1. Field of the Invention
The present invention relates to a liquid crystal panel, and more particularly, to a liquid crystal-on-silicon (LCoS) panel utilizing one or multiple spacer walls and one-drop-fill technology.
2. Description of the Prior Art
Liquid crystal-on-silicon (LCoS) micro-display panel is arguably the heart of the reflective LCoS projectors and rear-projection televisions. The LCoS micro-display devices are tiny, less expensive, and have high resolution. As known in the art, the difference between a LCoS micro-display and a conventional thin film transistor-liquid crystal display (TFT-LCD) is materials used for forming substrates. Both of a cover and a backplane are made of glass in a TFT-LCD, nevertheless, the cover in a LCoS display is made of glass, but the backplane in a LCoS display is a semiconductor silicon substrate. Therefore, a LCoS process combines LCD techniques and complementary metal-oxide semiconductor (CMOS) processes.
Please refer to
In LCD devices, the thickness of the liquid crystal layer 18, or the cell gap (i.e., the space between a transparent conducting substrate and a semiconductor substrate) has to be precisely controlled to a specific value so as to ensure the display performance. In order to maintain the cell gap, plastic beads, glass beads or glass fibers are normally interposed between two liquid crystal display substrates and used as spacers. Thus, this cell gap is defined by the spacer height. In a conventional LCD process, the spacers are positioned by spraying, so the positions between the two liquid crystal display substrates cannot be controlled accurately. Consequently, the display performance of the liquid crystal display device is affected due to light scattering by the spacers that are present in the light transmitting regions. Furthermore, the spacers tend to be mal-distributed so that the display performance in portions of the LCD with spacers bunched is impaired, and the uniformity of the cell gap cannot be precisely maintained.
According to the prior art, seal glue 20 is applied to the periphery of the display active area 14 of the silicon substrate 10. The seal glue 20 has a slit or break in it for liquid crystal injection in the subsequent processes. The prior art LCoS panel 10 has a drawback in that the design width of the seal glue 20 is about 2000 micrometers and the design width is about 500 micrometers, which occupy a large chip surface area. Further, in the traditional LC injection method, the cell will be vacuum filled by capillary attraction after the glass substrate 16 and the silicon substrate 12 are assembled. Such injection method has the drawbacks of wasting time and liquid crystal material.
Accordingly, it is the primary object of the present invention to provide an improved LCoS panel and method of making in order to solve the above-mentioned problems.
According to the claimed invention, a liquid crystal panel includes a first substrate having thereon a display active region; an inner spacer wall disposed on the first substrate along periphery of the display active region; an outer spacer wall disposed adjacent to the inner spacer wall on the first substrate, wherein the inner spacer wall and the outer spacer wall are of approximately equal height; a groove formed between the inner spacer wall and the outer spacer wall; a seal spread in the groove; a second substrate being supported by the inner spacer wall and the outer spacer wall and being glued to the first substrate via the seal, wherein the first substrate, the second substrate and the inner spacer wall define a chamber; and a liquid crystal layer filling the chamber by using one-drop-fill process.
According to another preferred embodiment, a method of fabricating a liquid crystal panel is disclosed. The method comprises the following steps:
(a) providing a first substrate comprising thereon a display active region;
(b) depositing a dielectric layer over the first substrate by using various deposition methods;
(c) etching a portion of the dielectric layer to expose the display active area and to form an inner spacer wall and an outer spacer wall enclosing the display active region, and a groove between the inner spacer wall and the outer spacer wall, wherein the inner spacer wall and the outer spacer wall are of approximately equal height;
(d) spreading seal in the groove;
(e) performing an one-drop-fill process to dispose drops of liquid crystal on the display active region within the inner spacer wall;
(f) placing a second substrate on the first substrate, wherein the second substrate is supported by the inner and outer spacer walls and is glued to the first substrate via the seal; and
(g) curing the seal.
These and other objectives of the present invention will no doubt become obvious to those of ordinary skill in the art after reading the following detailed description of the preferred embodiment that is illustrated in the various figures and drawings.
The accompanying drawings are included to provide a further understanding of the invention, and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention. In the drawings:
Please refer to
It is one salient feature of the invention that the display active region 54 of the silicon substrate 52 is surrounded by dual spacer walls including an inner spacer wall 62 and an outer spacer wall 64. According to the preferred embodiment of this invention, the inner spacer wall 62 and the outer spacer wall 64 are two parallel walls of approximately equal height. A groove 66 is provided in between the inner spacer wall 62 and the outer spacer wall 64 for accommodating seal 70. The groove 70 also increases the effective contact area between the seal 70 and the silicon substrate 52 such that the adhesion is improved. The inner spacer wall 62 and the outer spacer wall 64 have a flat top surface 62a and a flat top surface 64a, respectively. In addition, the plural bonding pads 522 are disposed on the shorter side of the silicon substrate 52.
According to this invention, the inner spacer wall 62 and the outer spacer wall 64 are fabricated at the last stage of the fabrication processes for making the silicon substrate 52. The inner spacer wall 62 and the outer spacer wall 64 are fabricated and defined along the periphery of the display active region 54 by using standard semiconductor processes such as chemical vapor deposition (CVD) methods, chemical mechanical polish (CMP), lithography and etching. According to the preferred embodiment, the inner spacer wall 62 and the outer spacer wall 64 are made of dielectric materials such as silicon dioxide, but not limited thereto.
In typical LCD devices, as mentioned above, spherical spacers such as plastic beads or glass beads are dispersed randomly on the entire silicon substrate, even in the display active region or viewing areas, or mixed with the glue seal. However, spacers in the viewing area of a display frequently lead to the reduced contrast of the display. In the present invention, the plastic beads or glass beads are not used and are replaced with the dual spacer walls, i.e., the inner spacer wall 62 and the outer spacer wall 64. By doing this, the cell gap is effectively controlled so as to assure the proper operation of the LCD devices. Since the conventional spherical spacers such as plastic beads or glass beads are omitted, the cost of the panel product can be reduced.
As shown in
Please refer to
As shown in
Since the inner spacer wall 162 and the outer spacer wall 164 are fabricated by standard semiconductor processes, the deviation of the height of the spacer walls is very small. The cell gap between the silicon substrate 152 and glass substrate is effectively controlled so as to assure the proper operation of the LCD devices. A groove 166 is formed between the inner spacer wall 162 and the outer spacer wall 164. As previously described, the groove 166 is used to accommodate seal and to increase the contact between the silicon substrate 152 and the seal.
As shown in
As shown in
Finally, as shown in
Those skilled in the art will readily observe that numerous modifications and alterations of the device and method may be made while retaining the teachings of the invention. Accordingly, the above disclosure should be construed as limited only by the metes and bounds of the appended claims.
This patent application is a continuation application of and claims priority to U.S. patent application Ser. No. 11/306,587, filed on Jan. 3, 2006, and entitled “LIQUID CRYSTAL PANEL HAVING MULTIPLE SPACER WALLS AND METHOD OF MAKING THE SAME” the entire contents of which are incorporated herein by reference.
Number | Name | Date | Kind |
---|---|---|---|
5982472 | Moore | Nov 1999 | A |
6355955 | Gardner | Mar 2002 | B1 |
6392733 | Gregory | May 2002 | B1 |
6646709 | Matsumoto | Nov 2003 | B2 |
6870591 | Lee et al. | Mar 2005 | B2 |
7038751 | Lee | May 2006 | B2 |
7102703 | Mathew et al. | Sep 2006 | B1 |
20020145698 | Imai | Oct 2002 | A1 |
20050073637 | Liao | Apr 2005 | A1 |
Number | Date | Country |
---|---|---|
1178094 | Dec 2004 | CN |
1632649 | Jun 2005 | CN |
1635427 | Jul 2005 | CN |
200240442 | Feb 2002 | JP |
2005309446 | Nov 2005 | JP |
574537 | Feb 2004 | TW |
591293 | Jun 2004 | TW |
200424723 | Nov 2004 | TW |
Number | Date | Country | |
---|---|---|---|
20090103038 A1 | Apr 2009 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 11306587 | Jan 2006 | US |
Child | 12344585 | US |