The present invention relates to a liquid crystal display device, and more particularly to a small display device including a front window.
In a liquid crystal display device, there is provided a TFT substrate in which pixel electrodes, thin film transistors (TFT) and the like are arranged in a matrix form. Further, a counter substrate is disposed opposite to the TFT substrate. In the counter substrate, color filters and the like are formed at locations corresponding to the pixel electrodes of the TFT substrate. Then, a liquid crystal is sandwiched between the TFT substrate and the counter substrate. Thus, the liquid crystal display device forms an image by controlling the transmittance of light of the liquid crystal molecules for each pixel.
Regarding the liquid crystal display device, there is a strong demand for reducing the overall size of the set itself and reducing the thickness of the liquid crystal display panel, with the size of the screen being fixed. In order to reduce the thickness of the liquid crystal display panel, the liquid crystal display panel is formed and thinned by polishing the outside.
The TFT substrate including pixel electrodes, TFT and the like, and the counter substrate including color filters, are glass substrates constituting the liquid crystal display device. The two glass substrates are standardized, for example, at a thickness of 0.5 mm or 0.7 mm. It is difficult to obtain glass substrates, other than such standardized substrates, from the market. In addition, very thin glass substrates have a problem in the production process in terms of mechanical strength and bending or deformation, which reduces the production yield. For this reason, the liquid crystal display panel is formed by the standardized glass substrates and is thinned by polishing the external surface of the liquid crystal display panel.
When the thickness of the liquid crystal display device is reduced, there is a problem of mechanical strength. If mechanical stress is applied to the display surface of the liquid crystal display panel, the liquid crystal display panel may be destroyed. In order to prevent this, a front window is attached to the side of the screen of the liquid crystal display panel when the liquid crystal display panel is mounted to a cellular phone set and the like.
In general, the front window is attached to the liquid crystal display panel with a UV curable resin. In order to improve design quality and image quality, as well as other improvements, a black border is printed around the front window. Ultraviolet light does not easily pass through the portion of the black border print, so that non-uniformity occurs in the UV curable resin.
Japanese Unexamined Publication No. 2009-192792 describes a method of curing the UV curable resin under the black border print by using the gradient the black border print, in order to eliminate the non-uniformity in the degree of curing of the UV curable resin. In other words, in Japanese Unexamined Publication No. 2009-192792, the area of the black border print is divided into two parts: one is the inner part where the color is light, and the other is the outer part where the color is deep. With this configuration, it is possible to prevent the stress in the curing of the resin.
However, in the technology described in Japanese Unexamined Publication No. 2009-192792, it is found that the stress generated on the glass substrate is not necessarily reduced and may increase the difference in the degree of curing of the UV curable resin. Further, the black border print is formed to increase the display quality level. However, there is also a problem that the screen is dims down when the blackening degree in the inner part of the black border print is low.
It is desirable that in a liquid crystal display device including a liquid crystal display panel to which a front window with a black border print is attached, yellow discoloration or other damage is prevented from occurring in the periphery of the display area of the liquid crystal display panel, by reducing the deformation due to the stress generated particularly on a counter substrate when an adhesive is cured onto the liquid crystal display panel.
The present invention is to solve the above problem. An example of one aspect of the present invention is as follows. There is provided a liquid crystal display device including a liquid crystal display panel to which a front window is attached. The liquid crystal display panel includes a TFT substrate in which pixels each having a pixel electrode and a TFT are formed, and a counter substrate in which color filters are formed. The TFT substrate and the counter substrate are bonded together by a sealing material. A liquid crystal is filled between the TFT substrate and the counter substrate. A lower polarization plate is attached to the side of the TFT substrate. Then, an upper polarization plate is attached to the side of the counter substrate. A black border is printed around the front window. The side of the front window in which the black border is printed is bonded to the upper polarization plate of the liquid crystal display panel by a UV curable resin. An inner end portion of the sealing material is formed in an inside of the inner end portion of the black border print of the front window.
In the liquid crystal display panel described above, preferably the inner end portion of the sealing material is 0.2 mm or more inside from the inner end portion of the black border print of the front window.
According to the present invention, it is possible to prevent the deformation of the counter substrate due to the curing shrinkage of the UV curable resin, in the liquid crystal display device in which the liquid crystal display panel and the front window are bonded together by the UV curable resin. Thus, it is possible to prevent yellow discoloration from occurring in the periphery of the display area.
Before the description of embodiments of the present invention, the problem occurred in the liquid crystal display device to which the present invention is applied will be described.
In
The front window 10 is bonded to the upper polarization plate 210 through an adhesive 50. The black border print 11 is formed in the lower periphery of the front window 10. The width of the black border print 11 in the short side where the flexible wiring substrate is not connected is about 10 mm. The adhesive 50 is a UV curable resin. The UV curable resin is initially a liquid that contains, for example, 27% to 30% acrylic oligomer. It is also possible to use acrylic resin containing UV reactive monomer or additive agent for photopolymerization and the like. In this case, the thickness of the adhesion can be about several μm to 30 μm.
During curing of the UV curable resin 50, curing shrinkage occurs. The curing shrinkage of the adhesive 50 occurs in the direction shown in the arrow of
The counter substrate 200 of the liquid crystal display panel is deformed as shown in
The deformation of the counter substrate 200 shown in
As an example of the filling method of the liquid crystal 60, there is One Drop Fill (ODF) method. One Drop Fill (ODF) is the method for precisely controlling the amount of liquid crystal 70, dropping the liquid crystal 70 into the counter substrate 200 in which the sealing material 150 is formed, and bonding the TFT substrate 100 and the counter substrate 200 to each other. The filling speed of the liquid crystal is faster in ODF than in the vacuum filling method. However, the TFT substrate 100 or the counter substrate 200 does not bend to the inside and is flat as shown in
The present invention is particularly effective with respect to a liquid crystal display panel in which a liquid crystal 70 is filled by the ODF process shown in
In
The liquid crystal is filled by the ODF process. In this case, the sealing material 150 is formed on the counter substrate 200, and the liquid crystal is dropped into the counter substrate 200 by the drop method. Then, the counter substrate 200 is bonded to the TFT substrate 100. The TFT substrate 100 is made larger than the counter substrate 200. An IC driver 40 and a flexible wiring substrate 30 are connected to the end portion of the TFT substrate 100 where the counter substrate does not overlap the TFT substrate 100.
A front window 10 is bonded to the upper polarization plate 210 attached to the counter substrate 200, by an adhesive 50 of UV curable resin. A black border print 11 is formed in the periphery of the front window 10. The width of the black border print is in the range of 0.5 mm to 10 mm. The feature of the present invention is that the inner end portion of the black border print 11 is inside the inner end portion of the sealing material 150 of the liquid crystal display panel.
In
The black border print 11 is formed in the lower periphery of the front window 10. The liquid crystal display panel and the front window 10 are bonded together by the UV curable resin 50. When the UV curable resin 50 is irradiated by ultraviolet light, curing shrinkage occurs. As a result, the film thickness of the adhesive 50 is reduced in the periphery of the liquid crystal display panel, and stress occurs in the counter substrate 200 of the liquid crystal display panel.
As the thickness of the counter substrate 200 is about 0.2 mm, so that the counter substrate 200 is easily deformed when the stress is applied. As a result, the gap between the TFT substrate 100 and the counter substrate 200 is changed as described with reference to
In the present invention, an inner end portion P1 of the sealing material 150 is located inside an inner end portion P2 of the black border print 11 of the front window 10. Preferably, the inner end portion P1 of the sealing material 150 is 0.2 mm or more inside from the inner end portion P2 of the black border print 11 of the front window 10. Further, in
In
As described above, according to the present invention, the sealing material 150 for bonding the TFT substrate 100 and the counter substrate 200 is formed at the location where the stress is the maximum, so that the counter substrate 200 is not likely to be deformed. Thus, the gap between the TFT substrate 100 and the counter substrate 200 can be kept constant.
Number | Date | Country | Kind |
---|---|---|---|
2011-213981 | Sep 2011 | JP | national |
The present application is a continuation of U.S. patent application Ser. No. 13/601,196, filed on Aug. 31, 2012, which claims priority from Japanese Patent Application JP 2011-213981 filed on Sep. 29, 2011. The entire disclosures of each of these applications are hereby incorporated herein by reference.
Number | Date | Country | |
---|---|---|---|
Parent | 13601196 | Aug 2012 | US |
Child | 14979849 | US |