The invention relates to a method of and an apparatus for continuously welding together plastic parts of a product along a joint region that extends around its circumference.
A known approach for welding plastic parts is to use a laser to apply the welding energy required to heat and melt the plastic at the joint region. EP 1 048 439 discloses a method of this type in which a through-welding process is used whereby a part that is transparent to laser light is welded to a part that is opaque to laser light. To accomplish this, the laser light source is moved along the joint region to melt the plastic while the parts are clamped relative to each other.
The known methods do not allow high cycle times and corresponding high unit production rates to be achieved for welding plastic parts. High cycle times and unit production rates are not achieved, for example, when producing final packaging for food or personal care products, or when manufacturing mass-produced medical products such as hollow needles. The closure that is securely clamped on a container typically is also secured by welding when these products are made.
The object of this invention is therefore to provide an apparatus for and a method of continuously welding together plastic parts that enables products to be produced with high cycle times and correspondingly high unit production rates.
This object is achieved according to the invention by an approach wherein the plastic product parts be welded are first moved into their joined position and secured there, after which the product for welding is conveyed past a stationary heat source, the product being rotated when being conveyed past the stationary heat source so as to apply the welding energy to the joint region.
According to the invention, the products have a joint region that extends around their circumferences. During welding they undergo two superimposed motions, of which one motion functions for transporting the product. The second product rotation enables the relative motion vis-à-vis the heat source to be executed such that the desired amount of welding energy is introduced into the entire joint region.
Claim 9 relates to an apparatus that is provided and suitable for implementing a method according to the invention. The subordinate claims comprise preferred, here especially preferred embodiments of the invention.
The additional product rotation can be provided by appropriately designed conveying elements. When welding products with curved surfaces, it is advantageously possible to generate the rotation by having the curved surface of the conveyed products be guided so as to roll along an outer surface, or a stationary or movable counter-holder. As a result, no separate drive means is required for one outer surface for the rotation, while, on the other hand, the approach provides a high level of flexibility by allowing a counter-holder to be moved to a specified position in which the containers can then roll along and in which it can then be moved back, for example, into a rest position.
Laser light sources are advantageously employed as the heat sources. Other suitable heat sources have a broadband infrared heat source in the shortwave or medium-wave range of the infrared, in particular, glass-tube, ceramic, metal-foil, or carbon heaters.
The laser light can be generated in point form or line form.
Welding is preferably effected in a through-welding process in which the outer part is transparent while the inner part is opaque to laser light. A possible alternative approach would be impact welding using the laser. The method of producing products is especially advantageous whereby a part is formed into rotationally symmetrical, specifically cylindrically tubular shape. The part is then turned in an additional rotation about its own axis, for example by guiding it so as to roll along an outer surface. A part of angular cross-section can also be welded by adjusting the rotational speed to match the product rotation of the part at the corners.
The invention will be described in more detail with reference to a method of and an apparatus for welding a closure to a cylindrically tubular beverage container.
The function of the apparatus showed in the figures is to continuously weld a closure 1 of a container 2 holding a liquid to the container 2 itself. To this end, roughly circular closures 1 that have a collar are first clamped onto the liquid container 2. The collar is located here so as to be fitted either inside as shown in
As
As an alternative to the laser light source, it is also possible to use one or more infrared light sources in either the short- or medium-wave region, such as, for example, glass-tube, ceramic, metal-foil, or carbon heaters.
In order to weld the plastic parts (here the container 2 to the closure 1), the product is conveyed past the stationary heat source 5. As it is being conveyed past the stationary heat source 5, the product 1, 2 is rotated while being conveyed, as is illustrated schematically in
In the case of rotationally symmetrical parts, such as for example cylindrically tubular parts as in this embodiment, the additional rotation is effected about the parts' own axes. If the products have appropriately curved outer surfaces, they can be guided so as to roll along an outer surface, thereby generating the rotation. This avoids the need for a separate rotational drive.
The additional rotation enables the welding energy delivered to the joint region to be adjusted in terms of the implementation, number, and speed of the rotations. Welding is preferably effected by the so-called through-welding process in which the outer part (here either the container 2 as in
Following the welding station 4, the products with the welded-together parts 1, 2 are passed on by a conveyor 6 for further processing, for example, to a packaging station.
In the embodiment of
The plastic parts (the container 2, the closure 1) are in each case manufactured from a weldable plastic, such as, for example, PE, PU, PVA, PET.