Claims
- 1. A method for continuously coating a fiber with a substantially bubble free coating comprising the steps of surrounding said fiber with helium at the point at which said fiber enters the meniscus of a liquid coating composition, drawing said fiber through a body containing said liquid coating composition, removing excess coating liquid from the fiber, and curing the coating liquid to form a solid protective layer thereon, wherein said fiber passes through cooling means prior to its passing into said coating liquid, and wherein said helium is provided by flowing said helium toward said fiber in an air displacing region located between said coating liquid and said cooling means.
- 2. The method of claim 1 wherein said fiber passes through cooling means prior to its passing through said coating liquid, and wherein said air displacing region is spaced from said cooling means.
- 3. The method of claim 1 wherein said coating liquid is contained in a coater and wherein said fiber passes through cooling means prior to its passing through said coater, and wherein said cooling means is located immediately adjacent said coater so that air cannot become entrained with said fiber after it passes out of said cooling means and before it passes into said coating liquid.
- 4. The method of claim 3 wherein jets of helium containing gas are directed toward said fiber as it passes through said cooling means.
- 5. The method of claim 1 wherein said fiber is subjected to a reduced pressure prior to its passing into said helium.
- 6. A method for coating a fiber with a substantially bubble free coating comprising the steps of:
- positioning an air displacing apparatus containing an atmosphere of helium adjacent to and above a liquid coater containing a liquid coating composition,
- drawing the fiber through the air displacing apparatus and surrounding the fiber with helium as the fiber exits the air displacing apparatus,
- drawing the fiber through the liquid coater such that the fiber is surrounded by helium as it enters the coating composition, and
- curing the coating liquid to form a solid protective layer thereon, wherein the fiber passes through cooling means prior to its passing into the coating liquid, and wherein the atmosphere is provided by flowing the atmosphere toward the fiber in an air displacing region located between the coating liquid and the cooling means.
- 7. The method of claim 6 wherein the fiber passes through cooling means prior to its passing through the coating liquid, and wherein the air displacing region is spaced from the cooling means.
- 8. The method of claim 6 wherein the fiber passes through cooling means prior to its passing through the coater, and wherein the cooling means is located immediately adjacent the coater so that air cannot become entrained with the fiber after it passes out of the cooling means and before it passes into the coating liquid.
- 9. The method of claim 8 wherein jets of helium containing gas are directed toward the fiber as it passes through the cooling means.
- 10. The method of claim 6 wherein the fiber is subjected to a reduced pressure prior to its passing into the atmosphere.
- 11. A process for continuously coating a fiber with a substantially bubble-free coating comprising the steps of:
- passing said fiber through cooling means;
- drawing said fiber through a coater containing a liquid coating composition;
- surrounding said fiber with helium such that at the interface at which said fiber enters the entrance surface of said liquid coating composition said entrance surface has an atmosphere comprising helium in an amount which is effective to provide a substantially bubble-free coating after curing;
- drawing said fiber out of said liquid coating composition, and
- curing said liquid coating composition on said fiber, wherein an atmosphere which surrounds said fiber downstream of said coater and prior to said curing step has a lower helium concentration than the atmosphere surrounding said fiber at said interface.
- 12. A process for continuously coating a fiber with a substantially bubble-free coating comprising the steps of:
- passing said fiber through cooling means;
- drawing said fiber through a coater containing a liquid coating composition;
- prior to coating said fiber, establishing a flow of He gas against said fiber to sweep entrained air therefrom and surrounding said fiber with helium such that at the interface at which said fiber enters the entrance surface of said liquid coating composition said entrance surface has an atmosphere comprising helium in an amount which is effective to provide a substantially bubble-free coating after curing;
- drawing said fiber out of said liquid coating composition, and
- curing said liquid coating composition on said fiber.
Parent Case Info
This is a division of application Ser. No. 08/409,231, filed Mar. 23, 1995.
US Referenced Citations (5)
Foreign Referenced Citations (3)
Number |
Date |
Country |
0 579 388 |
Jan 1994 |
EPX |
54-131042 |
Oct 1979 |
JPX |
1286941 |
Nov 1989 |
JPX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
409231 |
Mar 1995 |
|