Claims
- 1. A method of manufacturing a keypad member with a character illumination expressed and formed in a colored transparent or colored translucent layer, the method comprising the steps of:forming a colored transparent or colored translucent layer over a surface portion of a keypad member for a contact, the keypad member being made up of rubber molded by using transparent or semitransparent elastic materials, said elastic material is selected from a group consisting of natural rubber (polyisoprene rubber, butadiene rubber, styrene butadiene rubber, chloroprene rubber, nitryl rubber, butyl rubber, ethylene propylene rubber, acrylic rubber, silicone rubber, fluoric rubber, urethane rubber, styrene base thermoplastic elastomer, olefin base thermoplastic elastomer, ester base thermoplastic elastomer and urethane base thermoplastic elastomer; applying a dark layer, which is one of a silicone ink black layer, a gray layer or a dark color layer, on said colored transparent or colored translucent layer, said dark layer being applied as an intermediate layer for enhancing optical energy absorption; forming a colored surface layer on said intermediate layer with silicone ink having a color or colors other than black and gray, said surface layer having a thickness set within a range from 50 μm to 15 μm and being substantially unabsorbing of a laser beam and substantially unremovable directly by said laser beam; irradiating said colored surface layer with said laser beam in the shape of characters or figures; burning up said intermediate layer by absorption of the energy of said laser beam; and at the same time, burning up and removing said colored surface layer in the shape of the characters or figures by said burning of said intermediate layer.
- 2. The method in accordance with claim 1, wherein:said intermediate layer is formed of a material to burn up and withdraw from said colored translucent or transparent layer when irradiated by the laser beam.
- 3. The method in accordance with claim 1, wherein:said intermediate layer and said colored surface layer are formed of a material and thickness to have burning up and removal of said intermediate layer by the laser cause removal of said colored surface layer adjacent burned portions of said intermediate layer.
- 4. A method of manufacturing a keypad for a contact of a character illumination rubber switch made up of rubber, in which a colored transparent or colored translucent layer of any color is expressed and formed, the method comprising the steps of:forming a keypad member of rubber molded by using transparent or semitransparent elastic materials, said keypad member having a surface portion, said elastic materials is selected from a group consisting of natural rubber (polyisoprene rubber), butadiene rubber, styrene butadiene rubber, chloroprene rubber, nitryl rubber, butyl rubber, ethylene propylene rubber, acrylic rubber, silicone rubber, fluoric rubber, urethane rubber, styrene base thermoplastic elastomer, olefin base thermoplastic elastomer, ester base thermoplastic elastomer, and urethane base thermoplastic elastomer; forming a colored transparent or colored translucent layer over said surface portion of a keypad member; applying a dark layer, which is one of a black layer, gray layer or a dark color layer, on said colored transparent or colored translucent layer, said dark layer being applied as an intermediate layer for enhancing optical energy absorption; forming a colored surface layer on said intermediate layer with a color or colors other than black and gray, said surface layer being substantially unabsorbing of a laser beam and incompletely removable by said laser beam; irradiating said colored surface layer with a laser beam in the shape of characters or figures; burning up said intermediate layer by absorption of the energy of said laser beam and at the same time, burning up and removing said colored surface layer in the shape of the characters or figures by said burning of said intermediate layer.
- 5. The method in accordance with claim 4, wherein:said intermediate layer is formed of a material to burn up and withdraw from said colored translucent or transparent layer when irradiated by the laser beam.
- 6. The method in accordance with claim 4, wherein:said intermediate layer and said colored surface layer are formed of a material and thickness to have burning up and removal of said intermediate layer by the laser cause removal of said colored surface layer adjacent burned portions of said intermediate layer.
- 7. A method of manufacturing a keypad member with an illumination character, the method comprising the steps of:providing a keypad member formed of transparent elastic material; applying a base layer over a surface portion of said keypad member, said base layer being one of a colored transparent or a colored translucent layer; applying an intermediate layer on said base layer, said intermediate layer being removable by absorption of a laser beam and selected from a group consisting of silicone ink black layer, a silicone ink gray layer, and a silicone ink dark color layer; applying a colored surface layer to said intermediate layer, said surface layer substantially passing said laser beam and being incompletely removable by said passing of said laser beam through said surface layer without damaging said elastic material, said colored surface layer being a color other than black or gray; irradiating portions of said intermediate layer with said laser beam to remove said portions of said intermediate layer in the shape of characters or figures and at the same time, burning up and removing said surface layer in the shape of the characters or figures by said burning of said intermediate layer.
- 8. The method in accordance with claim 7, wherein:said intermediate layer is formed of a material to burn up and withdraw from said colored translucent or transparent layer when irradiated by the laser beam.
- 9. The method in accordance with claim 7, wherein:said intermediate layer and said colored surface layer are formed of a material and thickness to have burning up and removal of said intermediate layer by the laser cause removal of said colored surface layer adjacent burned portions of said intermediate layer.
- 10. The method in accordance with claim 5, wherein:said irradiating passes the laser beam through said surface layer without substantially directly removing said surface layer by said laser beam. intermediate layer.
- 11. The method in accordance with claim 7, wherein:said elastic material is selected from a group consisting of natural rubber (polyisoprene rubber), butadiene rubber, styrene butadiene rubber, chloroprene rubber, nitryl rubber, butyl rubber, ethylene propylene rubber, acrylic rubber, silicone rubber, fluoric rubber, urethane rubber, styrene base thermoplastic elastomer, olefin base thermoplastic elastomer, ester base thermoplastic elastomer and urethane base thermoplastic elastomer.
Priority Claims (1)
Number |
Date |
Country |
Kind |
8-340427 |
Dec 1996 |
JP |
|
RELATED APPLICATIONS
This is a continuation in part of application Ser. No. 08/967,748 filed Nov. 10, 1997 now abandoned, and the entire disclosure of this prior application is considered to be part of the disclosure of the accompanying application and is hereby incorporated by reference therein.
US Referenced Citations (5)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
08/967748 |
Nov 1997 |
US |
Child |
09/325907 |
|
US |