Claims
- 1. Method for joining together edge surfaces of polytetrafluoroethylene material by a butt joint, which comprises the steps of:
- (a) placing the polytetrafluoroethylene edge surfaces to be joined in abutting relationship;
- (b) clamping the polytetrafluoroethylene material by clamping means containing cooling channels on each side of the abutting surfaces except for a narrow unclamped strip along the abutting surfaces;
- (c) pressing-together the abutting surfaces;
- (d) applying heat selected solely from the group consisting of radiant heat or convection heat to the narrow unclamped strip by heating means maintained out of direct contact with said strip;
- (e) heating the abutting surfaces of said strip to a temperature above 327.degree. C.;
- (f) applying a cooling media to the cooling channels to cause a controlled temperature distribution in the strip to avoid buckling of the strip;
- (g) continuing said heating and cooling to produce a thickening of the seam formed between said abutting surfaces; and
- (h) cooling the resultant butt joint and removing surface notches by machining off said thickening.
- 2. Method according to claim 1, wherein said heat is radiant heat.
- 3. Method according to claim 1, wherein said heat is convection heat.
- 4. Method according to claim 1, wherein the abutting surfaces are heated to a temperature between 340.degree. and 430.degree. C.
- 5. Method according to claim 1, wherein the abutting surfaces are pressed against each other with pressures between 60 and 300 N/cm.sup.2.
- 6. Method according to claim 1, wherein the temperature and the pressure in the butt joint are maintained for 10 to 120 minutes.
- 7. Method according to claim 1, wherein the width of the heated strip is 0.2 to 3 times the thickness of the polytetrafluoroethylene material.
- 8. Method according to claim 7, wherein the width of the heated strip is 0.8 to 1.2 times the thickness of the polytetrafluoroethylene.
- 9. Method according to claim 1, wherein the polytetrafluoroethylene material has a thickness of 1 to 10 mm.
- 10. Method according to claim 1, wherein a thin foil of a fluorine-containing thermoplastic is inserted between the abutting surfaces.
- 11. Method according to claim 10, wherein said thin foil is a foil of tetrafluoroethylene-hexafluoropropylene copolymerisate.
- 12. Method according to claim 10, wherein said foil is a foil of a copolymer of tetrafluoroethylene and perfluoroalkylperfluorovinyl ether.
- 13. Method according to claim 10, wherein the abutting surfaces are pressed against each other with a pressure of 2 to 100 N/cm.sup.2.
- 14. Method according to claim 13 wherein the temperature and the pressure in the butt joint are maintained for 1 to 10 minutes.
Priority Claims (1)
Number |
Date |
Country |
Kind |
2549475 |
Nov 1975 |
DEX |
|
CROSS REFERENCE TO RELATED APPLICATION
This is a continuation of application Ser. No. 733,081, filed Oct. 18, 1976, now abandoned.
US Referenced Citations (6)
Foreign Referenced Citations (1)
Number |
Date |
Country |
2163420 |
Jul 1973 |
FRX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
733081 |
Oct 1976 |
|