The present application is based on Japanese patent application No. 2016-191474 filed on Sep. 29, 2016, the entire contents of which are incorporated herein by reference.
This invention relates to a light emitting device and a method of manufacturing the light emitting device.
A light emitting device is known wherein plural light emitting elements are densely disposed and covered by a first sealing member and a second sealing member, which include different phosphors, and wherein the first sealing member and the second sealing member are disposed in the form of a checkered pattern (see e.g. JP-B-5895597).
JP-B-5895597 states that the light emitting device can reduce color unevenness in light irradiation image caused by rotating an emission region at a center thereof by using a two-dimensional optical system such as a lens and a reflector.
The light emitting device disclosed by JP-B-5895597 is constructed such that the first sealing member is embedded in a space between the light emitting elements. Light that enters into the embedded first sealing member is emitted outside after being repeatedly reflected in the embedded first sealing member.
Thus, an optical path in the embedded first sealing member is longer than an optical path in the first sealing member or the second sealing member on the light emitting element. As a result, the amount of fluorescence emitted from the space between the light emitting elements may increase relatively so as to cause lattice-shaped color unevenness. Moreover, this problem may be significant according as the space between the light emitting elements is reduced.
It is an object of the invention to provide a light emitting device that allows a reduction in color unevenness even if plural light emitting elements is densely disposed, and a method of manufacturing a light emitting device.
According to embodiments of the invention, a light emitting device and a method of manufacturing a light emitting device defined by [1] to [5] and [6] to [10] below respectively are provided.
[1] A light emitting device, comprising:
a substrate;
a plurality of light emitting elements disposed on the substrate;
a transparent resin embedded in a space between the plurality of light emitting elements; and
a phosphor containing resin layer formed on the plurality of light emitting elements and the transparent resin,
wherein the transparent resin includes no phosphor.
[2] The light emitting device according to [1], wherein the phosphor containing resin layer comprises a plurality of regions different in fluorescent color.
[3] The light emitting device according to [2], wherein the phosphor containing resin layer comprises a first region and a second region different in fluorescent color, and
wherein the first region and the second region are distributed in a form of a checkered pattern.
[4] The light emitting device according to [2] or [3], wherein a border of the plural regions of the phosphor containing resin layer is located on the transparent resin.
[5] The light emitting device according to [4], wherein a top position of the transparent resin is higher than a top surface of the plurality of light emitting elements.
[6] A method of manufacturing a light emitting device, comprising:
embedding a transparent resin in a space between a plurality of light emitting elements disposed on a substrate; and
forming a phosphor containing resin layer on the plurality of light emitting elements and the transparent resin,
wherein the transparent resin includes no phosphor.
[7] The method according to [6], wherein the phosphor containing resin layer comprises a plural regions different in fluorescent color.
[8] The method according to [7], wherein the phosphor containing resin layer is formed such that a border of the plural regions different in fluorescent color locates on the transparent resin.
[9] The method according to [8], wherein the transparent resin is formed such that a top position of the transparent resin is higher than a top surface of the plurality of light emitting elements.
[10] The method according to any one of [6] to [9], wherein the transparent resin and the phosphor containing resin layer are formed by screen printing.
According to an embodiment of the invention, a light emitting device can be provided that allows a reduction in color unevenness even if plural light emitting elements is densely disposed, and a method of manufacturing a light emitting device.
Next, the present invention will be explained in conjunction with appended drawings, wherein:
The light emitting device 1 is provided with a substrate 10, a plurality of light emitting elements 11 disposed on the substrate 10, a transparent resin 15 embedded in a space between the plurality of light emitting elements 11, a phosphor containing resin layer 16 formed on the plurality of light emitting elements 11 and the transparent resin 15.
For example, the substrate 10 is a ceramic substrate such as Al2O3 substrate and AlN substrate, a metallic substrate such as Al substrate and Cu substrate of which an insulating film cover a surface, and a glass epoxy substrate, which have wiring 13 made of Cu etc. on a front surface and a pad electrode 14 made of Cu etc. on a back surface. The wiring 13 and the pad electrode 14 are electrically connected through a viahole etc. which pierces the substrate 10 in the thickness direction.
For example, the light emitting element 11 is a light emitting diode chip or a laser diode chip, and provided with a transparent element substrate and a multilayer crystal including an emission layer. The light emitting element 11 is a face-down type such as a flip-chip type.
The electrode 12 of the light emitting element 11 is connected to the wiring 13 on the front surface of the substrate 10. Power is supplied to the electrode 12 from the exterior through the pad electrode 14 and the wiring 13.
Although a layout and a number of the plurality of light emitting elements 11 are not limited, the plurality of light emitting elements 11 is disposed with high density. In this case, “High density” means that, for example, a width of space W between the light emitting elements 11 (the space between the adjacent light emitting elements 11) is not more than 200 μm.
Color unevenness can reduce in the case that the light emitting device 1 has a plural types of emission regions different in light emission colors by disposing the plurality of light emitting elements 11 with the high density. The case that “the light emitting device 1 has the plural types of emission regions different in the light emission colors” means that, for example, “the phosphor containing resin layer 16 has the plural types of regions different in fluorescent colors” or “the plurality of light emitting elements 11 comprises a plural types of light emitting elements different in light emission colors”. Furthermore, a light intensity control function can be added to the light emitting device 1 by individually supplying power to each type of light emitting element when the plurality of light emitting elements 11 comprises the plural types of light emitting elements different in the light emission colors.
The transparent resin 15 is the resin such as a silicon resin and an epoxy resin, and fails to include the phosphor.
As described above, since an optical path in the transparent resin 15 where the light enters becomes long if the transparent resin 15 includes the phosphor, an amount of fluorescence emitted from the transparent resin 15 is larger than an amount of fluorescence emitted from the phosphor containing resin layer 16. Thus, the color unevenness causes in the light emission of the light emitting device 1. Therefore, the color unevenness can reduce by the transparent resin 15 failing to include the phosphor.
The color unevenness caused if the transparent resin 15 includes the phosphor causes remarkably as the width of the space W between the light emitting elements becomes narrower. Therefore, reducing the color unevenness caused by the transparent resin 15 failing to include the phosphor causes more effectively if the width of the space W between the light emitting elements is particularly small, for example, not more than 100 μm. Moreover, when the width W is not more than 50 μm, the effect causes more effectively.
Furthermore, absorbing in transmitting the light through the transparent resin is smaller than absorbing in reflecting the light to a white resin. Therefore, reducing an amount of light caused by absorbing can be controlled compared to apply the white resin instead of the transparent resin 15.
The phosphor containing resin layer 16 comprises the transparent resin such as the silicon resin and the epoxy resin in which phosphor particles are separated. It is preferable that a refractive index of the transparent resin 15 is smaller than a refractive index of an element substrate of the light emitting element 11, and a refractive index of the phosphor containing resin layer 16 is smaller than the refractive index of the transparent resin 15 so as to improve light extraction efficiency.
The phosphor containing resin layer 16 may have the plural types of regions different in the fluorescent colors, that is, the plural types of regions including different phosphors. In this case, light emission color scattering of the light emitting device 1 can be controlled by forming the phosphor containing resin layer 16 so as not to locate a border of the plural types of regions different in the fluorescent colors just above the light emitting element 11, that is, so as to locate the border of the plural types of regions on the transparent resin 15.
In the examples described in
As the phosphor containing resin layer 16 includes the warm colored phosphor and the cool colored phosphor, the light emitting device 1 can emit the white light that mixes the reddish white light and the bluish white light and is near to sunlight. As the phosphor containing resin layer 16 is divided into the region including the warm colored phosphor and the region including the cool colored phosphor, the light emitting device 1 can prevent cool colored fluorescence having a short wavelength from reabsorbing in the warm colored phosphor.
In the example shown in
As shown in
Firstly, as shown in
Next, as shown in
For example, the transparent resin 15 is formed by screen printing. In this case, the transparent resin 15 can be embedded certainly in the space between the plurality of light emitting elements 11 by screen printing by using a mask of which opening width is narrower than the width of the space W between the light emitting elements 11. For example, the mask having the opening width in about 30 μm can be applied when the width W is 50 μm. Meanwhile, other method such as potting may be used in embedding the transparent resin 15.
Next, as shown in
Next, as shown in
For example, the first region 16a and the second region 16b in the phosphor containing resin layer 16 are formed by screen printing. Each of the first region 16a and the second region 16b may be formed firstly.
If the border of the plural types of regions of the phosphor containing resin layer 16 different in the fluorescent colors is located on the transparent resin 15, an expansion of the phosphor containing resin layer 16 where is firstly formed before resin hardening in a planar direction can be prevented by the top position of the transparent resin 15 higher than the top surface of the plurality of light emitting elements 11.
Specifically, for example, the first region 16a of the phosphor containing resin layer 16 can be prevented from spreading to a region where the second region 16b is formed in the process shown in
As shown in
According to the above embodiment, the light emitting device having less color unevenness can be obtained by embedding the transparent resin that fails to include the phosphor in the space between the light emitting elements even if the plurality of light emitting elements is disposed with the high density.
Although the embodiments have been described, the invention is not intended to be limited to the embodiments. The various kinds of modifications can be implemented without departing from the gist of the invention. For example, the light emitting elements may be divided by forming a scribing line by cutting.
Also, the claimed invention is not intended to be limited to the embodiments. Further, it should be noted that all combinations of the features described in the embodiments and the Examples are not necessary to solve the problems of the invention.
Number | Date | Country | Kind |
---|---|---|---|
2016-191474 | Sep 2016 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
20040129945 | Uemura | Jul 2004 | A1 |
20080231162 | Kurihara | Sep 2008 | A1 |
20080290351 | Ajiki | Nov 2008 | A1 |
20100053034 | Oyaizu | Mar 2010 | A1 |
20120091480 | Aoki | Apr 2012 | A1 |
20120091489 | Aoki | Apr 2012 | A1 |
20130141013 | Kodama et al. | Jun 2013 | A1 |
20130187540 | Tischler | Jul 2013 | A1 |
20130249407 | Kashiwagi | Sep 2013 | A1 |
20130249411 | Takahashi | Sep 2013 | A1 |
20140118988 | Aoki | May 2014 | A1 |
20140191258 | Akimoto et al. | Jul 2014 | A1 |
20150171281 | Nakabayashi | Jun 2015 | A1 |
20150204494 | Wada | Jul 2015 | A1 |
20150207045 | Wada | Jul 2015 | A1 |
20160041430 | Lee | Feb 2016 | A1 |
20160079487 | Kuroki | Mar 2016 | A1 |
20160284666 | Lee | Sep 2016 | A1 |
20170213947 | Miwa | Jul 2017 | A1 |
20180090470 | Miwa | Mar 2018 | A1 |
20180090646 | Kato | Mar 2018 | A1 |
Number | Date | Country |
---|---|---|
2005-109434 | Apr 2005 | JP |
2012-199218 | Oct 2012 | JP |
2013-65726 | Apr 2013 | JP |
5178623 | Apr 2013 | JP |
2013-098458 | May 2013 | JP |
2014-229676 | Dec 2014 | JP |
2015-138838 | Jul 2015 | JP |
5895597 | Mar 2016 | JP |
2017112295 | Jun 2017 | JP |
Entry |
---|
Japanese Office Action dated Sep. 10, 2019, in Japanese Patent Application No. 2016-191474, with an English translation. |
Number | Date | Country | |
---|---|---|---|
20180090470 A1 | Mar 2018 | US |