Claims
- 1. In a method of producing at least one fold in a plurality of superposed layers of paper webs, comprising the steps of:
- continually heating a liquid folding adjuvant, comprising essentially tap water, to a temperature in a range extending from essentially 30.degree. C. to 60.degree. C.;
- applying the heated tap water in the form of a thin jet to the top layer of said superposed layers of paper webs along a fold line;
- folding the web on which the heated tap water is applied along the fold line;
- applying glue from a glue applying system in the form of a stream to the layers of said superposed layers of paper webs below said top layer; and
- flushing the glue applying system with heated water.
Priority Claims (2)
Number |
Date |
Country |
Kind |
3735856 |
Oct 1987 |
DEX |
|
3740046 |
Nov 1987 |
DEX |
|
Parent Case Info
This is a continuation of co-pending application Ser. No. 07/259,736 filed on Oct. 19, 1988 now abandoned.
US Referenced Citations (9)
Non-Patent Literature Citations (1)
Entry |
IBM Technical Disclosure Bulletin, vol. 17, No. 4, pp. 1098-1099, Sep. 1974. |
Continuations (1)
|
Number |
Date |
Country |
Parent |
259736 |
Oct 1988 |
|