The invention relates to a method for heating an end section of a plastic pipe according to the preamble of claim 1 as well as a device for performing the corresponding method.
Plastic pipes produced by a continuous method are usually divided into certain lengths for storage, shipping and use. In sewer technology in particular, a number of different pipe lengths are assembled in a suitable manner to form pipelines at the construction site. One end of a pipe is provided with a sleeve into which the spigot end of another pipe can be inserted.
To produce a sleeve on a pipe, the corresponding end of the pipe is usually heated first to the deformation temperature and then the sleeve is shaped using a molding tool.
For heating the end section of a plastic pipe to the deformation temperature, it is known that the end section can be contacted by means of external heating jaws and the interior of the end section can be heated by a heating mandrel in a noncontact process. To compensate for manufacturing tolerances, a gap is usually provided between the heating mandrel and the interior wall of the pipe. Heat is transferred by means of radiant heat here. It is also known that the interior of the pipe can be heated by hot air.
It is known from DE 25 36 306 B2 that the end sections of a pipe can be heated by means of an infrared lamp, which is cooled by a stream of air during this heating. A similar design can also be found in EP 1 315 604 B1, in which several radiant heating elements are arranged eccentrically on a carrier that can be driven to rotate about the axis of the pipe, while gas jets assigned to them cool the interior of the plastic pipe at the site of the greatest thermal radiation. This cooling is necessary because high-energy input into the interior of the pipe is necessary to shorten the heating time, on the one hand, but, on the other hand, radiant heating without cooling the interior of the pipe would result in excessive surface temperatures. Instead of a radiant heating element, contact heating elements, which are designed as spreading mandrels, are also known but they are complex to manufacture and operate.
Another problem in heating plastic pipes is that there is a certain shrinkage of the diameter at the cut edge of a pipe, in particular when it is made of high-shrinkage plastics, such as polypropylene, polyethylene or PVC. When the end section of a pipe is heated by means of external heating jaws in contact with the pipe, there is no direct contact there because of the shrinkage of the end region of the pipe, so that adequate heating is not achieved on the exterior in the end region of the pipe. As a result, the dimensional stability may be impaired in subsequent production of the sleeve at the end of the pipe. At a construction site, when connecting the spigot end of one pipe with a maximum diameter by inserting it into a sleeve, it is often necessary to discard such pipes as not fitting.
Storage at an elevated temperature may also result in shrinkage in the end region of the pipe before beading and may make the pipe difficult to connect.
The object of the present invention is therefore to provide a method for heating an end section of a plastic pipe to prepare for the formation of a sleeve such that complete heating of the end section of the pipe up to the cut edge is possible. In addition, the invention is based on the object of providing a device for carrying out a corresponding method.
This object is achieved by the invention defined in claims 1 and 5. Refinements of the invention are defined in the dependent claims.
With the subject matter of the invention, the end section of a plastic pipe is heated in preparation for forming a sleeve due to the fact that the end section is brought in contact with heating jaws on the exterior, and on the interior it is heated to a temperature at or above the deformation temperature of the plastic pipe by means of a heating mandrel that can be inserted into the plastic pipe from the end.
This method according to the invention uses a heating mandrel, whose diameter along a first forward length section is selected to be slightly smaller than the internal diameter of the end section of the pipe. However, the diameter of the heating mandrel over a second length section following the first length section is increased, so that the end of the second length section comes in contact with the interior of the pipe when the end section of the pipe is heated, so that the end of the end section of the pipe is in contact with both the external heating jaws and the heating mandrel when the end section is being heated.
Although the heating mandrel forms a small gap from the interior of the pipe over the first longitudinal section, the gap is reduced toward the end of the second length section in such a way that the rear end of the heating mandrel can come in contact with the interior of the pipe on insertion into the pipe and thus the pipe can become wider to the extent that it can also come in contact with the external heating jaws along its cut edge, so that the pipe may be heated as required up to the cut edge.
The heating mandrel is preferably designed as a cylindrical metal body having a first diameter, which is selected along a first forward length section, and a second length section at the end of the heating mandrel with a second diameter, such that the second diameter is larger than the first diameter. The second length section increases in a wedge shape from the first diameter to the second diameter at the end of the heating mandrel.
On insertion of such a heating mandrel into a plastic pipe, the wedge shape at the end displaces any possible shrinkage of the plastic pipe outward, so that the external end of the plastic pipe, which is in contact with the cut edge, can itself come in contact with the external heating jaws on the exterior, thus allowing adequate heating of the pipe to take place. The first length section preferably extends into the region of beading to be formed in the pipe during the formation of the sleeve, and the second length section corresponds approximately to the length between the cut edge and the formation of the beading that is to be provided.
The heating temperatures for polypropylene and polyethylene pipes are preferably 150°-160° C. for the external heating jaws and 140°-180° C. for the surface of the heating mandrel.
In the case of PVC pipes, the preferred temperatures for the external jaws are 130°-150° C. and for the heating mandrel 120°-160° C.
The wedge angle of the second longitudinal section is approx. 2°-20°, preferably 5°.
The second length section is preferably also connected to a third cylindrical length section, whose diameter corresponds to the diameter of the rear end of the second length section.
The cylindrical heating mandrel is made in particular of solid aluminum or an aluminum alloy and has a central borehole to receive a central heating element, which may be designed as an electric heating cartridge, for example. Instead of a central heating element, the heating mandrel may also contain boreholes arranged in a ring on the circumference, each of which is designed to receive a heating rod. The heating mandrel may have an annular design, so that its total mass is reduced.
The invention will now be explained in greater detail on the basis of one exemplary embodiment, in which:
The cross section illustrated in
The external shell-type heating jaws 2, 3 are brought into contact with the exterior of the plastic pipe 1. When the heating jaws are closed, the pipe is secured in such a way that lateral displacement of the pipe on insertion of the heating mandrel is prevented, in particular when the rear inclination (second length section 5) widens the end of the pipe. The cylindrical heating mandrel 4 has a small distance of 0.5-2 mm from the interior of the plastic pipe to be able to equalize manufacturing tolerances in the plastic pipe, so that no clamping can occur in insertion of the heating mandrel into the plastic pipe and extraction therefrom.
The temperature of the external heating jaws is 150°-160° C. for propylene and polyethylene pipes, and the temperature of the heating mandrel is 140°-180° C.
When using the heating device for PVC pipes, the temperature of the external heating jaws is 130°-150° C. and the temperature of the heating mandrel is 120°-160° C.
To improve the sliding properties of the heating mandrel on insertion into and extraction out of the pipe, the surface of the heating mandrel is hard-anodized to yield a smooth, hard surface.
The forward edge of the heating mandrel 4 on the forward edge of the length section 6 may be designed with a bevel to prevent problems on insertion of the heating mandrel into the pipe due to an excessive shrinkage of the pipe at the end.
Number | Date | Country | Kind |
---|---|---|---|
12153486 | Feb 2012 | EP | regional |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/EP2013/051600 | 1/28/2013 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2013/113662 | 8/8/2013 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
3484321 | Oswald | Dec 1969 | A |
3728059 | de Putter | Apr 1973 | A |
3761550 | Seefluth | Sep 1973 | A |
3899565 | de Putter | Aug 1975 | A |
3991150 | De Putter | Nov 1976 | A |
4107249 | Murai | Aug 1978 | A |
4150087 | de Putter | Apr 1979 | A |
4157372 | Kyomen | Jun 1979 | A |
4207283 | French | Jun 1980 | A |
4217096 | Hayes | Aug 1980 | A |
4352659 | Salmela | Oct 1982 | A |
4406852 | Riegel | Sep 1983 | A |
4430052 | Olsson | Feb 1984 | A |
5057263 | Bengtsson | Oct 1991 | A |
5145629 | Nilsson | Sep 1992 | A |
5948332 | Prenger | Sep 1999 | A |
6596121 | Reynolds, Jr. | Jul 2003 | B1 |
20100264564 | Tabanelli | Oct 2010 | A1 |
Number | Date | Country |
---|---|---|
2536306 | Feb 1977 | DE |
3045374 | Jul 1982 | DE |
1315604 | Oct 2011 | EP |
Number | Date | Country | |
---|---|---|---|
20140349238 A1 | Nov 2014 | US |