The present invention relates to a method and an apparatus for the production of a particle based element, in particular a particle board or fiber board, as defined in the preambles of the respective independent claims.
DE 103 15 922 A1 discloses the production of particle boards, wherein spray tubes are arranged in between or in the region of falling particle streams in a dispersing section of the particle board production apparatus, where the particle mass is formed by dispersing particles. The spraying tubes provide water containing treatment medium to the particles, wherein the arrangement of the spraying tubes in between the particle streams allows that the treatment medium can be provided inside the particle mass.
However, according to this teaching, the treatment medium is only provided in a thin layer of the particle mass.
It is the object of the present invention to provide a better distribution of a modification substance in a particle mass during manufacture of a particle based element.
The invention provides a method for the production of a particle based element, in particular a particle board or fiber board, comprising the steps of dispersing particles in a dispersing section to form a particle mass, and providing a modification substance, modifying the properties of the particle mass, such that particles with accordingly modified properties are arranged in at least one predetermined region of the particle mass, wherein the modification substance is injected into the particles before the particles form the particle mass, and wherein the modification substance is injected into the particles in an injection direction, which is inclined towards the flow direction of the particle stream at the injection location.
This provides the effect that modification substance is not only sprayed onto the particle mass, but is rather injected in between the falling particles, such that a larger amount of particles is in contact with the modification substance. In particular, the inclined injection enables that a gradient regarding the concentration of the modification substance in the particle mass can be obtained. Thus, the properties of a great amount of particles in the particle mass can be modified, and in particular a smooth transition in between the modified areas of the particle mass and the unmodified areas of the particle mass can be obtained due to the concentration gradient of the modification substance.
The particles forming the particle mass are preferably in the form of fibers. In particular, the particles are wood chips or other natural fibers. However, it is also possible to use plastic chips or fibers, as well glass or stone fibers or different types of particles prepared within chemical processes e.g. polyurethane or polystyrene based particles. Preferably, the particle based element is in the form of a board.
The modification substance is usually injected in a generally fan-shaped or conically shaped form, comparable with a spray cone of a spraying can. The injection direction of the modification substance is in particular to be understood as the central axis of the spray cone or spray wedge or as the average direction of the individual trajectories of the modification substance immediately before entering the particle mass.
Preferably, the inclination angle of the injection direction with respect to the flow direction of the particle stream is at least 10 degrees and preferably more than 45 degrees. In particular, the injection direction is a vector, which comprises a component which is perpendicular to the flow direction of the particle stream and directed towards the particle stream at the injection location, and a component which is parallel to the flow direction of the particle stream. The parallel component of the vector may be directed in the same direction as the flow direction of the particle stream or in the opposite direction. If it is directed in the same direction, a smoother injection may be obtained with less diversion of the falling particles. If it is directed in the opposite direction a more thorough mixing of the particles and modification substance may be obtained. In a preferred embodiment, the modification substance is injected in an injection direction substantially perpendicular to the flow direction of the particle stream at the injection location. This enables a deep injection of the modification substance and thus, a beneficial distribution of the modification substance.
In one embodiment, the modification substance is a treatment fluid. The treatment fluid may in particular be water. Some possible other treatment fluids are adhesive, resin, steam, chemical additives, hardener for two or several component adhesives or catalysts. The treatment fluid modifies in particular the properties of particle mass. The modification may relate to the interaction of the particles or to inherent properties of the particles. For example, the treatment fluid may change the compressive properties of the particles, i.e. that the particles show a higher or lower compressibility when being subjected to pressure.
In one embodiment, the modification substance is adhesive. The adhesive may be provided as a fluid, but also as a solid, meltable adhesive, which is only activated in a heating and compressing step. This adhesive could be also activated with a time-set chemical reaction. In particular, the time-set chemical reaction is adapted to harden the adhesive in between 20 seconds and 220 seconds after application, more preferably in between 40 seconds and 200 seconds after application. This value is chosen in dependency of the distance in between the dispersion means and a press for compressing the particle mass and the conveying speed of the particle mass in between the dispersion means and the press. The localized application of adhesive as possible with the inventive method enables to strengthen certain parts of the particle based element, while reducing the amount of necessary adhesive, which is beneficial regarding the production costs and ecological aspects of the particle based element.
In one embodiment, the modification substance is a hardener or catalyst. In particular, the hardener or catalyst interacts with adhesive, which has been previously applied to the particles. The hardener or catalyst may increase the speed of the hardening process of the modified area and shorten the production time as well as increase the mechanical or physical properties, in particular strength, of the final particle based element.
In another embodiment, the modification substance is a further type of particles with different properties than the other particles provided in the particle mass. Thus, when injecting the modification substance, further particles are injected in a stream of other particles, such that the particles are at least partially mixed. The mixing of the particles is beneficial in contrast to the relatively discrete arrangement of particles in different layers next to each other as known in the prior art. The further type of particles may be particles of a different size, material or properties than the other particles. For example, the further type of particles may be wood chips of a smaller or larger size, but also artificially produced particles, which may modify the properties of adjacent particles, in particular by chemical reactions.
In one embodiment, the modification substance is injected while the particles are falling from a dispersion means onto a support. The support is in particular a conveyor, such as a conveyor belt. Alternatively, the support may be a stationary plate or mold. In particular, the dispersion means is adapted to distribute the particles, such that they fall onto the support to form a particle mass on the support. Preferably, this distribution is equal. The particle mass on the support is subsequently preferably compressed and/or heated such that the particles bond with each other and a rigid particle based element is formed.
In one embodiment, the modification substance is injected at least 20 millimeters (mm) into the falling particles in the injection direction. Thus, in the falling particles in a depth of at least 20 mm, a gradient regarding the amount of modification substance with respect to the dispersed particles is formed. In other embodiments, the modification substance is injected at least 100 mm into the falling particles in the injection direction.
After the particles have formed the particle mass by being arranged on each other on the support, the modification substance injected at one injection location is present in at least 6% of the height of the particle mass. Preferably, the modification substance injected at one injection location is distributed in less than 50%, more preferably less than 25%, of the height of the particle mass. An injection at two injection locations may thus cover 100% of the height of the particle mass.
In case the modification substance is injected at several injection locations, such as opposite injection locations, the modification substance is preferably present in up to 50% of the height of the particle mass.
The particle mass is usually compressed after being arranged on the support, wherein the coefficient of compression is usually around 1:8 to 1:12, preferably 1:10 for a fiber board, and 1:2 to 1:5, preferably 1:3 to 1:4, for a wood chip board. A compression coefficient of around 1:10, indicates that the height of the particle mass is reduced ten times during compression, wherein the density is increased about ten times.
Preferably, the modification substance is injected from the side into the falling particles. In particular, an injection means is provided adjacent to a particle stream of particles falling onto the support such that the particles do not come into contact with the injection means but that the injection means can inject the modification substance directly into the particle stream. In another embodiment, the injection means may be arranged in the particle stream of falling particles, such that it splits the particle stream, wherein modification substance may be injected from one or several sides into the falling particles.
In another embodiment, the modification substance is injected while the particles are conveyed to a dispersion means from which the particles fall onto a support. Thus, the modification substance is injected upstream of the dispersion means. The stream of particles upstream of the dispersion means is substantially laminar, i.e. the particles are not substantially mixed during conveying. Thus, the modification substance remains in a well defined area of the conveyed particle mass, until it reaches the dispersion means and during dispersion, such that the desired distribution of the modification substance in the particle mass on the support can be attained. Again, the support is in particular a conveyor, preferably a conveyor belt, but may as well be a plate or mold.
In one embodiment, the modification substance is injected into the falling particles, such that the trajectories of falling particles obtain an additional horizontal component and an improved mixing of the falling particles and the modification substance is attained.
The invention further provides an apparatus for the production of a particle based element, in particular a particle board or fiber board, comprising a dispersion means adapted to distribute the particles in a dispersing section, a support arranged below the dispersion means such that a particle mass is formed on the support by particles falling from the dispersion means onto to the support, and an injection means providing a modification substance to the particles, wherein the injection means is arranged above the upper edge of the particle mass on the support, wherein the injection means comprises a nozzle defining a main injection direction for the modification substance to the particles, which is inclined with respect to the flow direction of the particle stream at the injection location. In particular, the main injection direction is defined by a vector, which has at least one component which is directed towards the particle stream and perpendicular to the flow direction of the particle stream at the injection location, while the other component of the vector may be directed either parallel or opposite the flow direction of the particle stream.
Preferably, the injection means is arranged such that the particles pass at both sides of the injection means, and the injection means comprise at least two nozzles, provided at opposite sides of the injection means, each injecting the modification substance to the respective portions of the particles passing the respective sides of the injection means. In particular, the injection means may comprise several tools being arranged in a spaced relationship substantially in a horizontal direction in the dispersing section above the upper part of the particle mass. Preferably, the injection means are adapted such that the particles flow around the tools before reaching the upper part of the particle mass.
The particles may be treated by the injection means, such that they have different properties than the particles which are not treated by the injection means. In particular, treatment may be gradual, depending on the amount of modification substance which is provided to the respective particles.
Each of the tools may be adapted to provide modification substance at predetermined time intervals, such that a predetermined pattern of treated particles in the particles is created. In particular, the treatment may be provided at predetermined discrete points in time, while continuously dispersing the particles to form the particle mass. The treatment may be effected at predefined discrete locations in the particle mass. While the particle mass is moving with respect to the tools, different areas of the particle stream may be provided with modification substance such that the predetermined pattern of modified particles with respect to the other particles in the particle mass can be created.
Preferably, a press is provided downstream of the dispersing section, which is adapted to compress and bond the particle mass to form a particle based element. The compression of the particle mass is in particular carried out with a compression ratio of in between 1:12 to 1:2 as already specified above in more detail. Preferably, the tool or at least one of the tools of the injection means has a convex upper side facing the flow of particles in the dispersing section. In some embodiments, the upper sides of the at least one tool adjacent to an upper edge of the tool have an acute angle with respect to each other at the upper edge.
Preferably, the tools are arranged in a spaced relationship substantially in the conveying direction of the particle mass on the support above the upper part of the particle mass in the dispersing section. The tools may be arranged at different heights. However, preferably the tools are arranged at the same height. In particular, the at least one tool has at least one nozzle arranged at its side.
In some embodiments, the nozzle of the injection means may be a particle provision device, which allows providing particles with different properties. However, in other embodiments, the nozzle is adapted to supply a treatment fluid as a modification substance.
In particular, the modified particles may be arranged in a wavelike form, zigzag form, in one or more, in particular 2, 3, 4, 5 or 6 parallel layers, which may be adjacent or in a distance to each other. Further, the modified particles may be arranged only locally in the aforementioned shapes, while the remaining particle mass is not modified.
The invention further relates to a particle based element, manufactured by a method according to the invention or by an apparatus according to the invention as specified above.
Preferably, the modification substance is provided in a layer of the particles mass, which has a height of about 6% to 100% of the height of the layer. A height of 100% is particularly obtained by providing an injection means with two tools, which each inject modification substance to about 50% of the particle mass.
Preferably, the concentration of the modification substance is distributed according to a continuous gradient in the layer. In particular, the distribution of the modification substance in the layer decreases approximately according to a degree 2 polynomial, i.e. a parabola, according to the function C=a(z−h)+b(z−h)2, wherein C is the concentration, z is the height direction coordinate of the particle mass, h is the location of the highest concentration of the modification substance, and a and b are the coefficients defining the polynomial.
Thus, the continuous gradient can be approximated either linear, in case b=0, or quadratic. The invention further relates to the method for the production of a particle based element, in particular a particle board or fiber board, comprising the steps of dispersing the particles in a dispersing section to form a particle mass, and locally injecting a modification substance, such that particles with accordingly modified properties are arranged in at least one predetermined region of the particle mass, wherein the modification substance is adhesive and is injected before the particles form the particle mass.
The distribution of adhesive before the particles are arranged on the support where they form a particle mass, and in particular during the dispersing of the particles is beneficial, as in the falling particle stream there are relatively large intervals in between the particles, such that the adhesive may be sprayed and distributed over a larger area within the falling particles, which leads to a better distribution of the adhesive in the particle mass. Thus, a distribution of the adhesive according to a gradient can be obtained in the particle mass, which greatly improves the stability of a particle board formed from the particle mass.
In the following, the invention will be described by means of exemplary embodiments, which are shown in the following figures:
In
An injection means 9 is arranged in the central subsection 7, wherein the injection means 9 comprises a tool 10 with nozzles 11 and 12 at opposite sides thereof. The nozzles 11, 12 are directed from the tool 10 towards the stream of falling particles in the subsections 6 and 8. Thus, the main injection direction defined by the nozzles 11, 12 is substantially horizontal and perpendicular to the side of the falling particles to which the respective nozzles 11, 12 are directed. However, the main injection direction may also be inclined with respect to the perpendicular direction towards the side of the falling particles. The injection means 9 provides through each of the nozzles 11, 12 the modification substance, which may be in the form of additional particles having different properties than the particles 2 provided by the dispersion means 4, or may be a treatment fluid, such as water or adhesive. The area of the particles next to the injection means in particular next to the nozzles is the injection location.
As can be seen in
As shown in
The distribution of the concentration of the modification substance 13 in the particle mass 15 is shown in the diagram on the right hand side of
Preferably, the injection means 9 extends linear in the normal direction of the drawing plane, wherein several discrete nozzles or one or several long slit-like nozzles may be provided along its extension. This applies for all injection means discussed in the following.
In
The injection means 9 according to
The subsequently arranged tools 16, 18, respectively tools 17, 19 may each provide a different modification substance. For example the upstream tools 16, 17 may provide adhesive, and the downstream tools 18, 19 may provide hardener for this adhesive.
In
In particular, the dispersion means 4 distributes the particles sufficiently equal, that the relative distribution of the modification substance 13 in the particles 2 is generally maintained when particles pass the dispersion means 4.
The distribution of the modification substance 13 in the particle mass 15 is shown in the diagram on the right hand side, wherein the more concentrated distribution and, thus, the smaller height of the layer L can be seen.
In
In
By injecting the modification substance in an injection direction, which is inclined towards the flow direction 200 of the falling particles, and which is in particular perpendicular to the flow direction 200 of the falling particles, an improved mixing of the particles and modification substance 13 can be obtained, such that a gradient as shown in the diagram in
However, the injection of modification substance 13 to the sides of the falling particles can as well be implemented above the dispersing means 4, as shown in the fifth embodiment of the invention according to
A sixth embodiment of the apparatus according to the invention is shown in
Generally, the at least one tool of the injection means 9 may comprise several nozzles, which inject modification substance 13 in several directions, where the main injection direction is the average direction of the nozzles at each side of the tool.
The method according to the invention is illustrated by Figures relating to the apparatus according to the invention. Generally modification substance is injected by means of the injection means 9 in a direction which is inclined towards the flow direction of the particle stream at the injection location. The injection location is generally the location which is adjacent to the nozzles of the injection means or the intersection of the spray cone or wedge formed by the modification substance injected by the nozzles and the volume of the particles.
According to an embodiment of the invention, a particle based element is provided in which one or several layers of particles mixed with modification substance are arranged. The concentration of the modification substance may be as illustrated in the Figures above. However, in same embodiments there may as well be a gradient of modification substance over the whole height of the particle mass. Furthermore, there may be adjacent layers in the particle mass, wherein the modification substance is distributed according to the same gradient, i.e., having a concentration which gets higher or lower in the same direction. Furthermore, the injection means may only operate in predetermined intervals, such that only parts of the particle mass in the conveying direction are provided with modification substance. Further, several injection means may be provided at different locations of the particle stream, which may each be operated at predetermined intervals, such that specific shapes of the modification substance can be created in particle mass, in particular 3D-shapes, such as a wavelike pattern or zigzag pattern.
Number | Date | Country | Kind |
---|---|---|---|
13001788.2 | Apr 2013 | EP | regional |