Redox flow batteries store electrical energy in a chemical form and subsequently dispense the stored energy in an electrical form via a spontaneous reverse redox reaction. Conversion between the chemical and electrical energy occurs in a reactor cell. One issue with conventional redox flow batteries is that over time the electrolyte state of charge can become imbalanced, thereby decreasing battery capacity due to hydrogen generation from the electrolyte via side reactions. For example, hydrogen gas is emitted as an electrochemical byproduct during battery charging. As another example, in a hybrid redox flow battery, hydrogen gas is emitted as a byproduct of a corrosion reaction at a negative (plating) electrode. Because hydrogen gas production consumes protons instead of the electro-active material in the battery, hydrogen gas generation not only results in an electrolyte state of charge imbalance which reduces the battery capacity, but also a rise in electrolyte pH which can lead to electrolyte stability issues.
Electrolyte rebalancing methods and systems typically employ an auxiliary rebalancing cell (electrochemical or photochemical) to convert the hydrogen gas back to protons via an auxiliary electrochemical reaction. For example, Thaller (U.S. Pat. No. 4,159,366) discloses a redox flow system including an electrochemical rebalancing cell, where hydrogen gas evolved from the battery negative electrode flows through the rebalancing cell anode and positive electrolyte flows through the rebalancing cell cathode. Electrochemical reactions occurring at the electrodes of the rebalancing cell convert gaseous hydrogen back to protons, consume the imbalanced positive electrolyte, and rebalance the electrochemical capacity of the positive and negative electrolytes.
The inventors have recognized various issues with the above system. Namely, electrochemical fuel cells are complex systems that are costly to manufacture and to operate. A simpler and cheaper effective alternative to providing an auxiliary cell for rebalancing electrolytes in redox flow batteries is needed.
One approach that addresses the above issues is a method of rebalancing electrolytes in a redox flow battery system, comprising directing hydrogen gas generated on the negative electrode of the redox flow battery system to a catalyst surface, and fluidly contacting the hydrogen gas with the positive electrolyte comprising a metal ion at the catalyst surface. Such operation may occur with the positive metal ion chemically reduced by the hydrogen gas at the catalyst surface and/or a state of charge of the electrolyte substantially balanced. In one embodiment, the metal ion may comprise an imbalanced positive metal ion. In another embodiment, the electrolyte pH and the electrolyte state of charge remain substantially balanced.
It should be understood that the summary above is provided to introduce in simplified form a selection of concepts that are further described in the detailed description. It is not meant to identify key or essential features of the claimed subject matter, the scope of which is defined uniquely by the claims that follow the detailed description. Furthermore, the claimed subject matter is not limited to implementations that solve any disadvantages noted above or in any part of this disclosure.
The present description relates to methods and systems for rebalancing electrolytes in a redox flow battery system. The description primarily describes an all-iron hybrid redox flow battery (IFB) as an example redox flow battery system, however the methods and systems for rebalancing electrolytes disclosed in the present description also apply to other types of redox flow batteries such as an iron/chromium redox flow battery system.
Referring now to
When a charge current is applied to the battery terminals 40 and 42, the positive electrolyte is oxidized (lose one or more electrons) at the positive electrode 28, and the negative electrolyte is reduced (gain one or more electrons) at the negative electrode 26. During battery discharge, reverse redox reactions occur on the electrodes. In other words, the positive electrolyte is reduced (gain one or more electrons) at the positive electrode 28, and the negative electrolyte is oxidized (lose one or more electrons) at the negative electrode 26. The electrical potential difference across the battery is maintained by the electrochemical redox reactions in the positive electrode compartment 22 and the negative electrode compartment 20, and can induce a current through a conductor while the reactions are sustained. The amount of energy stored by a redox battery is limited by the amount of electro-active material available in electrolytes for discharge, depending on the total volume of electrolytes and the solubility of the electro-active materials.
During operation of a redox flow battery system, sensors and probes may monitor and control chemical properties of the electrolyte such as electrolyte pH, concentration, state of charge, and the like. For example, sensors 62 and 60 maybe be positioned to monitor positive electrolyte and negative electrolyte conditions at the positive electrolyte source 52 and the negative electrolyte source 50, respectively. As another example, sensors 72 and 70 may monitor positive electrolyte and negative electrolyte conditions at the positive electrode compartment 22 and the negative electrode compartment 20, respectively. Sensors may be positioned at other locations throughout the redox flow battery system to monitor electrolyte chemical properties and other properties. For example a sensor may be positioned in an external acid tank (not shown) to monitor acid volume or pH of the external acid tank, wherein acid from the external acid tank is supplied via an external pump (not shown) to the redox flow battery system in order to reduce precipitate formation in the electrolytes. Additional external tanks and sensors may be installed for supplying other additives to the redox flow battery system. Sensor information may be transmitted to a controller 80 which may in turn actuate pumps 30 and 32 to control electrolyte flow through the cell 18, or to perform other control functions, as an example. In this way, the controller 80 may be responsive to, one or a combination of sensors and probes.
Hybrid flow batteries are redox flow batteries that are characterized by the deposit of one or more of the electro-active materials as a solid layer on an electrode. Hybrid batteries may, for instance, include a chemical that plates via an electrochemical reaction as a solid on a substrate throughout the battery charge process. During battery discharge, the plated species may ionize via an electrochemical reaction, becoming soluble in the electrolyte. In hybrid battery systems, the charge capacity (e.g., amount of energy stored) of the redox battery may be limited by the amount of metal plated during battery charge and may accordingly depend on the efficiency of the plating system as well as the available volume and surface area available for plating.
In a hybrid flow battery system the negative electrode 26 may be referred to as the plating electrode and the positive electrode 28 may be referred to as the redox electrode. The negative electrolyte within the plating side (e.g., negative electrode compartment 20) of the battery may be referred to as the plating electrolyte and the positive electrolyte on the redox side (e.g. positive electrode compartment 22) of the battery may be referred to as the redox electrolyte.
Anode refers to the electrode where electro-active material loses electrons and cathode refers to the electrode where electro-active material gains electrons. During battery charge, the positive electrolyte gains electrons at the negative electrode 26; therefore the negative electrode 26 is the cathode of the electrochemical reaction. During discharge, the positive electrolyte loses electrons; therefore the negative electrode 26 is the anode of the reaction. Accordingly, during charge, the negative electrolyte and negative electrode may be respectively referred to as the catholyte and cathode of the electrochemical reaction, while the positive electrolyte and the positive electrode may be respectively referred to as the anolyte and anode of the electrochemical reaction. Alternatively, during discharge, the negative electrolyte and negative electrode may be respectively referred to as the anolyte and anode of the electrochemical reaction, while the positive electrolyte and the positive electrode may be respectively referred to as the catholyte and cathode of the electrochemical reaction.
For simplicity, the terms positive and negative are used herein to refer to the electrodes, electrolytes, and electrode compartments in redox battery flow systems.
One example of a hybrid redox flow battery is an all iron redox flow battery (IFB), in which the electrolyte comprises iron ions in the form of iron salts (e.g., FeCl2, FeCl3, and the like), wherein the negative electrode comprises metal iron. For example, at the negative electrode, ferrous ion, Fe2+, receives two electrons and plates as iron metal on to the negative electrode 26 during battery charge, and iron metal, FeO, loses two electrons and re-dissolves as Fe2+ during battery discharge. At the positive electrode, Fe2+ loses an electron to form ferric ion, Fe3+, during charge, and during discharge Fe3+ gains an electron to form Fe2+: The electrochemical reaction is summarized in equations (1) and (2), wherein the forward reactions (left to right) indicate electrochemical reactions during battery charge, while the reverse reactions (right to left) indicate electrochemical reactions during battery discharge:
Fe2++2e− FeO −0.44 V (Negative Electrode) (1)
2Fe2+↔2Fe3++2e−+0.77 V (Positive Electrode) (2)
As discussed above, the negative electrolyte used in the all iron redox flow battery (IFB) may provide a sufficient amount of Fe2+ so that, during charge, Fe2+ can accept two electrons from the negative electrode to form FeO and plate onto a substrate. During discharge, the plated FeO may then lose two electrons, ionizing into F2+ and be dissolved back into the electrolyte. The equilibrium potential of the above reaction is −0.44V and thus this reaction provides a negative terminal for the desired system. On the positive side of the IFB, the electrolyte may provide Fe2+ during charge which loses electron and oxidizes to Fe3+. During discharge, Fe3+ provided by the electrolyte becomes Fe2+ by absorbing an electron provided by the electrode. The equilibrium potential of this reaction is +0.77V, creating a positive terminal for the desired system.
The IFB provides the ability to charge and recharge its electrolytes in contrast to other battery types utilizing non-regenerating electrolytes. Charge is achieved by applying a current across the electrodes via terminals 40 and 42. The negative electrode may be coupled via terminal 40 to the negative side of a voltage source so that electrons may be delivered to the negative electrolyte via the positive electrode (e.g., as Fe2+ is oxidized to Fe3+ in the positive electrolyte in the positive electrode compartment 22). The electrons provided to the negative electrode 26 (e.g., plating electrode) can reduce the Fe2+ in the negative electrolyte to form FeO at the plating substrate causing it to plate onto the negative electrode.
Discharge can be sustained while FeO remains available to the negative electrolyte for oxidation and while Fe3+ remains available in the positive electrolyte for reduction. As an example, Fe3+ availability can be maintained by increasing the concentration or the volume of the positive electrolyte to the positive electrode compartment 22 side of cell 18 to provide additional Fe3+ ions via an external source, such as an external positive electrolyte tank 52. More commonly, availability of FeO during discharge may be an issue in IFB systems, wherein the FeO available for discharge may be proportional to the surface area and volume of the negative electrode substrate as well as the plating efficiency. Charge capacity may be dependent on the availability of Fe2+ in the negative electrode compartment 20. As an example, Fe2+ availability can be maintained by providing additional Fe2+ ions via an external source, such as an external negative electrolyte tank 50 to increase the concentration or the volume of the negative electrolyte to the negative electrode compartment 20 side of cell 18.
In an IFB, the positive electrolyte comprises ferrous ion, ferric ion, ferric complexes, or any combination thereof, while the negative electrolyte comprises ferrous ion or ferrous complexes, depending on the state of charge of the IFB system. As previously mentioned, utilization of iron ions in both the negative electrolyte and the positive electrolyte allows for utilization of the same electrolytic species on both sides of the battery cell, which can reduce electrolyte cross-contamination and can increase the efficiency of the IFB system, resulting in less electrolyte replacement as compared to other redox flow battery systems.
Efficiency losses in an IFB may result from electrolyte crossover through the separator 24 (e.g., ion-exchange membrane barrier, micro-porous membrane, and the like). For example, ferric ions in the positive electrolyte may be driven toward the negative electrolyte by a ferric ion concentration gradient and an electrophoretic force across the separator. Subsequently, ferric ions penetrating the membrane barrier and crossing over to the negative electrode compartment 20 may result in coulombic efficiency losses. Ferric ions crossing over from the low pH redox side (e.g., more acidic positive electrode compartment 22) to high pH plating side (e.g., less acidic negative electrode compartment 20) can result in precipitation of Fe(OH)3. Precipitation of Fe(OH)3 can damage the separator 24 and cause permanent battery performance and efficiency losses. For example, Fe(OH)3 precipitate may chemically foul the organic functional group of an ion-exchange membrane or physically clog the small micro-pores of an ion-exchange membrane. In either case, due to the Fe(OH)3 precipitate, membrane ohmic resistance may rise over time and battery performance may degrade. Precipitate may be removed by washing the battery with acid, but the constant maintenance and downtime may be disadvantageous for commercial battery applications. Furthermore, washing may be dependent on regular preparation of electrolyte, an adding to process cost and complexity. Adding specific organic acids to the positive electrolyte and the negative electrolyte in response to electrolyte pH changes may also mitigate precipitate formation during battery charge and discharge cycling.
Additional coulombic efficiency losses may be caused by reduction of H+ (e.g., protons) and subsequent formation of H2 (e.g., hydrogen gas), and the reaction of protons in the negative electrode compartment 20 with electrons supplied at the plated iron metal electrode to form hydrogen gas.
The IFB electrolyte (e.g., FeCl2, FeCl3, FeSO4, Fe2(SO4)3, and the like) is readily available and can be produced at low costs. The IFB electrolyte offers higher reclamation value because the same electrolyte can be used for the negative electrolyte and the positive electrolyte, consequently reducing cross contamination issues as compared to other systems. Furthermore, owing to its electron configuration, iron may solidify into a generally uniform solid structure during plating thereof on the negative electrode substrate. For zinc and other metals commonly used in hybrid redox batteries, solid dendritic structures may form during plating. The stable electrode morphology of the IFB system may increase the efficiency of the battery in comparison to other redox flow batteries.
Further still, iron redox flow batteries reduce the use of toxic raw materials and can operate at a relatively neutral pH as compared to other redox flow battery electrolytes. Accordingly, IFB systems reduce environmental hazards as compared with all other current advanced redox flow battery systems in production.
Turning now to
As a result, the negative electrolyte in the negative electrode compartment 20 tends to stabilize at a pH range between 3 and 6, wherein formation of ferrous hydroxide ion (FeOH+) at 112, precipitation of ferric hydroxide, Fe(OH)3 at 114, and hydrogen evolution at 104 are all reduced. At the positive electrode compartment 22, ferric ion, Fe3+, has a much lower acid disassociation constant (pKa) than that of ferrous ion, Fe2+. Therefore, as more ferrous ions are oxidized to ferric ions, the positive electrolyte tends to stabilize at a pH less than 2, in particular at a pH closer to 1 within region 120.
Accordingly, maintaining the positive electrolyte pH in a first range in which the positive electrolyte (positive electrode compartment 22) remains stable and maintaining the negative electrolyte pH in a second range in which the negative electrolyte (negative electrode compartment 20) remains stable may reduce low cycling performance and increase efficiency of redox flow batteries. For example, maintaining a pH of a negative electrolyte in an IFB between 3 and 4 may reduce iron corrosion reactions and increase iron plating efficiency, while maintaining a pH of a positive electrolyte less than 2, in particular less than 1, may promote the ferric/ferrous ion redox reaction and reduce ferric hydroxide formation.
As indicated by equation (3) and (4), evolution of hydrogen can cause electrolyte imbalance in a redox flow battery system. For example, during charge, electrons flowing from the positive electrode to the negative electrode (e.g., as a result of ferrous ion oxidation), may be consumed by hydrogen evolution via equation (3), thereby reducing the electrons available for plating given by equation (1). Because of the reduced plating, battery charge capacity is reduced. Additionally, corrosion of the iron metal further reduces battery capacity since a decreased amount of iron metal is available for battery discharge. Thus, an imbalanced electrolyte state of charge between the positive electrode compartment 22 and the negative electrode compartment 20 can develop as a result of hydrogen production via reaction (3) and (4). Furthermore, hydrogen gas production resulting from iron metal corrosion and proton reduction both consume protons, which can result in a pH increase of the negative electrolyte. As discussed above with reference to FIG. 2, an increase in pH may destabilize the electrolyte in the redox battery flow system, resulting in further battery capacity and efficiency losses.
An approach that addresses the electrolyte rebalancing issues that can be caused by hydrogen gas production in redox flow battery systems comprises reducing the imbalanced ion in the positive electrolyte with hydrogen generated from the side reactions. As an example, in an IFB system, the positive electrolyte comprising ferric ion may be reduced by the hydrogen gas according to equation (5):
Fe3++½H2→Fe2++H+ (5)
In the IFB system example, by reacting ferric ion with hydrogen gas, the hydrogen gas can be converted back to protons, thereby maintain a substantially constant pH in the negative electrode compartment 20 and the positive electrode compartment 22. Furthermore, by converting ferric ion to ferrous ion, the state of charge of the positive electrolyte in the positive electrode compartment 22 may be rebalanced with the state of charge of the negative electrolyte in the negative electrode compartment 20. Although equation (5) is written for rebalancing electrolytes in an IFB system, the method of reducing an electrolyte with hydrogen gas may be generalized by equation (6):
In equation (6), M x+ represents the positive electrolyte M having ionic charge, x, Mz+ represents the reduced electrolyte M having ionic charge, z.
A catalyst comprising graphite or comprising supported precious metal (e.g., carbon-supported Pt, Rd, Ru, or alloys thereof) catalyst may increase the rate of reaction described by equation (5) for practical utilization in a redox flow battery system. As an example, hydrogen gas generated in the redox flow battery system may be directed to a catalyst surface, and hydrogen gas and electrolyte (e.g., comprising ferric ion) may be fluidly contacted at the catalyst surface, wherein the hydrogen gas chemically reduces the ferric ion to ferrous ion and produces positive hydrogen ions (e.g., protons). As described above, the catalyst surface may comprise graphite. In some examples, the reaction described by equation (5) may proceed at a faster rate when the catalyst comprises a precious metal-based catalyst, such as carbon-supported Pt, Rd, Ru, or alloys thereof. As an example, in cases where the partial pressure of hydrogen gas (e.g. hydrogen gas concentration) is high and when a slower rate of reaction can be tolerated, the less costly graphite catalyst may be used. On the other hand, a small amount (e.g., 0.2 to >0.5 wt %) of precious metal catalyst supported on carbon can increase the rate of reaction as compared to using a graphite catalyst. Different types of catalysts, such as Pt, Pd, Ru or alloys of the above, and the like, and different amounts (0.2 to >0.5 wt %) thereof can be utilized depending on a reaction speed for any specific battery system. Furthermore, alloys of the catalyst can be utilized to reduce cost and increase corrosion stability of the catalyst. For example 10% addition of rhodium to platinum can reduce the corrosion of platinum by the ferric ion by over 98% (Handbook of Corrosion Data, Bruce D. Craig, David S. Anderson).
Turning now to
The reaction products of the trickle bed reactor 230 are returned to the electrolyte source 240. A sensor 270 may comprise one or a plurality of sensors and/or measurement devices to measure chemical properties of electrolyte solution 242. As an example, sensor 270 may comprise a potentiostat and a three-electrode sensor comprising a glassy carbon working electrode, a platinum mesh counter electrode, and an Ag/AgCl reference electrode for performing cyclic voltammetry to measure dynamic electrolyte concentration profiles. The potentiostat may be set at a scan rate of l/minute to analyze the electrolyte solution 242. For the case of an IFB system, the electrolyte solution comprises ferric ion solution, and the cyclic voltammetry may determine the changes in ferric ion concentration in the electrolyte solution by measuring the ferric-to-ferrous reduction peak. Sensor 270 may further comprise a pH meter for measuring changes in the ferric ion solution pH during the test.
In order to characterize the reaction kinetics of the ferric ion reduction reaction, a model for the trickle bed reactor 230 may be represented by equations (7)-(9):
Where r′=rate of reaction (mol/s-g), r=rate of reaction (mol/s-l), N=molar flow (mol/s), dX=conversion (%), dW=weight of catalyst (g), ρcat=density of catalyst (g/l), C=concentration of species, k=reaction constant (l/s), x=the order of reaction on ferric ion concentration, and y=the order of reaction on hydrogen partial pressure.
An example of the test results is shown in
Using the above-described apparatus, a series of experiments may be carried out to characterize the reaction kinetics, in particular, to study how the reaction rate changes with ferric ion concentration and hydrogen partial pressure. In experiments carried out by the subject inventors, it was found that varying ferric ion concentration did not influence the reaction rate. Thus, it was determined that the order of the reaction (equation (5)) with respect to ferric ion concentration was zero (e.g., x=0 in equation (9)).
Next,
Next,
Where A is a pre-exponential factor, R is the universal gas constant, T is the temperature in kelvin, and Ea is the activation energy for the reaction. By plotting the experimental data as a natural log of the reaction rate constant, k, against the inverse reaction temperature measured in kelvin, and by fitting a linear trend line 610 to the plotted data, the reaction rate constant parameters, A and Ea, may be determined from the ln(k) intercept and the slope of a fitted linear trend line, respectively. Determining the reaction rate constant activation energy may help to increase the efficiency of a rebalancing method and system for rebalancing electrolytes in a redox flow battery system. For example, after determining the reaction rate parameters for the hydrogen reduction of an electrolyte metal ion (e.g., ferric ion in an IFB), an efficiency of an electrolyte rebalancing method and system may be increased.
Turning now to
During battery charge, gaseous hydrogen may be generated on the negative side of the battery (e.g., at negative electrode 26) due to both electrochemical and corrosion side reactions (equations (3), and (4)) as previously described. Equation (4) is written for corrosion of iron metal electrode, for example in an IFB system, however, corrosion of other metals producing hydrogen gas may also occur in other types of hybrid redox flow battery systems or other redox flow battery systems. The hydrogen generated from the electrochemical and corrosion side reactions may accumulate at the negative electrolyte source 50 and the positive electrolyte source 52. A pressure equalization line 704 may connect negative source 50 and positive electrolyte source 52, thereby equating a pressure between a gas head spaces 757 and 755 of positive and negative electrolyte sources, respectively. In this way, hydrogen gas may be distributed to the recirculating flow paths of the electrolyte at the negative and positive sides of the battery, respectively. In particular, the hydrogen gas may be supplied to the trickle bed reactors 710, 712. Ejectors 730 and 732 may be located between the outlet of the negative electrode compartment 20 and the positive electrode compartment 22 of battery cell 18 and trickle bed reactors 710 and 712, respectively. Ejectors 730 and 732 may deliver a predetermined amount or flow rate of hydrogen gas to trickle bed reactors 710 and 712, respectively. Ejectors 730, 732 may be connected to the gas head space 757 of positive source 52 and the gas head space 755 of negative electrolyte source 50. For example, negative electrolyte flowing from the negative electrode compartment 20 may pass through ejector 730, thereby drawing gas (e.g., hydrogen gas) from gas head space 757 of positive electrolyte source 52, and positive electrolyte flowing from the positive electrode compartment 22 may pass through ejector 732, thereby drawing gas (e.g., hydrogen gas) from gas head space 755 of negative electrolyte source 50. The sizes of ejectors 730 and 732 may be predetermined based on a predetermined amount of hydrogen generated and a predetermined speed of the reduction reaction. For example, the sizes of ejectors 730 and 732 may be increased to increase the hydrogen gas flow to the trickle bed reactors 710, 712, respectively, relative to the flow of electrolyte recirculated by pumps 30, and 32, respectively. In some examples, the sizes of ejectors 730, and 732 may be different, the sizes of each ejector predetermined according to the predetermined hydrogen flow rates to trickle bed reactors 710 and 712. For example, in an IFB, because the ferric ion concentration may be higher in the positive electrolyte at the positive side of the redox flow battery system, a larger portion of the hydrogen gas may be drawn through ejector 732. As a further example, the ejectors may be sized according to the reaction rate parameters determined as discussed above for equation (9) and system conditions such as reaction temperature. As a further example, ejectors 730 and 732 may also comprise mechanical pumps for delivering liquid electrolyte and hydrogen gas to trickle bed reactors 710 and 712, respectively, wherein the mechanical pumps may be controlled by controller 80.
Because the amount of generated hydrogen in the redox flow battery system may be approximately equal to the amount of unbalanced ferric ions, recirculating the generated hydrogen to both the positive electrolyte source 52 (and positive electrode compartment 22) and the negative electrolyte source 50 (and negative electrode compartment 20), may aid in completely rebalancing the electrolytes. For example, recirculating the generated hydrogen to the negative electrolyte source 50 may aid in rebalancing free ferric ions that crossover through separator 24 from the positive electrode compartment 22.
Redox flow battery system 700 may further comprise an external source 790 of hydrogen gas. External source 790 may supply additional hydrogen gas to the positive electrolyte source 52 and the negative electrolyte source 50. External source 790 may alternately supply additional hydrogen gas to the inlet of trickle bed reactors 710, 712. As an example, a mass flow meter or other flow controlling device (which may be controlled by controller 80) may regulate the flow of the hydrogen gas from external source 790. The external source of hydrogen may supplement the hydrogen gas generated in redox flow battery system 700. For example, when gas leaks are detected in redox flow battery system 700 or when the reduction reaction rate is too low at low hydrogen partial pressure, an external source of hydrogen gas may be supplied in order to rebalance the state of charge of the electro-active species in the positive electrolyte and negative electrolyte. As an example, controller 80 may supply hydrogen gas from external source 790 in response to a measured change in pH or in response to a measured change in state of charge of an electrolyte or an electro-active species. For example an increase in pH of the negative electrolyte source 50, or the negative electrode compartment 20, may indicate that hydrogen is leaking from the redox flow battery system 700 and/or that the reaction rate is too slow with the available hydrogen partial pressure, and controller 80, in response to the pH increase, may increase a supply of hydrogen gas from external source 790 to the redox flow battery system 700. As a further example, controller 80 may supply hydrogen gas from external source 790 in response to a pH change, wherein the pH increases beyond a first threshold pH or decreases beyond second threshold pH. For example, a first threshold pH for the negative electrolyte may be 4 and a second threshold pH for the negative electrolyte may be 3. In other words if the pH for the negative electrolyte is measured beyond a first range (e.g., less than 3 or greater than 4), then controller 80 may adjust (e.g., increase or decrease, or shut off, etc.) the external hydrogen gas supply rate to return the pH to the first range. As another example, if the pH of the negative electrolyte is greater than 4, then controller 80 may increase the external gas supply rate to supply additional hydrogen to increase the rate of reduction of ferric ions and the rate of production of protons, thereby reducing the positive electrolyte pH. Furthermore, the negative electrolyte pH may be lowered by hydrogen reduction of ferric ions crossing over from the positive electrolyte to the negative electrolyte or by proton generated at the positive side crossing over to the negative electrolyte due to a proton concentration gradient and electrophoretic forces. In this way, the pH of the negative electrolyte may be maintained within the stable region from 3-4, while reducing the risk of precipitation of ferric ions (crossing over from the positive electrode compartment) to Fe(OH)3. Other control schemes for controlling the supply rate of hydrogen gas from external source 790 responsive to a change in an electrolyte pH or to a change in an electrolyte state of charge, detected by other sensors such as an oxygen-reduction potential (ORP) meter or an optical sensor, may be implemented. Further still, the change in pH or state of charge triggering the action of controller 80 may be based on a rate of change or a change measured over a time period. The time period for the rate of change may be predetermined or adjusted based on the time constants for the redox flow battery system. For example the time period may be reduced if the recirculation rate is high, and local changes in concentration (e.g., due to side reactions or gas leaks) may quickly be measured since the time constants may be small.
Turning now to
Catalyst layer 1206 may include one or more different types of catalyst materials such as platinum, palladium, ruthenium, alloys thereof. The weight percent of the catalyst material on the substrate layer 1204 may be from 0.2 wt % to greater than 0.5 wt %. The substrate layer 1204 coated with the catalyst layer 1206 may be porous and permeable to hydrogen gas, hydrogen ions, and to electrolyte including the positive electrolyte and the negative electrolyte from positive electrolyte source 52 and negative electrolyte source 50. When hydrogen gas and metal ions in the electrolyte are fluidly contacted at the catalyst layer 1206, the catalyst layer 1206 may catalyze a redox reaction whereby the hydrogen gas may be oxidized to hydrogen ions and the metal ions may be reduced (e.g. according to equations (5) and (6)). The substrate layer 1204 may be coated entirely with the catalyst layer 1206 to increase a redox reaction rate of hydrogen gas and metal ions at the catalyst layer surface.
Catalyst bed 1200 may further comprise a spacing layer 1210 positioned on the catalyst layer. As shown in
Turning now to
As shown in
An alternate configuration of reactor vessel 1300 is shown in
In the example configurations of reactor vessels 1300 of
Increasing packing density in a packed catalyst bed of a reactor vessel may result in increased reaction rates. Increasing the number of layers in the jelly roll structured catalyst bed may increase the catalyst density in the reactor vessel 1300, and may increase a redox reaction rate per pass, which may allow for a more compact or smaller sized reactor vessel. However, the pressure drop across the reactor vessel 1300 may be increased, reducing flow rates. Furthermore, increasing the number of layers in the jelly roll structure may call for additional flow distribution analysis to verify that the hydrogen gas to electrolyte mixture concentrations are suitable and to ensure that distribution of flows and concentrations of hydrogen gas and electrolyte species are adequate throughout the catalyst bed. The reactor vessels 1300 may include inlet and/or outlet baffle or other flow distribution means to increase uniformity of flow distribution across the catalyst bed. Increasing a thickness of the spacing layer 1210 or porosity may aid in reducing a pressure drop across the reactor vessel 1300, for a given number of layers in the jelly roll. By extending across an axial length of the jelly roll structured catalyst bed 1220, the spacing layer 1210 can aid in distributing the electrolyte fluid and the hydrogen gas across the entire surface of the catalyst layer 1206 within the catalyst bed because electrolyte fluid and hydrogen gas can flow axially, radially, and angularly across the spacing layers within the jelly roll structure. Furthermore, the spacing layers in the jelly roll structure intervene and maintain successive substrate and catalyst layers separated thereby reducing a risk of pinching or lamination of successive catalyst layers in the jelly roll structure which could increase the pressure drop across the catalyst bed and reduce accessibility of the catalyst layer to the electrolyte fluid and hydrogen gas. In contrast, in a packed catalyst bed (e.g., catalyst beds 740, 742), channeling and irregularities in interparticle distributions within the packed bed may give rise to uneven distribution of fluid within the catalyst bed, reducing specific reaction rates for a give catalyst bed loading.
Turning now to
Turning now to
In this manner, a redox flow battery system may comprise: a redox flow battery cell, and a catalyst bed fluidly connected to the battery cell, wherein the catalyst bed includes a substrate layer and a catalyst layer coated on the substrate layer spiral wound into a jelly roll structure. Additionally or alternatively, the catalyst bed further includes a spacing layer positioned on the catalyst layer spiral wound into the jelly roll structure, wherein the spacing layer separates successive catalyst and substrate layers within the jelly roll structure. Additionally or alternatively, wherein the catalyst layer comprises one or more of Pt, Pd, Ru or alloys thereof. Additionally or alternatively, the substrate layer comprises carbon paper or carbon cloth. Additionally or alternatively, the substrate layer comprises a membrane. Additionally or alternatively, the spacing layer comprises a plastic mesh. Additionally or alternatively, the redox flow battery system comprise
Turning now to
For the case of a redox flow battery system comprising a plurality of cells stacked in series or in parallel, a redox plate of an adjacent redox flow battery cell may be positioned immediately adjacent to a back face of the negative electrode, wherein a back face of the negative electrode is opposite to the face of the negative electrode contacting separator 816.
In one example, cell 800 may comprise a cell for a hybrid redox flow battery system, for example, an IFB system. In an IFB system, the negative electrode 818 may include a substrate structure on which the iron metal, FeO, may plate (solidify) during IFB charge, the positive electrolyte may comprise ferric ion, and ferrous ion, and the negative electrolyte may comprise ferrous ion. Accordingly, the positive electrolyte may comprise a first metal ion and the negative electrolyte may comprise a second metal ion, wherein an oxidation state of the first metal ion may be higher than an oxidation state of the second metal ion.
Turning now to
Accordingly, in the redox flow battery cell 900, hydrogen generated at the negative electrode 818 may react with electro-active species such as a metal ion (e.g., ferric ion in an IFB system) at the interface between the separator 816 and the negative electrode 818. For example, ferric ions crossing over the separator 816 from the positive electrode 814 may be reduced by the hydrogen gas produced at the negative electrode. In this way, the hydrogen reduction reaction may occur at/or near the position where the hydrogen gas is generated so that the hydrogen gas may be quickly oxidized (e.g., when reducing ferrous ion to ferric ion) to produce protons. Thus, the redox flow battery cell 900 may more efficiently maintain a substantially balanced electrolyte state of charge and also more efficiently maintain a substantially stable electrolyte pH as compared to other redox flow battery cell configurations where the hydrogen reduction reaction for rebalancing the electrolytes takes place at a location further away from the negative electrode. For example, the redox flow battery system of
Turning now to
In this manner, a redox flow battery system may comprise a positive electrode in fluid communication with a positive electrolyte comprising a first metal ion, a negative electrode in fluid communication with a negative electrolyte comprising a second metal ion, an electrically insulating ion conducting surface separating the positive electrode from the negative electrode, and a catalyst surface in fluid communication with the first metal ion, the second metal ion, or a combination thereof, and hydrogen gas, wherein the hydrogen gas and the first metal ion, the second metal ion, or a combination thereof are fluidly contacted at the catalyst surface. The first metal ion may comprise a metal ion having a higher oxidation state, and the second metal ion may comprise a metal ion having a lower oxidation state. In one example, the redox flow battery system may comprise an iron redox flow battery system, the negative electrode may comprise an iron plating electrode, and the positive electrolyte and the negative electrolyte may comprise a ferric ion, ferrous ion, or a combination thereof. The redox flow battery system may further comprise an external source of hydrogen gas in fluid communication with the catalyst surface, and the catalyst may comprise a catalyst bed in a trickle bed reactor.
The redox flow battery system may further comprise a pump fluidly positioned between the positive electrode and the trickle bed reactor, wherein the pump supplies the hydrogen gas and the positive electrolyte to the trickle bed reactor. The pump may comprise an ejector, wherein a flow of the positive electrolyte through the ejector draws the hydrogen gas through the ejector to the trickle bed reactor, and the catalyst may comprise a catalyst layer positioned between the electrically insulating ion conducting surface and the negative electrode. The redox flow battery system may further comprise an electrically-insulative fluid-permeable substrate between the catalyst layer and the negative electrode, wherein the catalyst layer is disposed on the electrically-insulative fluid-permeable substrate. The catalyst layer may comprise one or more of a graphite catalyst layer and a precious metal-based catalyst layer.
In this manner, a redox flow battery system, may comprise: a redox flow battery cell, an electrolyte source supplying metal ions to the redox flow battery cell, a catalyst bed, including a catalyst layer coated on a substrate layer spiral wound into a jelly roll structure, a recirculation device fluidly connected between the redox flow battery cell and the catalyst bed, and a controller, including executable instructions stored in memory to operate the recirculation device to direct hydrogen gas and metal ions from the redox flow battery cell to the catalyst bed, and operate the recirculation device to direct oxidized hydrogen gas and reduced metal ions from the catalyst bed to the electrolyte source. Additionally or alternatively, the hydrogen gas is oxidized at the catalyst layer to hydrogen ions and the metal ions are reduced at the catalyst layer, and the executable instructions further comprise operating the recirculation device to direct the hydrogen ions and the reduced metal ions from the catalyst layer to the electrolyte source. Additionally or alternatively, the redox flow battery system may comprise a hydrogen gas source external to the redox flow battery cell, wherein the executable instructions further comprise directing hydrogen gas from the hydrogen gas source to the catalyst bed.
Turning now to
Next, method 1100 continues at 1130, where electrolyte may be directed to the catalyst surface. The electrolyte may comprise a positive electrolyte and/or a negative electrolyte, and the electrolyte may comprise one or multiple metal ions. The electrolyte may be directed to a catalyst electrolytes may be directed to a catalyst surface from an external source. As a further example, the catalyst surface may be positioned relative to the negative electrode and/or positive electrode so that the electrolyte may be directed, or may be self-directed (e.g., electrolyte may gravity flow) to the catalyst surface.
At 1140, method 1100 comprises fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface. As an example, fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface may comprise mixing the hydrogen gas with a liquid electrolyte and injecting the gas-liquid mixture into a trickle bed reactor, thereby fluidly contacting the gas-liquid mixture at a catalyst surface comprising a packed catalyst bed of a trickle bed reactor. As a further example, fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface may comprise positioning a catalyst surface relative to a positive and/or negative electrode wherein hydrogen gas and electrolyte are each directed to and fluidly contact each other at the catalyst surface (e.g., fluidly contacting the hydrogen gas with electrolyte at the thin catalyst layer 910 or 1010).
Next, at 1150, method 1100 comprises determining if a change in pH is detected, for example, to control a negative electrolyte pH within a pre-determined range. Determining a pH change may comprise measuring a change in pH with an appropriate pH meter or other sensor and/or probe positioned, for example, at a battery cell or electrolyte source. Detecting a change in pH may comprise detecting a pH increase or a pH decrease. Furthermore, detecting a change in pH may comprise detecting a pH increase or pH decrease beyond a first pH range or a second pH range. For example, in an IFB, the first pH range may be from 3 to 4, corresponding to a pH range over which the negative electrolyte is stable, and the second pH range may be from 1 to 2, corresponding to a pH range over which the positive electrolyte is stable. As another example, the first pH range may correspond to a pH less than 4. The first pH range and the second pH range may be predetermined depending on the particular redox flow battery system. For example, a Pourbaix diagram may be used to predetermine the first pH range and the second pH range for the redox flow battery system.
If the detected pH is within the predetermined range, method 1100 continues at 1160, where it is determined if an electrolyte state of charge (SOC) imbalance is detected. Detecting an electrolyte SOC imbalance may comprise measuring a change in one or a plurality of electrolyte concentrations, measuring a change in one or a plurality of electrolyte SOC's, and the like. For example, if the total concentration of ferric ions in the positive electrolyte, indicated by its ORP, is substantially imbalanced with the total concentration of ferrous ions, indicated by its ORP, in the negative electrolyte in an IFB system, then an electrolyte SOC imbalance may be detected. As a further example, the electrolyte SOC imbalance may be determined by averaging measured electrolyte concentrations or electrolyte SOCs over a predetermined time interval. For example, during a predetermined time interval at a known charging or discharging current, the exact amount of electrons transferred in coulombs can be calculated by multiplying the charging or discharging current in Amperes by the predetermined time interval in seconds. Based on the total coulombs transferred and the positive and negative reactions for a redox flow battery system, changes in the amounts of species in the positive and negative electrolytes can be determined. If the measured electrolyte SOC does not balance with changes in the amounts of species calculated from the total coulombs transferred, then an electrolyte SOC imbalance may be determined. If an electrolyte SOC imbalance is not detected, method 1100 ends.
If a negative electrolyte pH is above the predetermined pH range at 1150, or an electrolyte SOC imbalance is detected at 1160, method 1100 continues at 1170, where external hydrogen may be supplied from an external source. For example, in an IFB, if the pH of the negative electrolyte increases beyond a first range corresponding to the range where the ferric ions is stable, hydrogen gas may be supplied (e.g., via a controller) to the IFB cell to drive the reduction of ferric ion at the catalyst surface. In this way, the supplied hydrogen gas from an external source may increase the hydrogen partial pressure at the catalyst surface, and may thereby speed up the hydrogen reduction of ferric ion at the catalyst surface, producing protons and reducing the pH of the positive electrolyte. A controller may also supply external hydrogen responsive to a detected electrolyte SOC imbalance. Supplied hydrogen gas from an external source may increase the rate of hydrogen reduction of ferric ion at the catalyst surface, thereby rebalancing the electrolyte SOC in the positive and negative electrolytes.
In this manner, a method of rebalancing electrolytes in a redox flow battery system may comprise directing hydrogen gas in the redox flow battery system to a catalyst surface, fluidly contacting the hydrogen gas with an electrolyte comprising a metal ion at the catalyst surface; and chemically reducing the metal ion by the hydrogen gas at the catalyst surface, wherein a state of charge of the electrolyte remains substantially balanced. In another example, a method of rebalancing electrolytes in a redox flow battery system may comprise directing hydrogen gas in the redox flow battery system to a catalyst surface, fluidly contacting the hydrogen gas with an electrolyte comprising a metal ion at the catalyst surface, and chemically reducing the metal ion by the hydrogen gas at the catalyst surface, wherein a pH of the electrolyte remains within a predetermined range. In a further example, a method of rebalancing electrolytes in a redox flow battery system may comprise directing hydrogen gas in the redox flow battery system to a catalyst surface, fluidly contacting the hydrogen gas with an electrolyte comprising a metal ion at the catalyst surface, and chemically reducing the metal ion by the hydrogen gas at the catalyst surface, wherein a state of charge of the electrolyte remains substantially balanced and a pH of the electrolyte remains within a predetermined range.
The methods of rebalancing electrolytes in a redox flow battery system may further comprise measuring a pH of the electrolyte and supplying hydrogen from an external source in response to a change in the pH of the electrolyte. The methods may further comprise measuring a state of charge of the electrolyte and supplying hydrogen from an external source in response to a change in the state of charge of the electrolyte. Further still, the redox flow battery system may comprise an iron redox flow battery system, and the metal ion may comprise ferric ion.
Directing the hydrogen gas to the catalyst surface may comprise directing the hydrogen gas to a catalyst bed in a trickle bed reactor, wherein fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface comprises fluidly contacting the hydrogen gas with the electrolyte at the catalyst bed of the trickle bed reactor. Furthermore, the redox flow battery system may comprise a positive electrode and a negative electrode, wherein directing the hydrogen gas to the catalyst surface may comprise directing the hydrogen gas to a catalyst layer positioned at an electrically insulating ion conducting surface separating the positive electrode and the negative electrode.
In this manner, a method of operating a redox flow battery system may comprise recirculating a positive electrolyte to a positive electrode, recirculating a negative electrolyte to a negative electrode, directing hydrogen gas to a first catalyst surface, directing the positive electrolyte to the first catalyst surface, and fluidly contacting the hydrogen gas with the positive electrolyte at the first catalyst surface, wherein the positive electrolyte is chemically reduced by the hydrogen gas at the first catalyst surface, a positive electrolyte pH is maintained within a first range, and a state of charge of the positive electrolyte and a state of charge of the negative electrolyte remain substantially constant. The method may further comprise measuring the positive electrolyte pH, measuring the negative electrolyte pH, and supplying hydrogen gas from an external source to the redox flow battery system in response to at least one of a change in the positive electrolyte pH and the negative electrolyte pH. Directing hydrogen gas to a first catalyst surface may comprise directing the hydrogen gas to a first catalyst bed in a first trickle bed reactor, and wherein fluidly contacting the hydrogen gas with the positive electrolyte at the first catalyst surface comprises fluidly contacting the hydrogen gas with the positive electrolyte at the first catalyst bed in the first trickle bed reactor.
The method of operating the redox flow battery system may further comprise directing hydrogen gas to a second catalyst bed in a second trickle bed reactor, directing the negative electrolyte to the second catalyst bed, and fluidly contacting the hydrogen gas with the negative electrolyte at the second catalyst bed, wherein the negative electrolyte is chemically reduced by the hydrogen gas at the second catalyst surface, and a negative electrolyte pH is maintained within a second range. Directing hydrogen gas to a first catalyst surface may comprise directing the hydrogen gas to a catalyst layer adjacent to an electrically insulating ion conducting surface separating the positive electrode from the negative electrode.
Turning now to
At 1520, a spacing layer 1210 may be positioned on the catalyst layer 1206. As described above, the spacing layer 1210 may comprise a porous mesh, foam or sponge. In some example, the spacing layer 1210 may include a plastic material, such as a plastic mesh or a polymer foam or polymer sponge. The porosity of the spacing layer 1210 may be selected to promote higher flows of electrolyte fluid and hydrogen gas through the pores of the spacing layer 1210 as compared to flows of the electrolyte fluid and hydrogen gas through the pores of the substrate layer 1204 and the catalyst layer 1206. The spacing layer 1210 may completely cover the catalyst layer 1206. At 1530, the substrate layer 1204 with the catalyst layer 1206 may be spiral wound to form a jelly roll structured catalyst bed 1220. If the spacing layer 1210 is positioned on top of the catalyst layer 1206, the spacing layer 1210 may also be spiral wound and incorporated into the jelly roll structured catalyst bed 1220 such that the spacing layer 1210 separates successive substrate layers 1204 and catalyst layers 1206 within the jelly roll. In this way, the spacing layer can aid in distributing fluid inside the catalyst bed across the entire surface of the catalyst layer 1206.
Next, method 1100 continues at 1120 where hydrogen gas may be directed from positive and/or negative electrodes to a catalyst surface. As an example, hydrogen that may be generated at a negative electrode from corrosion and/or electrochemical side reactions (e.g., equations (3)-(6)) may be directed to a catalyst surface via pumps and/or ejectors (e.g., ejectors 730, 732; pumps 30, 32). As a further example, hydrogen from an external source (e.g. external source 790) may be directed to a catalyst surface (e.g. step 1170). The catalyst surface may comprise catalyst surfaces of a packed catalyst bed (e.g., 740 or 742) and/or a catalyst layer (e.g., 910 or 1010) positioned between the separator and the negative electrode. For the case of a catalyst layer, e.g., catalyst layer 910 or non-conductive supported catalyst layer 1010 is positioned relative to the negative electrode and/or positive electrode so that the hydrogen may be directed, or may be self-directed (e.g., hydrogen gas may rise) to the catalyst surface. Other catalyst surfaces that catalyze the hydrogen reduction reaction (e.g., equation (6)) may be employed. For example, the catalyst surface comprising a packed catalyst bed may include a packed catalyst bed within a reactor type other than a trickle bed reactor. As a further example, the catalyst surface may comprise a jelly roll structured catalyst bed 1220 inside a reactor vessel 1300.
Next, method 1100 continues at 1130, where electrolyte may be directed to the catalyst surface. The electrolyte may comprise a positive electrolyte and/or a negative electrolyte, and the electrolyte may comprise one or multiple metal ions. The electrolyte may be directed to a catalyst electrolytes may be directed to a catalyst surface from an external source. As a further example, the catalyst surface may be positioned relative to the negative electrode and/or positive electrode so that the electrolyte may be directed, or may be self-directed (e.g., electrolyte may gravity flow) to the catalyst surface. In steps 1120, 1170, and 1130, the hydrogen gas and electrolyte may be directed to the catalyst bed via a recirculation device fluidly positioned between the redox flow battery cell and the catalyst bed. The recirculation device may include a pump, ejector, and the like.
At 1140, method 1100 comprises fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface. As an example, fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface may comprise mixing the hydrogen gas with a liquid electrolyte and injecting the gas-liquid mixture into a trickle bed reactor, thereby fluidly contacting the gas-liquid mixture at a catalyst surface comprising a packed catalyst bed of a trickle bed reactor. As a further example, fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface may comprise positioning a catalyst surface relative to a positive and/or negative electrode wherein hydrogen gas and electrolyte are each directed to and fluidly contact each other at the catalyst surface (e.g., fluidly contacting the hydrogen gas with electrolyte at the thin catalyst layer 910 or 1010). As a further example, fluidly contacting the hydrogen gas with the electrolyte at the catalyst surface may include directing hydrogen gas and the electrolyte radially and axially through successive layers of a jelly roll structured catalyst bed.
Method 1500 continues at 1540 where hydrogen ions and reduced metal ions produced from the redox reaction of hydrogen gas and metal ions and the catalyst surface are recirculated back to the redox flow battery cell. In some examples, the hydrogen ions and reduced metal ions may be recirculated to an electrolyte source (e.g. 50, 52) prior to being recirculated back to the redox flow battery cell. The recirculation of the hydrogen ions and the reduced metal ions may be driven by the recirculation device fluidly positioned between the redox flow battery cell and the catalyst bed, or may be driven by additional recirculation device(s) fluidly positioned between the catalyst bed and the electrolyte source or downstream from the catalyst bed between the catalyst bed and the redox flow battery cell.
Next, at 1150, method 1500 comprises determining if a change in pH is detected, for example, to control a negative electrolyte pH within a pre-determined range. Determining a pH change may comprise measuring a change in pH with an appropriate pH meter or other sensor and/or probe positioned, for example, at a battery cell or electrolyte source. Detecting a change in pH may comprise detecting a pH increase or a pH decrease. Furthermore, detecting a change in pH may comprise detecting a pH increase or pH decrease beyond a first pH range or a second pH range. For example, in an IFB, the first pH range may be from 3 to 4, corresponding to a pH range over which the negative electrolyte is stable, and the second pH range may be from 1 to 2, corresponding to a pH range over which the positive electrolyte is stable. As another example, the first pH range may correspond to a pH less than 4. The first pH range and the second pH range may be predetermined depending on the particular redox flow battery system. For example, a Pourbaix diagram may be used to predetermine the first pH range and the second pH range for the redox flow battery system.
If the detected pH is within the predetermined range, method 1500 continues at 1160, where it is determined if an electrolyte state of charge (SOC) imbalance is detected. Detecting an electrolyte SOC imbalance may comprise measuring a change in one or a plurality of electrolyte concentrations, measuring a change in one or a plurality of electrolyte SOC's, and the like. For example, if the total concentration of ferric ions in the positive electrolyte, indicated by its ORP, is substantially imbalanced with the total concentration of ferrous ions, indicated by its ORP, in the negative electrolyte in an IFB system, then an electrolyte SOC imbalance may be detected. As a further example, the electrolyte SOC imbalance may be determined by averaging measured electrolyte concentrations or electrolyte SOCs over a predetermined time interval. For example, during a predetermined time interval at a known charging or discharging current, the exact amount of electrons transferred in coulombs can be calculated by multiplying the charging or discharging current in Amperes by the predetermined time interval in seconds. Based on the total coulombs transferred and the positive and negative reactions for a redox flow battery system, changes in the amounts of species in the positive and negative electrolytes can be determined. If the measured electrolyte SOC does not balance with changes in the amounts of species calculated from the total coulombs transferred, then an electrolyte SOC imbalance may be determined. If an electrolyte SOC imbalance is not detected, method 1500 ends.
If a negative electrolyte pH is above the predetermined pH range at 1150, or an electrolyte SOC imbalance is detected at 1160, method 1500 returns to 1120 or 1170, where additional hydrogen gas may be directed to the catalyst bed. For example, in an IFB, if the pH of the negative electrolyte increases beyond a first range corresponding to the range where the ferric ions is stable, hydrogen gas may be supplied (e.g., via a controller) to the IFB cell to drive the reduction of ferric ion at the catalyst surface. In this way, the supplied hydrogen gas from an external source may increase the hydrogen partial pressure at the catalyst surface, and may thereby speed up the hydrogen reduction of ferric ion at the catalyst surface, producing protons and reducing the pH of the positive electrolyte. A controller may also supply external hydrogen responsive to a detected electrolyte SOC imbalance. Supplied hydrogen gas from an external source may increase the rate of hydrogen reduction of ferric ion at the catalyst surface, thereby rebalancing the electrolyte SOC in the positive and negative electrolytes.
In this manner, a method of rebalancing electrolytes in a redox flow battery system may comprise: directing hydrogen gas from a redox flow battery cell to a catalyst bed, oxidizing the hydrogen gas at the catalyst bed to form hydrogen ions, and recirculating the hydrogen ions from the catalyst bed to the redox flow battery cell. Additionally, or alternatively, the method may comprise coating a substrate layer with a catalyst layer, and spiral winding the substrate layer and the catalyst layer into a jellyroll structure to form the catalyst bed. Additionally, or alternatively, the method may comprise positioning a spacing layer on the catalyst layer and spiral winding the spacing layer with the substrate layer and the catalyst layer into the jellyroll structure to form the catalyst bed. Additionally, or alternatively, directing hydrogen gas from the redox flow battery cell to the catalyst bed comprises directing hydrogen gas axially into the jellyroll structure of the catalyst bed. Additionally, or alternatively, directing hydrogen gas from the redox flow battery cell to the catalyst bed comprises directing hydrogen gas radially through the spiral wound substrate and catalyst layers of the jellyroll structure. Additionally, or alternatively, the method may comprise directing electrolyte comprising metal ions from the redox flow battery to the catalyst bed, oxidizing the hydrogen gas to form hydrogen ions and reducing the metal ions at the catalyst bed. Additionally, or alternatively, the method may comprise recirculating the hydrogen ions and the reduced metal ions from the catalyst bed to the redox flow battery cell.
As will be appreciated by one of ordinary skill in the art, the methods described in
It will also be appreciated that the configurations and routines disclosed herein are exemplary in nature, and that these specific embodiments are not to be considered in a limiting sense, because numerous variations are possible. For example, the above technology may be applied to other flow battery types. The subject matter of the present disclosure includes all novel and nonobvious combinations and subcombinations of the various systems and configurations, and other features, functions, and/or properties disclosed herein.
The following claims particularly point out certain combinations and subcombinations regarded as novel and nonobvious. These claims may refer to “an” element or “a first” element or the equivalent thereof. Such claims should be understood to include incorporation of one or more such elements, neither requiring nor excluding two or more such elements. Other combinations and subcombinations of the disclosed features, functions, elements, and/or properties may be claimed through amendment of the present claims or through presentation of new claims in this or a related application.
Such claims, whether broader, narrower, equal, or different in scope to the original claims, also are regarded as included within the subject matter of the present disclosure.
This concludes the description. The reading of it by those skilled in the art would bring to mind many alterations and modifications without departing from the spirit and the scope of the description. For example, hybrid redox flow battery systems, all-iron hybrid redox flow battery systems, and other redox flow battery systems may all take advantage of the present description.
The present application is a Continuation of U.S. patent application Ser. No. 17/937,391 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Sep. 30, 2022. U.S. patent application Ser. No. 17/937,391 is a Continuation of U.S. patent application Ser. No. 17/151,611 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Jan. 18, 2021. U.S. patent application Ser. No. 17/151,611 is a Continuation of U.S. patent application Ser. No. 16/201,974 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Nov. 27, 2018. U.S. patent application Ser. No. 16/201,974 is a Continuation of U.S. patent application Ser. No. 15/182,543 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Jun. 14, 2016. U.S. patent application Ser. No. 15/182,543 is a continuation-in-part of U.S. patent application Ser. No. 14/199,794 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Mar. 6, 2014. U.S. patent application Ser. No. 14/199,794 claims priority to U.S. Provisional Patent Application No. 61/832,671 entitled “METHOD AND SYSTEM FOR REBALANCING ELECTROLYTES IN A REDOX FLOW BATTERY SYSTEM”, filed Jun. 7, 2013. U.S. patent application Ser. No. 15/182,543 is also a continuation-in-part of U.S. patent application Ser. No. 14/588,225 entitled “METHOD AND SYSTEM TO MAINTAIN ELECTROLYTE STABILITY FOR ALL IRON REDOX FLOW BATTERIES” filed on Dec. 31, 2024. U.S. patent application Ser. No. 14/588,225 claims priority to U.S. Provisional Application No. 61/949,040 filed Mar. 6, 2014. The entire contents of each of which are hereby incorporated by reference for all purposes.
Number | Date | Country | |
---|---|---|---|
61832671 | Jun 2013 | US | |
61949040 | Mar 2014 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 17937391 | Sep 2022 | US |
Child | 18505880 | US | |
Parent | 17151611 | Jan 2021 | US |
Child | 17937391 | US | |
Parent | 16201974 | Nov 2018 | US |
Child | 17151611 | US | |
Parent | 15182543 | Jun 2016 | US |
Child | 16201974 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 14199794 | Mar 2014 | US |
Child | 15182543 | US | |
Parent | 14588225 | Dec 2014 | US |
Child | 15182543 | US |