The present invention generally pertains to a folding side mirror structure and, more particularly, toward improved folding side mirror structure that permits use of dissimilar metals.
Assemblies including dissimilar metals, such as those having magnesium parts in combination with steel parts, suffer from galvanic corrosion. This inherent corrosion problem is exacerbated when the assembly is used in a wet environment. Due to these problems, the use of magnesium in automobiles has been rather limited, despite the weight savings and manufacturing efficiencies that could result from its implementation.
Folding automobile side mirrors are a particular application wherein galvanic corrosion resulting from the interaction of magnesium and steel has prevented the introduction of magnesium parts. For example, with reference to
Insofar as the spring 24 is ordinarily made from steel, and due to the fact that the spring 24 is in direct contact with the bracket 16, it is not possible to form the bracket 16 from magnesium. Moreover, the upwardly open annular chamber 18 receives and holds water that may be introduced into the folding mirror assembly (e.g. from rain, condensation, etc.), which would accelerate any galvanic corrosion should a steel/magnesium junction be present. Due in part to these problems, magnesium parts have not been incorporated into folding automobile side mirrors of the design illustrated in FIG. 6.
There has also been proposed, as illustrated in
A plastic washer 50 is placed over the lower end of the pivot post 40a, and is held in place by a lock nut 52. The spring 48 is received and retained between the washer 50 and the downwardly facing surface of the annular flange 42b. Accordingly, the spring 48, which is made of steel, is in direct contact with the inner base 42 at the annular flange 42b.
Therefore, while the problems associated with water intrusion at the hinge (i.e., in the area of the spring) are reduced or eliminated with the alternative design shown in
Accordingly, there exists a need in the art for an improved folding automobile side mirror that is configured so as to permit at least some of the mirror components to be formed from magnesium.
The present invention is directed toward an improved folding automobile side mirror assembly that is formed, at least partially, from magnesium. The present invention is further directed toward an improved hinge assembly for a folding automobile side mirror assembly that limits water intrusion and retention within the mirror assembly. The present invention is further directed toward such an improved hinge assembly that permits use of dissimilar metals, such as magnesium and steel, while minimizing risks associated with galvanic corrosion.
In accordance with the present invention, a folding automobile side mirror assembly, includes an outer base, an inner base, a bracket, upper and lower washer members, a lock nut, and a spring. The outer base is secured to a surface of a vehicle; the inner base and the bracket are disposed within a mirror housing that is pivotally secured to the outer base. The inner base includes an upstanding cylindrical wall that has an annular wall member extending inwardly therefrom while the bracket includes inner and outer cylindrical walls that are connected at upper ends thereof by an upper wall member.
In further accordance with the present invention, the upstanding cylindrical wall of the inner base is received between the inner and outer cylindrical wall members of the bracket. The upper and lower washer members are secured around inner cylindrical wall of the bracket and each includes a radially extending flange. The radially extending flange of the upper washer member is in engagement with the annular wall member of the inner base upstanding cylindrical wall. The lower washer member is disposed at a location spaced from the upper washer member and is held in place by the lock nut.
In further accordance with the present invention, the spring is disposed around the inner cylindrical wall and is in engagement with the radially extending flanges of the upper and lower washer members. The inner base is formed from a first metal and the spring is formed from a second metal, with the first and second metals being dissimilar and subject to galvanic corrosion. Preferably, magnesium or an alloy thereof is used as the first metal and steel is used as the second metal. The upper washer member is disposed between inner base and the spring and prevents galvanic corrosion therebetween.
These and further features of the invention will be apparent with reference to the following description and drawings, wherein:
With reference to
With reference to
Although the present invention is particularly concerned with structures and methods to permit use of magnesium and alloys thereof in assemblies that are ordinarily used in wet environments and in the presence of other steel parts, it is more broadly concerned with structures and methods that permit the use of dissimilar metals that would otherwise be subject to galvanic corrosion. Accordingly, the present invention, although described herein with reference to the preferred embodiment (which employs a part made from magnesium used in a mirror assembly incorporating steel), is not to be limited to this specifically described and presently preferred embodiment. Rather, it is considered apparent that one skilled in the art, with knowledge of the present invention, would be capable of altering the materials used (i.e., to use another combination of dissimilar metals that would otherwise be susceptible to galvanic corrosion) without departing from the scope and spirit of the present invention.
With further reference to
The upper washer member 114, which is generally L-shaped in cross section, is pushed on over the inner cylindrical wall 110a of the bracket 110 so as to have an elongated cylindrical leg 114a extending along the outer surface of the brackets inner cylindrical wall 110a and an annular rim 114b extending away from the inner cylindrical wall 110a and toward the inner surface of the inner base upstanding cylindrical wall 112a. Preferably, as best seen in
The lower washer member 116, which is pushed on over the inner cylindrical wall 110a of the bracket member 110 but retained at a location spaced downwardly from the upper washer member 114 a predetermined amount, is preferably identical to the upper washer member 114 but is inverted relative to the upper washer member 114. To that end, the lower washer member 116 has an elongated cylindrical leg 116a extending along the outer surface of the bracket's inner cylindrical wall 110a and an annular rim 116b extending away from the inner cylindrical wall 110a and toward the inner surface of the inner base upstanding cylindrical wall 112a.
The spring 108 is received between the upper and lower washer members 114, 116 and, more particularly, is in engagement with the annular rims 114b, 116b of the washer members 114, 116. The spring 108 is held in compression so as to exert a downward force on the lower washer member 116 and the bracket 110 and thereby help to retain the bracket 110 in engagement with the inner base 112.
The lock nut 118, which is pushed on over the lower end of the bracket inner cylindrical wall 110a, is downwardly adjacent and in face-to-face contact with the lower surface of the lower washer member annular rim 116b. To facilitate assembly and retention, the bracket inner cylindrical wall 110a preferably includes a circumferential groove into which an inwardly projection flange from the lock nut 118 is snap-fittingly inserted. The groove and flange cooperate to hold the lock nut 118 in place, and thereby retain the spring 108 in a compressed or biasing condition.
As noted hereinbefore, the spring 108 is preferably formed from steel, which is conventional. However, the inner base 112 is formed from magnesium. While the hinge assembly 106 is protected from water intrusion due to its closed upper end (via the bracket wall 110c), there would ordinarily still remain direct steel to magnesium contact at the flange 112b where the upper end of the spring 108 contacts the inner base 112. However, in the assembly according to the present invention, such corrosive contact is precluded by the placement of the upper washer member 114 therebetween. Accordingly, by introduction of the upper washer member 114 in this particular location, the damaging effects of galvanic corrosion are prevented and it is now possible to make the inner base 112 out of magnesium in an application in which, heretofore, the use of magnesium parts was impossible.
While the present invention has been described hereinbefore with particularity, it is considered apparent that the present invention is capable of numerous modifications, rearrangements, and substitutions of parts and, accordingly is not limited to the preferred embodiment specifically disclosed herein. Rather, the present invention is only to be defined by the claims appended hereto.
| Number | Name | Date | Kind |
|---|---|---|---|
| 3751141 | Brown | Aug 1973 | A |
| 4186905 | Brudy | Feb 1980 | A |
| 4626083 | Nakayama et al. | Dec 1986 | A |
| 4692000 | Wada et al. | Sep 1987 | A |
| 5315442 | Sato et al. | May 1994 | A |
| 5383057 | Kimura et al. | Jan 1995 | A |
| 5384660 | Oishi | Jan 1995 | A |
| 5432641 | Mochizuki | Jul 1995 | A |
| 5467222 | Oishi | Nov 1995 | A |
| 5477392 | Mochizuki et al. | Dec 1995 | A |
| 5684646 | Boddy | Nov 1997 | A |
| 5703731 | Boddy et al. | Dec 1997 | A |
| 5703732 | Boddy et al. | Dec 1997 | A |
| 5721646 | Catlin et al. | Feb 1998 | A |
| 5722629 | Lang et al. | Mar 1998 | A |
| 6132050 | Sakata et al. | Oct 2000 | A |
| 6371619 | Assinder et al. | Apr 2002 | B1 |
| 6399218 | Hitomi et al. | Jun 2002 | B2 |
| 6449107 | Tachibe et al. | Sep 2002 | B2 |
| 6481858 | Inagaki et al. | Nov 2002 | B2 |
| 6533202 | Koike | Mar 2003 | B1 |
| 20010015390 | Hitomi et al. | Aug 2001 | A1 |
| 20010022926 | Kitayama et al. | Sep 2001 | A1 |
| 20010030819 | Hattori et al. | Oct 2001 | A1 |
| Number | Date | Country |
|---|---|---|
| 2000-159012 | Jun 2000 | JP |