1. Field of the Invention
The present invention relates to a method for fabricating a metal-plastic composite body, and more particularly, to a fabricating method using insert injection molding technology to form plastic mold members, light-guiding pattern of logos, camera lens, or fill (flash) light lens directly on a metal piece or a metal housing.
2. Description of the Prior Art
In recent years, metal housings with lightweight and high rigidity properties have become more and more necessary since the portable electronic products are developed to be lighter, shorter and smaller. In order to follow such requirements, the technology for composite materials that combines metal housing with plastic mold members has become a main focus in the industry. The conventional method for fabricating the above-mentioned composite article may comprise the steps of molding the metal piece and the plastic piece separately, applying an adhesive on the metal piece, and then stacking and bonding the metal piece and plastic piece together by pressing. However, the metal housing used in 3C product is usually provided with irregular curved surfaces rather than simple plane structures, and the plastic piece may also have corresponding curved surfaces. It is very difficult for two curved surfaces to bond to each other, thereby hindering the yield enhancement.
In relevant prior art, a method for tightly bonding carbon fiber reinforced plastic (CFRP) pre-preg with a metal alloy is disclosed in Japanese Patent Publication No. 2011-73191. Please refer to
A method for fabricating a composite body composed of metal alloys and thermosetting resin is disclosed in Japanese Patent Publication No. 2010-274600. Please refer to
A method for fabricating buttons is disclosed in Japanese Patent Publication No. 2007-179952. The method features the following steps: bonding a metal coating of an outer key top piece and a white coating of an inner key top piece via a fusion layer.
A method for fabricating push-buttons is disclosed in Japanese Patent Publication No. 2009-81030. In this method, the adhesive used for bonding the cover member and the key top is applied in dot arrays between said cover member and said key top, in order to facilitate the degassing process during the fabrication.
A metal surface treatment method is disclosed in China Patent Publication No. 1827839. The method comprises: applying a primer first, coating a metal film by vacuum deposition, and then spray a transparent hard film on a metal piece for protection. The purpose of said method is to fabricate the Mg alloy product with a metal texture by surface-treating a raw piece of Mg alloy via vacuum deposition process.
A method of fabricating metal-resin composite articles by injection molding is disclosed in Japanese Patent Publication No. 2011-11505. Please refer to
A method for fabricating composite articles is disclosed in Japanese Patent Publication No. 2011-11505. The method comprises: forming a decorative sheet on one surface of a metal body simultaneously with the injection of a molten resin, thereby forming a composite article composed of the metal body and the injected resin in the desired mold shape.
Please refer to
The main purpose of the present invention is to provide a method for fabricating an improved metal-plastic composite body in order to overcome the shortcomings and disadvantages in prior art.
The other purpose of the present invention is to provide a fabricating method using insert injection molding technology to formed plastic mold members, light-guiding pattern of logo, camera lens, or fill (flash) light lens directly on a metal piece or a metal housing.
According to one embodiment of the present invention, a method for bonding a plastic member onto a metal housing is provided comprising the steps of: preparing a metal housing having an inner surface and an outer surface, wherein the metal housing has at least one hollow-carved area; subjecting the metal housing to a physical processing, thereby forming a bonding area on the inner surface; forming an adhesive layer on the bonding area; performing a first injection molding to bond a plastic mold member on the adhesive layer; and performing a second injection molding to form an optical plastic member in the hollow-carved area.
These and other objectives of the present invention will no doubt become obvious to those of ordinary skill in the art after reading the following detailed description of the preferred embodiment that is illustrated in the various figures and drawings.
The accompanying drawings are included to provide a further understanding of the embodiments, and are incorporated in and constitute a part of this specification. The drawings illustrate some of the embodiments and, together with the description, serve to explain their principles. In the drawings:
It should be noted that all the figures are diagrammatic. Relative dimensions and proportions of parts of the drawings have been shown exaggerated or reduced in size, for the sake of clarity and convenience in the drawings. The same reference signs are generally used to refer to corresponding or similar features in modified and different embodiments.
In the following detailed description of the invention, reference is made to the accompanying drawings which form a part hereof and wherein are shown, by way of illustration, specific embodiments in which the invention may be practiced. These embodiments are described in sufficient details to enable those skilled in the art to practice the invention. Other embodiments may be utilized; structural, logical, and electrical changes may be made without departing from the scope of the present invention.
Please refer to
The plastic mold member 12 is injection-molded on a bonding area SB at one inner surface S1 of the metal housing 10. To be more specific, the bonding area SB is formed by physical processing or chemical processing before performing the inject-molding of bonding area SB. The plastic mold member 12 is inject-molded on an adhesive layer 112, thereby establishing a tight bonding with the metal housing 10. The above-mentioned physical processing for forming bonding surface SB may include roughening treatment by sandblast, laser etching, plasma treatment, UV plasma treatment, or die pressing, while the chemical processing may include chemical etching and shaping.
According one embodiment of present invention, the metal housing 10 is further provided with a hollow-carved logo area 10a, like the dashed area depicting “LOGO” in capital letters in
According to one embodiment of present invention, a decorating layer 101 may be coated on an outer surface S0 of the metal housing 10 to obtain various textures and appearances. Furthermore, in order to obtain an uniform metal texture so that the logo on metal housing 10 will be imperceptible to the user when the light source 22 on the outer surface S0 of metal housing 10 is off, a Ni metal film may be coated on the outer surface S0 of the metal housing 10 and the outer surface 14a of the optical plastic member 14 to provide a logo with a hidden backlight effect.
According to another embodiment of the present invention, the optical plastic member 14 may also be integrated with a camera lens or a flash (fill) light lens on the metal housing 10. If the optical plastic member 14 is integrated with flash (fill) light lens on metal housing 10, the light diffusing pattern or the prism pattern may be formed directly on the inner surface.
Please refer to
After the deburring process, a bonding area is formed on the inner surface of metal housing (step M05). According to one preferred embodiment of the present invention, the bonding area may be subjected to a surface treatment by a physical process, such as sandblast. Of course, other physical processes, like laser etching, plasma treatment, UV plasma treatment or die molding, may also be utilized to obtain the roughened surface. Alternatively, the bonding area may also be formed by chemical processes like chemical etching and shaping. Then, a cleaning process (step M06) and a process for coating adhesive (step M07) are performed. The adhesive coating or adhesive bonding primers can be formed on the surface-treated bonding area by a spraying, a dispensing or a printing method to form an adhesive layer on said bonding area. A baking process is finally performed (step M08). This way the sub-flow S100 is completed. The metal housing treated by the sub-flow S100 is ready to undergo the following steps of insert injection molding (i.e. sub-flow S102).
The sub-flow S102 will be described hereinafter. First, a feeding step and an inspection step for a plastic material are performed (step P01), wherein the plastic material may be polycarbonate (PC) resin, acrylonitrile butadiene styrene (ABS) resin or polyphenylene sulfide (PPS) resin, etc. A drying process (step P02) is performed, followed by an first insert injection molding process to injection-mold the plastic material on the metal housing treated by sub-flow S100 (step P03). To be more specific, the plastic material is injection-molded directly on the adhesive layer of the bonding area of the metal housing. The metal housing can, for example, be a cell phone housing or a battery cover, while the injection-molded plastic mold members may be input/output jacks, assembly structures and/or reinforcement structures. Since the insert injection molding is a well-known process, the relevant details are omitted herein for simplicity. Then, perform a deburring process (step P04), and a second insert injection molding process (step P05) is subsequently performed to simultaneously form an optical plastic member in the hollow-carved logo area on metal housing and a patterned light-guiding structure on the inner surface of said optical plastic member. The optical plastic member may be formed of polycarbonate (PC) resin or Polymethyl-methacrylate (PMMA) acrylic material. Next, a surface finishing step may be optionally carried out (step P06), such as sandblast, hair-line surface treatment, physical vapor deposition (PVD) process, anodic treatment or spray treatment, etc. Please note that the foregoing PVD treatment further includes a Ni-plating process, which may especially conceal the characters on the surface of the housing. In addition, a decorating layer may be formed on the outer surface of the metal housing by printing, coating, or anodized aluminum treatment to obtain various colors, patterns and texture designs. Finally, a shaping step (step P07) and a back-end quality control step (step P08) are performed. The sub-flow S102 is then completed.
Please refer to
After the cleaning process, perform a surface finishing step (step M17), such as sandblast, hair-line surface treatment, PVD process, anodic treatment or spray treatment, etc. Please note that the foregoing PVD treatment further includes a Ni-plating process which may especially conceal the characters on the surface of housing. In addition, a decorating layer may be formed on the outer surface of the metal housing by printing, coating, or anodized aluminum treatment to obtain various colors, patterns and texture designs. Then, perform a process for coating adhesive (step M18), like coating the adhesive or the adhesive bonding primers on the surface-treated bonding area by a spraying, a dispensing or a printing method to form an adhesive layer on said bonding area. Then, perform a baking process (step M19), thereby completing the sub-flow S200. The metal housing treated by the sub-flow S200 is ready to undergo the following insert injection molding (i.e. sub-flow S202).
The sub-flow S202 will be described hereinafter. First, perform a feeding step and an inspection step for a plastic material (step P11), wherein the plastic material may be polycarbonate (PC) resin, acrylonitrile butadiene styrene (ABS) resin or polyphenylene sulfide (PPS) resin, etc. Perform a drying process (step P12) and an first insert injection molding process (step P13) to inject-mold the plastic material or plastics on the metal housing previously treated by sub-flow S200. To be more specific, the plastic is inject-molded directly on the adhesive layer on the bonding area of metal housing. For example, the metal housing maybe a cell phone housing or a battery cover, while the injection-molded plastic mold members may be input/output jacks, assembly structures and/or reinforcement structures. Since the insert injection molding is a well-known process, the relevant details are omitted herein for simplicity. Then, perform a deburring process (step P14). A second insert injection molding process (step P15) is subsequently performed to simultaneously form an optical plastic member in the hollow-carved logo area on the metal housing and a patterned light-guiding structure on the inner surface of said optical plastic member. The optical plastic member may be formed of polycarbonate (PC) resin or Polymethyl-methacrylate (PMMA) acrylic material. Finally, perform a shaping step (step P15) and a back-end quality control step (step P16), thereby completing the sub-flow S202.
Those skilled in the art will readily observe that numerous modifications and alterations of the device and method may be made while retaining the teachings of the invention. Accordingly, the above disclosure should be construed as limited only by the metes and bounds of the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
100135017 | Sep 2011 | TW | national |