The present disclosure relates to the field of electronic technologies, and in particular to a method for making a cover plate, a cover plate, and an electronic device.
Optical components inside electronic devices may be configured to detect environmental parameters or human body parameters. For example, the health functions of a smart watch include a blood oxygen detection function. The current mainstream blood oxygen detection method is photoplethysmography (PPG). The operating principle of PPG is as follows. Light rays emitted by a light emitter enter the outside world through a transparent area of a housing of a smart watch, and then pass through tissues and arterial veins in a skin. A part of the light rays is absorbed and another part of the light rays is reflected back to a light sensor. Light signals received by the light sensor are converted into electrical signals, and blood oxygen data is obtained after conversion.
An existing structure of the PPG generally includes a housing, and the housing includes a back cover. The back cover is provided with a first optical window and a second optical window. The optical signals emitted by the light emitter may pass through the first optical window to reach the skin, and the light signals returning from the skin may pass through the second optical window to enter the light sensor. However, the light rays emitted by the light emitter and emitted into the first optical window may pass through the second optical window and then received by the light sensor. That is, the light signals emitted by the light emitter are directly received by the light sensor without being absorbed and reflected by the skin, which leads to deviations in the calculation results, thereby reducing the accuracy of the detection results.
In a first aspect, the embodiments of the present disclosure provide a method for making a cover plate. The method includes the operations:
In a second aspect, the embodiments of the present disclosure provide a method for making a cover plate. The method includes the following operations:
In a third aspect, the embodiments of the present disclosure provide a cover plate. The cover plate includes a first window area, a second window area, a first light-shielding area, a second light-shielding area, and a peripheral area.
The first window area is configured to allow light rays to pass through.
The second window area is configured to allow the light rays to pass through, wherein the first window area is spaced apart from the second window area.
The first light-shielding area is configured to shield the light rays, wherein the first light-shielding area surrounds the first window area.
The second light-shielding area is configured to shield the light rays, wherein the second light-shielding area surrounds the second window area.
The peripheral area surrounds the first light-shielding area and the second light-shielding area.
In a fourth aspect, the embodiments of the present disclosure provide an electronic device. The electronic device includes a cover plate mentioned above, a light emitter, and a light detector.
The light emitter is disposed on a side of the cover plate, and light rays emitted by the light emitter enter a first window area and are transmitted to another side of the cover plate away from the light emitter through the first window area.
The light detector and the light emitter are disposed on the same side of the cover plate, and the light rays that enter a second window area from the side of the cover plate away from the light detector pass through the second window area and enter the light detector.
In order to more clearly illustrate the technical solutions in some embodiments of the present disclosure, hereinafter, a brief introduction will be given to the accompanying drawings that are used in the description of some embodiments.
Referring to the drawings, the same reference numerals represent the same components. The principle of the present disclosure is illustrated by being implemented in a suitable environment. The following description is based on some embodiments illustrated in the present disclosure, which should not be considered as limiting other embodiments of the present disclosure that are not described in detail here.
As illustrated in
At block 110, a first light-transmitting material, a second light-transmitting material, and a light-shielding material are provided.
Each of the first light-transmitting material and the second light-transmitting material may be selected from at least one of transparent glass, transparent plastic, a transparent ceramic, and a sapphire. The transparent plastic may be polymethyl methacrylate (PMMA). In some embodiments, a light transmittance of the first light-transmitting material to light rays of 400 nm-1200 nm is greater than or equal to 20%, such as 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or 100%. A light transmittance of the second light-transmitting material to the light rays of 400 nm-1200 nm is greater than or equal to 20%, such as 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or 100%.
The first light-transmitting material and the second light-transmitting material may be the same material or different materials.
The light-shielding material may be selected from at least one of opaque glass, opaque plastic, an opaque ceramic, and a metal. The opaque plastic may be polycarbonate (PC), polyamide (PA), polyetheretherketone (PEEK), etc., and a color of the “opaque” may be black or dark. In some embodiments, a light transmittance of the light-shielding material to the light rays of 400 nm-1200 nm is less than or equal to 10%, such as 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or 0.
At block 120, the first light-transmitting material and the second light-transmitting material are disposed at intervals, and the light-shielding material is disposed on a periphery of the first light-transmitting material and a periphery of the second light-transmitting material.
As illustrated in
As illustrated in
The first light-transmitting material 111 may be a single first light-transmitting rod material, or the first light-transmitting material 111 includes a plurality of first light-transmitting fiber filaments. The second light-transmitting material 121 may be a single second light-transmitting rod material, or the second light-transmitting material 121 includes a plurality of second light-transmitting fiber filaments.
At block 130, the first light-transmitting material, the second light-transmitting material, and the light-shielding material are squeezed, to obtain the composite rod material.
As illustrated in
In some embodiments, a percentage difference between a thermal expansion coefficient (CTE) of the light-shielding material 131 and a thermal expansion coefficient of the first light-transmitting material 111 is less than or equal to 20%. The thermal expansion coefficient of the light-shielding material 131 needs to be as close as possible to the thermal expansion coefficient of the first light-transmitting material 111, which avoids or reduces a phenomenon of internal cracking of the light-shielding material 131 and/or the first light-transmitting material 111 caused by excessive CTE difference after high-temperature treating and cooling. For example, the percentage difference between the thermal expansion coefficient of the light-shielding material 131 and the thermal expansion coefficient of the first light-transmitting material 111 may be 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficient of the light-shielding material 131 and the thermal expansion coefficient of the first light-transmitting material 111 is 0, the thermal expansion coefficient of the light-shielding material 131 is equal to the thermal expansion coefficient of the first light-transmitting material 111.
In some embodiments, the percentage difference between the thermal expansion coefficient of the light-shielding material 131 and a thermal expansion coefficient of the second light-transmitting material 121 is less than or equal to 20%. The thermal expansion coefficient of the light-shielding material 131 needs to be as close as possible to the thermal expansion coefficient of the second light-transmitting material 121, which avoids or reduces the phenomenon of internal cracking of the light-shielding material 131 and/or the second light-transmitting material 121 caused by the excessive CTE difference after high-temperature treating and cooling. For example, the percentage difference between the thermal expansion coefficient of the light-shielding material 131 and the thermal expansion coefficient of the second light-transmitting material 121 may be 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficient of the light-shielding material 131 and the thermal expansion coefficient of the second light-transmitting material 121 is 0, the thermal expansion coefficient of the light-shielding material 131 is equal to the thermal expansion coefficient of the second light-transmitting material 121.
When a cross-sectional size of the composite rod material 170 that is obtained after squeezing is greater than a cross-sectional size of a target product (a cover plate), a step of pulling the composite rod material 170 may be provided after squeezing, to adjust the cross-sectional size of the composite rod material 170. And accordingly, cross-sectional sizes of a first window area 11, a second window area 12, and a light-shielding area 13 are simultaneously adjusted. Compared with the method of only squeezing, squeezing and pulling may quickly obtain the target product that meets the size requirements, thereby greatly improving the production efficiency and reducing the production cost. The bonding effect between the materials in the composite rod material 170 may be improved through pulling the composite rod material 170, so that the bonding between the materials of the composite rod material 170 is tighter.
From the perspective of improving the pulling effect, in some embodiments, a softening point temperature of the first light-transmitting material 111 is higher than or equal to a softening point temperature of the light-shielding material 131, and a softening point temperature of the second light-transmitting material 121 is higher than or equal to the softening point temperature of the light-shielding material 131. Otherwise, when the softening point temperature of the first light-transmitting material 111 or the softening point temperature of second light-transmitting material 121 is lower than the softening point temperature of the light-shielding material 131, during the process of heating the material before pulling, it is easy to occur a phenomenon that the light-shielding material 131 has not become soft and cannot be pulled, and the first light-transmitting material 111 or the second light-transmitting material 121 has been melted or softened, thereby causing inability to process. Therefore, in some embodiments, the softening point temperature of the light-shielding material 131, the softening point temperature of the first light-transmitting material 111, and the softening point temperature of the second light-transmitting material 121 are equal to each other.
When the first light-transmitting material 111, the second light-transmitting material 121, and the light-shielding material 131 are all softened in the composite rod material 170, the composite rod material 170 may be pulled. The cross-sectional size of each of the light-transmitting material 111, the second light-transmitting material 121, and the light-shielding material 131 may be simultaneously changed by pulling the composite rod material 170. When the first light-transmitting material 111 and the second light-transmitting material 121 are not softened, while the light-shielding material 131 has softened, the composite rod material 170 may also be pulled. In this case, the pulling is only for the light-shielding material 131, and only the cross-sectional size of the material 131 is changed by pulling, while the cross-sectional sizes of the first light-transmitting material 111 and the second light-transmitting material 121 are not changed.
In order to eliminate an internal stress generated during processing, and avoid or reduce the possibility of subsequent deformation and cracking of the composite rod material 170, in some embodiments, after squeezing, or squeezing and pulling, annealing the composite rod material 170 may be provided. An annealing temperature is determined according to specific properties of the material.
At block 140, the composite rod material is treated, to obtain the cover plate.
As illustrated in
As illustrated in
The first window area 11 is formed by the first light-transmitting material 111, the second window area 12 is formed by the second light-transmitting material 121, and the light-shielding area 13 is formed by the light-shielding material 131.
When the cover plate 10 is applied to an electronic device with a photoplethysmographic (PPG) structure, both the first window area 11 and the second window area 12 should allow the light rays ranging from visible light to near infrared light (wavelength ranging from 400 nm to 1200 nm) to pass through. The higher the light transmittance of each of the first window area 11 and the second window area 12, the better. The lower the light transmittance of the light-shielding area 13 to the light rays ranging from the visible light to the near infrared light, the better.
In the above method for making the first type of cover plate, the first light-transmitting material 111, the second light-transmitting material 121, and the light-shielding material 131 are combined by squeezing, or by squeezing and pulling, so that the cover plate 10 is obtained. Both the first window area 11 and the second window area 12 in the cover plate 10 are surrounded by the light-shielding area 13, which may avoid optical crosstalk between the first window area 11 and the second window area 12.
As illustrated in
At block 210, a first composite material, a second composite material, and a peripheral material are provided; the first composite material includes the first light-transmitting material and a first light-shielding material surrounding the first light-transmitting material, and the second composite material includes the second light-transmitting material and a second light-shielding material surrounding the second light-transmitting material.
Each of the first light-transmitting material and the second light-transmitting material may be selected from at least one of the transparent glass, the transparent plastic (such as PMMA), the transparent ceramic, and the sapphire. The light transmittance of the first light-transmitting material to the light rays of 400 nm-1200 nm is greater than or equal to 20%, such as 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or 100%. The light transmittance of the second light-transmitting material to the light rays of 400 nm-1200 nm is greater than or equal to 20%, such as 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or 100%.
Each of the first light-shielding material and the second light-shielding material may be selected from at least one of the opaque glass, the opaque plastic, the opaque ceramics, and the metal. The opaque plastic may be PC, PA, PEEK, etc., and the color of “opaque” may be black or dark. Both the first light-shielding material and the second light-shielding material may be black glass material. The black glass material may be an ordinary black glass material that is obtained by adding color powders to the transparent glass, or may be a black glass ceramic.
The light transmittance of the first light-shielding material to the light rays of 400 nm-1200 nm is less than or equal to 10%, such as 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or 0. The light transmittance of the second light-shielding material to the light rays of 400 nm-1200 nm is less than or equal to 10%, such as 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or 0.
The first light-transmitting material and the second light-transmitting material may be the same material or different materials. The first light-shielding material and the second light-shielding material may be the same material or different materials.
The peripheral material may be the glass, the plastic, the ceramic, the metal, etc., and a color of the peripheral material may be transparent, dark, or black.
At block 220, the first composite material and the second composite material are disposed at intervals, and the peripheral material is disposed on a periphery of the first composite material and a periphery of the second composite material.
As illustrated in
As illustrated in
The first composite material 181 may include a first composite rod body formed by combining the first light-transmitting material 111 and a first light-shielding material 141. In this case, providing the first composite material 181 may include the following operations:
By combining the first light-transmitting material 111 and the first light-shielding material 141 to form the first composite rod body, subsequently squeezing the first composite material 181 and the peripheral material 161 may improve the bonding effect between the first light-transmitting material 111, the first light-shielding material 141, and the peripheral material 161, thereby improving the production yield.
As illustrated in
As illustrated in
The first light-shielding material 141 may be deformed under the action of the external force and at the room temperature. For example, when the first light-shielding material 141 is the metal or the plastic that has plasticity at the room temperature, the first light-transmitting material 111 and the first light-shielding material 141 may be combined by only squeezing without heating. Of course, the first light-transmitting material 111 and the first light-shielding material 141 may also be heated to improve the plasticity of the material. The first light-shielding material 141 may be non-deformable at the room temperature. For example, when the first light-shielding material 141 is the glass or the plastic that does not have plasticity at the room temperature, it is necessary to heat the first light-shielding material 141 to soften the first light-shielding material 141. And then the first light-shielding material 111 and the first light-shielding material 141 may be combined by squeezing. In this case, squeezing the first light-transmitting material 111 and the first light-shielding material 141 to obtain the first composite rod body may include: after heating the first light-transmitting material 111 and the first light-shielding material 141, squeezing the first light-transmitting material 111 and the first light-shielding material 141, to obtain the first composite rod body. Before squeezing, the first light-transmitting material 111 may or may not have plasticity.
In some embodiments, a percentage difference between the thermal expansion coefficient of the first light-transmitting material 111 and a thermal expansion coefficient of the first light-shielding material 141 is less than or equal to 20%. A definition of “percentage difference” is: if A is greater than or equal to B, a percentage difference between A and B=(A−B)/B. All “percentage difference” recited in the present disclosure adopts this definition. The thermal expansion coefficient of the light-shielding material 131 needs to be as close as possible to the thermal expansion coefficient of the first light-shielding material 141, which avoids or reduces the phenomenon of internal cracking of the first light-transmitting material 111 and/or the first light-shielding material 141 caused by the excessive CTE difference after the high-temperature treating and cooling. In some embodiments, the percentage difference between the thermal expansion coefficient of the first light-transmitting material 111 and the thermal expansion coefficient of the first light-shielding material 141 may be 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficient of the first light-transmitting material 111 and the thermal expansion coefficient of the first light-shielding material 141 is 0, the thermal expansion coefficient of the first light-transmitting material 111 is equal to the thermal expansion coefficient of the first light-shielding material 141.
When a cross-sectional size and a length of the first composite rod body need to be changed, a step of pulling the first composite rod body may be provided after squeezing. From the perspective of improving the pulling effect, in some embodiments, the softening point temperature of the first light-transmitting material 111 is higher than or equal to a softening point temperature of the first light-shielding material 141. Otherwise, when the softening point temperature of the first light-transmitting material 111 is lower than the softening point of the first light-shielding material 141, during the process of heating the material before pulling, it is easy to occur a phenomenon that the first light-shielding material 141 has not become soft and cannot be pulled, and the first light-transmitting material 111 has been melted or softened, thereby causing inability to process. In some embodiments, the softening point temperature of the first light-shielding material 141 is equal to the softening point temperature of the first light-transmitting material 111.
When both the first light-transmitting material 111 and the first light-shielding material 141 are softened in the first composite rod body, the first composite rod body may be pulled. The cross-sectional sizes of the first light-transmitting material 111 and the first light-shielding material 141 may be simultaneously changed by pulling the first composite rod body. When the first light-transmitting material 111 is not softened, while the first light-shielding material 141 has been softened, the first composite rod body may also be pulled. In this case, the pulling is only for the first light-shielding material 141, and only the cross-sectional size of the first light-shielding material 141 is changed by pulling, while the cross-sectional size of the first light-transmitting material 111 is not changed.
In order to eliminate the internal stress generated during processing, and avoid or reduce the possibility of subsequent deformation and cracking of the first composite rod body, in some embodiments, after squeezing, or after squeezing and pulling, annealing the first composite rod body may be provided. An annealing temperature is determined according to the specific properties of the material.
The second composite material 182 may include a second composite rod body formed by combining the second light-transmitting material 121 and a second light-shielding material 151. In this case, providing the second composite material 182 may include the following operations:
By combining the second light-transmitting material 121 and the second light-shielding material 151 to form the second composite rod body, subsequently squeezing the second composite material 182 and the peripheral material 161 may improve the bonding effect between the second light-transmitting material 121, the second light-shielding material 151, and the peripheral material 161, thereby improving the production yield.
As illustrated in
As illustrated in
The second light-shielding material 151 may be deformed under the action of the external force and at the room temperature. For example, when the second light-shielding material 151 is the metal or the plastic that has plasticity at the room temperature, the second light-transmitting material 121 and the second light-shielding material 151 may be combined by only squeezing without heating. Of course, the second light-transmitting material 121 and the second light-shielding material 151 may also be heated to improve the plasticity of the material. The second light-shielding material 151 may be non-deformable at the room temperature. For example, when the second light-shielding material 151 is the glass or the plastic that does not have the plasticity at the room temperature, it is necessary to heat the second light-shielding material 151 to soften the second light-shielding material 151. And then the second light-shielding material 121 and the second light-shielding material 151 may be combined by squeezing. In this case, squeezing the second light-transmitting material 121 and the second light-shielding material 151 to obtain the second composite rod body, may include: after heating the second light-transmitting material 121 and the second light-shielding material 151, squeezing the second light-transmitting material 121 and the second light-shielding material 151, to obtain the second composite rod body. Before squeezing, the second light-transmitting material 121 may or may not have plasticity.
In some embodiments, a percentage difference between the thermal expansion coefficient of the second light-transmitting material 121 and a thermal expansion coefficient of the second light-shielding material 151 is less than or equal to 20%. The thermal expansion coefficient of the second light-transmitting material 121 needs to be as close as possible to the thermal expansion coefficient of the second light-shielding material 151, which avoids or reduces the phenomenon of internal cracking of the second light-transmitting material 121 and/or the second light-shielding material 151 caused by the excessive CTE difference after the high-temperature treating and cooling. In some embodiments, the percentage difference between the thermal expansion coefficient of the second light-transmitting material 121 and the thermal expansion coefficient of the second light-shielding material 151 may be 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficient of the second light-transmitting material 121 and the thermal expansion coefficient of the second light-shielding material 151 is 0, the thermal expansion coefficient of the second light-transmitting material 121 is equal to the thermal expansion coefficient of the second light-shielding material 151.
When a cross-sectional size and a length of the second composite rod body need to be changed, a step of pulling the second composite rod body may be provided after squeezing. From the perspective of improving the pulling effect, in some embodiments, the softening point temperature of the second light-transmitting material 121 is higher than or equal to a softening point temperature of the second light-shielding material 151. Otherwise, when the softening point temperature of the second light-transmitting material 121 is lower than the softening point of the second light-shielding material 151, during the process of heating the material before pulling, it is easy to occur a phenomenon that the second light-shielding material 151 has not become soft and cannot be pulled, while the second light-transmitting material 121 has been melted or softened, thereby causing inability to process. In some embodiments, the softening point temperature of the second light-shielding material 151 is equal to the softening point temperature of the second light-transmitting material 121.
When both the second light-transmitting material 121 and the second light-shielding material 151 are softened in the second composite rod body, the second composite rod body may be pulled. The cross-sectional sizes of the second light-transmitting material 121 and the second light-shielding material 151 may be simultaneously changed by pulling the second composite rod body. When the second light-transmitting material 121 is not softened, while the second light-shielding material 151 has been softened, the second composite rod body may also be pulled. In this case, the pulling is only for the second light-shielding material 151, and only the cross-sectional size of the second light-shielding material 151 may be changed by pulling, while the cross-sectional size of the second light-transmitting material 121 is not changed.
In order to eliminate the internal stress generated during processing, and avoid or reduce the possibility of subsequent deformation and cracking of the second composite rod body, in some embodiments, after squeezing, or after squeezing and pulling, annealing the second composite rod body may be provided. An annealing temperature is determined according to the specific properties of the material.
As illustrated in
As illustrated in
The first light-transmitting material 111 may be the single first light-transmitting rod material, or the first light-transmitting material 111 includes the plurality of first light-transmitting fiber filaments. The second light-transmitting material 121 may be the single second light-transmitting rod material, or the second light-transmitting material 121 includes the plurality of second light-transmitting fiber filaments.
At block 230, the first composite material, the second composite material, and the peripheral material are squeezed, to obtain the composite rod material.
As illustrated in
In some embodiments, in the first light-transmitting material 111, the first light-shielding material 141, and the peripheral material 161, a percentage difference between thermal expansion coefficients of any two is less than or equal to 20%. A thermal expansion coefficient of the peripheral material 161 needs to be as close as possible to the thermal expansion coefficient of the first light-transmitting material 111 and the thermal expansion coefficient of the first light-shielding material 141, which avoids or reduces the phenomenon of internal cracking of the first light-transmitting material 111 and/or the first light-shielding material 141 and/or the peripheral material 161 caused by the excessive CTE difference after the high-temperature treating and cooling. In some embodiments, in the first light-transmitting material 111, the first light-shielding material 141, and the peripheral material 161, the percentage difference between the thermal expansion coefficients of any two may be 20%, 15%, 10%, 5%, 4%, or 3%. %, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficients of any two of the first light-transmitting material 111, the first light-shielding material 141, and the peripheral material 161 is 0, the thermal expansion coefficient of the first light-transmitting material 111, the thermal expansion coefficient of the first light-shielding material 141, and the thermal expansion coefficient of the peripheral material 161 are equal to each other.
In some embodiments, in the second light-transmitting material 121, the second light-shielding material 151, and the peripheral material 161, a percentage difference between the thermal expansion coefficients of any two is less than or equal to 20%. The thermal expansion coefficient of the peripheral material 161 needs to be as close as possible to the thermal expansion coefficient of the second light-transmitting material 121 and the thermal expansion coefficient of the second light-shielding material 151, which avoids or reduces the phenomenon of internal cracking of the second light-transmitting material 121 and/or the second light-shielding material 151 and/or the peripheral material 161 caused by the excessive CTE difference after the high-temperature treating and cooling. In some embodiments, in the second light-transmitting material 121, the second light-shielding material 151, and the peripheral material 161, the percentage difference between the thermal expansion coefficients of any two may be 20%, 15%, 10%, 5%, 4%, or 3%. %, 2%, 1%, or 0. When the percentage difference between the thermal expansion coefficients of any two of the second light-transmitting material 121, the second light-shielding material 151, and the peripheral material 161 is 0, the thermal expansion coefficient of the second light-transmitting material 121, the thermal expansion coefficient of the second light-shielding material 151, and the thermal expansion coefficient of the peripheral material 161 are equal to each other.
In some embodiments, a difference between the thermal expansion coefficient of the first light-transmitting material 111 and the thermal expansion coefficient of the peripheral material 161 is defined as a first difference. A difference between the thermal expansion coefficient of the first light-transmitting material 111 and the thermal expansion coefficient of the first light-shielding material 141 is defined as a second difference. An absolute value of the first difference is less than or equal to an absolute value of the second difference. Since an area formed by the peripheral material 161 is a non-working area, there is no requirement for the light transmittance, the selection range of the peripheral material 161 is relatively wide. By selecting the peripheral material 161 with the thermal expansion coefficient closer to that of the first light-transmitting material 111, the phenomenon of the internal cracking of the first light-transmitting material 111 caused by excessive CTE difference after the high-temperature treating and cooling may be avoided or reduced.
In some embodiments, a difference between the thermal expansion coefficient of the second light-transmitting material 121 and the thermal expansion coefficient of the peripheral material 161 is defined as a third difference. A difference between the thermal expansion coefficient of the second light-transmitting material 121 and the second light-shielding material 151 is defined as a fourth difference. An absolute value of the third difference is less than or equal to an absolute value of the fourth difference. By selecting the peripheral material 161 with the thermal expansion coefficient closer to that of the second light-transmitting material 121, the phenomenon of the internal cracking of the second light-transmitting material 121 caused by excessive CTE difference after the high-temperature treating and cooling may be avoided or reduced.
In some embodiments, the first light-transmitting material 111, the second light-transmitting material 121, and the peripheral material 161 are the same material. That is, the first light-transmitting material 111, the second light-transmitting material 121, and the peripheral material 161 are all light-transmitting materials. In this way, the thermal expansion coefficients of the first light-transmitting material 111, the second light-transmitting material 121, and the peripheral material 161 are equal to each other. After squeezing and cooling, the first light-transmitting material 111 and the second light-transmitting material 121 are not easy to crack.
When the cross-sectional size of the composite rod material 170 that is obtained after squeezing is greater than the cross-sectional size of the target product (the cover plate), the step of pulling the composite rod material 170 may be provided after squeezing, to adjust the cross-sectional size of the composite rod material 170. And accordingly, the cross-sectional sizes of the first window area 11, the second window area 12, and the light-shielding area 13 are simultaneously adjusted. Compared with the method of only squeezing, squeezing and pulling may quickly obtain the target product that meets the size requirements, thereby greatly improving the production efficiency and reducing the production cost. The bonding effect between the materials in the composite rod material 170 may be improved through pulling the composite rod material 170, so that the bonding between the materials of the composite rod material 170 is tighter.
From the perspective of improving the pulling effect, in some embodiments, the softening point temperature of the first light-transmitting material 111 is higher than or equal to the softening point temperature of the first light-shielding material 141, and the softening point temperature of the first light-shielding material 141 is higher than or equal to a softening point temperature of the peripheral material 161. Otherwise, when the softening point temperature of the first light-shielding material 141 is lower than the softening point temperature of the peripheral material 161, during the process of heating the material before pulling, it is easy to occur a phenomenon that the peripheral material 161 has not become soft and cannot be pulled, while the first light-shielding material 141 has been melted or softened, thereby causing inability to process. When the softening point temperature of the first light-transmitting material 111 is lower than the softening point temperature of the first light-shielding material 141, during the process of heating the material before pulling, it is easy to occur the phenomenon that the first light-shielding material 141 that is located on the periphery has not become soft, while the first light-transmitting material 111 that is located inside has been melted or softened, thereby causing inability to process. In some embodiments, the softening point temperature of the first light-transmitting material 111, the softening point temperature of the first light-shielding material 141, and the softening point temperature of the peripheral material 161 are equal to each other.
From the perspective of improving the pulling effect, in some embodiments, the softening point temperature of the second light-transmitting material 121 is higher than or equal to the softening point temperature of the second light-shielding material 151, and the softening point temperature of the second light-shielding material 151 is higher than or equal to the softening point temperature of the peripheral material 161. Otherwise, when the softening point temperature of the second light-shielding material 151 is lower than the softening point temperature of the peripheral material 161, during the process of heating the material before pulling, it is easy to occur a phenomenon that the peripheral material 161 has not become soft and cannot be pulled, while the second light-shielding material 151 has been melted or softened, thereby causing inability to process. When the softening point temperature of the second light-transmitting material 121 is lower than the softening point temperature of the second light-shielding material 151, during the process of heating the material before pulling, it is easy to occur the phenomenon that the second light-shielding material 151 that is located on the periphery has not become soft and cannot be pulled, while the second light-transmitting material 121 that is located inside has been melted or softened, thereby causing inability to process. In some embodiments, the softening point temperature of the second light-transmitting material 121, the softening point temperature of the second light-shielding material 151, and the softening point temperature of the peripheral material 161 are equal to each other.
When the first light-transmitting material 111, the second light-transmitting material 121, the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161 are all softened in the composite rod material 170, the composite rod material 170 may be pulled. The cross-sectional size of each of the first light-transmitting material 111, the second light-transmitting material 121, the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161 may be simultaneously changed by pulling the composite rod material 170. When the first light-transmitting material 111 and the second light-transmitting material 121 are not softened, while the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161 have been softened, the composite rod material 170 may also be pulled. In this case, the pulling is only for the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161.
The cross-sectional sizes of the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161 are changed by pulling, while the cross-sectional sizes of the first light-transmitting material 111 and the second light-transmitting material 121 are not changed. When the first light-transmitting material 111, the second light-transmitting material 121, the first light-shielding material 141, and the second light-shielding material 151 are not softened, while the peripheral material 161 has been softened, the composite rod material 170 may also be pulled. In this case, the pulling is only for the peripheral material 161, and only the cross-sectional size of the peripheral material 161 is changed, while the cross-sectional sizes of the first light-transmitting material 111, the second light-transmitting material 121, the first light-shielding material 141, and the second light-shielding material 151 are not changed.
In order to eliminate the internal stress generated during processing, and avoid or reduce the possibility of subsequent deformation and cracking of the composite rod material 170, in some embodiments, after squeezing, or after squeezing and pulling, annealing the composite rod material 170 may be provided. The annealing temperature is determined according to the specific properties of the material.
At block 240, the composite rod material is treated, to obtain the cover plate.
As illustrated in
As illustrated in
In the above method for making the second type of cover plate, the first light-transmitting material 111, the second light-transmitting material 121, the first light-shielding material 141, the second light-shielding material 151, and the peripheral material 161 are combined by squeezing or by squeezing and pulling, so that the cover plate 10 is obtained. In the cover plate 10, the first light-shielding area 14 is disposed on a periphery of the first window area 11, and the second light-shielding area 15 is disposed on a periphery of the second window area 12, which may avoid the optical crosstalk between the first window area 11 and the second window area 12.
In some embodiments of the present disclosure, the cover plate is provided. As illustrated in
In some embodiments, a difference between a thermal expansion coefficient of a material of the first window area 11 and a thermal expansion coefficient of a material of the peripheral area 16 is defined as the first difference. A difference between the thermal expansion coefficient of the material of the first window area 11 and a thermal expansion coefficient of a material of the first light-shielding area 14 is defined as a second difference. The absolute value of the first difference is less than or equal to the absolute value of the second difference. The cover plate 10 is prepared according to the method for making the cover plate that is shown in
In some embodiments, a difference between a thermal expansion coefficient of a material of the second window area 12 and the thermal expansion coefficient of the material of the peripheral area 16 is defined as the third difference. A difference between the thermal expansion coefficient of the material of the second window area 12 and a thermal expansion coefficient of a material of the second light-shielding area 15 is defined as the fourth difference. The absolute value of the third difference is less than or equal to the absolute value of the fourth difference. The cover plate 10 is prepared according to the method for making the cover plate that is shown in
The material of the peripheral area 16 may be a light-transmitting material or an opaque material. In some embodiments, a light transmittance of the light-transmitting material to the light rays of 400 nm-1200 nm is greater than or equal to 20%, such as 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or 100%. A light transmittance of the opaque material to the light rays of 400 nm-1200 nm is less than or equal to 10%, such as 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or 0. The peripheral area 16 is the non-working area, and there is no requirement for the light transmittance. Thus, a light transparency and a color of the peripheral area 16 may be adjusted according to specific requirements, so as to increase the richness of the appearance of the cover plate 10 and enhance the visual expression of the cover plate 10, thereby enhancing the visual expression and market competitiveness of the electronic device including the cover plate 10.
In some embodiments, the material of the first window area 11, the material of the second window area 12, and the material of the peripheral area 16 are the same material. That is, the material of the first window area 11, the material of the second window area 12, and the material of the peripheral area 16 are the light-transmitting materials. In this case, a proportion of the light-transmitting material in the cover plate 10 shown in
In some embodiments, each of the material of the first window area 11, the material of the second window area 12, and the material of the peripheral area 16 is a colorless transparent glass material. Each of the material of the first light-shielding area 14 and the material of the second light-shielding area 15 is the black glass material.
When the prepared cover plate 10 is applied to the electronic device with the PPG structure, both the first window area 11 and the second window area 12 should allow the light rays ranging from the visible light to the near infrared light (wavelength ranging from 400 nm to 1200 nm) to pass through. The higher the light transmittance of each of the first window area 11 and the second window area 12, the better. The lower the light transmittance of each of the first light-shielding area 14 and the second light-shielding area 15 to the light rays ranging from the visible light to the near-infrared light, the better.
The number of the first window area 11 provided on the cover plate 10 may be one or more, and the number of the second window area 12 provided on the cover plate 10 may be one or more.
The first light-shielding area 14 and the second light-shielding area 15 may be disposed at intervals or connected to each other.
In the cover plate 10 provided by the embodiments of the present disclosure, the first light-shielding area 14 is disposed on the periphery of the first window area 11, and the second light-shielding area 15 is disposed on the periphery of the second window area 12, which may avoid optical crosstalk between the first window area 11 and the second window area 12.
In some embodiments of the present disclosure, an electronic device is provided. The electronic device may be a wearable device, such as a watch, a bracelet, a ring, an arm cover, clothing, etc. In some embodiments, the electronic device has a health monitoring function. The health monitoring function includes, but not limited to, a blood oxygen monitoring function, a heart rate monitoring function, etc. In some embodiments, the health monitoring function of the electronic device is realized by photoplethysmography (PPG). The following electronic device being a smart watch with health monitoring function is taken as an example for illustration.
As illustrated in
The operating principle of the electronic device 100 is as follows. The light rays emitted by the light emitter 20 pass through the first window area 11 of the cover plate 10 and enter the skin. A part of the light rays is absorbed, another part of the light rays is reflected. The reflected light rays pass through the second window area 12 of the cover plate 10 to enter the light detector 30. Light signals received by the light detector 30 may be converted, to obtain relevant physiological information of the human body, such as the blood oxygen data, etc.
As illustrated in
The electronic device 100 provided by the embodiments of the present disclosure adopts the above cover plate 10, which may avoid the light rays emitted by the light emitter 20 to pass through the second window area 12 from the first window area 11 without entering the skin, and then to be received by the optical detector 30. And accordingly, errors in the optical signals received by optical detector 30 may be avoided, thereby improving signal-to-noise ratios of the optical signals received by optical detector 30, and improving the accuracy of detection results.
The method for making the cover plate, the cover plate, and the electronic device provided in the embodiments of the present disclosure are described in detail above. In the present disclosure, some or embodiments or examples are used to illustrate the principles and implementation methods of the present disclosure. The descriptions of the above embodiments are only used to help understand the present disclosure. Furthermore, for those of ordinary skill in the art, based on the idea of the present disclosure, there will be changes in the specific implementation and application scope. In summary, the contents of the present specification should not be construed as limiting the disclosure.
Number | Date | Country | Kind |
---|---|---|---|
202110610012.6 | Jun 2021 | CN | national |
The present application is a continuation of International Patent Application No. PCT/CN2022/093619, filed May 18, 2022, which claims priority to Chinese Patent Application No. 202110610012.6, filed Jun. 1, 2021, both of which are herein incorporated by reference in their entirety.
Number | Date | Country | |
---|---|---|---|
Parent | PCT/CN2022/093619 | May 2022 | US |
Child | 18516548 | US |