Claims
- 1. In a method for applying a coating of stannic oxide to a glass surface by contacting the surface with a finely divided liquid tin compound while maintaining the glass surface at a temperature of between 450.degree. and 600.degree. C., whereupon the tin compound is pyrolyzed to form stannic oxide, the improvements which reside in (1) employing monobutyltin trichloride as the tin compound and (2) isolating and recovering the unpyrolyzed monobutyltin trichloride for subsequent reuse in accordance with said method.
- 2. A method as described in claim 1 wherein the isolation and recovery of the unpyrolyzed butyltin trichloride is effected by combining the compound with water to form an aqueous solution and subsequently separating said compound from the aqueous solution.
BACKGROUND OF THE INVENTION
This application is a continuation-in-part of application Ser. No. 507,074, filed Sept. 18, 1974 and now abandoned.
US Referenced Citations (9)
Foreign Referenced Citations (1)
Number |
Date |
Country |
47-14592 |
Jan 1972 |
JPX |
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
507074 |
Sep 1974 |
|