1. Field of the Invention
The present invention relates to a panel module; and more particularly to a method for maintaining vacuum-tight of a panel module.
2. Description of the Related Art
Panel modules have become a crucial element of a display. The vacuum inside the panel module is highly required and important, which decays performance of components inside the panel module. During the manufacturing process of the panel module, after exhausting inside of the panel module and completing aging process, an exhaust tube connected to the panel module is burnt out and sealed by hydrogen-oxygen torch to maintain vacuum inside the panel module and also assure normal functions of the components inside the panel module. However, because the pressure inside the panel module is smaller than the pressure outside the panel module during an annealing process to use the hydrogen-oxygen torch to heat and seal the exhaust tube, ambient air will flow into the panel module to decrease the vacuum inside the panel module. The performance and functions of the components inside the panel module thus decay.
However, during the annealing process to use the hydrogen-oxygen torch to heat the glass tube 40 to gradually shrink one end of the glass tube 40, ambient air will flow into the panel module and the vacuum inside the panel module deteriorates. The quality and performance of the components inside the panel module are adversely affected. Accordingly, a method for effectively maintaining the vacuum inside the panel module is desired.
One objective of the present invention is to provide a method for maintaining vacuum-tight of a panel module, by which a sealing material is suspended within the panel module right above an exhaust opening of a substrate of the panel module, when the air inside the panel module is exhausted to attain a predetermined vacuum, the sealing material is heated and molten to drop down to seal an exhaust tube connected to the exhaust opening, and during a subsequent annealing process for burning out the exhaust tube, ambient air is prohibited from flowing into the inside of the panel module such that the panel module becomes vacuum-tight.
For achieving the above objective, the present invention provides a method for maintaining vacuum-tight of a panel module, which comprises providing a panel module at least including a first substrate, a second substrate and a side frame, the side frame disposed between the first substrate and the second substrate, and the second substrate having an exhaust opening; suspending a sealing material within the panel module such that the sealing material is placed right above the exhaust opening; connecting an exhaust tube to the exhaust opening of the second substrate; exhausting inside of the panel module via the exhaust tube so that the inside of the panel module attains a predetermined vacuum; heating the sealing material such that the sealing material is molten, and dropping down to seal the exhaust tube, thereby the inside of the panel module becomes sealing-tight; and burning out the exhaust tube.
In one another aspect, the present invention provides a high vacuum panel module including a first substrate, a second substrate having an exhaust opening, a side frame disposed between the first substrate and the second substrate, an exhaust tube connected to the exhaust opening, and a sealing material sealing the exhaust tube. By the sealing material sealing the exhaust tube, the inside of the panel module becomes vacuum-tight so as to prohibit ambient air from flowing into the inside of the panel module during a subsequent annealing process for burning out the exhaust tube.
It is preferable that the sealing material is an inorganic material.
It is preferable that the sealing material is heated by high frequency waves to be molten and then drop down to seal the exhaust tube.
It is preferable that the sealing material has a melting point in a range of 420° C. to 450° C.
It is preferable that the sealing material is suspended by a conductive member.
The present invention suspends the sealing material inside the panel module right above the exhaust opening. After exhausting the inside of the panel module, the sealing material is heated and molten to drop down to seal an exhaust tube connected to the exhaust opening. As such, the inside of the panel module becomes sealing-tight. The present method is simple and easy to accomplish, which can resolve the problem of flow back of ambient air during an annealing process subsequent to exhausting the air inside the panel module. The present invention improves manufacturing yield of the panel modules.
The present invention provides a method for maintaining vacuum-tight inside a panel module, which suspends a sealing material within the panel module right above an exhaust opening of a substrate. When the inside of the panel module is exhausted to attain a predetermined vacuum, the sealing material is heated and molten to drop down to seal an exhaust tube connecting to the exhaust opening so as to prohibit ambient air from flowing into the panel module. Once the sealing material is hardened, the rest of the exhaust tube is burnt out, and a finished product of the panel module with vacuum-tight is provided.
The present method for maintaining vacuum-tight inside the panel module will be described in detail according to following embodiments with reference to accompanying drawings.
Referring to
A conductive member 21 serving as a suspending element is disposed right above the exhaust opening 21 within the panel module 1. The conductive member 21 has excellent thermal conductivity. The conductive member 21 is used to suspend a sealing material 2 right above the exhaust opening 10c. The sealing material 2 preferably is an inorganic compound with a melting point in a range of 420° C. to 450° C., such as a glass-powder pill. It should be noted that the projection of the sealing material 2 upon the cross-sectional area of the exhaust tube 40 is at least larger than the smallest cross-sectional area of the exhaust tube 40 so as to assure that the sealing material 2 can seal the exhaust tube 40 when the sealing material 2 drops down.
Next, referring to
Finally, the exhaust tube 40b is burnt out by hydrogen-oxygen torch. The panel module 1 with required vacuum-tight is accomplished, as shown in
Referring to
Finally, the exhaust tube 40b is burnt out by hydrogen-oxygen torch. The panel module 1′ with required vacuum-tight is accomplished, as shown in
While the invention has been described by way of examples and in terms of preferred embodiments, it is to be understood that those who are familiar with the subject art can carry out various modifications and similar arrangements and procedures described in the present invention and also achieve the effectiveness of the present invention. Hence, it is to be understood that the description of the present invention should be accorded with the broadest interpretation to those who are familiar with the subject art, and the invention is not limited thereto.
Number | Date | Country | Kind |
---|---|---|---|
95108097 | Mar 2006 | TW | national |