Claims
- 1. In a method for fusion bonding at least two articles composed of high melting point thermoplastic including the steps of bringing a fusable surface portion of each article to be bonded into engagement with a contact surface portion of a heated platen until each said fusable surface portion is fused, and thereafter bringing the fused surfaces together in face-to-face relationship, said method being characterized in that:
- (a) each said contact surface portion of said platen is heated to a temperature substantially greater than the fusion temperature of the thermoplastic article and in the range of from 650.degree. F. to 1000.degree. F.;
- (b) said fusable surface portions are simultaneously held in engagement with the contact surface portions until the fusable surface portions become fused;
- (c) the fusable surface portions, once fused, are rapidly transferred into surface-to-surface contact with each other, and maintained in surface-to-surface contact until the fused surface portions become substantially solifified; and
- (d) the contact surface portions of the heating platen are abraded to renew and expose said contact surfaces for engagement with fusable surface portions of each of a subsequent plurality of thermoplastic articles to be treated.
- 2. The method as defined in claim 1 being particularly characterized in that said abrading operation is undertaken with at least one wire bristle brush.
- 3. The method as defined in claim 1 being particularly characterized in that said thermoplastic articles are selected from the group consisting of nylon and fluorinated hydrocarbons.
- 4. The method as defined in claim 1 being particularly characterized in that the transfer time for articles with fused surfaces between the point of contact with the platen and the point of contact with each other is less than about two seconds.
- 5. The method as defined in claim 1 being particularly characterized in that said thermoplastic articles are nylon reinforced with glass fibers.
- 6. The method as defined in claim 5 being particularly characterized in that said glass fiber reinforcement comprises from between 10% and 33% of each nylon-glass reinforcement article.
- 7. The method as defined in claim 1 being particularly characterized in that the time of engagement between the heated platen and the thermoplastic articles is about fifteen seconds.
- 8. The method as defined in claim 1 being particularly characterized in that the surface temperature of the heated platen is approximately 300.degree. F. greater than the melting point of the thermoplastic.
Parent Case Info
This is a continuation of application Ser. No. 06/794,472, filed Nov. 4, 1985 now abandoned.
US Referenced Citations (4)
Non-Patent Literature Citations (1)
Entry |
Richardson, "Nylon", Modern Plastics Enc., pp. 36, 41-42, 1977-1978. |
Continuations (1)
|
Number |
Date |
Country |
Parent |
794472 |
Nov 1985 |
|