The present disclosure relates to automotive vehicle structures. More particularly, the present disclosure relates to automotive structural components.
Automotive vehicles, including vehicles powered by internal combustion engines, electric vehicles powered by batteries, and hybrid vehicles, include a variety of components that are assembled together to define the overall vehicle. The various components may include the engine, drivetrain, differential, control systems, and the like. Additionally, the vehicle is made up of many structural components that define the vehicle shape, which can also be referred to as the vehicle body.
Vehicles are typically constructed in stages, with different portions of a vehicle being assembled in different locations and at different times. This type of modular assembly process provides efficiency benefits for assembling the vehicle.
Accordingly, different modular portions may be assembled for a later overall assembly. One modular portion of the vehicle is the vehicle chassis. The vehicle chassis may include a structural component commonly referred to as a cradle. The cradle provides structure support to a variety of components and vehicle sub-assemblies, which can be mounted to the cradle prior to the final assembly. Once mounted to the cradle, additional components or subassemblies may be mounted to the cradle. At a later time, the vehicle body may be ultimately attached to the cradle as part of the vehicle assembly process.
When assembled, each vehicle component must be able to withstand the various loads and forces that occur during typical vehicle use, such as impacts loads, acceleration loads, bumps, and the like. In response to undergoing loads during use, these vehicle components can in turn result in loads being applied to the cradle to which they are mounted. Heavier components may cause additional loads relative to lighter components.
Additionally, different vehicle constructions and installed components can result in different stiffness requirements for the cradle or sub-frame. These stiffness requirements can drive the sizing requirements for the cradle or sub-frame.
Vehicle cradles are typically made of a strong and stiff material, such as steel, to be able to sufficiently withstand the various loads that occur during typical vehicle use and provide the necessary stiffness. The cradle may be stamped from a particular sheet of steel material to define the overall shape of the cradle that can receive the various components thereon.
Due to the varying load levels and stiffness requirements undergone by the cradle due to different attached components, some portions of the cradle receive higher loads and/or require different stiffness than others. The cradle is typically designed and manufactured to be able to withstand the highest load levels undergone by the cradle as well as the highest stiffness requirements. Efforts have been made to distribute the load across the cradle in order to reduce the overall weight of the cradle by using a thinner gauge of material along the cradle body.
However, it is typically not possible to distribute the load and design the cradle such that each portion of the cradle undergoes the same loads and require the same stiffness. Accordingly, some portions of the cradle are more robust than necessary, because the load requirements and stiffness requirements in those areas are lower. Reducing the thickness of the cradle overall will result in the cradle not being able to withstand the higher loads and/or stiffness requirements at other areas. A cradle with a higher thickness can have material removed in the reduced load areas, however such actions can be time consuming, difficult, and expensive. Moreover, excess material is necessary for the initial build prior to material removal, increasing initial cost outlays, with the excess material being costly waste.
Other automotive structural components can similarly include varying requirements for strength, stiffness, and the like at the different locations of the component. For example, these components may include a body-in-white component, a bumper, a closure panel, the B-pillar, A-pillar, C-pillar, etc. Various vehicle testing standards include requirements for crash resistance and specific crumple characteristics, which can also lead to differing desired thickness at different locations of the vehicle structural component.
In view of the above, improvements can be made the design and manufacture of vehicle structural components that can satisfy variable stiffness requirements that occur across the structural component without being overly heavy or robust at areas with reduced stiffness requirements.
In one aspect, a vehicle structural component is provided comprising: a substrate of the vehicle structural component, the substrate having a substrate thickness; at least one patch member having a size and shape smaller than the substrate, the at least one patch member having a patch thickness; wherein the at least one patch member is bonded to the substrate via a full surface bond between the patch member and the substrate; and wherein a total thickness of the vehicle structural component includes the patch thickness and the substrate thickness at the location of the patch member.
In one aspect, the component includes a bonding layer disposed between the patch member and the substrate.
In one aspect, the bonding layer is brazed and fully wetted between the patch member and substrate.
In one aspect, the bonding layer is an adhesive layer.
In one aspect, the at least one patch member is bonded to the substrate via resistance seam welding.
In one aspect, the stiffness and tensile strength of the structural component at the location of the patch member is at least 90% of the stiffness and tensile strength of a single component having a thickness equal to the total thickness of the patch and the substrate.
In one aspect, the thickness of the structural component varies.
In one aspect, the thickness of the substrate defines a minimum thickness of the structural component.
In one aspect, the stiffness at the minimum thickness of the substrate is less than the stiffness at a location of the patch.
In another aspect, a method of providing variable thickness to a vehicle structural component is provided, the method comprising: providing a substrate having a substrate thickness; providing a patch having a patch thickness; applying the patch to the substrate; and fully bonding the patch to the substrate.
In one aspect, the patch includes a bonding layer disposed on the surface of the patch and the bonding layer is disposed between the patch and the substrate.
In one aspect, the patch is bonded to the substrate via resistance seam welding.
In one aspect, the patch is bonded to the substrate via adhesive bonding.
In one aspect, the patch is bonded to the substrate via brazing.
In one aspect, the method include applying at least one pair of conductive weld wheels against the patch and the substrate on opposite sides thereof and applying current and pressure thereto.
In one aspect, the at least one pair of weld wheels comprises a single pair of weld wheels, the method further comprising applying the single pair of weld wheels along a first path to create a first weld nugget along the first path, and applying the single pair of weld wheels along the second path to create a second weld nugget.
In one aspect, the first and second path are parallel and adjacent, such that the first and second weld nuggets combine to define a continuous surface bond.
In one aspect, the at least one conductive weld wheel comprises: a first pair of weld wheels being radially aligned and defining a first space radially therebetween; and a second pair of weld wheels being radially aligned and defining a second space radially therebetween; wherein the first and second pairs of weld wheels are offset laterally and roll in the same direction; wherein the first and second pairs of weld wheels are configured to receive a patch and a substrate within the first and second space simultaneously.
In another aspect, a system for creating a full surface bond between a substrate and a patch is provided, the system comprising: a first pair of weld wheels being radially aligned and defining a first space radially therebetween; and a second pair of weld wheels being radially aligned and defining a second space radially therebetween; wherein the first and second pairs of weld wheels are offset laterally and roll in the same direction; wherein the first and second pairs of weld wheels are configured to receive a patch and a substrate within the first and second space simultaneously.
In one aspect, the first and second pairs of weld wheels are axially offset.
In one aspect, the first and second pairs of weld wheels are axially aligned.
In one aspect, the substrate is provided in blank form. In another aspect, the substrate is provided in a shaped form.
Other advantages of the present invention will be readily appreciated, as the same becomes better understood by reference to the following detailed description when considered in connection with the accompanying drawings wherein:
With reference to
It will be appreciated that various vehicle types include a variety of different vehicle components. Accordingly, the specific arrangement of the vehicle cradle 12 and its variable thickness as described herein is dependent on the arrangement of said various components. It will be further appreciated that the various components and predetermined layout may be arranged such that the vehicle cradle 12 will have different load and stiffness requirements at different areas, and that such requirements may be determined via computer modeling or the like, with specific regions being identified as having relatively higher or lower load requirements. Areas with relatively higher load and stiffness requirements will typically require a greater thickness. Reference will be made herein to the various vehicle cradles 12 illustrated; however it will be appreciated that the specific shapes of the cradle 12 and the variable thicknesses are exemplary and not limiting to the specific cradles and thickness shown.
It will be further appreciated that the combination of patches 20 with a vehicle substrate 22 or substrate 22 may be applied to other vehicle structural components and are not limited to the chassis, sub-frame, cradle, or the like. For example, various body frame components, such as A-pillars, B-pillars, and the like may have fully bonded stiffening patches 20 to increase thickness and stiffness at selected areas.
In one aspect, the cradle 12 may have a generally box-like overall shape defined by a plurality of linking structure, sections, or sections 14, as shown in
The sections 14 may combine to define the overall shape and layout of the cradle 12 and may also define a plurality of mounting locations 16 (such as sleeves, bushings, holes, or the like) for various vehicle components. The cradle 12 may be a perimeter cradle (
The cradle 12 illustrated in
The sections 14 making up the cradle 12 shape may accordingly include a plurality of zones 18 distributed along the sections 14. The zones 18 may be defined relative to each other as areas of the cradle 12 (or the sections 14 thereof) where different gauges or thicknesses are preferable to account for increased loads at the various zones 18. Accordingly, different zones 18 may have different load requirements, and correspondingly different thickness requirements.
As described above, the cradle 12 of the present disclosure is configured as a variable gauge cradle, such that different zones 18 may have different thicknesses. The specific thickness for selected zones 18 may be determined based on CAE modeling (Finite Element Analysis) and/or CAD modeling. Based on the modeling of the cradle 12, it may be determined which of the zones 18 require relatively large thicknesses and which of the zones 18 require relatively small thicknesses. It will be appreciated that the actual thicknesses of various zones 18 may depend on the specific design and shape of the cradle 12, as well as the specific components intended to be installed on the cradle 12 and the locations of these components. Accordingly, across different vehicle types and installations, the zones 18 that require a thicker gauge will be different from vehicle to vehicle and the various components intended to be installed.
In one aspect, the cradle 12 may have an “infinitely variable” thickness. In this approach, the CAE modeling may identify various zones and a preferred thickness at each zone 18, relative to a baseline thickness. In one example, the cradle 12 may have a thickness that ranges from 1 mm to 5 mm. The thicknesses may be determined using a stiffness based optimization program. The minimum thickness may be 1 mm, with the CAE modeling determining in which zones 18 the thickness shall be increased relative to the minimum thickness. The size and shape of the zones 18 having different thicknesses may depend on the modeling. In one example, a baseline reference mass for a similar cradle without variable thickness may be 25 kg, with a final mass as determined by the CAE model of a variable thickness cradle 12 being 18.6 kg using the stiffness based modeling and infinitely variable thickness of the cradle 12, such that a 6.4 kg mass savings is realized. The reduction in overall weight is due to the traditional cradle having extra thickness in regions or zones 18 where such thickness is unnecessary, such that the baseline thickness is higher than necessary relative to a variable thickness cradle. The variable thickness cradle 12 may have a baseline thickness that is relatively lower than the traditional cradle, with increased thickness in select locations, thereby requiring less material and resulting in lower overall weight. In several structurally sensitive zones, the select locations where additional material is also added includes along the radiuses of the formed sheet metal.
In a related example, CAD modeling may be used based on FEA results. In this example, thickness less than 1.5 mm may be set at 1 mm, thicknesses between 1.5 and 2.5 mm may be set at 2 mm, thicknesses between 2.5 and 4.5 may be set at 3.5 mm, and thicknesses greater than 4.5 mm may be set at 5 mm. Thus, the gauge range for the cradle 12 is still between 1 and 5 mm, but with specific stepped thicknesses to address different ranges of the results of the CAE modeling. In this approach, the baseline reference mass is 25 kg (the same as above), and the final mass of the CAD model is 20.7 kg, for a mass savings of 4.3 kg. Thus, there is still a mass savings realized relative to the initial baseline, although the mass savings is less than the “infinitely variable” thicknesses.
In the above CAD modeling example, thickness of the cradle 12 may be built up in layers having fixed thicknesses, resulting in stepped differences in thickness between different zones 18.
Of course, it will be appreciated that while the infinitely variable thickness is preferable, in practice, localized thicknesses based on ranges may be easier to implement. One approach to increasing thickness in localized zones may be accomplished using patches 20, as further described below.
With reference to
In one aspect, the thickness of the base sheet may be the minimum gauge of the sheet of material forming the panel portion of cradle 12, which may also be referred to as the baseline thickness. In the above examples (with a range of 1 mm to 5 mm), the thickness of the substrate 22 may be 1 mm. The thickness of the patch 20 may be the difference between the desired gauge or thickness and the thickness of the substrate 22. Accordingly, in the above examples, for the zone 18 where a 2 mm thickness would be desired used, the patch 20 may be 1 mm thick and applied to the 1 mm substrate 22. For the zone 18 that is 5 mm thick, the patch 20 may be 4 mm thick and applied to the 1 mm substrate 22. Various other patch thicknesses may be used in other zones 18. In the case of a thicker patch 20, the stepped difference in thickness relative to the baseline thickness is greater than for thinner patches 20. The stepped difference in thickness may be reduced, eased, or transitioned by layering multiple patches 20 over each other, with these patches having different perimeter sizing or surface areas.
In one aspect, multiple patches 20 may be applied in a stack to reach the desired overall thickness. For example, for a 5 mm zone, four 1 mm thick patches 20 may be applied to the 1 mm thick substrate 22. The edges or adjacent stacked layers of patches 20 may be offset relative to each other, thereby allowing for an eased transition from the baseline thickness to the maximum thickness of the zone 18.
Accordingly, the use of the patches 20 in localized areas allows for the ability to create parts, components, or subframes, such as the cradle 12, with a variable thickness throughout. The patches 20 may be used to locally thicken various portions of the sub-frame or cradle 12. By using defined stiffness targets for the cradle 12, patch level and element (small discretized structural unit) level gauge optimization may be used to identify areas or zones 18 of the sub-frame or cradle 12 that can benefit from varying thickness. Accordingly, if a single area or zone 18 requires an increased gauge or thickness, it may be locally thickened rather than having to increase the gauge or thickness of the entire component, thereby saving on overall mass and increasing product performance.
According to analysis of this approach, a perimeter type cradle 12 may save about 8% of mass, and a k-frame type cradle may save from 1-5% of mass when using the patches 20 to locally thicken zones 18 from a baseline thickness. For an infinitely variable gauge or thickness design with gauges ranging from 1.6-5 mm, perimeter cradles 12 may save 14% of mass, with k-frame cradles 12 saving about 11%. Of course, the specific weight savings relative to traditional cradles is dependent on the actual weight of the traditional cradle design and the specific layout of components across the cradle 12. However, as illustrated, some degree of weight savings relative to a traditional cradle may be realized by selectively increasing thickness from a reduced baseline thickness is made possible by the present disclosure.
In another example, when modeling the cradle 12 with stiffness based optimization, but with a gauge range of 1.6-5 mm rather than 1-5 mm, there are fewer zones 18 in which increased thicknesses are identified. The baseline thickness in this approach, being thicker at 1.6 mm vs 1.0 mm in the previous example, therefore requires fewer areas where increased thickness is desired. In an infinitely variable approach, there are still multiple zones 18 in which increased thickness is necessary. Again, the baseline mass of the cradle 12 is 25 kg, with the mass of the infinitely variable cradle 12 being reduced in this case to 21.4 kg, for a 3.6 kg mass savings.
In another example, another approach to varying thickness of the cradle 12 using patches 20 may be used. In this approach, the gauges range from 1.0 to 5 mm. The cradle 12 is split into multiple zones 18 based on the average thickness. The baseline mass is 25 kg, with the resulting mass of this approach being 22.7 kg, for a mass savings of 2.3 kg. The minimum thickness is 1.0 mm, with a variety of different thicknesses disposed around the cradle 12, up to a thickness of 5 mm. Other zones 18 have a thickness that is between 1 and 5 mm. In this approach, single patches 20 are used, with different patches 20 having different thicknesses to arrive at the overall thickness.
In the above-described models, the result of the variable thickness cradles is compared to a baseline mass. The baseline mass is based on an “original” thickness of the illustrated cradle 12, which is less than 4 mm. When modeling the desirable thickness for a variable thickness cradle 12, the maximum thickness may be set at the original thickness or may be set at a maximum thickness that is greater than the original thickness. The maximum thickness being greater than the original thickness for the same given layout of components allow the variable gauge cradle 12 to provide additional thickness and strength in zones 18 of need. In the traditional cradle, a thickness corresponding to the maximum thickness of the variable gauge would result in cradle 12 that is overly heavy.
When modeling with a maximum thickness based on the original thickness, the resulting necessary thickness is less variable, because a structural optimization process does not add larger thicknesses in certain areas. Accordingly, additional thickness is added in other areas to compensate.
When modeling with a maximum that is above the original thickness, for example with a maximum thickness of 4 mm, the thickness across the cradle 12 can vary more, because areas of need can be addressed specifically, and therefore other areas can have further reduced thicknesses.
For example, with the baseline mass of 25 kg, when the range is from 0.0 to 4 mm, the CAE modeled mass is below the baseline. When the range is from 0.0 to original thickness, the CAE modeled mass is below the baseline.
In another example, a CAE model of a k-frame style cradle 12 is used. The thickness ranges from 1.005 to 5.8 mm. Much of the cradle 12 has a minimum thickness, with various zones 18 having higher thicknesses. In particular, sleeves 16 (such as those shown in
In yet another model of the k-frame style cradle 12, the gauges range from 1.6 to 5 mm. In this example, a larger portion of the cradle 12 is at the minimum thickness, with fewer zones 18 having increased thickness relative to the previous example. The sleeves 16, again, may have maximum thickness. The baseline mass is 20.0 kg, and this model results in a mass of 17.7 kg, for a mass savings of 2.3 kg.
Thus, in view of the above, the variable gauge cradle 12 may provide the necessary stiffness of a typical cradle, but with reduced mass, by having localized areas or zones 18 with increased thickness. The increased thickness may be greater than the original thickness of the traditional cradle, allowing for reduced thicknesses in other areas.
Accordingly, a cradle or sub-frame may include a plurality of interconnected sections 14 that define a shape of the cradle 12, as shown in
In another aspect, the variable thickness of the cradle 12 may be accomplished by other manufacturing methods other than additional sheets of material. For example, metal deposition techniques, such as cold spray or sintering (additive manufacturing methods), may be used to add thickness to identified local zones 18 of the cradle 12. The additional material may be built up on the substrate 22 and may define the patch 20.
In another aspect, the above-described variable gauge or thickness may be applied to other structural components of the vehicle other than the cradle 12. For example, the variable gauge approach may be applied to frame rails, B-pillars, and the like.
In view of the above, and with reference to
The cradle 12 shown in
The cradle 12 further includes a pair of end sections 19 that extend outwardly from the front portion 17. The end sections 19 include support sleeves 16 configured for mating with additional vehicle structure. The cradle 12 forms a generally closed loop and includes an open space defined by the closed loop shape.
The side portions 13 also include support sleeves 16 configured for mating with additional vehicle structure. The portions 13, 15, 17 described herein may be in the form of generally hollow structures formed by an assembly of formed sheet metal portions, and may also be generally described as section 14.
Of course, it will be appreciated that while the infinitely variable thickness may be preferable for a cradle or the like, in practice, localized thicknesses based on ranges may be easier to implement. One approach to increasing thickness in localized zones may be accomplished using patches 20.
With reference to
In one aspect, the patches 20 may be bonded to the substrate 22 via resistance spot welding. In resistance spot welding, the patch 20 is applied to the substrate/substrate 22, and a spot welding device passes a current through the patch 20 and the substrate 22, which melts the material of the patch 20 and substrate such that they are welded together at the location of the spot weld. Patches 20 may be applied to the substrate 22 via the spot welding, with spot welding occurring at a plurality of locations across the surface of the patch 20 to increase the bonded surface area of the patch 20.
Accordingly, the spot welding process that produces a single spot weld is repeated a number of times until a sufficient surface area between the patch 20 and the substrate 22 has been bonded. With enough spot welding locations, the patch 20 and the substrate 22 may be bonded together over a substantial portion of the surface area, increasing the strength of the bond between the patch 20 and the substrate 22. In this approach, the overall gauge of the component may be increased at the areas of the spot weld, with the overall gauge being approximately the thickness of the substrate 22 plus the thickness of the patch 20.
In one aspect, the patch 20 may be fully bonded to the substrate 22. To fully bond the patch 20 to the substrate 22, the patch 20 is applied to the substrate 22 and the entire surface area or substantially the entire surface area of the patch 20 is welded and/or bonded to the substrate 20. Full surface bonding may be accomplished in multiple ways. In one aspect, resistance seam welding may be used. In another aspect, brazing may be used. In yet another aspect, adhesive bonding may be used.
As described above, full surface bonding between the patch 20 and the substrate 22 may be accomplished using resistance welding. More particularly, resistance seam welding may be used. Resistance seam welding is another form of electric resistance welding.
Resistance seam welding is illustrated schematically in
Unlike spot welding, which uses a plurality of distinct spots across a surface, the seam welding technique creates a strip of bonded surface along the path that the wheels 24 travel. The seam welding process may be repeated to create a plurality of adjacent strips of bonded surface area. Due to the continuous length of the strips, far fewer welding steps are used relative to the spot welding process. Additionally, the continuous length of the strips provides for continuous coverage of the overlapping surface area between the patch 20 and the substrate 22, unlike a series of spot welds that may include gaps.
The width of the weld strip may be varied by the width of the wheels 24. Weld wheels 24 with a thinner width will produce a thinner weld strip, and wheels 24 with a wider width will produce a wider weld strip. The plurality of weld strips may be created sequentially, where a first weld strip is created, and the wheels 24 or the work piece is shifted, aligning the wheels 24 with the adjacent area to be welded. The plurality of weld strips need not necessarily be created adjacent the prior strip, but may also be offset and separate from the prior strip, with the gap that is created therebetween being filled by another weld strip at a later time.
In one aspect, the previously applied weld strip is allowed to cool and fully cure prior to application of the subsequent weld. The subsequent weld strip may have a path that partially overlaps the previously applied weld strip. Alternatively, the subsequent path may be aligned such that there is little to no overlap. Preferably, there are no lateral gaps between the weld strips after each of the intended weld strips are created. However, it will be appreciated that some nominal gaps may occur between adjacent weld strips.
If necessary, the wheels 24 may be returned to an area where a gap exists, such that the gap is eliminated by a further weld strip. Such additional or further welds strips may be created on an ad hoc basis in response to detecting an unintended gap, or the further weld strips to fill the gaps may be planned. For example, if it is desirable for the weld strips to be fully cured prior to applying an adjacent weld strip, weld strips may be created in a pattern such that a gap is intended to be created, and then the gap may be filled later after the two strips with the gap between them have cured.
The direction of the weld path is preferably in the direction where tensile strength is desired or the direction in which shearing loads may occur between the patch 20 and the substrate 22. Thus, the determination of the direction of the weld strip may vary depending on the type of structural component and its expected loads. However, the resulting weld and bond created by the seam welding is still robust in a direction transverse to the direction of the weld strips.
The resulting weld that occurs from the path of the weld wheels 24 may be wider than the width of the wheels 24. The heating of the material between the wheels 24 will cause material adjacent the wheels 24 to become heated, as well, which may lead to the adjacent material also melting and bonding. Accordingly, even if there is a nominal gap between the weld paths, the material in the area of the gap may still be bonded due to the heat that extends beyond the edges of the weld wheels 24.
In the above-described approach, the wheels 24 have been described as having paths that are generally parallel to each other and offset laterally to ultimately cover substantially the entire surface area of the bond. In another approach, subsequent weld paths may be used that are transverse to the direction of a previous weld path. For example, subsequent weld paths may be applied perpendicular to a previous weld path. For another example, subsequent weld paths may be at an oblique angle relative to other weld paths.
The above-described approach has referred to a single pair of wheels 24. However, in one aspect, multiple pairs of wheels 24, as shown in
The wheels 24 may be arranged laterally adjacent and axially aligned, such that they are applied to the patch 20 and the substrate at the same time. Alternatively, the wheels 24 may be staggered, such as that shown in
In another aspect, the patches 20 may be bonded to the substrate via a full surface bond created by brazing. Brazing involves joining two metal materials by melting an intermediate layer, which may also be referred to as a bonding layer 23. The material used for the bonding layer 23 in a brazing process may have a melting point that is lower than the melting point of the metals being joined. Brazing may provide a very strong bond between the same or different metals. In the brazing process, the metals themselves are not typically melted. Rather, the metals and the plating layer are heated to a temperature that is above the melting temperature of the brazing material but below the melting temperature of the metals being joined. Thus, the brazing material will melt, but the metals will not.
The brazing material, being melted between the metals to be joined, will thereby flow into the gaps formed between the metal parts. The brazing process may therefore be beneficially used with the patches 20 and the substrate 22. Upon melting and flowing into the gaps between the metal components, the brazing material will then be cooled, thereby creating a strong bond between the patch 20 and the substrate 22. Thus, a full surface bond between the base metals (the patch 20 and the substrate 22) may be formed by the brazing process.
In another aspect, as mentioned previously, full surface bonding between the patch 20 and the substrate 22 may be achieved via adhesive bonding. Similar to brazing and resistance seam welding, an adhesive layer of material may be disposed between the patch 20 and the substrate 22 across the entire surface of the interface therebetween. The adhesive layer may also be referred to as the bonding layer 23. The bonding layer 23 in the form of an adhesive layer may be applied to one of both of the patch 20 and substrate 22, such that when the patch 20 is placed on the substrate 22, the adhesive is disposed between them. Thus, the bonding layer 23 in the form of an adhesive may bond to both the patch 20 and the substrate 22, thereby joining the patch 20 to the substrate 22.
The adhesive bonding layer 23 may be in the form of a tape or peel-able layer that may adhere to one or both of the patch 20 and substrate 22, thereby allowing the bonding layer 23 to be applied to one of the components and then be later applied to the other of the components at the time of bonding. The adhesive bonding layer 23 may be activated in response to being heated to a target temperature (which is less than a melting temperature of the patch 20 or substrate 22). Similar to the brazing process, upon cooling, the adhesive bonding layer 23 may thereby provide a full surface bond between the patch 20 and the substrate 22.
The adhesive bonding layer 23 may be a single material that bonds to both the patch 20 and the substrate 22. In another aspect, the adhesive bonding layer 23 may be two different materials that individually may not provide for a bond between the patch 20 and the substrate 22. However, upon mixing the materials, the individual materials will combine to form an adhesive that bonds with both the patch 20 and the substrate 22.
The adhesive may be applied to the patch 20 and/or substrate 22 in a generally solid state, whereby upon heat or another activating event, the adhesive bonding layer 23 may provide a bond between the patch 20 and the substrate 22. In another aspect, the adhesive may be applied in a generally liquid form that may be “painted” or otherwise distributed across the surface of the interface between the patch 20 and the substrate 22. In one aspect, the adhesive may be applied generally evenly across the interface between the patch 20 and/or substrate. In another aspect, the adhesive may be applied such that it does not initially cover the entire surface of the interface, but upon pressure and or heating/activation, the adhesive will flow into the un-covered areas to thereby cover the full interface area between the patch 20 and the substrate 22.
Accordingly, in view of the above, the full surface bond between the patch 20 and the substrate 22 may be achieved via resistance seam welding, brazing, or adhesive bonding. Additionally, a full surface bond between the patch 20 and the substrate 22 may be accomplished by other bonding methods that may include a bonding layer that may be configured to cover the full area of the interface between the patch 20 and the substrate 22.
With reference again to the resistance seam welding process, and with reference to
The patch 20 may be applied to the substrate 22 with the bonding layer 23 facing the substrate 22 and contacting the substrate 22. Put another way, the bonding layer 23 is disposed between the patch 20 and the substrate 22. However, it will be appreciated that the patch 20 and bonding layer 23 that is applied to the patch 20 may also be referred to collectively as the patch 20.
Upon application of the current and force provided by the wheels 24 to the patch 20 and substrate 22 in the resistance seam welding process, a weld nugget 25, which may be in the form of a strip as described above, will be created at the location of the bonding layer 23, as shown in
In one aspect, the substrate 22 may be made of galvanized steel. The patch 20 may also be made of galvanized steel.
In another aspect, the substrate 22 may be made of uncoated steel. The patch 20 may also be made of uncoated steel.
As described above, the patch 20 may be plated with the bonding layer 23. In another aspect, the substrate 22 may be plated with the bonding layer 23 in addition to or alternatively from the patch 20.
The patch 20 may have a variety of different shapes, depending on the shape of the substrate 22 or other component to which it is attached. For example, the patch may be a square or rectangle, or it may be in the form of an elongated strip. The patch may have a complex shape with a variety of perimeter shapes that correspond to the shape of the surface area to which it will be bonded.
In one aspect, the patch 20 is bonded to the substrate 22 when the substrate in its “blank” form, meaning the form of the substrate prior to being stamped, formed, or otherwise shaped into its final structural shape. In this aspect, the patch 20 may have a shape that does not necessarily match the shape of the area where the patch 20 will ultimately exist in the final form of the component. The final shape of the structural component may then be stamped or cut from the bonded patch 20 and substrate 22 combination.
In another aspect, the patch 20 may be bonded to the substrate 22 after the substrate 22 has been stamped or otherwise formed/shaped into its final component shape. In this aspect, the patch 20 may be shaped to correspond to the shape of the area to which it will be applied. However, the patch 20 may also have a non-matching shape, and the patch may be further processed to remove excess material that does not correspond to the final shape of the substrate 22 or the bonded area.
The patch 20 may have a variety of thicknesses. It one aspect, the patch 20 may be up to 4 mm thick with chassis grade steel (HR340LA). However, other thicknesses may also be used, such as 1 mm, 2 mm, 3 mm. Additional thickness ranges may also be possible with other materials.
In one aspect, the speed of the wheels 24 may be controlled during the bonding process. In one example, 250 mm/min may be the speed at which the wheels 24 travel to heat and bond the patch 20 to the substrate 22. In another example, 1 m/min may be used for an increased speed, which is possible with HR340LA. The pass width may, in one aspect, be 10-20 mm. The current applied by the wheels 24 may be up 22 kA. The current that is used may depend on the speed that is used.
In one example, using a 6×6 inch patch 20 with a 2 mm thickness and using four weld heads/wheels 24, the total contact time between the wheels 24 and the patch 20 is 18.4 seconds when bonding the patch 20 to the substrate 22 in the form of a blank.
In one example, illustrated in
In further examples, shown in
The material of the patches 20 and substrate 22 may be HR340LA, either galvanized (coated) or uncoated. In one aspect, the substrate 22 may be 2 mm thick, with an additional 2 mm added via the patches 20. The combined substrate 22 and patches 20, after bonding, may be resistant to tension, lap shear, and 4-point bending, which provides confirmation of a successful bond therebetween.
In one aspect, shown in
The coupons 27 may be cut from the combined patch 20 and substrate 22 in the direction of the rolling force applied by the wheel 24 (
FIGS. 20-22 illustrate the results of 4 point bending. The solid 4 mm coupons are shown separated and lower than the other coupons as extension increases in both
As described above, larger surface areas relative to the size of the wheel 24 may be accomplished using multiple passes of the wheel 24. The multiple passes may be applied simultaneously or staggered within a short period of time. This approach provides time savings relative to conducting subsequent passes after the bond has cooled.
As described above, the patch 20 may be applied to the substrate 22 in blank form, where stamping may occur at a later time. However, the patch 20 may also be applied to a pre-stamped substrate in some instances, depending on the shape of the substrate 22 after stamping or forming.
The use of the patches 20 bonded to the substrate 22 provides additional advantages beyond the increased stiffness. For example, the addition of patches 20 to the substrate 22 increases corrosion resistance. Moreover, the thickness of the combined substrate 22 and patch 20 can be further increased in the event of a modified stiffness requirement, which may require an additional thickness beyond what was initially intended. For example, an initial design requirement may call for a first stiffness requirement in a particular location on a vehicle structural component. However, a design change at a later time and after manufacturing of the base structural component has begun may require additional stiffness in an isolated area. The existing structural component can be modified with the fully bonded stiffening patch 20 described herein
In one aspect, the thickness of the substrate 22 may be the minimum desired gauge of the cradle 12. In one example, the thickness of the substrate 22 may be 1 mm. The thickness of the patch 20 may be the difference between the desired gauge or thickness in the area of the patch 20 and the thickness of the base substrate 22. Accordingly, prior examples of
However, in another aspect, multiple patches 20 may be applied in a stack to reach the desired overall thickness. For example, for a 5 mm zone, four 1 mm thick patches 20 may be applied to the 1 mm thick substrate 22.
Accordingly, the use of the patches 20 in localized areas allows for the ability to create parts, such as the cradle 12, with a variable thickness throughout. The patches 20 may be used to locally thicken various portions of the sub-frame or cradle 12. By using defined stiffness targets for the cradle 12, free-size gauge optimization may be used to identify areas or zones 18 of the sub-frame or cradle 12 that can benefit from varying thickness. Accordingly, if a single area or zone 18 requires an increased gauge or thickness, it may be locally thickened rather than having to increase the gauge or thickness of the entire component, thereby saving on overall mass and increasing product performance.
According to analysis of this approach, a perimeter type cradle 12 may save about 8% of mass, and a k-frame type cradle may save from 1-5% of mass when using the patches 20. For an infinitely variable gauge or thickness design with gauges ranging from 1.6-5 mm, perimeter cradles 12 may save 14% of mass, with k-frame cradles 12 saving about 11%.
Thus, in view of the above, the structural component 12 having localized patches may provide the necessary stiffness of a typical component, but with reduced mass, by having localized areas or zones 18 with increased thickness created by the fully bonded patches 20. The increased thickness may be greater than the baseline or original thickness of the typical component, allowing for reduced thicknesses in other areas.
Accordingly, a component 12 may have sections 14 that define a shape of the component 12. The sections 14 may have a first thickness disposed along a first portion of the sections 14, wherein the first thickness is a minimum thickness of the cradle 12. The sections 14 may further include a second thickness disposed at a second portion of the section 14. The sections 14 may further include a third thickness disposed at a third portion of the sections 14, wherein the third thickness is a maximum thickness of the component 12. The second thickness may be greater than the first thickness and less than the third thickness. In one aspect, the second and third thicknesses are defined by a patch 20 applied to the section 14, such that the combined thickness of the section 14 and the patch 20 defines the thickness of the section 14.
In another aspect, the variable thickness of the component 12 may be accomplished by other manufacturing methods other than patches. For example, metal deposition techniques, such as cold spray or sintering, may be used to add thickness to identified local zones 18 of the component 12.
In another aspect, the above-described variable gauge or thickness may be applied to other structural components of the vehicle other than the illustrated component 12. For example, the variable gauge approach may be applied to frame rails, B-pillars, and the like.
Obviously, many modifications and variations of the present invention are possible in light of the above teachings and may be practiced otherwise than as specifically described while within the scope of the appended claims. These antecedent recitations should be interpreted to cover any combination in which the inventive novelty exercises its utility. The use of the word “said” in the apparatus claims refers to an antecedent that is a positive recitation meant to be included in the coverage of the claims whereas the word “the” precedes a word not meant to be included in the coverage of the claims.
This PCT International Patent application claims the benefit of and priority to U.S. Provisional Patent Application Ser. No. 62/883,830 filed on Aug. 7, 2019, and titled “Method For Using Multiple Resistance Seam Welding Heads To Bond Patches,” and U.S. Provisional Patent Application Ser. No. 62/891,641 filed on Aug. 26, 2019, and titled “Fully Bonded Stiffening Patch For Automotive Structural Components,” the entire disclosures of which are hereby incorporated by reference.
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/US2020/045186 | 8/6/2020 | WO |
Number | Date | Country | |
---|---|---|---|
62883830 | Aug 2019 | US | |
62891641 | Aug 2019 | US |