Claims
- 1. A method for fabricating an electroluminescent display, said method comprising:providing a substrate comprising a flexible base layer having a conducting surface on one side thereof, said base layer being at least 1000 times less permeable to oxygen and water than a PET film of the same thickness as said base layer, said substrate further comprising a plurality of wells defined by a barrier layer, each of said wells having an electrode layer connected electrically with said conducting surface; moving a first dispenser relative to said substrate so as to quantitatively deposit a first electroluminescent material on said substrate, different amounts of said first electroluminescent material being deposited at different locations on said substrate in response to signals defining an illumination pattern to be generated by said display; and depositing a conducting material on said first electroluminescent material.
- 2. The method of claim 1, further comprising the step of quantitatively depositing a second electroluminescent material on said substrate, said second electroluminescent material emitting light at a different wavelength than said first electroluminescent material.
- 3. The method of claim 1, wherein said conducting material comprises a hole transport material that facilitates the injection of holes into said first electroluminescent material.
- 4. The method of claim 1, wherein said conducting material comprises an electron transport material that facilitates the injection of electrons into said first electroluminescent material.
- 5. The method of claim 1, further comprising the step of depositing a non-luminescent material on said substrate at locations on said display that are not to emit light prior to depositing said conductive material.
- 6. The method of claim 5, wherein said non-luminescent material is an electrical insulator.
CROSS REFERENCE TO RELATED APPLICATION(S)
This is a divisional of copending application Ser. No. 09/363,964 filed on Jul. 29, 1999 now U.S. Patent No. 6,174,613.
US Referenced Citations (10)
Number |
Name |
Date |
Kind |
4684353 |
DeSouza |
Aug 1987 |
A |
5701055 |
Nagayama et al. |
Dec 1997 |
A |
5902688 |
Antoniadis et al. |
May 1999 |
A |
5902689 |
Vleggaar et al. |
May 1999 |
A |
5948552 |
Antoniadis et al. |
Sep 1999 |
A |
5972419 |
Roitman |
Oct 1999 |
A |
6016845 |
Quigley et al. |
Jan 2000 |
A |
6146225 |
Sheats et al. |
Nov 2000 |
A |
6210814 |
Thompson et al. |
Apr 2001 |
B1 |
6221438 |
Matthies |
Apr 2001 |
B1 |
Non-Patent Literature Citations (1)
Entry |
Yang et al., “Enhanced performance of polymer light-emitting diodes using high-surface area polyaniline network electrodes,” J. Appl. Phys., Jan. 15, 1995, vol. 77, No. 2, pp. 694-698. |