The present invention concerns an aircraft part, such as a turbine blade or a distributor fin, as well as a method for manufacturing such a part.
It is desirable to reduce the fuel consumption of aircraft turbomachines. For this purpose, it is known that it is necessary to increase the gas temperature of the fuel burned in the turbomachine and reduce the quantity of air used for cooling a turbine of the turbomachine. However, creep resistance of the materials used for the manufacture of the turbine parts decreases above high temperatures, for example above 900° C.
Materials made of monocrystalline nickel-based superalloy have mechanical properties allowing them to resist creep at high temperature, for example above 900° C., and a particularly high resistance to oxidation relative to other metal alloys. Thus, monocrystalline superalloy is used for the manufacture of many turbomachine parts, such as turbine blades.
The manufacture of monocrystalline superalloy parts comprises, in a known manner, a step of casting the part, during which the superalloy in liquid form is poured into a ceramic mould, formed beforehand by molten wax.
The microstructure of the as-cast alloy has numerous chemical heterogeneities. Indeed, the alloy solidifies not by flat growth but by dendritic growth. Thus the core, the various layers of dendrites and the interdendritic areas do not have the same chemical composition, because their solidification occurs successively. Moreover, when the alloy solidifies, the γ′ forming elements (for example, Al, Ta and Ti) segregate in the liquid metal differently from W or Mo, which have a substantial concentration in the core of the dendrites. These inhomogeneities reduce the creep resistance of the superalloy.
In this regard, it is known to heat treat the part so as to allow diffusion of the elements of the superalloy and thus homogenize their concentration in the part. This treatment is commonly called solution heat treatment. The solution heat treatment can be either partial, i.e., subsolvus, for example by treating the part at a temperature 50° C. below the solvus temperature of the superalloy. The solution heat treatment may also be complete, supersolvus, for example by treating the part at a temperature close to the solvus of the γ′, for example 50° C. greater than the solvus temperature of the γ′.
In reference to
In this regard, it is known to thermally treat the part following the solution heat treatment S1. The heat treatment(s) are commonly called aging or tempering heat treatments. In the case of superalloy AM1, the part is treated after solution heat treatment by a first tempering R1 at 1100° C. for five hours. This treatment makes it possible to optimize the size, morphology and distribution of γ′ precipitates. The part is treated after first tempering R1 by a second tempering R2, at 870°, for 16 hours. The second tempering R2 makes it possible to increase the volume fraction of the γ′ phase of the superalloy.
After the solution heat treatment S1, the first tempering R1 and the second tempering R2, superalloy AM1 comprises cubic γ′ precipitates distributed homogeneously and aligned.
In reference to
The plastic deformation D1 applied to the part causes a defect in the microstructure of the part. If the part is placed in a high temperature atmosphere after the plastic deformation D1, for example greater than 900° C., the defect can cause a change of the crystalline structure of the part. This recrystallization can cause a reduction in the service life of the part under working conditions.
One goal of the invention is to propose a solution to prevent recrystallization of a nickel-based superalloy part following a plastic deformation undergone by the part.
This goal is attained in the context of the present invention by means of a manufacturing method for an aircraft part, the part comprising a monocrystalline nickel-based superalloy substrate, the method successively implementing the following steps:
Since the homogenization treatment of the crystalline structure is implemented between the moment at which a plastic deformation can be applied to the part and between the first tempering, the deformation can be distributed homogeneously throughout the part before the first tempering. Thus, recrystallization can be avoided during the tempering treatments.
The invention is advantageously supplemented by the following characteristics, taken individually or in any one of the technically-possible combinations thereof:
Other characteristics, objectives and advantages of the invention will appear from the following description, which is purely illustrative and non-limiting and should be read with regard to the attached drawings, in which:
Throughout the figures, similar elements bear identical references.
“Superalloy” means an alloy exhibiting very good resistance to oxidation, corrosion, creep and cyclic stresses (especially mechanical or thermal stresses) at high temperature and high pressure.
A superalloy can have a biphasic microstructure comprising a first phase (called “γ phase”) forming a matrix and a second phase (called “γ′ phase”) forming precipitates hardening in the matrix. The coexistence of these two phases is designated by γ-γ′ phase.
The “base” of the superalloy designates the main metal component of the matrix. In most cases, superalloys comprise a cobalt or nickel base. The superalloy base is preferentially a nickel base.
“Nickel-based superalloys” have the advantage of offering a good compromise between resistance to oxidation and resistance to breakage at high temperature and weight, which justifies their use in the hottest parts of turbojets.
Nickel-based superalloys are made up of a γ phase (or matrix) of the face-centered γ-Ni cubic austenitic type, optionally containing α-substitution additives in solid solution (Co, Cr, W, Mo, Re), and a γ′ phase (or precipitates) of the γ′-Ni3X type, with X=Al, Ti or Ta. The γ′ phase has an L12 ordered structure, derived from the face-centered cubic structure, consistent with the matrix, i.e., having an atomic lattice very close to the latter.
By its ordered nature, the γ′ phase has the remarkable property of having mechanical resistance that increases with temperature up to approximately 800° C. The very strong consistency between the γ and γ′ phases gives a very high hot mechanical strength for nickel-based superalloys, which itself depends on the γ/γ′ ratio and on the size of the hardening precipitates.
The term “mass fraction” designates the ratio of the mass of an element or a group of elements to the total mass.
The aircraft part comprises a monocrystalline nickel-based superalloy substrate. The superalloy chosen can be predominantly composed of nickel and preferentially have a mass fraction of chromium comprised between 7% and 9%, of cobalt comprised between 5.5% and 7.5%, of aluminium comprised between 4% and 6%, of titanium comprised between 1% and 2%, of tantalum comprised between 7% and 9%, of molybdenum comprised between 1% and 3% and of tungsten comprised between 4.5% and 6.5%, the superalloy also comprising carbon and zirconium, Especially, the superalloy called “AM1” (registered trademark) can be chosen.
Other nickel-based superalloys can also be used for the manufacture of the substrate, especially the superalloy called “CMSX-4Plus” (registered trademark). The superalloy can be predominantly composed of nickel and preferentially has a mass fraction of chromium comprised between 2.5% and 4.5%, of cobalt comprised between 9% and 11%, of aluminium comprised between 4.5% and 6.5%, of titanium comprised between 0.5% and 1%, of tantalum comprised between 7% and 9%, of molybdenum comprised between 0.3% and 1%, of tungsten comprised between 5% and 7%, and of rhenium comprised between 4% and 5.5%.
In reference to
The method comprises, after the moulding step, a solution heat treatment S1 of the part. The part is put into solution at a first temperature T1. Temperature T1 is comprised between the solvus temperature of the γ′ phase and the melting temperature of the superalloy. Solution heat treatment makes it possible to diffuse the elements of the superalloy in the substrate of the part. The concentration of the different elements in the substrate is therefore homogenized.
The part is then cooled to room temperature at a controlled speed.
The part can then be demoulded. For example, it is possible to break the mould using vibration. Demoulding can lead to a high local concentration of stresses on the part, these stresses leading to a plastic deformation D1.
The part can undergo plastic deformation D1 by other means, such as assembling the part to another part or handling or moving the part. In particular, the plastic deformation D1 can be unintentional.
A step of homogenization S2 of the crystalline structure of the part is implemented following the plastic deformation(s) undergone by the part. In reference to
Indeed, the temperature corresponding to the solvus of the superalloy decreases after the solution heat treatment S1. Thus, the upper bound of the second temperature T2 allows preventing recrystallization of the substrate during the homogenization S2. Moreover, the temperature is sufficiently high to decrease the internal stresses caused by plastic deformation effectively. Thus, the lower bound of the temperature T2 allows preventing recrystallization of the substrate during one or more later tempering treatments and during the homogenization S2.
The second temperature T2 is preferentially strictly comprised between 1280° C. and 1350° C., especially between 1280° C. and 1300° C., and preferentially between 1285° C. and 1295° C. Especially, when the nickel-based superalloy used for the manufacture of substrate is “CMSX-4Plus”, the second temperature T2 can be comprised between 1330° C. and 1335° C.
The homogenization S2 is implemented by the heat treatment of the part at a second temperature T2 for at least 10 minutes, especially for 20 minutes, and preferentially for one hour.
Thus, the treatment time for the homogenization S2 is adapted to the reaction kinetics of the homogenization S2 in the substrate of the part.
In reference to
In reference to
After the homogenization S2, the part is cooled to room temperature.
A first tempering R1 at a fourth temperature T4 comprised between 1000° C. and 1200° C. for at least 3 hours, and a second tempering R2 at a fifth temperature T5 comprised between 800° C. and 900° C. for at least 10 hours are then implemented. These treatments make it possible to optimize the size, morphology and distribution of γ′ precipitates, as well as the volume fraction thereof.
The tensile stress is preferentially applied to the part so that the deformation rate is less than 10−3 s−1 at any point of the part.
Thus, it is possible to prevent the appearance of slip bands in the microstructure of the substrate.
In reference to
Number | Date | Country | Kind |
---|---|---|---|
1907174 | Jun 2019 | FR | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/EP2020/068115 | 6/26/2020 | WO |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2020/260645 | 12/30/2020 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
20030047252 | Caron et al. | Mar 2003 | A1 |
20080240926 | Kobayashi et al. | Oct 2008 | A1 |
20130142637 | Harris | Jun 2013 | A1 |
20210246533 | Rame et al. | Aug 2021 | A1 |
Number | Date | Country |
---|---|---|
0 063 511 | Oct 1982 | EP |
1 211 336 | Jun 2002 | EP |
1 398 393 | Mar 2004 | EP |
6-293945 | Oct 1994 | JP |
WO 2019097162 | May 2019 | WO |
Entry |
---|
US 4,923,525 A, 05/1990, Khan et al. (withdrawn) |
International Search Report, issued in PCT/EP2020/068115, dated Oct. 8, 2020. |
Written Opinion of the International Searching Authority, issued in PCT/EP2020/068115, dated Oct. 8, 2020. |
Number | Date | Country | |
---|---|---|---|
20220243312 A1 | Aug 2022 | US |