1. Field of the Invention
The present invention relates to a method and a device for measuring the resistivity anisotropy of rocks exhibiting layerings such as laminations. This layering is due to the existence of clay layers or of compacted sand beds of different grain sizes. When the formation is 100% water saturated, the resistivity contrast is low (factor 3 for example). But in oil zones, this contrast is very high because of a very different water saturation.
Measurement of the resistivity index of core samples exhibiting such layerings is necessary to obtain a precise estimation of the water saturation from log data obtained for example by means of the measuring while drilling (MWD technique).
Knowledge of the resistivity anisotropy in two preferred directions is useful to determine the water saturation of the porous medium present between the laminations. In fact, the vertical resolution of well logging tools is often insufficient to detect the resistivity fluctuations resulting from the accumulation of the various layerings according to the depth. Furthermore, the laminations contain few hydrocarbons and can be of very low permeability because they often essentially consist of clay. Thus, it is well-known that measurement of the mean resistivity in a direction does not allow determination of the water saturation in the layers that can produce hydrocarbons.
2. Description of the Prior Art
EP-701,128 (U.S. Pat. No. 5,610,524) and French patent 2,581,573 (U.S. Pat. No. 5,979,223) filed by the assignee describe various methods and devices intended for continuous measurement of the curve of the resistivity index of a solid sample initially saturated with a first wetting fluid, such as a geologic sample, independently of the capillary pressure curve. The porous solid sample is contained in a sealed sheath placed in an elongate containment cell between two terminal parts. Channels through both terminal parts communicate with an injection system allowing injection of a second, non-wetting fluid into the sample at a first end of the cell and draining of the first fluid out of the cell at the opposite end, through a semipermeable membrane permeable to the first fluid. The sample is contained in a sheath and subjected to a radial pressure by injection of oil under pressure into the annular space between the body of the cell and the sheath. A membrane wettable only by the second fluid is interposed between the sample and the first end of the cell to carry out re-imbibition operations.
Electrodes interposed between the sample and the sample sheath allow application of an electric current and detection of the potential differences that appear between distinct points in response to the application of the electric current. The electrodes are connected to a device measuring the complex impedance of the sample. The longitudinal extension of the electrodes is relatively great in relation to the length of the sample so as to involve the largest possible part of the volume of the sample in the impedance measurements while avoiding short-circuits through the ends of the sample likely to distort the measurements.
One or more injection pressure stages are applied and the continuous variations of the resistivity index as a function of the mean saturation variation are measured without waiting for the capillary equilibria to be established.
Since the annular space between the sheath and the outer wall of the cell are under high pressure, the electric conductors connecting the electrodes to the measuring device run through the outer wall of the cell through sealed ducts (glass bead connectors for example).
In order to improve the measuring accuracy when operating at much higher frequencies in the 100 kHz–10 MHz range for example, it is possible to advantageously use the connection device described in French patent 2,809,821 (U.S. Pat. No. 6,571,606) filed by the assignee, which allows a shielded cable connection of the electrodes to a measuring device, located on either side of a wall separating an enclosure under pressure from the outside medium.
The method according to the invention allows measurement of the resistivity anisotropy of a porous sample traversed by at least one layering of different conductivity, such as a lamination, this sample being initially saturated with a first fluid. The method comprises setting the sample in a device comprising an elongate containment cell, with a first semipermeable filter permeable to the first fluid and arranged substantially in contact with a first end of the sample, and means for injecting under pressure a second fluid through a second end of the sample, the application of electrodes against the sample allowing application of an electric current and detection of the potential differences that appear between distinct application points in response to the application of the electric current, establishing at least one injection pressure stage for the second fluid and carrying out continuous precise measurements of the variations in the complex electric impedance of the sample at several frequencies during a displacement stage of the saturating fluid.
The method comprises:
According to a first implementation mode, the orientation of the sample in relation to the fixed direction of the electric field created by applying the electric current is changed prior to carrying out stage b) so that the layering is substantially in the same direction as the electric field.
According to another implementation mode, the direction of the electric field created by applying the electric current in relation to the sample is changed prior to carrying out stage b).
Electrodes, whose length ranges between ¼ and ¾ of the length of the sample and for example of the order of half the length of the sample, can be used.
According to an implementation mode, continuous precise measurements of the variations in the complex electric impedance of the sample at several frequencies during a drainage stage are performed.
According to an implementation mode, continuous precise measurements of the variations in the complex electric impedance of the sample at several frequencies during an imbibition stage are performed.
The device according to the invention allows measurement of the resistivity anisotropy of a porous sample crossed through by at least one layering of different conductivity, such as a lamination, comprising a containment cell for a sample initially saturated with a first fluid, pairs of electrodes pressed against the periphery of the sample allowing application of an electric current and detection of the potential differences that appear between distinct points of the sample in response to the application of the electric current, the electrodes being connected to a device for measuring the impedance of the sample, a first semipermeable filter permeable to the first fluid and arranged substantially in contact with a first end of the sample, and injection means for injecting under pressure a second fluid through a second end of the sample.
The device comprises a plurality of pairs of electrodes distributed over the periphery of the sample, which can be selectively connected to the measuring device so as to position the electric field created by applying the electric current to the sample respectively in the same direction as the layering, in stage b) substantially, and in a transverse direction to this layer in stage a).
Other features and advantages of the invention will be clear from reading the description hereafter of a non-limitative embodiment example, with reference to the accompanying drawings wherein:
The method according to the invention can be implemented by an experimental system intended for measurement of the variations in the resistivity index of a porous solid sample, resulting from forced displacements of a first electricity-conducting wetting fluid such as brine, for example, by injection of a second, non-conducting fluid such as oil, for example (drainage stage), or of the second fluid by the first fluid (imbibition stage) as described in the aforementioned patents filed by the assignee. The method comprises for example (
Channels 8 run through terminal part 3 and communicate with the network of grooves 7, on the terminal face thereof, with a first source 9 delivering the second fluid under pressure. Similarly, channels 10 run through terminal part 2 and communicate with the corresponding network of grooves 7 with a collection device 11 intended to recover the first fluid drained out of the sample as a result of the injection of the second fluid. An element 12 installed on circuit 9 is intended to measure the volume of fluid displaced out of sample S. A low-cost capacitive detector having a 0.05-cc precision and a 0.01-cc resolution, similar to the detector used in the device described in French patent application Patent 2,772,477 filed by the assignee, is preferably used.
The device comprises for example two pairs of electrodes E1, E2 which are cast inside sheath 4 so as to be tightly pressed against the peripheral wall of the sample, allowing an electric current to be applied. The potential difference V created in response to the application of the electric current is measured by means of another pair of electrodes E′1, E′2, similarly cast.
This separate allocation of the pairs of electrodes, one to the application of a current and the other to the measurement of potential differences, allows avoiding resistances due to contacts. The electrodes are, for example, of square shape and made of Monel. The angular extension of a pair of electrodes around the sample is below 90°. Their length has to be less than the length of the s ample so as to avoid end short-circuits exterior to the sample, directly through the fluids, which would distort the measurements. However, their length has to be great enough in relation to the length of the sample so that the current lines involve the largest part of the volume thereof with a relatively regular distribution. This length can vary in significant proportions depending on the diameter of the sample. In the experiments carried out, it has been found that the length of the electrodes can advantageously range between ¼ and ¾ of the length of the sample, and preferably be of the order of half this length.
The annular space 13 between body 1 and sheath 4 communicates with pressure means 14 allowing injection of a liquid under pressure which exerts a radial confining pressure on sample S. The radial confining pressure around the sample is for example of the order of some MPa, enough to provide good electric contact of the electrodes. Thus, under normal conditions, the contact resistance is generally of the same order as the resistance of the sample, which has to be measured with a low water saturation.
The assembly is placed in a thermostatically-controlled enclosure (not shown).
All the electrodes P are provided with a hollow extension 15 running through the thickness of sheath 4, and the electrodes are connected to an impedance meter RLC 16 coupled with a measurement acquisition device 17.
Implementation
Sample S, whose resistivity anisotropy is to be measured, is a rock bar (sandstone for example) exhibiting a layering such as a thin clay layer. This sample is saturated with a first fluid.
The sample S is first placed (
A second fluid, such as oil, is then injected through channels 8 at a first pressure and the variations in the complex impedance of the sample are continuously measured at several frequencies between 0.1 Hz and several tens of MHz, which are recorded by acquisition device 16, 17. The data are analyzed using a generalized resistivity index or impedance index which is a function of the saturation and of the frequency f, as defined below:
The previous operations are subsequently repeated after rotating the bar so that the layering (lamination) is now parallel to the direction of electric field EP (
In order to save dismantling the containment cell to reach the bar so as to rotate it and to change its orientation in relation to the electric field, it is possible to use a cell with electrodes distributed all over the periphery of the bar and to selectively connect them to measuring device 16, 17 so that the electric field EP created through the bar once set in the sheath and application of the electric current is alternately perpendicular and parallel to the layering (
Exploitation of Results
The resistivity anisotropy of the sample is deduced from the impedance measurements successively performed in the two directions.
A recent exploitation method allows, from knowledge of the resistivity anisotropy, to go back to the saturation in the hydrocarbon-producing layers. Resistivity anisotropy results for interpretation of resistivity logs are given in: “Anisotropy Of Resistivity In Oil Bearing Thin-Bedded Formations: Experiment and Modeling”, Clavaud J. B. and J. Lavigne, Proceedings of the 2003 International Conference of the Society of Core Analysts, 21–24, Pau, September 2003.
Knowledge of the volume fraction of the laminations and of the resistivity anisotropy as measured in the system described allows calculation of the water saturation of layers likely to produce hydrocarbons.
Number | Date | Country | Kind |
---|---|---|---|
03 11958 | Oct 2003 | FR | national |
Number | Name | Date | Kind |
---|---|---|---|
4686477 | Givens et al. | Aug 1987 | A |
4924187 | Sprunt et al. | May 1990 | A |
4926128 | Givens | May 1990 | A |
5093623 | Givens et al. | Mar 1992 | A |
5105154 | Givens et al. | Apr 1992 | A |
5610524 | Longeron et al. | Mar 1997 | A |
6229312 | Fleury et al. | May 2001 | B1 |
20010046811 | Fleury et al. | Nov 2001 | A1 |
Number | Date | Country | |
---|---|---|---|
20050104596 A1 | May 2005 | US |