of the curved surface at welding sites that are distanced from the apex of the curved surface. The laser irradiation mechanism includes a function to cause the laser beam to incline if the laser beam resides within a fixed range. By utilizing this function skillfully, the laser beam is made to incline toward the center of curvature of the curved surface at welding sites that are distanced from the apex of the curved surface. Owing to such inclination, the overlapping of the helix with itself can be mitigated, and productivity can be enhanced.
An embodiment of the present invention will be described below with reference to the accompanying drawings.
As shown in
The workpieces 11, 12 are constituted from a cylindrical first workpiece 11, and a cylindrical second workpiece 12 that is inserted into the first workpiece 11. A curves surface of the second workpiece 12 is superimposed on a curved surface of the first workpiece 11.
In the present invention, the curved surfaces are joined with each other, and welding sites 13 thereof exhibit a circular arcuate shape. A plane 14 that passes through such welding sites 13 coincides with the plane of the drawing sheet in this example.
A tangent line 16 (including lines parallel to the tangent line 16) that are on the plane 14 and passes through an apex 15 of the curved surface is defined as an x-axis. An axis that is perpendicular to the x-axis and extends to the rear of the drawing is defined as a y-axis. The y-axis is an axis that extends in a width direction of a later-described weld line.
A workpiece fixing unit 20 is constituted from a cradle 21 on which the workpieces 11, 12 are supported, and a clamp 22 that presses the workpieces 11, 12 toward the cradle 21. The clamp 22 is driven by a clamp cylinder 23.
The moving mechanism 40 is a mechanism that causes the laser irradiation mechanism 30 to move linearly along the x-axis. The moving mechanism 40, for example, is made up from a rail 41 that extends along the x-axis, a slider 42 that is supported on the rail 41 and supports the laser irradiation mechanism 30, and a moving cylinder 43 that moves the slider 42 along the x-axis.
When the workpieces 11, 12 are placed on or separated away from the workpiece fixing unit 20, the moving mechanism 40 is moved to a standby position so as not to interfere with the workpieces 11, 12. The moving mechanism 40 preferably is a robot arm.
As shown in
The laser beam 31 is moved along the y-axis by the mirror 33. Further, by moving the lens 36 relatively with respect to the mirror 33, the focal point 39 of the laser beam 31 is moved along the z-axis. The y-axis motion and the z-axis motion are combined so that the focal point 39 draws a circle.
Upon drawing the circle, movement of the laser irradiation mechanism 30 along the x-axis is provided in addition thereto. Thus, as shown in
Thus, according to the present invention, as shown in
As shown in
As shown in
As a result, as shown in
When the laser irradiation mechanism 30 is moved along the x-axis to a position distanced from the apex 15 of the curved surface, then as shown in
In general, if the laser beam 31 is advanced continuously, at the leading end thereof, a molten portion (molten pool) referred to as a keyhole is formed. Immediately after the molten portion, a semi-solidified portion is formed, and after the semi-solidified portion, a solidified portion (corresponding to the welded metal) is formed.
As shown in
More specifically, as shown in
As shown in
However, when the conventional welding method is considered in which the laser beam is oriented toward the center of curvature of the workpiece, the welding process described next may also be recommended.
More specifically, as shown in
The method of the present invention can be applied to a variety of applications. One example thereof will be described next.
As shown in
According to the conventional art, as shown by the comparative example of
The positional control of the laser irradiation mechanism 101 is cumbersome.
In contrast thereto, with the exemplary embodiment shown in
Moreover, although in the exemplary embodiment two workpieces are superimposed, three or more workpieces may be superimposed. Further, the present invention can also be applied to butt welding.
Further, although in principle the material of the workpieces is carbon steel, stainless steel, titanium alloy, aluminum alloy, or other materials may be used.
Furthermore, the workpieces are not limited to being circular tubes or pipes, and may be arcuate members that are formed by being pressed locally such as pressed articles or the like.
The present invention is preferably applied to laser welding for welding curved surfaces.
10 . . . laser welding device, 11 . . . workpiece (first workpiece), 12 . . . workpiece (second workpiece), 13 . . . welding sites, 14 . . . plane, 15 . . . apex, 16 . . . tangent line, 20 . . . workpiece fixing unit, 30 . . . laser irradiation mechanism, 31 . . . laser beam, 39 . . . laser beam focal point, 39B . . . central axis of helix, 40 . . . moving mechanism, 50 . . . control unit, 52 . . . welded metal portion, 53 . . . center of curvature
Number | Date | Country | Kind |
---|---|---|---|
2014-162754 | Aug 2014 | JP | national |