The invention relates to a method for the continuous production of a pipe according to the preamble of claim 1. Furthermore, the invention relates to a device for producing such a pipe.
Thermally insulated, corrugated pipes are well known and are used, for example, for district heating supply. Such pipes are also used to transport liquids or gases for other applications, especially in the oil and gas industry. A well-known method for their continuous production is described in EP 0 897 788 A1. In this method, at least one inner pipe is wrapped in a foil tube and plastic material is inserted into the foil tube, which foams up and forms the thermal insulation. After passing through forming jaws to form the corrugation, the outer jacket is extruded onto the corrugated surface of the tube. This method has proven to be successful. In order to achieve a deep corrugation, which is preferred for the windability of the line pipe for transport and for enabling small radii during its installation, WO 2010/085906 A1 proposes to process the line pipe with additional forming tools during its production after the extruder. This allows a deep corrugation to be achieved, but the method is complex and extends the production line. WO 2014/122278 A1 proposes to achieve a very flexible pipe and a manufacturing device with low space requirements by extruding the outer jacket directly onto the still expanding composite of foil tube and thermal insulation and passing the resulting composite of still expanding thermal insulation and the smooth outer jacket through a corrugator in which the thermal insulation and the outer jacket expand further together. The outer jacket material is pressed by the expanding thermal insulation foam into the recesses of the corrugator. A further method is known from WO 2008/142211 A1. An inner pipe surrounded by cured PU foam is wrapped with a PE mat, after which a foil is tightly wrapped around the PE mat. The corrugated jacket is applied to this composite in a corrugator, wherein the heat causes the foil to burst and the PE mat to expand to its original state, clamping the insulated pipe in the corrugated jacket.
The objective of the invention is to create a further manufacturing method. This shall produce a pipe with a deep corrugation and thus high flexibility.
In a manufacturing method of the type mentioned above, this is achieved by feeding the outer jacket separately from the inner pipe, which is surrounded by the foil tube, into the corrugator and forming it in the corrugator, whereupon the foaming of the thermal insulation takes place in the already formed outer jacket.
In the present invention or the method for the continuous production of a heat-insulated, corrugated line pipe with an inner pipe, the corrugated outer jacket is thus first produced with an extruder and with a corrugator and the inner pipe arranged in a foil tube together with a foam-forming starting material is led into the corrugator, in which the outer jacket of the line pipe previously formed in the corrugator is filled with the heat-insulating foam. The method is also well suited for the production of pipes with a very thin thermal insulation.
The corrugation of the outer jacket in the corrugator takes place independently of the foaming pressure, which enables a very well controllable formation or shaping of the corrugated outer jacket without any defects in the outer jacket and, if desired, with a large corrugation depth. The foam formation which only takes place in the already formed outer jacket has no significant influence on the shape of the outer jacket, especially since the foam formation after the previous formation of the corrugated outer jacket is preferably still taking place in the corrugator in which the outer jacket is held stable. For the formation of the outer jacket in the corrugator, a vacuum-corrugator is used in particular, in which the forming is carried out by a vacuum acting between the corrugator's mould parts and the outer jacket to be formed.
In order to ensure that the foaming only takes place in the corrugator, a mixture of starting materials is used to form the insulating foam, the reactivity of which is adjusted so that, depending on the speed of the production line for the line pipe and the temperature conditions, the foaming reaction only takes place in the corrugator. Usually, a two-component mixture is used, in particular comprising polyol and isocyanate to form a polyurethane foam. In particular, the reactivity is adjusted in such a way that the foam is formed after 10 seconds to 60 seconds and particularly after 15 seconds to 20 seconds. With the specified starting time, the foam formation occurs mainly only after the formation of the finished formed outer jacket in the corrugator or the mixture of the foam-forming components is still liquid when it arrives in the corrugator—lying in the foil forming the foil tube. In addition or alternatively, the foam formation of the starting material in the foil tube is influenced by cooling as it passes through the extruder.
Preferably, the method is carried out in such a way that a protective pipe running through the extruder is used, in which the inner pipe surrounded by the foil tube is led through the extruder, whereby the protective pipe runs into the closed mould parts of the corrugator. The outer jacket is corrugated in the corrugator above the protective pipe. Preferably, the protective pipe is provided on the outside and preferably also on the inside with a friction-reducing coating, particularly with a coating containing or consisting of polytetrafluoroethylene (PTFE). The outside coating prevents the outer jacket material exiting the extruder from sticking to the protective pipe if the outer material, which normally comes directly from the extruder into the vacuum zone of the corrugator, should come into contact with the protective pipe, which is not intended but can happen. Usually the outer jacket material is high-density polyethylene (HDPE) or another plastic material used for the outer jacket of the above-mentioned type of line pipes, whereby its adhesion to the protective pipe can be avoided by a PTFE coating or other adhesion and friction reducing coating of the protective pipe. Preferably, the protective pipe is adjustable in the longitudinal direction of the extruder, whereby the position of the front end of the protective pipe in the corrugator can be adjusted. This allows the protective pipe to be fed into the corrugator until the outer jacket is completely formed before it is exposed to the foaming pressure of the forming thermal insulation foam.
It is desired that the foil of the foil tube, which is pressed by the expanding foam against the inner side of the corrugated outer jacket, is bonded or welded to the outer jacket under the effect of the existing process heat. This is the case with a foil made of polyethylene (PE). Advantageously, a polyethylene (PE) coated foil can particularly also be used, particularly a polyamide foil coated on both sides with polyethylene, the advantage of which is a higher temperature resistance. Advantageously, a foil with a low thickness of 0.01 to 0.20 mm and particularly with a thickness of 50 μm to 120 μm is used.
Furthermore, the invention has the objective to provide a device for the production of a thermally insulated, corrugated line pipe.
This objective is reached with a device according to claim 11.
The device for carrying out the method thus has a protective pipe, by means of which the inner pipe surrounded by the foil tube can be guided separately from the extrusion and corrugation of the outer jacket into the corrugator.
Preferably, the device is designed so that the end of the protective pipe guided into the corrugator is located in the area of the corrugator in which the mould blocks of the corrugator are completely closed. Preferably, the protective pipe is held in the device in such a way that it can be adjusted in its longitudinal direction. Furthermore, it is preferable that a cooling device is provided by which the protective pipe can be cooled within the extruder, whereby foaming that occurs too early can be easily avoided. Furthermore, the device is preferably designed in such a way that the protective pipe is provided with a friction-reducing coating on the outside and inside.
Further embodiments, advantages and applications of the invention result from the dependent claims and from the following description of the figures. It is thereby shown in:
The extrudate exits from extruder 27 and enters the mould parts of the corrugator 28, in which the outer jacket 4 of the line pipe 1 is given the desired corrugation shape and finished. This takes place in the area 28′, in which the inner pipe 2 surrounded by the foil tube still runs in the protective pipe 26. When the inner pipe 2 leaves the protective pipe 26, the expanding thermal insulation foam can fill the already corrugated outer jacket 4 to form the pipe 1. This filling preferably takes place inside the corrugator 28. A measuring device 29 known to the skilled person, which follows the corrugator 28, checks whether the inner pipe 2 is centered in the line pipe 1 within the given tolerance. A cooling station 30 and a transport port 31 that pulls the pipe and a winding station 33 for forming a coil 32 of the finished pipe 1 follow.
The production speed of the device can, for example, be between 3 m/min and 6 m/min.
The protective pipe 26 runs in longitudinal direction of the device in extruder 27. The inner pipe 2 with the foil tube is fed through the extruder inside the protective pipe. The free end 26′ of the protective pipe 26 lies in the corrugator 28.
The extrusion of the material of the outer jacket 4 of the line pipe is carried out by the extruder 27 in a manner basically known to the skilled person. The plastic outer jacket material, for example HDPE, is melted in the extruder and leaves the annular outlet 27′ of the extruder 27 as extrudate. This is done completely separated from the inner pipe, which is separated from the extruder by the protective pipe inside the protective pipe. The corrugated outer jacket 4 can then be produced in the corrugator. The extruded outer jacket material is fed directly into the corrugator 28 from the extruder. The corrugator 28 is shown in
The starting time for the reaction of the reaction components filled into the foil tube via the mixing head is set in such a way that the foam formation and thus the so-called foam front mainly occurs only in the end area of the protective pipe or after the end 26′ of the protective pipe. In
The starting time of the component mixture that forms the thermal insulation foam must be set according to the length of the manufacturing device from the point where the reaction components are filled into the foil tube to the end of the protective pipe where the reaction begins and according to the production speed for the line pipe in meters per second. This setting for the start of the reaction can be adjusted in the range of 10 seconds to 60 seconds and particularly in the range of 15-20 seconds. The setting of such a reaction time or start time is known to the skilled person, and corresponding components for the foam formation are commercially available and their start time is defined. If necessary, a retarding agent can be added to the foam components. In the present method, a flexible PUR insulating foam is preferably used and the polyol and isocyanate components used for its production are known to the skilled person with the setting of the start time.
Preferably, a coolant for the protective pipe is provided in extruder 27 around the outside of protective pipe 26, for example in the form of a cooling coil surrounding it or a cooling pipe 16, as shown in
The protective pipe 26 is preferably provided with a friction-reducing coating, for example a PTFE coating, at least in the extrusion area of the extruder, which prevents the extruded outer jacket material from sticking to the protective pipe. Although it is not extruded onto the protective pipe, the extrudate may come into contact with the protective pipe. On the inside, the protective pipe 26 is also provided with a friction-resistant coating, particularly a PTFE coating. This allows the foil tube to slide along the inner surface of the protective pipe with as little friction as possible.
As material for the foil tube, a PE foil already known for this purpose can be used. When the thermal insulation foam is foamed, this foil bonds with the still hot inner surface of the outer jacket 4. A composite foil can also be used, for example a foil produced with the layer sequence PE-PA-PE. An advantage of a foil with polyamide is its excellent temperature resistance, particularly up to 200 degrees Celsius, compared to a pure PE foil. Preferably, a thin foil with a thickness in the range of 0.01 mm to 0.20 mm and particularly with a thickness of 50 micrometers to 120 micrometers is used for the foil tube. A thin foil facilitates the penetration of the thermal insulation foam into the already formed cavities of the corrugation of the outer jacket, if this is desired for the manufactured line pipe 1. In other words, by choosing a comparatively thicker foil, the filling of the cavities can be reduced or largely prevented, if this is desired.
It is also preferable to adjust the length of the protective pipe inside the device 10 in order to adjust the length of the end 26′ of the protective pipe in the corrugator. This allows the end of the protection tube to be adjusted to the range in which the outer jacket is completely formed.
In the present invention or the method for the continuous production of a heat-insulated, corrugated line pipe 1 with an inner pipe 2, the corrugated outer jacket is thus first produced with an extruder 27 and with a corrugator 28 and the inner pipe 2, which is arranged in a foil tube together with a foam-forming starting material, is guided with delayed foam formation into the corrugator, in which the previously corrugated outer jacket of the line pipe is filled with the heat-insulating foam. The device 10 provided for the execution of the method has a protective pipe 26, by means of which the inner pipe surrounded by the foil tube can be guided separately from the extrusion and corrugation of the outer jacket into the corrugator.
While the present application describes preferred embodiments of the invention, it must be clearly stated that the invention is not limited there and can be implemented in other ways within the scope of the following claims.
Number | Date | Country | Kind |
---|---|---|---|
00570/18 | May 2018 | CH | national |
This application is a National Stage application of International Patent Application No. PCT/EP2019/060583, filed on Apr. 25, 2019, which claims priority to Swiss Patent Application No. 00570/18 filed on May 7, 2018, each of which is hereby incorporated by reference in its entirety.
Filing Document | Filing Date | Country | Kind |
---|---|---|---|