The invention relates to a method for operating a joining apparatus, wherein a component that consists of at least two parts is processed by means of an energy beam in such a manner that the at least two parts are joined in a joining region by means of the energy beam, wherein several components are supplied and processed one after the other by means of a conveying apparatus, as well as to a joining apparatus that operates as claimed in the method according to the features of the respective preambles of the independent claims.
DE 10 2007 042 0739 A1 makes known a method for operating a joining apparatus as well as a joining apparatus that operates as claimed therein. It makes known a clamping apparatus for clamping at least two parts of a component in a processing machine that is protected against radiation, the two parts being mounted in such a manner in the clamping apparatus that a pressure is generated in the joining region, that is in the two regions of the parts of the components that are to be joined together. By means of an energy beam, in this case a laser beam, the joining faces of the two parts that adjoin one another are heated up such that they melt together and are then non-detachably interconnected. The disadvantage of the processing machine, however, is that the two parts of the component have to be moved in, that they then are moved together and fixed in their position by means of the clamping apparatus, that the joining process is carried out after this and subsequently the finished component can be removed from the processing machine. Such a processing machine can easily be used for producing small quantities of components. However, it is not possible to produce large quantities economically in a series production using such a processing machine.
If the laser processing machine from DE 10 2007 042 0739 A1 had a conveying apparatus, the following sequence would be produced: component is moved into the laser processing machine→belt stops→where applicable component is removed or clamped by clamping mask→welding carried out by laser→component conveyed further. Disadvantages: clock pulse process, belt always has to carry out start/stop motions, the clock time for many moved elements (belt, removal mechanisms, clamping apparatus) is undesirably longer.
Consequently, for the application of series production of such components, non-cited DE 10 2011 055 460.2 has already proposed a method for the continuous welding of plastics material components of a product along a joining region that extends on the circumference, where the plastics material components to be welded are first of all moved into their joining position and are fixed there and, for welding, the product is then conveyed past a fixed heat source, the product being subject to a rotational self-movement in the region of the fixed heat source in addition to the conveying motion in order to introduce the welding energy into the joining region. The method is certainly better suited for series production, but still has the following disadvantages. On the one hand, the method can only be carried out if the product is subject to a rotational self-movement. This means that only rotationally symmetrical plastics material components can be processed using the method. A further disadvantage is that the energy beam is always focused precisely in one single point, the point corresponding to the joining region of the two parts of the plastics material component to be joined.
Consequently, the object underlying the invention is to provide a method for operating a joining apparatus as well as a joining apparatus that operates as claimed in the method, by way of which method or apparatus the advantages depicted in the introduction are avoided. In particular, it is to be possible to produce a large quantity of components economically and flexibly.
The object is achieved as claimed in the method in that the energy beam, by way of which the respective component is processed, is adjusted along the joining region in dependence on the motion of the component. As a result, in an advantageous manner, this is not only a question of a continuous motion of the component such that clock pulse advancement of the direction of motion (stop and go) can be omitted, but also the course of the energy beam is adapted to the motion of the component. Consequently, it is possible as claimed in the invention to join, in particular to laser weld, a contour (joining region) of the component whilst the component is being guided in its direction of motion through the joining apparatus (in particular the laser beam welding machine). This means that in an advantageous manner two motions are superposed, namely the motion of the component (consisting of two or more than two parts to be joined) in the direction of motion when running through the joining apparatus, and that at the same time the energy beam (laser beam) is adapted to the weld contour (joining region) with an additionally superposed motion for following the component advancement (component motion). This means in an advantageous manner for the realization of the invention that several components with parts that are to be joined can be supplied to the energy beam one after the other on a conveying apparatus of the joining apparatus. During the continuous conveying of the component, which can be effected in a linear, rotational or similar manner, the energy beam is first of all directed onto the joining region thereof, the energy beam traveling over the joining region by means of suitable means in order to connect together in a non-detachable manner the two parts of the component to be joined. The joining region, in this case, can be rotationally symmetrical, it also being possible, however, to realize other forms, such as, for example, rectangular, quadratic or oval or other joining regions. It is simply necessary to know the course of the joining region so that using simple means the laser beam can be adjusted in line with the joining region, the component being moved on at the same time on the conveying apparatus. Once the first supplied component is joined in its joining region and consequently is finished, the energy beam is directed onto the next supplied component and the procedure is carried out in the identical manner as has been described for the first component. Likewise, the procedure is the same for the next supplied components. The advantage of this overall is that components are supplied continuously one after the other without any interruption in the motion and can be processed in their joining region by means of the energy beam without interrupting the continuous motion of the component feed.
In a further development of the invention, the energy beam is adjusted by means of an optical apparatus along the joining region during the motion of the component. The advantage of this is that the source for generating the energy beam (in particular a laser beam source) can be arranged in a stationary manner, whereas the energy beam (in particular a laser beam) generated by the energy source is deflected by means of the optical apparatus. The deflection is effected in such a manner that the deflected energy beam is guided in a corresponding manner in line with the joining region and at the same time the progressive motion of the component is taken into account. This means that in this case too there are two superposed motions, namely first of all the motion of the energy beam for traveling over the joining region and at the same time a motion of the energy beam for taking into account the progressive motion of the component.
In a further development of the invention, the focus of the energy beam is adjusted to the joining region during the motion of the component. This means that the focus of the energy beam is tuned to or adjusted in such a manner to the operating region (joining region) that the focus does not have to be adjusted in the processing window (the point that is contacted by the energy beam precisely in the joining region). In reverse, this means that the focus is adjusted in view of the course of the point of the joining region to be processed as well as of the progressive motion of the component.
In a further development of the invention, the joining region is scanned during the motion of the component and the energy beam is adjusted in line with the joining region in dependence on the scanning operation. The advantage of this is that the joining region to be processed is automatically recognized by means of the scanning and consequently the energy beam can be adjusted along the scanned joining region whilst at the same time taking into account the progressive motion of the component during the conveying thereof. Consequently, in an advantageous manner arbitrary courses of joining regions are possible such that the method is not restricted to rotationally symmetrical components, but arbitrary joining regions are able to be processed.
The invention is explained in more detail and described below by way of the figures.
Although not shown in
The optical apparatus of the energy beam apparatus 13, 23 can be realized and can operate on the one hand such that the generated energy beam 14, 24 is moved along in view of the motion of the component 12, 22 along the joining region of the one component 12, 22. Once the joining region of the one component 12, 22 has been processed and consequently the two parts of the one component 12, 22 have been joined in a non-detachable manner, the energy beam 14, 24 can be directed to the next supplied components 12, 22 and there can travel over the joining region in view of the progressive motion of the next supplied component 12, 22. On the other hand, however, it is also conceivable that the generated energy beam 14, 24 is supplied at the same time not only to one component 12, 22 (as described above) but that through corresponding deflection, the energy beam 14, 24 changes (“jumps back and forth”) from one component 12, 22 to the next supplied component 12, 22 in the short-term in succession and in an alternating manner such that as a result the number of components to be processed in the run-through can be noticeably increased. In this case, depending on the processing speed of the energy beam 14, 24, its energy intensity and the speed of the progressive motion of the conveying apparatuses 11, 21, it cannot be ruled out that not only two components 12, 22 but more than two such components are processed at the same time.
In a preferred manner, laser beams are used as energy beams (heat sources). Likewise, a broadband infrared light source in the short or medium wave infrared range is suitable as a heat source, in particular a glass tube, ceramic, metal foil or carbon radiation emitter.
10, 20 Joining apparatus
11, 21 Conveying apparatus
12, 22 Component
13, 23 Energy beam apparatus
14, 24 Energy beam
15 Processing region
16 Weld line
17 Conveying direction
Number | Date | Country | Kind |
---|---|---|---|
10 2010 055 293.3 | Dec 2010 | DE | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP11/73647 | 12/21/2011 | WO | 00 | 6/28/2013 |