Any and all applications for which a foreign or domestic priority claim is identified in the Application Data Sheet as filed with the present application are hereby incorporated by reference under 37 CFR 1.57.
The present disclosure relates to a method and equipment for studying and establishing the physic-chemical conditions of stiction between a braking element, in particular a brake pad, and an element to be braked, in particular a vehicle brake disc.
It is known that, particularly under harsh operating and/or environmental conditions, for example, frequent off-road driving and/or driving on muddy tracks or routes exposed to brackish air or acid rain, this may result, in use, in the “gluing” of one or more of the brake pads of a vehicle to the relative brake disc made of cast iron or steel. This is generally due to corrosive phenomena that affect the brake disc and that, during braking, result in the corrosion products combining with the friction material of the brake pad causing accidental adhesion of the brake pad to the brake disc, adhesion that is temporarily maintained even when the vehicle brake is deactivated. This phenomenon of adhesion is known by the English technical term “stiction”, a term that derives from the contraction and merging of the terms “static” and “friction”, i.e. the term “static friction”.
The occurrence of a stiction gluing phenomenon on a vehicle in use involves various drawbacks, such as jolts/straining during braking and, subsequently the releasing of the brake, increased energy consumption and, in extreme cases, breakage of the friction material of the brake pad, which leads to vehicle breakdown and/or the necessity for the premature replacement of the brake pads.
Currently, there is no standardized and precise method or system for envisaging or at least reliably detecting the occurrence of “stiction” phenomena, nor that provides easily interpretable results in order to experimentally establish the chemical-physical conditions that can cause the onset thereof.
The purpose of this disclosure is to provide a simple and reliable method and simple and reliable equipment for studying and establishing the physic-chemical conditions of stiction between two mechanical elements and, specifically, between a braking element, in particular a brake pad, and an element to be braked, in particular a vehicle brake disc, in other words, to study and determine in the laboratory the causes of the stiction gluing phenomenon in vehicles.
This disclosure therefore provides a method and equipment for studying and establishing the physic-chemical conditions of stiction between two mechanical elements, and specifically between a braking element, in particular a brake pad, and an element to be braked, in particular a vehicle brake disc, having the characteristics set forth in the attached claims.
This disclosure will now be described in more detail with reference to the figures of the annexed drawings, in which:
With reference to
The stiction cell 1 comprises (
The support 9 is, as will be seen, a block of polymeric resin wherein there is embedded/incorporated, in the preferred embodiment illustrated, a disk sample 5, and which further contains an insulated electrical contact 12 for the connection of the sample 5 to the potentiostat as a working electrode.
The slide 8 slides along the respective lateral guides 11 of the body 6 that prevent the slide from rotating and is movable along the guides 11 to and from the first support 7.
The second support 9 consists of a prismatic block of an epoxy resin designed to carry internally embedded, in use, the second mechanical element 5, as is well illustrated in
This prismatic block is provided with the contact 12 consisting of an electrically insulated wire connected to the second mechanical element 5; the support 7 is carried by the body 6 in a static, fixed and predetermined position, arranged in axis with the support 9.
The handling device 10 preferably includes a metal screw 13 arranged in axis with the supports 7 and 9 and mechanically connected to the slide 8 and a metallic nut 14 engaged by the screw 13 and mounted through the body 6, integral to the same.
The slide 8 consists of a metallic bar, preferably prismatic.
The electric wire 12 is mechanically and electrically attached to a second face 17 of the mechanical element 5 opposite the face 15 by means of a welding spot 18 (
The equipment 3 comprises the electrochemical cell 2 in the entirety thereof (
The electrochemical cell 2 is therefore electrically composed by the working electrode consisting in the example illustrated by the sample of the element to be braked 5 (disc) assembled such that it is in contact with all or part of a braking element 4 (pad) by means of the stiction cell 1; by the reference electrode 20 consisting of any reference electrode that can be used for electrochemical measurements (for example an Ag/AgCl electrode (3M KCl); and by the counter-electrode 19 consisting of any counter-electrode that can be used for electrochemical measurements (for example a Pt electrode).
The electrolyte consists of any electrically conductive aqueous solution, for example from an aqueous solution of sodium chloride, for example at a concentration of 1% by weight of NaCl.
The equipment 3 also comprises a potential/current generator 23 consisting of an electronic potentiostat/galvanostat to which the reference electrode 20 and the counter-electrode 19 are electrically connected by means of appropriate cables 24 and to which the insulated electric wire 12 is also electrically connected, such that the second mechanical element 5, when it is electrically connected to the insulated electric wire 12, constitutes a working electrode of the electrochemical cell 2. Obviously, depending upon the experiments to be performed, a voltage generator only can be used, such as a potentiostat, or an electrical current generator only, such as a galvanostat, can be used instead of an instrument that can be used to generate both potential differences, fixed or variable, and preset or variable value electrical currents, and to polarize the working electrode in order to obtain potentiostatic or potentiodynamic polarization curves, everything according to settings that can be adjusted on the instrument 23. The equipment 3 finally comprises a torque wrench 25 of any known type for rotating the screw 13 in such a way as to push the second support 9 towards the first support 7 by applying a predetermined and known amount of torque to the screw 13.
By turning the screw 13 the exposed face 15 of the mechanical elements 5 is brought into contact with the mechanical element 4 and then pushed against it with a known and predetermined force, which is adjustable by means of the torque wrench 25.
The equipment 3 is, according to an aspect of the disclosure, completed by a test bench 26 illustrated schematically in
The test bench 26 includes a support base 27 designed to receive in use the mechanical elements 4 and 5, which are glued together by stiction, as will be seen, by the effect of the electrochemical process that occurred previously within the electrochemical cell 2; the support base 27 is equipped with a pusher 28 and a vice 29 designed to apply in use a progressively increasing thrust to one of the mechanical elements 4, 5 while the other is held firm by the vice 29. For example, the vice 29, which is movable on the base 27 and which holds the element 5 glued to the element 4 due to stiction but with the element 4 not tightened by the vice 29, is pushed by a lever 30 towards the pusher 28, fixed on the support base 27; an instrument 31, connected to the pusher 28 and integrally carried by the base 27 completes the test bench 26, in order to measure the thrust, i.e., the force, exchanged between pusher 28 and the element 4 due to the movement of the vice 29.
In particular, as will be seen, as a result of exposure to the electrolyte 21 and the electrochemical procedure carried out by the electrochemical cell 2, whilst the screw 13 pushes the face 15 against the element 4 with the predetermined force, the two mechanical elements 4 and 5 are made to permanently adhere to each other due to a stiction gluing phenomenon and are carried to the test bench 26 joined together; furthermore, the element 5 is rigidly incorporated into the support 9, which is then also transferred to the test bench 26 and which is used for example in order to block the element 5 on the support base 27 by means of the vice 29, while the pusher 27 acts laterally against the mechanical element 4.
Using the equipment 3 described thus far, a method can be followed for studying and establishing the physic-chemical conditions of stiction between two mechanical elements 4, 5, in particular between a braking element and a vehicle element to be braked.
In fact, according to the method of the disclosure, the first mechanical element 4 is a sample of predetermined first dimensions taken from a vehicle braking element in such a way as to include a friction material 32 (
The second mechanical element 5, on the other hand, is a sample of predetermined second dimensions taken from a vehicle braking element, in particular it consists of a portion of a brake disc made of steel or cast iron of transverse dimensions (i.e. measured perpendicularly to the screw 13) that are greater (for example double or triple) than those of the element 4.
This brake disc portion, forming the mechanical element 5, is cut from a production brake disc specimen; then to this portion of brake disc 5 the electric wire 12 is soldered onto the face 17 opposite the face 15 and finally the brake disc 5 portion, with the end of the wire 12 soldered to it, is incorporated into the support 9, which is integrally formed by embedding the element 5 and an end portion of the electric wire 12 facing towards the brake disc 5 portion, leaving the face 15 uncovered, i.e. not covered by the support 9. When the stiction cell 1 bearing the portions of brake pad 4 and brake disc 5 is immersed in the electrolyte 21, the face 15 that comes into contact with the electrolyte 21 is therefore larger than that of the brake pad portion 4 and, therefore, of the transverse dimensions of the portion of friction material 32 that has been cut integrally with the portion of brake pad 4.
According to one aspect of the disclosure, the face 15 therefore has a portion 33 exceeding the transverse dimensions of the first mechanical element 4: this portion 33, generally of an annular form and peripherally external is masked, with the exception of a small annular region 35 immediately adjacent to the mechanical element 4, in this case, immediately adjacent to the friction material 32. For example, the masking is carried out with an electrically non-conductive lacquer 34 or with a water-resistant adhesive tape and having a central hole with a predetermined diameter, in such a way as to always have the same exposed disc surface area.
The small region 35 is therefore left uncovered by the lacquer or the adhesive tape. It should be noted that here and hereinafter the term “small” means a measurement of the order of a few millimeters.
On the basis of that which has hitherto been described, the method therefore includes the steps of:
The electrochemical tests that are performed are chosen from the group consisting of:
1) OCP (“open circuit potential”) measures along time;
2) potentiostatic or potentiodynamic polarization curves;
3) chrono-potentiometric measures;
4) chrono-amperometric measures;
5) any combination of the above;
The execution of the electrochemical tests is finalized to cause corrosive phenomenons on the second mechanical element 5 which establish the chemical-physical conditions for the stiction phenomenon.
In this way, different types of electrochemical measurements are obtained, such as the current-voltage diagrams of the type shown in
According to a first preferred embodiment, the method comprises the steps of:
In a second preferred embodiment, the method comprises the step of applying in succession a first predetermined and constant potential to the mechanical element 5 constituting the working electrode for a first period of time and then a second predetermined and constant potential for a second period of time; and the step of detecting by means of the potential/current generator 23 or with another instrument the value of the electric current passing between the second mechanical element 5 and the counter-electrode 19 during the application of the first, and thereafter the second, predetermined and constant potential (chrono-ammeter measurement). In a third preferred embodiment of the method, a chrono-potentiometric measurement is performed wherein a fixed current is passed between the working electrode (element 5) and the counter-electrode 19 and the potential of the element 5 is measured with respect to the working electrode for a predetermined length of time (for example 1 h).
Subsequently, a potentiodynamic measurement is taken starting from a first predetermined potential and up to a second predetermined potential using a scanning speed (i.e. a speed of variation of the potential) which is fixed (potentiodynamic polarization curve).
The current set on the potential/current generator 23 according to a further possible embodiment and/or the electrical potential applied to the second mechanical element 5 according to the preferred embodiments described above are chosen in order to induce the corrosion of the first face 15 of the second mechanical elements 5, due to anodic dissolution; in particular, insofar as the face 15 is partially masked by the lacquer 34 or the adhesive tape, corrosion is induced only in the region 35 and on the portion of the surface 15 that is in direct contact with the anti-friction material 32 of the mechanical element 4 constituted by the portion of brake pad.
At the end of the electrochemical measurements performed in the electrolyte 21, the electrochemical cell 2 made using the stiction cell 1 is disconnected from the potentiostat. The stiction cell 1 is then extracted from the test electrolyte and placed in the oven where it is subjected to a drying/desiccation treatment. Subsequently, the stiction cell 1 must again be left to cool at room temperature for a predetermined period of time, such as a few hours.
Following the drying/desiccation procedure within the oven and the subsequent cooling at room temperature, the first face 15 of the second mechanical elements 5 adheres to the first mechanical element 4 due to a stiction gluing phenomenon; in particular, the portion of the surface 15 in contact with the anti-friction material 32, undergoes stiction gluing.
The method described thus far also includes the steps of picking up the mechanical elements 4 and 5 (the latter together with the support 9 within which it is incorporated) thus glued together due to stiction, from the electrochemical cell 2 and mounting them on a test bench 26 with the mechanical element 5 and the support 9 arranged downwards, i.e., towards the support base 27 and the step of detaching the second mechanical element 5 from the first mechanical element 4 by means of a pusher 28 acting laterally on the first mechanical element 4 and in a direction parallel to the first face 15, measuring a second force (F2) (
An important aspect is also the way in which the first predetermined force F1 is generated and applied, by means of the rotation of the screw 13 within the nut 14 carried by the body 6 within a non-conductive material that also carries the supports 7 and 9, applying to screw 13, a predetermined torque using the torque wrench 25.
Finally, to avoid external electrical interference that could alter the measurements, the electrochemical cell 2 is housed within a Faraday cage.
To ensure proper operation, the brake disc and brake pad samples that make up the mechanical elements 5 and 4 respectively are sanded, for example, using silicon carbide abrasive paper and then preconditioned, by immersing them in the electrolyte 21 for a few minutes, for example ten, before assembling them on the stiction cell 1 or in the electrochemical cell 2; further, after the assembly of the electrolytic cell 2, a certain period of time is allowed to pass, such as 20-30 minutes, before performing the electrochemical tests, in the manner described above.
The usefulness of the described method and equipment is obvious.
In the first place, it is possible to study under precise and reproducible conditions the phenomenon of stiction gluing, and also to evaluate the gravity thereof according to the value of the force F2 measured.
Secondly, in this way it is possible, testing under the same conditions, different materials both for the brake disc and, especially for the friction material 32 of the brake pad 4, to verify which materials are more suitable for resisting/avoiding the phenomenon of stiction in use. In practice, the method described serves as an accelerated laboratory stiction test in order to test the couples (brake disc and friction material) of the most suitable materials to be used in production.
For example, applying one of the test procedures described above (chrono-potentiometric plus potentiodynamic polarization) to two different friction materials A and B, a detachment force F2 of 150 N was recorded for material A with chemical-physical characteristics that favor the phenomenon of stiction and only 10 N for a material B with chemical-physical characteristics that make it resistant to the phenomenon of stiction. In addition, the F2 detachment forces detected for such samples are in line with the indications received from field tests for the friction materials A and B.
Similarly, the specific physical-chemical conditions that cause the phenomenon on specific materials can be understood, and thus the phenomenon itself may be prevented when some or all of these conditions occur in use on the vehicle.
The purposes of the disclosure are therefore fully achieved.
Number | Date | Country | Kind |
---|---|---|---|
102016000089576 | Sep 2016 | IT | national |
Number | Date | Country | |
---|---|---|---|
Parent | 16330364 | Mar 2019 | US |
Child | 17671472 | US |