1. Technical Field
The present disclosure relates to a metallic decorative part and a manufacturing method for the same.
2. Description of the Related Art
Recently, electronic devices, such as mobile phones, notebook computers, and personal digital assistants, are widely used. These electronic devices generally include housings having colorful and beautiful decorative surfaces. The decorative surfaces may be highly reflective.
Referring to
In the punching process, the first surface 801 becomes rough because the first mold 701 presses the first surface 801. The side surface 803 often forms a plurality of burrs 804 adjacent to the first surface 801 because of shear stresses F1, F2. In addition, a portion 805 of the second surface 802 adjacent to the side surface 803 often is rounded and depressed, resulting in a poor appearance and unsuitable for use as a decorative surface. Therefore, only the first surface 801 can be used as a decorative surface. However, a complex polishing process is needed to polish the first surface 801 and the side surface 803, resulting in an undesirable flatness and thicknesses of the metallic part 80.
Therefore, a new metallic decorative part and a manufacturing method for the same are desired in order to overcome the above-described shortcomings.
The components in the drawings are not necessarily drawn to scale, the emphasis instead being placed upon clearly illustrating the principles of the present disclosure.
Referring to
The metallic part 10 may be made of a metallic plate which has a mirror-like flat surface. A material of the metallic part 10 may be for example, stainless steel or copper. In the illustrated embodiment, the metallic part 10 is made of stainless steel. It may be understood that, the metallic part 10 may also be arc-shaped.
Referring to
It may be understood that, if a surface of the metal plate 20 is already a mirror-like surface, the polishing process may be omitted.
In step 202, a specialized film is adhered on the first surface 211 to prevent the first surface 211 from being damaged during the following process.
In step 203, a plurality of position holes 221 are punched or drilled in the metal plate 20. The position holes 221 may be adjacent to two sides of the metal plate 20 for locating the metal plate 20.
In step 204, a groove 23 may be formed in the first surface 211 of the metal plate 20 by a numerical control (NC) milling device (not shown). An outline of the sidewall 231 of the groove 23 corresponds to an outline of the metallic part 10. A ratio of the depth of the groove 23 with respect to the thickness of the metal plate 20 is larger than ⅓. In the illustrated embodiment, the ratio of the depth of the groove 23 with respect to the thickness of the metal plate 20 is about ½ to about ⅔. In this range, the groove 23 may be formed easily and the first surface 101 has a nice flatness.
In the illustrated embodiment, the position holes 221 of the metal plate 20 are sleeved on the positioning pins of the NC milling device, so that the metal plate 20 is fixed on a worktable of the NC milling device. A milling blade is driven to mill the first surface 211 of the metal plate 20, thereby forming the groove 23. A sidewall 231 of the groove 23 forms a side surface of the metallic part 10, so that a side surface 103 of the metallic part 10 has a plurality of milling traces.
Referring also to
A material of a connecting portion 29 between the preforming portion 27 and the remaining portion 25 is reduced because of the groove 23, the preforming portion 27 is easily separated from the metal plate 20, and the yield rate is enhanced. Since the first surface 211 is separated by a space from the connecting portion 29, a deformation of the first surface 211, which will become the first surface 101 of metallic part 10, is reduced or eliminated. Additionally, the first surface 101 is substantially perpendicular to the side surface 103 such that the first surface 101 and the side surface 103 cooperatively define a sharp-cornered edge. Furthermore, even if the side surface 103 forms a plurality of burrs, the burrs are adjacent to the second surface, so that after the metallic part 10 is assembled to an electronic device, the burrs are hidden from view.
In step 206, the specialized film on the first surface 101 of the metallic part 10 is removed and a protective film is adhered on the first surface 101.
In step 207, an adhesive may be coated on the second surface so that the metallic part 10 can be adhered onto other components.
It should be pointed out that the specialized film prevents the first surface from being scratched. In addition, if there are gas holes, cracks or impurities in the first surface, after the step 201, the gas holes, cracks or impurities are exposed and can be easily spotted by visual examination. It may be understood that, the metal plate 20 may be other shaped such as arc-shaped.
Finally, while various embodiments have been described and illustrated, the embodiments are not to be construed as being limited thereto. Various modifications can be made to the embodiments by those skilled in the art without departing from the true spirit and scope of the embodiments as defined by the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
200810303073.2 | Jul 2008 | CN | national |