Claims
- 1. A method of making a face mask, comprising the steps of:providing a plurality of lengths of Grade 2, commercially pure titanium wire, having a diameter of from about 0.21 to about 0.24 inches; forming each length at room temperature to a desired bend angle by bending the length at room temperature using rotary bending apparatus to a first bend angle that is from about 1.25 to about 1.35 times greater than the desired bend angle; welding each of the thus formed lengths to at least one other of the lengths in an ambient, oxygen containing environment, wherein the face mask complies with the Standard Method of impact and Performance Requirements of the National Operating Committee on Standards for Athletic Equipment (Jul. 14, 1987, revised Jul. 10, 1990).
- 2. The method of claim 1, wherein the step of providing a plurality of lengths of Grade 2, commercially pure titanium wire, having a diameter of from about 0.21 to about 0.24 inches comprises providing lengths of titanium wire in an amount such that each length has a length of from about 6 to about 20 inches and the combined weight of all of the lengths is less than about 10 ounces.
- 3. The method of claim 1, further comprising the step of forming additional desired bends in end portions of one or more of the lengths, wherein each additional bend has a second desired bend angle and bending is accomplished by bending the end portions of the lengths at room temperature using press brake bending apparatus to a second bend angle that is from about 1.05 to about 1.15 times greater than the second desired bend angle.
- 4. The method of claim 1, wherein the step of welding comprises welding using a press-type projection welder in the presence of air.
- 5. A method of claim 1, further comprising the steps of coating the face mask with a vinyl compound.
- 6. A method of making a face mask, comprising the steps of:providing a plurality of titanium wire members; positioning the wire members in a desired configuration; and interconnecting the wire members to one another by welding using resistance spot welds formed in an ambient, oxygen containing environment, wherein the face mask complies with the Standard Method of impact and Performance Requirements of the National Operating Committee on Standards for Athletic Equipment (Jul. 14, 1987, revised Jul. 10, 1990).
CROSS-REFERENCE TO RELATED APPLICATION
This is a divisional application of U.S. application Ser. No. 09/514,624, filed Feb. 28, 2000 (Abandoned). This application is also related to U.S. application Ser. No. 09/911,749, filed Jul. 23, 2001 (now U.S. Pat. No. 6,421,829), which is a continuation of U.S. application Ser. No. 09/514,624, filed Feb. 28, 2000 (Abandoned).
US Referenced Citations (16)
Foreign Referenced Citations (2)
Number |
Date |
Country |
0084649 |
Aug 1983 |
EP |
358151973 |
Sep 1983 |
JP |
Non-Patent Literature Citations (1)
Entry |
Titanum Industries, Inc. Data and Reference Manual Mar. 1998. |