The present disclosure relates to a method for manufacturing a battery module, and more particularly, to a method for manufacturing a battery module which may minimize an error caused by an operator during a process of manufacturing the battery module.
There has been increasing technology development and demand for a mobile device, and demand for a secondary battery as an energy source is thus rapidly increasing. Accordingly, many studies have been conducted on the secondary battery which may meet various needs.
The secondary battery is spotlighted as the energy source for a power device such as an electric bicycle, an electric vehicle or a hybrid electric vehicle, as well as a mobile device such as a mobile phone, a digital camera or a laptop computer.
A small battery pack in which one battery cell is packed may be used for a small device such as the mobile phone or the camera. However, a medium-sized or large-sized battery pack, which is a battery pack having two or more battery cells connected in parallel and/or in series with each other, may be used for a mid- to large-sized device such as the laptop computer or the electric vehicle. Accordingly, the number of battery cells included in the battery pack may be variously set based on required output voltage or charge/discharge capacity.
Meanwhile, the battery pack may be formed by connecting the plurality of battery cells in series/parallel with each other. In this case, the battery pack may be generally formed by first forming at least one battery module including the battery cells, and then adding other components thereto by using the at least one battery module.
In the case of such a battery module, there is a gradually emerging importance of technology which may efficiently cool heat occurring in the battery cell as the required battery capacity is increased. To this end, introduced is a structure which may improve thermal conductivity of the battery module by applying a resin for heat dissipation to the inside of a case of the battery module.
However, when the resin is injected into the case of such a battery module through an injection hole, a manufacturing process may be carried out in a state in which a lower surface of the battery module is turned upside down, thus making it difficult to check a condition of the battery module, included in its upper surface, etc. For this reason, defects may often occur by finishing the process in a state where the resin is not sufficiently cured.
An exemplary embodiment of the present disclosure provides a method for manufacturing a battery module, which may minimize a process error caused by an operator by making it easy to check a process condition of an injected resin or the like even during processes of injecting the resin into the battery module and curing the same.
However, technical problems to be solved by an exemplary embodiment of the present disclosure are not limited to the aforementioned problems, and may be variously expanded in the scope of a technical idea included in the present disclosure.
According to an exemplary embodiment of the present disclosure, a method for manufacturing a battery module includes: forming a battery cell stack by stacking a plurality of plate-shaped battery cells parallel and adjacent to each other; accommodating the battery cell stack in a module frame including four plates surrounding at least four surfaces of the battery cell stack; attaching adhesive tapes to perimeters of an injection hole and of an observation hole formed in a lower plate among the four plates; injecting a thermal conductive resin solution through the injection hole; and writing injection information of the injecting a thermal conductive resin solution on at least a portion of the adhesive tapes.
The method may further include curing the thermal conductive resin solution based on the injection information after injecting the thermal conductive resin solution, and then removing the adhesive tapes.
Curing time of the thermal conductive resin solution may be one hour to two hours.
The injection hole may include at least two holes formed in a central portion of the lower plate in a length direction.
The observation hole may be spaced apart from the injection hole in a length direction of the lower plate and positioned at each of two ends of the lower plate in the length direction.
The thermal conductive resin solution may be a thermal resin.
The thermal conductive resin solution may be cured to form a thermal conductive resin layer between the battery cell stack and the lower plate.
The injection of the thermal conductive resin solution may be performed until the thermal conductive resin solution is observed through the observation hole.
The adhesive tapes may have holes respectively corresponding to the observation hole and the injection hole, and the excess thermal conductive resin solution overflown out of the injection hole or the observation hole may also be removed by removing the adhesive tapes.
The injection information of the injecting a thermal conductive resin solution may include injection time of the injecting a thermal conductive resin solution.
The adhesive tapes may be transparent, and attached so as to block the observation hole.
The adhesive tapes may have a characteristic changed by temperature change or time elapse.
The characteristic may be at least one of color or transparency of the adhesive tapes.
The writing injection information may be performed with an ink, and the ink may have a characteristic changed by temperature change or time elapse.
The characteristic may be at least one of color or transparency of the ink.
As set forth above, an exemplary embodiment of the present disclosure may provide the method for manufacturing a battery module, which may minimize the process error caused by the operator by making it easy to check the process condition of the injected resin or the like even during the processes of injecting the resin into the battery module and curing the same.
Hereinafter, exemplary embodiments of the present disclosure are described in detail with reference to the accompanying drawings so that those skilled in the art to which the present disclosure pertains may easily practice the present disclosure. The present disclosure may be implemented in various different forms and is not limited to exemplary embodiments provided herein.
A portion unrelated to the description is omitted in order to obviously describe the present disclosure, and the same or similar components are denoted by the same reference numeral throughout the present specification.
In addition, the size and thickness of each component shown in the accompanying drawings are arbitrarily shown for convenience of explanation, and therefore, the present disclosure is not necessarily limited to contents shown in the accompanying drawings. The thicknesses are exaggerated in the drawings in order to clearly represent several layers and regions. In addition, in the drawings, the thicknesses of some layers and regions are exaggerated for convenience of explanation.
In addition, when an element such as a layer, a film, a region, or a substrate is referred to as being “on” or “above” another element, it may be “directly on” another element or may have a third element interposed therebetween. On the contrary, when an element is referred to as being “directly on” another element, there is no third element interposed therebetween. In addition, when an element is referred to as being “on” or “above” a reference element, it may be positioned on or below the reference element, and it may not necessarily be “on” or “above” the reference element toward an opposite direction of gravity.
In addition, throughout the present specification, unless explicitly described to the contrary, “including” any components may be understood to imply the inclusion of other elements rather than the exclusion of any other elements.
Further, throughout the specification, the word “on the plane” may indicate a case where a target is viewed from the top, and the word “on the cross section” may indicate a case where a cross section of a target taken along a vertical direction is viewed from the side.
Referring to
The battery cell stack 110 may be a secondary battery assembly including the plurality of battery cells 112. The battery cell stack 110 may include the plurality of battery cells 112, and each battery cell may include an electrode lead 114. The battery cell stack 110 may be formed by stacking the plurality of battery cells 112 on each other and connecting the battery cells with each other by using the electrode lead 114. The battery cell 112 may be a pouch-type battery cell having a plate shape, and is not limited thereto. The electrode lead 114 may be a positive electrode lead or a negative electrode lead. Here, an end of the electrode lead 114 of each battery cell 112 may be bent in one direction, and may thus come into contact with the end of the electrode lead of another battery cell 112 adjacent thereto. The two electrode leads 114 in contact with each other may be fixed to each other through welding or the like, thereby making the battery cells 112 in the battery cell stack 110 be electrically connected to each other.
The plurality of battery cells 112 may be vertically stacked on each other so that the electrode leads 114 are aligned in one direction to form the battery cell stack 110. The battery cell stack 110 may have at least one opening 128 open in a length direction of the battery cell stack 110, and may be accommodated in the module frame 120 including the four plates surrounding at least four surfaces of the battery cell stack 110. For example, the module frame 120 may have an upper plate 121 and a lower plate 126, which are perpendicular to a surface on which the battery cell stack 110 is mounted, and a pair of side plates 124 which are parallel to the surface on which the battery cell stack 110 is mounted. In addition, this exemplary embodiment describes an example of the module frame 120 having a square tube in which the upper plate 121, the lower plate 126 and the pair of side plates 124 are integrally formed with each other, and the present disclosure is not limited thereto. The present disclosure may also use the module frame 120 formed so that three surfaces thereof form a U-shaped frame and a plate forming the other surface covers an open surface of the U-shaped frame.
The lower plate 126 of the module frame 120 may include a plurality of injection holes 125 (shown in
Next, referring to
Next, referring to
At least one injection hole 125 and at least one observation hole 123 may be formed in the lower plate 126. At least one injection hole 125 may be formed in a central portion of the lower plate 126, and the thermal conductive resin solution 122 may be injected through the injection hole 125 formed in the central portion, flow to both side portions of the lower plate, and thus be entirely spread over and applied to a space between the lower plate 126 and the battery cell stack 110. Here, the observation hole 123 may be formed at each of two ends of the lower plate 126 in the length direction to check whether the thermal conductive resin solution 122 is sufficiently injected.
Next, referring to
The adhesive tapes 210 and 220 attached to the perimeters of the injection hole 125 and observation hole 123 may include holes respectively corresponding to the injection hole 125 and the observation hole 123. These adhesive tapes 210 and 220 may be removed after an injection process and a curing process are finished, and here, the excess thermoplastic resin solution 122 overflown out of the hole may also be removed. That is, the adhesive tapes 210 and 220 may serve as a kind of masking tapes.
Next, referring to
The thermal conductive resin solution 122 may form the thermal conductive resin layer 122′ made of a thermal conductive material to dissipate heat occurring in the battery cell stack 110 to the outside, and may be made of thermal resin for example. An example of the thermal resin may be silicone, urethane, epoxy or the like.
The thermal conductive resin solution 122 may be injected through the injection hole 125, and whether an injection amount is sufficient may be determined by observing, through the observation hole 123, whether the thermal conductive resin solution 122 arrives at either end of the lower plate 126 in the length direction.
The thermal conductive resin solution 122 injected in a liquid state may be naturally cured after the injection is completed to form the thermal conductive resin layer 122′. Here, when the adhesive tapes 210 and 220 are removed while curing time is not sufficiently elapsed, an incomplete filling phenomenon may occur in which the thermal conductive resin solution 122 fails to sufficiently fill the space between the lower plate 126 and the battery cell stack 110. That is, as shown in
Therefore, in order to prevent an error in removing the adhesive tapes 210 and 220 before the sufficient curing time is elapsed, the injection information of the injected thermal conductive resin solution 122 may be written on at least a portion of the adhesive tapes 210 and 220, for example, the adhesive tape 210 attached to the perimeter of any one observation hole 123, as shown in
In particular, as shown in
The curing time may be taken one hour to two hours so that the thermal conductive resin solution 122 may be completely cured by the natural curing, is not limited thereto, and may be appropriately adjusted based on the type and amount of the injected thermal conductive resin. Accordingly, not only the injection time but also the type and amount of the injected resin may be written on the adhesive tape 210, and the present disclosure is not particularly limited thereto.
In addition, the adhesive tapes 210 and 220 may each be a tape having its own characteristic in which its color or transparency is changed by time elapse, or a tape having a characteristic in which its color or transparency is changed by temperature change. Accordingly, even if the operator does not write the injection information by mistake, it may be inferred how much time is elapsed or how much the curing of the inner thermal conductive resin solution 122 is progressed based on the change in the color or transparency of the adhesive tape 210 or 220, thereby doubly preventing the process error. Here, in order to more accurately check the change in color of the adhesive tape 210 or 220 over time, the operator may check a color change table over time or the like after the attachment of the adhesive tape 210 or 220. In addition, the thermal conductive resin solution 122 may be mixed while being injected into the module through a nozzle, have a slight temperature rise as a reaction occurs during its mixing, and then return to its original temperature when the curing is completed. Accordingly, the curing time may be inferred by using the adhesive tapes 210 and 220 which are sensitive to this temperature difference.
In addition to the adhesive tapes 210 and 220, an ink for marking on the adhesive tapes 210 and 220 may have a characteristic in which its color is changed by time elapse or temperature change. It is thus possible to doubly check process information by using such an ink.
Next, referring to
Here, some of the resin solution flowing out through the observation hole 123 and the injection hole 125 and then cured may also be removed together with the adhesive tapes 210 and 220, and it is thus possible to complete the battery module 100 having a neat appearance. In particular, in an exemplary embodiment of the present disclosure in which the adhesive tapes 210 and 220 are removed after the sufficient curing time is elapsed by utilizing the injection information written on the adhesive tape 210, the thermal conductive resin layer 122′ is formed to sufficiently fill the space between the lower plate 126 and the battery cell stack 110 as shown in
Hereinafter, the description describes a method for manufacturing a battery module according to another exemplary embodiment of the present disclosure with reference to
Another exemplary embodiment of the present disclosure omits the description of the same part as that of the method for manufacturing a battery module according to an exemplary embodiment described above, and only describes a different part.
Referring to
In addition, the information on the thermoplastic resin solution 122 injected into the transparent adhesive tape 210′ may be written and the curing time may be controlled by checking the information, thereby making it possible to remove the adhesive tape 210′ after the sufficient curing is achieved. Even in this exemplary embodiment, when the adhesive tape 210′ is removed before the sufficient curing time is elapsed, an uncured portion may be attached to and removed from the adhesive tape 210′ through the hole, resulting in the incomplete filling problem. However, it is possible to prevent the occurrence of the defect due to the incomplete filling by writing the information on the injected thermoplastic resin solution 122 on the transparent adhesive tape 210′ and checking the information to secure the sufficient curing time.
Although the exemplary embodiments of the present disclosure have been described in detail hereinabove, the scope of the present disclosure is not limited thereto. That is, various modifications and alterations made by a person of ordinary skill in the art by using a basic concept of the present disclosure as defined in the following claims fall within the scope of the present disclosure.
Number | Date | Country | Kind |
---|---|---|---|
10-2020-0094336 | Jul 2020 | KR | national |
10-2021-0095773 | Jul 2021 | KR | national |
This application is a National Stage Application of International Application No. PCT/KR2021/009872, filed on Jul. 29, 2021, which claims priority to and the benefit of Korean Patent Application No. 10-2020-0094336 filed on Jul. 29, 2020, and Korean Patent Application No. 10-2021-0095773 filed on Jul. 21, 2021, the disclosures of which are incorporated herein by reference in their entireties.
Filing Document | Filing Date | Country | Kind |
---|---|---|---|