1. Field of the Invention
The present invention relates to a method of cutting off glass panes or panels, especially rectangular glass panes or panels, from a continuously produced glass sheet, in which the glass sheet is continuously tested for glass faults prior to the cutting process and the glass sheet regions containing the glass faults or defects are determined and from the results of the fault detection an optimized cutting pattern for a given glass sheet section is determined in a cutting optimizing device. The cutting pattern comprises a plan for cutting the glass panes or panels into crosscut pieces and for cutting away glass panes of respective predetermined sizes arranged next to each other in corresponding ones of said crosscut pieces.
The invention also relates to an apparatus for cutting off the glass panes from the glass sheet including a conveying device for the glass sheet and for the crosscut pieces cut from it, a fault detecting device for detecting faults in the glass sheet, a crosscutting device for cutting off crosscut pieces, a glass pane cutting device and a cutting optimization device connected to the fault detecting device, the crosscutting device and the glass pane cutting device. The cutting optimization device comprises means for calculating an optimized cutting pattern for a given glass sheet section.
2. Description of the Related Art
During glass pane manufacture, especially during manufacture of display glass, a glass sheet is continuously produced, so-called crosscut pieces are cut off in further process steps, glass borders of the crosscut pieces are removed and the glass panes are cut to the desired size from the crosscut pieces. The “crosscut pieces” by definition are glass sheet strips with borders extending perpendicular to the feed direction of the glass sheet, from which one or more useful glass panes are cut away.
Prior to cutting off the glass panes a fault detection process for detecting faults in the glass sheet is performed so that the regions, which are not acceptable because of either the number and/or type of faults or defects, can be located. During the determination of the cutting pattern, which provides a surface-covering glass pane arrangement, the fault information is considered so that as small-sized glass panes as possible contain the fault-containing glass sheet regions to be cut off, whereby the available glass sheet regions are cut out without gaps. The optimized cutting pattern must be designed so that the glass panes in the crosscut pieces are next to each other without gaps, so that the crosscut piece defines the respective glass pane size. The crosscut pieces are placed next to each other without gaps. In so far as there are no strip-like waste regions between the crosscut pieces, which contain faults of this type, they must be separated or removed.
After the cutting process the finished glass panes, which contain the faults, from the crosscut pieces must be separated from the good glass panes.
When the batch permits the making of small-sized glass panes, the waste occurring in the known method can be reduced from the batch. However in a batch from which only large-sized glass panes are made, these large panes thus must be separated, when only small regions have unacceptable faults within the glass panes.
Additional waste can arise when a border at the edge region is damaged during the cutting process. Also in this case the entire adjacent glass pane next to the border must be discarded.
It is an object of the present invention to provide a method and apparatus for cutting off glass panes from a continuously produced glass sheet, which provides a higher yield, particularly of good quality glass panes without glass faults.
This object is attained with a method, in which the cutting lines for the glass panes to be cut off within each crosscut piece are placed in the fault-containing glass sheet regions to be discarded, so that the widths of the glass sheet regions to be discarded are minimized while providing a largest possible number of usable glass panes.
The invention is founded on the understanding that the yield of usable glass panes can be increased, when, starting from a cutting pattern of the highest quality, based on an analysis of the fault type and/or number, the positions of the glass panes within the respective crosscut pieces are moved perpendicular to the feed direction of the glass sheet, taking the location of the faults into account, so that the size of the glass sheet regions to be discarded are minimized. A flexible cutting pattern is provided, which is adjusted to the faults present in the respective crosscut pieces.
The quality taking into account the types and/or number of faults and the pane sizes desired by the customer is determined anew for each batch.
Different quality or also a downgrading of quality can be taken into account during the determination of the optimized cutting pattern. This can mean, for example, that glass panes with different quality can be placed in one crosscut piece. Alternatively it can mean that glass panes, which can be arranged in one crosscut piece beside glass panes of lower quality, are stepped down, when a larger glass pane size can be obtained with an entirely higher quality.
The glass panes within a crosscut piece can contact each other. However it is also possible that a strip that should be discarded can arise between the glass panes because of a fault-containing region. So that a clean separation of this strip is possible, which depends on each cutting process, a minimum width of this strip to be discarded must be maintained, in order to prevent breakage or damage to the adjacent glass pane during the cutting away process.
Preferably the widths BS of the glass sheet region or regions to be thrown out or discarded are greater than or equal to a minimum allowable strip width BR of the glass sheet region to be discarded.
Preferably this minimum allowable strip width BR is fixed at greater than or equal to 100 mm. These widths BR are apparatus or equipment specific. The widths BR can take smaller values, when the plant or equipment or apparatus permits that.
Thickness fluctuations, which are preferably accounted for during the cutting optimization, occur during glass sheet manufacture. A so-called good glass region is defined with the help of a similarly online measured thickness profile, which preferably is taken into account during calculation of the cutting pattern.
Preferably the glass fault detection is performed prior to cutting off of the borders, because the cutting off of the borders assumes that the crosscut piece size is established, which is determined by the cutting pattern. That means that the glass fault detection and the cutting pattern must be calculated before the crosscut pieces are cut away.
Preferably after cutting off the borders of the crosscut pieces an edge control process for finding edge faults can be performed. When the borders are cut off edge faults can be produced, so that the concerned adjacent glass panes must be separated after the conventional cutting pattern process. According to the invention a so-called post-optimization process is performed, in which these edge faults are taken into account during calculation of the cutting pattern.
It is possible to again determine the cutting pattern with the help of fault information from the edge control process and to calculate a further optimized cutting pattern, which is however connected with a considerable computational effort and corresponding time delay.
However basically there are only four variants for the results of the edge control process:
Because of the reduced number of possibilities the appropriate cutting pattern can preferably be made available or supplied already after the fault detection. Several cutting patterns are determined, in which a cutting line of at least one glass pane is placed at the edge of the good glass or no cutting line is placed at the edge of the good glass region, so that a distance BR is maintained from the edge of the good glass region.
The appropriate cutting pattern is selected from the previously calculated cutting patterns determined according to the results of the edge control process, so that no time loss occurs during the cutting pattern determination at his point in the execution of the method.
The apparatus for cutting off the glass panes is characterized by a cutting optimization device for calculating or determining at least one cutting pattern for a predetermined glass sheet section, in which the cutting lines for the glass pane to be cut away are placed sufficiently closely to the fault-containing glass sheet regions so that the widths Bs of the glass sheet regions to be discarded are minimized while providing a largest possible number of usable glass panes.
Preferably the apparatus has a main line and a branch line and the glass pane cutting device is arranged in the branch line. The branch line branches or splits off from the main line downstream from the edge control device, preferably at right angles from the main line.
The division of the apparatus into a main line and a branch line has the advantage that the unchanged remaining crosscut pieces can be further conveyed on the main line and can then already be packaged, while the remaining crosscut pieces can be cut into smaller sized glass panes in the branch line. The branch line has the further advantage that the crosscut pieces for the cutting process need not be rotated, because they have the correct orientation for the cutting devices when they are guided to the branch line.
Preferably an edge control device is arranged after the border trimming station, which is connected with the cutting optimization device. The data from the edge control device are thus transferred to the cutting optimization device, which can perform a post-optimization in the case of edge faults. When—as has already been explained in connection with the method according to the invention—already several further optimized cutting patterns have been calculated, a correctly fitting optimized cutting pattern can be selected from the previously calculated further optimized cutting patterns according to the measured edge faults.
Preferably a thickness-measuring device is arranged in the main line. The thickness profile is measured online with this thickness-measuring device, in order to determine the good glass widths. The thickness-measuring device is preferably connected to the cutting optimization device in this case.
The objects, features and advantages of the invention will now be described in more detail with the aid of the following description of the preferred embodiments, with reference to the accompanying figures in which:
a to 2c are three crosscut pieces with defect- or fault-containing glass sheet regions and cutting patterns according to the state of the art;
a to 3c are three crosscut pieces with defect- or fault-containing glass sheet regions, as shown in
In
Each crosscut piece 2 shown in
The glass fault 10 is located in the center pane 3b in
In
In this case, as in all the following examples, each of the glass sheet regions 13-15 must have a minimum width BR, so that the glass strip can be cut away without breaking and damage to the borders of the glass panes.
Another example of the cutting method of the prior art is shown in
According to the inventive cutting method shown in
In
According to
In
In
The apparatus for cutting off glass panes from a continuously produced glass sheet is shown in
The data regarding the detected glass sheet regions, which can include faults, are transmitted or input to the cutting optimization device 102 from the fault-detecting device 103. The cutting optimization device 102 is connected with the crosscutting device 104 (crosscutting bridge 104a and breaking roller 104b) and with the glass pane cutting unit 108 in the branch line 101. The cut-away crosscut pieces 2 are moved apart from each other in an accelerating section 105 downstream of the breaking roller 104b. The edge portions of the crosscut pieces 2 are removed in a subsequent or following border trimming station 106. The edges of the crosscut piece are tested for edge faults in the following edge control device 107. Those crosscut pieces 2, whose dimensions correspond to the predetermined desired glass pane size, are conveyed to the end of the main line 100 and packaged. Those crosscut pieces 2, which should be cut into smaller-sized pieces, are conveyed onto the branch line 101 and fed to the glass pane cutting unit 108 there. In this process the crosscut pieces are not rotated so that their wide sides are oriented parallel to the feed direction in the branch line 101. This has the advantage that the crosscut pieces 2 are already oriented in the correct manner for the glass pane cutting device 108.
The cutting optimization device 102 determines an optimum cutting pattern based on the faults found in the fault-detecting device 103. After that the glass panes on the branch line 101 are cut in the glass pane cutting device 108. The cutting optimization device 102 is also connected to the edge control device 107, which is arranged downstream of the border trimming station 106 in the main line 100. If an edge fault 18 should occur during border breaking or trimming, a fault signal is transmitted to the cutting optimization device 102. The cutting optimization device 102 performs a post-optimization of the cutting pattern prior to further cutting and transmits the appropriate information to the glass pane cutting unit 108, where the glass panes are subsequently cut according to the post-optimized cutting pattern. It is also possible to put possible cutting patterns for the post-optimization in the control unit of the glass pane cutting unit 108.
The disclosure in German Patent Application 103 35 247.3-45 of Aug. 1, 2003 is incorporated here by reference. This German Patent Application describes the invention described hereinabove and claimed in the claims appended herein below and provides the basis for a claim of priority for the instant invention under 35 U.S.C. 119.
While the invention has been illustrated and described as embodied in a method and apparatus for cutting off glass panes, especially rectangular glass panes, from a continuously generated glass sheet, it is not intended to be limited to the details shown, since various modifications and changes may be made without departing in any way from the spirit of the present invention.
Without further analysis, the foregoing will so fully reveal the gist of the present invention that others can, by applying current knowledge, readily adapt it for various applications without omitting features that, from the standpoint of prior art, fairly constitute essential characteristics of the generic or specific aspects of this invention.
Number | Date | Country | Kind |
---|---|---|---|
103 35 247.3 | Aug 2003 | DE | national |
This is a continuation of U.S. patent application Ser. No. 10/895,220, filed on Jul. 20, 2004. The invention described in the aforesaid U.S. patent application is also described and claimed herein below. The aforesaid U.S. patent application provides the basis for a claim of priority of invention for the invention claimed herein below under 35 U.S.C. 120.
Number | Date | Country | |
---|---|---|---|
Parent | 10895220 | Jul 2004 | US |
Child | 12264971 | US |